Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Alicyclic ring monomers in polyamide backbone
What ifWhat if the polyamide monomer units are derived predominantly from alicyclic ring compounds with no linear or branched hydrocarbon majority?
Claim language“a linear or branched hydrocarbon compound”
The polyamide is synthesized by polycondensation of 1,4-cyclohexanedicarboxylic acid and 1,4-cyclohexanediamine to place saturated six-membered rings along more than 60 mol % of the polymer backbone. The rigid alicyclic rings restrict segmental chain rotation, raising the glass transition temperature above 140 degrees Celsius and lowering equilibrium moisture uptake compared to acyclic chains. Lower water absorption slows amide bond cleavage in hot aqueous environments while preserving melt processability.
1.1Semi-aromatic polyamide with lower aliphatic content
What ifWhat if the polyamide contains 50 mol % linear hydrocarbon moieties with the remaining 50 mol % derived from aromatic dicarboxylic acids?
Claim language“80 mol % or more”
Equimolar amounts of hexamethylenediamine and a mixture of terephthalic acid and isophthalic acid undergo polycondensation to form a semi-aromatic polyamide with 50 mol % aliphatic diamine units and 50 mol % aromatic diacid units. The phenylene rings lower the density of hydrophilic amide groups per unit volume and stiffen the polymer backbone, reducing equilibrium water absorption below 2.5 mass %. Compounding this resin with a functionalized polyolefin yields a blend with dimensional stability and resistance to aqueous glycol hydrolysis.
1.2Polyolefin-continuous phase at higher mass ratio
What ifWhat if the polyolefin mass ratio is between 0.55 and 0.75 so that the polyolefin forms the continuous phase?
Claim language“is 0.15 to 0.40”
Compounding the functionalized polyolefin at a mass ratio of 0.55 to 0.75 relative to the combined polymer mass inverts the blend morphology during twin-screw extrusion. The hydrophobic polyolefin forms a continuous matrix that encapsulates discrete polyamide domains ranging from 0.5 to 3 micrometers in diameter. Because the nonpolar matrix acts as a moisture barrier around the amide phase, water diffusion to the polyamide is reduced while melt flow remains uniform in blow molding and extrusion.
1.3Post-molding cross-linked polyamide network
What ifWhat if the polyamide resin forms an insoluble cross-linked network after molding?
Claim language“a molecular weight distribution curve”
A low-viscosity linear polyamide is compounded with 1 to 3 mass % of a polyfunctional unsaturated coagent such as triallyl isocyanurate and shaped by injection molding or extrusion. The molded article is exposed to electron-beam irradiation at a dose of 50 to 150 kilograys to generate free radicals that link adjacent polymer chains into a three-dimensional covalent network. The resulting insoluble gel fraction resists hydrolytic chain scission and creep at elevated temperatures without requiring high-molecular-weight fractions during melt processing.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Subsea flexible pipe inner barrier liner
A twin-screw extruder compounds the aliphatic polyamide resin and the reactive polyolefin at a mass ratio of 0.25 into pellets and feeds them to a single-screw crosshead extrusion line. The crosshead die extrudes the molten composition directly over an interlocked metallic carcass to form a continuous tubular barrier layer with a wall thickness between 5 mm and 12 mm. A helical tape-wrapping head applies steel tensile armor wires and an outer protective sheath around the extruded barrier layer. During subsea hydrocarbon transport, the grafted polyamide-polyolefin matrix resists hydrolytic chain scission from warm acidic water while maintaining ductility under cyclic bending loads.
Selective laser sintering powder for fluid manifolds
Cryogenic grinding or precipitation from a heated solvent converts the compounded aliphatic polyamide and reactive polyolefin resin into free-flowing powder particles with a median diameter between 40 μm and 70 μm. A dry-blending tumbler mixes the polymer powder with 0.2 mass percent fumed silica flow aid before loading the powder bed of a laser sintering machine. A recoater blade deposits 0.1 mm layers onto a build platform preheated to 15 °C below the polyamide melting peak, and a carbon dioxide laser scans cross-sectional toolpaths to fuse the particles into internal-channel fluid manifolds. The reactive polyolefin phase reduces curl distortion during cooling and imparts impact resistance and moisture stability to the sintered manifold walls.
