patent.fyi
Applications  /  US 2026/0365863
United States Patent Application Publication

US 2026/0365863 A1

Published
Nov 19, 2026
Filed
May 18, 2026
Earliest date on the face
May 19, 2025
Classification
C09D 7/62
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Crosslinking with a polythiol curing agent

What ifWhat if the resin system uses a polythiol crosslinker rather than an amine curing agent?
Claim language“an amine curing agent”

A multi-functional mercaptan compound containing three or four terminal thiol groups mixes with the epoxy binder at 4 to 6 parts by weight alongside 0.2 parts of a quaternary phosphonium salt accelerator. Thiolate anions attack the epoxide rings directly at ambient temperature to form thioether linkages without releasing volatile byproducts. The resulting crosslinked network reaches handling strength within 45 minutes and exhibits low moisture uptake on steel surfaces.

1.2Using a vinyl ester matrix binder

What ifWhat if the coating binder is a bisphenol-A vinyl ester resin instead of the epoxy resin?
Claim language“the epoxy resin”

A methacrylated bisphenol-A vinyl ester prepolymer dissolved in styrene monomer replaces the epoxide binder at 8 to 12 parts by weight. Addition of 0.15 parts of a cobalt naphthenate promoter and 0.2 parts of methyl ethyl ketone peroxide initiates free-radical chain polymerization across the terminal vinyl groups at ambient temperature. The polymerized ester network bonds to reinforcement fibers and resists acidic fluids along pipeline walls.

1.3Reducing viscosity with propylene carbonate

What ifWhat if the reactive diluent is propylene carbonate rather than glycerol triglycidyl ether?
Claim language“glycerol triglycidyl ether”

Propylene carbonate is added at 1 to 2 parts by weight to lower the dynamic viscosity of the resin-bitumen blend below 1500 millipascal-seconds at 25 degrees Celsius. During curing, primary amine groups open the five-membered cyclic carbonate ring to form urethane linkages integrated into the polymer backbone. This ring-opening reaction reduces solvent emission while maintaining coating flexibility.

1.5Co-spraying dry fibers with liquid resin

What ifWhat if dry chopped carbon fibers are sprayed directly into the liquid resin stream instead of immersing the carbon fiber?
Claim language“immersing the carbon fiber”

A dual-nozzle spray head atomizes the mixed resin-curing-agent liquid at 0.4 megapascals while a rotary cutter chops continuous carbon roving into 6-millimeter lengths and projects the dry strands into the fan pattern. The fibers contact the resin droplets in flight and embed uniformly as the film builds on the substrate. A ribbed metal consolidation roller passes over the wet layer to expel entrapped air and complete fiber wet-out.

1.7Curing with substrate induction heating

What ifWhat if the applied coating cures through electromagnetic induction heating of the metal substrate rather than curing at room temperature?
Claim language“curing at room temperature”

A portable alternating-current induction coil passes along the coated steel pipe to generate eddy currents that raise the substrate surface temperature to 85 to 100 degrees Celsius. Heat conducts outward from the metal interface into the resin layer, driving crosslinking from the base upward and allowing trapped gas bubbles to escape before the outer skin gels. The coating reaches full crosslink density within 15 to 25 minutes.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Protective composite coating for marine concrete pilings

A carbon fiber-reinforced epoxy-bitumen composite coating covers submerged and splash-zone surfaces of reinforced concrete bridge pilings and pier columns. Technicians clean the concrete surface by high-pressure water jetting, immerse chopped or woven carbon fiber in a polyetheramine curing agent, and blend the wetted reinforcement with bisphenol-A epoxy resin, bitumen, diaminodiphenylmethane, and glycerol triglycidyl ether. Application occurs by trowel or roller onto the damp-primed concrete column in a continuous wrap to form a barrier against chloride ion ingress and tidal abrasion. The coating cures at ambient marine temperatures to bind the concrete surface and limit spalling of internal steel reinforcement.

Chemical barrier lining for industrial secondary containment basins

The carbon fiber-reinforced epoxy-bitumen composite coating lines the interior floors and bund walls of concrete secondary containment basins surrounding acid and solvent storage tanks. After abrasive scarification and moisture testing of the concrete slab, workers saturate carbon fiber mat in an aliphatic amine curing agent and blend it with bisphenol-A epoxy resin, bitumen, diaminodiphenylmethane, and glycerol triglycidyl ether. The mixture is troweled onto the floor and coved wall joints in a monolithic 2 millimeter layer that bridges hairline shrinkage cracks in the concrete. Room-temperature curing yields a low-permeability chemical containment lining that holds spilled liquids until pump-out recovery.

Component substitution

Basalt fiber and phenalkamine curing agent formulation

Continuous or chopped basalt fiber replaces carbon fiber as the reinforcing phase, and a cashew nutshell liquid phenalkamine curing agent replaces the polyetheramine and aliphatic amine curing agents. Pretreated basalt fiber is immersed in the phenalkamine liquid until full wet-out occurs, then combined with a pre-blended mixture of bisphenol-A epoxy resin, bitumen, diaminodiphenylmethane, and trimethylolpropane triglycidyl ether as the reactive diluent. The resulting paste is spread onto an abrasive-blasted steel substrate to form an electrically insulating, moisture-tolerant composite layer. Crosslinking between the phenalkamine amine groups and the epoxy and triglycidyl ether components proceeds at ambient temperature without external heating.

Parameter or scale variation

High fiber loading coating with heated post-curing

The formulation increases the carbon fiber fraction to 4 to 8 parts by weight while adjusting the bisphenol-A epoxy resin to 10 to 14 parts, the polyetheramine curing agent to 4 to 6 parts, bitumen to 1.5 to 2.5 parts, diaminodiphenylmethane to 1.5 to 2.5 parts, and glycerol triglycidyl ether to 2 to 3 parts to keep viscosity workable. Pretreated carbon fiber is immersed in the curing agent for 20 to 30 minutes at 35 degrees Celsius before mechanical stirring into the resin-bitumen blend for 10 minutes at 300 revolutions per minute. Operators apply the mixture in two successive coats of 1.2 millimeters each to a total dry film thickness of 2.4 millimeters on a prepared steel surface. After an initial gel period of 4 hours at 25 degrees Celsius, inductive heating blankets hold the coated section at 65 degrees Celsius for 3 hours to drive crosslinking to completion.

Combination with existing systems

Composite coating integrated with cathodic protection monitoring

The carbon fiber-reinforced epoxy-bitumen composite coating operates alongside an impressed-current cathodic protection system on buried metallic storage vessels or conduits. Before applying the resin-fiber mixture, technicians install an electrically insulating fiberglass veil primer layer on the grit-blasted steel substrate to prevent direct electrical contact between the conductive carbon fibers and the metal wall. Embedded reference electrodes and coupon test leads pass through sealed ports in the composite layer and connect to an external rectifier and potential logger. During service, the cured composite acts as the primary physical barrier against soil moisture while the cathodic protection circuit polarizes localized coating holidays.

Automated or data-driven variant

Sensor-guided robotic mixing and helical spray application

A dual-stream metering unit feeds the curing-agent suspension containing wetted short-cut carbon fiber and the pre-blended epoxy, bitumen, diaminodiphenylmethane, and glycerol triglycidyl ether stream through positive-displacement pumps into a static mixer. Inline mass-flow meters and an ultrasonic viscometer transmit real-time ratio and viscosity readings to a programmable logic controller that adjusts pump speeds and inline heater power to hold the mix ratio and viscosity within target bounds. A rail-mounted robotic applicator traverses the pretreated substrate while an optical laser profilometer measures wet film thickness immediately downstream of the nozzle. Closed-loop control software modulates carriage traverse speed and pump output from the profilometer feedback to deposit a uniform layer thickness across the coated area.

Specific version of a part

Dual-stage planetary vacuum mixing sequence

A jacketed planetary mixer blends the epoxy resin, molten bitumen, diaminodiphenylmethane, and glycidyl ether at 50 degrees Celsius and 60 revolutions per minute for 15 minutes until uniform. After cooling the base blend to 25 degrees Celsius, the wetted carbon fiber curing-agent mixture is added under a vacuum of 10 kilopascals at 30 revolutions per minute for 8 minutes. Vacuum agitation prevents fiber breakage and removes entrained air before application.

Ultrasonic bath wetting of oxidized fibers

Short carbon fibers previously oxidized in 30 percent nitric acid at 60 degrees Celsius for 2 hours and dried at 105 degrees Celsius are submerged in the liquid amine curing agent inside a stainless steel tank. An ultrasonic transducer operating at 40 kilohertz agitates the bath for 20 minutes while keeping the liquid below 35 degrees Celsius. Acoustic cavitation separates fiber bundles and drives the low-viscosity curing agent into surface micro-grooves.

Abrasive blast preparation and airless spraying

The steel pipeline exterior is abrasive-blasted with angular aluminum oxide grit to remove mill scale and create a surface roughness profile of 50 to 75 micrometers, followed by solvent wiping to clear residual dust. A plural-component airless spray pump applies the resin mixture at a fluid pressure of 18 megapascals to build a wet film thickness of 400 to 600 micrometers in two cross-hatched passes. The coated pipe cures in ambient air at 20 to 25 degrees Celsius and relative humidity below 70 percent for 24 hours.

Blended diamine and triamine polyetheramine system

The amine curing component combines a low-molecular-weight polyoxypropylene diamine with an average molar mass of 230 grams per mole and a polyoxypropylene triamine with an average molar mass of 440 grams per mole in a 2:1 weight ratio. The diamine provides rapid initial viscosity build and tight crosslink spacing, while the branched triamine adds toughness and impact resistance to the cured film. Total amine hydrogen weight is balanced to a 1:1 stoichiometric ratio with the epoxide groups in the resin blend.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2013/0012669 A1
Published
Jan 10, 2013
Filed
Jun 21, 2012
Class
C09J 163/02
Document BUS 2021/0371717 A1
Published
Dec 2, 2021
Filed
Aug 6, 2021
Class
C09J 175/08
Claim 1
Document A
Document B
1.1wherein the curing agent is an amine curing agent, the amine curing agent is one or more selected from the group consisting of a polyetheramine curing agent and an aliphatic amine curing agent, and the polyetheramine curing agent is one or more selected from the group consisting of D230, D400, T403, D2000, and T5000;
100 parts by weight of Epicoat 828 (an epoxy resin), 5 parts by weight of D-400 (a polyetheramine curing agent), and 20 parts by weight of KBM-303 (an epoxy silane coupling agent) were mixed evenly to obtain a thermosetting resin composition, which was then evaluated according to the following evaluation methods.
A · US 2013/0012669 A1 · ¶ 78
Example 13 Silquest A 187 Momentive Epoxy silane FC 4430 3M Wetting agent CARDURA E10 Momentive Reactive diluent Amicure CG 1200 Airproducts dicyandiamide Curing accelerator U.S.
B · US 2021/0371717 A1 · ¶
1.2wherein the epoxy resin is one or more selected from the group consisting of E51 resin and E44 resin;
Polyepoxides useful herein can be monomeric (e.g., the diglycidyl ether of bisphenol A, diglycidyl ether of bisphenol F, diglycidyl ether of tetrabromobisphenol A, novolac-based epoxy resins, and tris-functional epoxy resins), higher molecular weight resins (e.g., the diglycidyl ether of bisphenol A advanced with bisphenol A) or polymerized unsaturated monoepoxides (e.g., glycidyl acrylates, glycidyl methacrylate, allyl glycidyl ether, etc.) to homopolymers or copolymers.
B · US 2021/0371717 A1 · ¶ 49
1.3wherein the glycidyl ether comprises glycerol triglycidyl ether;
Examples of the glycidyl ether epoxy resin include, but are not limited to, triglycidyloxy methane epoxy resin and tetraglycidyl ether diaminodiphenylmethane epoxy resin.
A · US 2013/0012669 A1 · ¶ 27
1.4wherein a method for preparing the carbon fiber-reinforced resin-based composite coating comprises the following steps:
1.5immersing the carbon fiber that has been pretreated in the curing agent to obtain a curing-agent mixture containing wetted carbon fiber;
1.6mixing the epoxy resin, the bitumen, the diaminodiphenylmethane, and the glycidyl ether, and mixing the resulting mixture with the curing-agent mixture containing wetted carbon fiber to obtain a resin mixture; and
1.7coating the resin mixture onto a pretreated substrate surface, and curing at room temperature to obtain the carbon fiber-reinforced resin-based composite coating.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.3. Only Document B has a passage for 1.2. Both have a passage for 1.1. Both are classified in CPC C09J.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Therefore, in addition to good flexibility and mechanical properties, the thermal-curable resin composition presently used in the art should be improved in viscosity stability and edge coating property.
A · US 2013/0012669 A1 · ¶ 10
This invention relates to a thermosetting resin composition, more particularly to a thermosetting resin composition having good viscosity stability and edge coating property.
A · US 2013/0012669 A1 · ¶ 3
This excess of aromatic hydroxy groups (e.g., bisphenol A), as well as the remaining OH functional group of the toughening polymer, limit the shelf life stability of the final adhesive formulation.
B · US 2021/0371717 A1 · ¶ 3
Such tougheners are useful in epoxy adhesive formulations, such as one-part structural adhesives that can be used in the automotive industry.
B · US 2021/0371717 A1 · ¶ 1
Cite aspatent.fyi, US 2026/0365863 A1, claim 1, first published 2026-11-23T17:42:24-05:00, https://patent.fyi/US20260365863/, SHA-256 f438edf25032bb7049b077a017a3d7794910104af0f51687ae10c866dffc5bb6
First published
Permanent addresshttps://patent.fyi/US20260365863/
Content fingerprint (SHA-256)f438edf25032bb7049b077a017a3d7794910104af0f51687ae10c866dffc5bb6
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi