patent.fyi
Applications  /  US 2026/0365867
United States Patent Application Publication

US 2026/0365867 A1

Published
Nov 19, 2026
Filed
May 7, 2026
Earliest date on the face
May 15, 2025
Classification
C09D 11/322
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Dissolved dye as colorant

What ifWhat if a dissolved dye provides the color?
Claim language“a pigment”

A water-soluble sulfonated azo dye dissolves in the aqueous vehicle. The dye travels with the jetted droplets and deposits on the receiving surface as the water evaporates.

1.2Resin with lower acid value

What ifWhat if the pigment dispersion resin has an acid value of 120 mg KOH/g?
Claim language“an acid value of 200 mg KOH/g or more”

Styrene segments of a styrene-acrylic resin adsorb onto the pigment during bead milling. Potassium hydroxide neutralizes the resin's carboxylic acid groups, and the resulting carboxylates repel neighboring pigment particles.

1.2Pigment with bonded sulfonate groups

What ifWhat if sulfonate groups bonded to the pigment surface stabilize the dispersion?
Claim language“a pigment dispersion resin”

Carbon black carries covalently bonded arylsulfonate groups on its surface. The sulfonate groups ionize in water and provide electrostatic repulsion between particles.

1.3Cationic polymer in receiving layer

What ifWhat if a cationic polymer in the receiving layer fixes the pigment after the droplet lands?
Claim language“a polyethyleneimine”

A porous silica coating carries poly(diallyldimethylammonium chloride) on the receiving sheet. The coating absorbs the aqueous vehicle, and the cationic polymer binds anionic groups on the dispersed pigment near the surface.

1.4Glycerol for nozzle moisture

What ifWhat if glycerol supplies the moisture retention in the ink?
Claim language“3-methyl-1,5-pentanediol or 1,2-pentanediol”

Glycerol lowers the water activity of the ink at the nozzle opening and slows evaporation during idle periods. The glycerol concentration sets the balance between moisture retention and viscosity at the printhead temperature.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Inkjet marking of ceramic tiles

An aqueous ink contains cobalt aluminate pigment, a pigment dispersion resin with an acid value of 250 mg KOH/g, polyethyleneimine with a number-average molecular weight of 1,200, and 1,2-pentanediol. A bead mill disperses the pigment in water with the resin, and a mixing tank receives the dispersion, the diol, and a dilute aqueous solution of polyethyleneimine. A piezoelectric printhead applies the filtered ink to a porous unfired glaze on a ceramic tile. The glaze takes up the liquid vehicle, and kiln firing fixes the pigment in the glaze.

Component substitution

Glycerol as the moisturizing agent

Glycerol replaces the pentanediol moisturizing agent in an aqueous ink containing carbon black, a pigment dispersion resin with an acid value of 250 mg KOH/g, and polyethyleneimine with a number-average molecular weight of 1,200. A bead mill disperses the carbon black with the resin in water before glycerol and diluted polyethyleneimine are blended into the dispersion. Glycerol slows water loss at idle nozzles, and its mass fraction sets the viscosity together with the water content. A viscometer measures the finished ink at the printhead operating temperature, and the glycerol and water proportions are adjusted to meet the head's specified viscosity range.

Parameter or scale variation

Higher molecular weight polyethyleneimine formulation

An aqueous carbon black ink uses a dispersion resin with an acid value of 240 to 260 mg KOH/g, 8 to 12 percent 1,2-pentanediol by mass, and polyethyleneimine with a number-average molecular weight of 2,200 to 2,600. Carbon black is bead-milled in an aqueous solution of the partially neutralized resin before the diol is blended into the dispersion. An aqueous stock containing 1 percent polyethyleneimine by mass is metered into the stirred dispersion to give 0.02 to 0.08 percent polyethyleneimine by mass in the finished ink. Particle size is measured after each addition, and the selected dosage keeps the measured 90th-percentile particle diameter below 250 nm after 24 hours at 25 °C.

Combination with existing systems

Single pass printing with ink recirculation

A stationary piezoelectric print bar receives an aqueous ink containing pigment, a dispersion resin with an acid value of 250 mg KOH/g, polyethyleneimine with a number-average molecular weight of 1,200, and 3-methyl-1,5-pentanediol. A pump draws ink from a covered reservoir through a particle filter and membrane degasser into the print bar supply manifold. A return manifold routes ink back to the reservoir, and pressure regulators maintain crossflow through the head while holding nozzle pressure slightly below ambient. A web encoder synchronizes drop ejection with the moving substrate, and a downstream hot-air dryer removes water from the print.

Inkjet printing with inline fabric pretreatment

A textile line prints an aqueous ink containing pigment, a dispersion resin with an acid value of 250 mg KOH/g, polyethyleneimine with a number-average molecular weight of 1,200, and 1,2-pentanediol. An upstream pad applicator deposits an aqueous calcium chloride pretreatment with an acrylic binder on cotton fabric, and heated air dries the treated fabric before it reaches the printhead. The ink rewets the surface treatment, and calcium ions reduce the mobility of the pigment dispersion on the fabric. A downstream oven dries the print and forms the binder film that holds pigment on the fibers.