A hydrogenated styrene-ethylene-butylene-styrene triblock copolymer functionalized with pendant cyclic anhydride groups replaces the reactive polyolefin component at a mass fraction of 0.20 to 0.35 relative to the total polymer mass. The aliphatic polyamide resin and the functionalized triblock copolymer pass through a co-rotating twin-screw extruder held between 230 °C and 260 °C to graft the anhydride groups onto terminal amine sites of the polyamide chains. The resulting graft copolymer stabilizes dispersed elastomeric domains with average diameters between 0.2 μm and 0.8 μm inside the continuous aliphatic polyamide phase. The substituted elastomeric phase lowers the flexural modulus and absorbs impact energy at temperatures down to -40 °C while preserving melt stability during blow molding.
Parameter or scale variation
Elevated polyolefin loading for flexible pneumatic tubing
The mass ratio of the reactive polyolefin to the combined mass of the aliphatic polyamide resin and the reactive polyolefin increases to a range of 0.42 to 0.55. Melt blending occurs in a twin-screw extruder operating at a screw speed of 250 rpm to 400 rpm and a specific mechanical energy input of 0.18 kWh/kg to 0.28 kWh/kg to establish a co-continuous phase morphology. The co-continuous extrudate passes through an annular tubing die and a vacuum sizing tank cooled to 20 °C to produce flexible conduits with outer diameters of 4 mm to 16 mm and wall thicknesses of 0.5 mm to 1.5 mm. The elevated polyolefin fraction reduces water absorption below 0.6 mass percent at saturation and increases elongation at break above 250 percent while retaining covalent interfacial bonding between phases.
Combination with existing systems
Multilayer automotive coolant line with barrier core
A three-extruder co-extrusion die combines an inner fluid-contact layer of the aliphatic polyamide and reactive polyolefin composition with a middle gas-barrier layer of ethylene-vinyl alcohol copolymer and an outer abrasion-resistant polyamide jacket. Tie layers of anhydride-modified polyolefin sit between the inner layer, the middle barrier layer, and the outer jacket so that adjacent layers bond chemically during co-extrusion at 245 °C. The composite tube exits the die into a water-bath calibrator and a rotary cutter that trims segments to specified lengths for thermoforming into curved engine-bay routing geometries. The inner layer contacts hot glycol-water coolant at 120 °C without blistering or hydrolytic embrittlement while the middle core limits permeation of vapor and dissolved gases.
Automated or data-driven variant
Inline rheometry and gravimetric feeder control system
A continuous compounding line integrates gravimetric loss-in-weight feeders for the aliphatic polyamide resin and the reactive polyolefin with an inline capillary rheometer and a near-infrared spectrometer mounted on the extruder die adapter. The near-infrared spectrometer samples the molten stream every 2 seconds to quantify residual unreacted functional groups and phase ratio, while the inline rheometer tracks shear viscosity across a shear rate sweep from 10 s^-1 to 1000 s^-1. A multivariable model-predictive controller compares the measured viscosity and grafting conversion against target setpoints derived from molecular weight distribution calibration data. The controller adjusts feeder mass-flow ratios, barrel zone temperatures, and screw rotation speed in real time to maintain target melt elasticity and constant phase dispersion during continuous pelletization.
Specific version of a part
Long-chain polyamide 610 from linear monomers
Polyamide 610 is synthesized by polycondensation of linear hexamethylenediamine and linear sebacic acid, yielding a homopolymer in which 100 mol % of the monomer units derive from linear hydrocarbon compounds. The ten-carbon diacid and six-carbon diamine repeat units produce a methylene-to-amide ratio of 8 to 1, lowering amide group concentration compared to shorter aliphatic polyamides. This chain structure limits water uptake to 1.2 to 1.8 mass % at saturation and slows hydrolytic chain cleavage in hot water.
Balanced 0.25 polyolefin mass ratio formulation
Gravimetric loss-in-weight feeders meter 75 mass % aliphatic polyamide pellets and 25 mass % reactive polyolefin pellets into the main throat of a co-rotating twin-screw extruder, establishing a mass ratio of 0.25. Kneading blocks in the central barrel zones apply controlled shear at 200 to 300 revolutions per minute to disperse the polyolefin phase uniformly throughout the continuous polyamide matrix. At this 0.25 ratio, the blend achieves notched impact resistance at minus 40 degrees Celsius while maintaining melt viscosity suitable for extrusion blow molding.
Bimodal blend of two polyamide grades
A high-viscosity aliphatic polyamide produced by solid-state post-condensation with a weight-average molecular weight above 120,000 grams per mole is melt-blended with a lower-viscosity grade having a weight-average molecular weight of 40,000 to 60,000 grams per mole. Size-exclusion chromatography using hexafluoroisopropanol eluent calibrated against polymethyl methacrylate reference samples verifies the target ratio of high-molecular-weight to low-molecular-weight fractions in the distribution curve. The high-molecular-weight tail supplies melt strength during parison formation while the lower-molecular-weight fraction reduces shear viscosity during mold filling.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1the aliphatic polyamide resin has 80 mol % or more of a moiety derived from a linear or branched hydrocarbon compound based on the total monomer units;
The aliphatic polyamide can be a homo- or copolymer and is derived from one or more diamine monomers containing 4 to 10 carbon atoms and one or more aliphatic dicarboxylic acids with 6 to 12 carbon atoms. As the polyamide is aliphatic, both the diamine and the diacid are aliphatic in nature.
A · US 2014/0187709 A1 · ¶ 25
Put another way, both the diamine and diacid forming, through polycondensation, recurring RPA are free of any aromatic groups. In some embodiments, the aliphatic polyamide polymer has at least 60 mol %, at least 70 mol %, at least 80 mol %, at least 90 mol %, at least 95 mol %, at least 95 mol %, at least 99 mol %, or at least 99.9 mol % of recurring unit RPA.
B · US 2022/0220293 A1 · ¶ 25
1.2a mass ratio of a content of the polyolefin (B) to a total mass of a content of the aliphatic polyamide resin (A) and the content of the polyolefin (B), [(B)/{(A)+(B)}], is 0.15 to 0.40; and
Described herein are polymer compositions including an a functionalized polyolefin, an aliphatic polyamide, and a glass fiber, where the weight ratio of the functionalized polyolefin to the total weight of the aliphatic polyamide and the functionalized polyolefin in the polymer composition (“polyolefin weight ratio”) is from 55% to 95%.
B · US 2022/0220293 A1 · abstract
1.3the aliphatic polyamide resin has the following characteristic in a molecular weight distribution curve in terms of polymethyl methacrylate:
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document B has a passage for 1.2. Both have a passage for 1.1. Both are classified in CPC C08L, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The invention relates to polymer compositions including a functionalized polyolefin, an aliphatic polyamide, and a glass fiber, the polymer composition having excellent dielectric performance and mechanical performance.
B · US 2022/0220293 A1 · ¶ 2
Related claim parts: 1.1
Therefore the composition should have a low level of water absorption.
A · US 2014/0187709 A1 · ¶ 15
Related claim parts: 1.2
Therefore there is a need for an improved composition that can be used in the production of components for light-emitting diodes, that is cost effective and that displays improved results for certain ageing behavior, especially an improved resistance against yellowing.
A · US 2014/0187709 A1 · ¶ 6
The composition according to the invention can be used in the production of components for light-emitting diodes, is cost efficient and has a better behavior towards ageing.
A · US 2014/0187709 A1 · ¶ 15
It was surprisingly discovered that the polymer compositions had excellent dielectric performance and improved mechanical performance, relative to corresponding polymer compositions.
B · US 2022/0220293 A1 · ¶ 7
Due to the excellent dielectric performance and increased mechanical performance, the polymer composition can be desirably incorporated into mobile electronic device applications.
B · US 2022/0220293 A1 · ¶ 7
Cite aspatent.fyi, US 2026/0365852 A1, claim 1, first published 2026-11-23T17:22:55-05:00, https://patent.fyi/US20260365852/, SHA-256 80f5a265dd2b3b6e70581819f275fd08d956c1d5770944c643946bf666680ed0