Automated or data-driven variant

Sensor controlled ink batch blending

A stirred batch tank receives a pigment concentrate made with a dispersion resin with an acid value of 250 mg KOH/g, plus water, 1,2-pentanediol, and diluted polyethyleneimine with a number-average molecular weight of 1,200 from separate feed tanks. A controller uses load cells to meter the concentrate, water, and diol, then adds the polyethyleneimine solution in small increments after the first three feeds are mixed. An automated sampler dilutes an aliquot by a fixed ratio for particle size measurement after each increment, and the controller stops the polyethyleneimine feed if the measured diameter exceeds the batch limit. An inline viscometer and temperature probe guide the final metered water addition before the ink is filtered and transferred to a holding tank.

Specific version of a part

Beta copper phthalocyanine pigment

Beta-phase copper phthalocyanine supplies cyan color as dispersed solid particles. Bead milling breaks down agglomerates, and filtration removes coarse particles before the ink enters the printhead.

Styrene acrylic dispersion resin

A styrene-acrylic acid copolymer has an acid value of 250 mg KOH/g before neutralization. Styrene segments adsorb onto the pigment, and neutralized acrylic acid groups hydrate in the aqueous vehicle.

Branched polyethyleneimine at 1,200

A branched polyethyleneimine has a number average molecular weight of 1,200 g/mol and contains primary, secondary, and tertiary amine groups. A dilute aqueous stock keeps the polymer concentration low at the point where it mixes into the pigment dispersion.

Two pentanediols in water

The aqueous vehicle contains 4% by mass 3-methyl-1,5-pentanediol and 1% by mass 1,2-pentanediol, based on total ink mass. Both diols dissolve in the vehicle and remain at the nozzle opening as water evaporates.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2012/0038704 A1
Published
Feb 16, 2012
Filed
Jul 29, 2011
Class
B41J 2/015
Document BUS 2023/0120244 A1
Published
Apr 20, 2023
Filed
Dec 6, 2022
Class
A61K 47/593
Claim 1
Document A
Document B
1.1a pigment;
1.2a pigment dispersion resin having an acid value of 200 mg KOH/g or more and 300 mg KOH/g or less;
The acid value of the pigment dispersion resin is 150 to 250 mg KOH/g.
A · US 2012/0038704 A1 · abstract
1.3a polyethyleneimine having a number average molecular weight of 600 or more and 1,800 or less;
Polyethyleneimine (PEI, Mw 800 Da, 2.40 g, 3.0 mmol) was dissolved in a mixture of chloroform (25 mL) and methanol (5 mL).
B · US 2023/0120244 A1 · ¶ 91
1.4a moisturizing agent including at least one of 3-methyl-1,5-pentanediol or 1,2-pentanediol; and
Of the additives that can be used in the recording liquid of these disclosures, examples of humectants or penetration enhancers include ethylene glycol monobutyl ether, triethylene glycol monomethyl ether, triethylene glycol monobutyl ether, diethylene glycol monomethyl ether, ethylene glycol monomethyl ether, triethylene glycol, hexylene glycol, octane diol, thiodiglycol, 2-butyl-2-ethyl-1,3-propanediol, 3-methyl-1,5-pentanediol, 2-ethyl-2-methyl-1,3-propanediol, 2-butyl-2-e
A · US 2012/0038704 A1 · ¶ 41
1.5water.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.2 1.4. Only Document B has a passage for 1.3.

Additional background

Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.

The disclosure of the present invention relates to an inkjet recording liquid and an inkjet recording device using the liquid, and relates especially to satisfactory intermittent discharge properties and bronzing suppression.
A · US 2012/0038704 A1 · ¶ 2
The problem to be solved by these disclosures, which were developed in light of this prior art, is to provide an inkjet recording liquid whereby the intermittent discharge properties of the ink in low-temperature, low-humidity environments are improved and bronzing is suppressed, as well as an inkjet recording device using the liquid.
A · US 2012/0038704 A1 · ¶ 10
However, delivery of DNA or RNA in vivo may be challenging due to properties of the DNA or RNA, or of the carrier system for the DNA or RNA.
B · US 2023/0120244 A1 · ¶ 3
However, it has been found that PEI with a high molecular weight (e.g., 25000 g/mol) is toxic to cells even though it is efficacious for transfection, and PEI with a low molecular weight is low in toxicity, but also is low in transfection efficiency.
B · US 2023/0120244 A1 · ¶ 4
On the other hand, when the molecular weight is 3000 or less, the steric hindrance of the molecule is small and, in addition, the degree of freedom in the liquid/film of the molecule is maintained and it is possible to obtain a high sensitivity.
C · US 9,290,015 B2 · ¶ 101

Related claim parts: 1.3

Document C: US 9,290,015 B2, published Mar 22, 2016. Cited for this statement only.

Cite aspatent.fyi, US 2026/0365867 A1, claim 1, first published 2026-11-23T17:42:24-05:00, https://patent.fyi/US20260365867/, SHA-256 853b3403c998e5ec71ce60bdbfc424cb392aff24c1b213f70daa7f1a45a86fc3
First published
Permanent addresshttps://patent.fyi/US20260365867/
Content fingerprint (SHA-256)853b3403c998e5ec71ce60bdbfc424cb392aff24c1b213f70daa7f1a45a86fc3
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi