Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Monolithic gradient film without a substrate
What ifWhat if the protective film uses a single depth-graded polymer sheet with no separate substrate layer?
Claim language“a substrate layer”
A single cast ultraviolet-curable resin sheet undergoes differential curing from one face so the top region crosslinks into a rigid protective skin while the bottom region stays tacky and compliant. A removable release liner carries the sheet during coating, curing, and lamination and strips off after placement on an optical panel. Controlling photoinitiator concentration and irradiation wavelength sets the modulus transition between the protective surface and the adhesive underside.
1.2Dry electrostatic cling replacing adhesive film
What ifWhat if the first surface holds onto an optical panel by dry electrostatic cling rather than an adhesive film?
Claim language“an adhesive film”
A smooth, non-tacky thermoplastic polyurethane or plasticized vinyl layer on the first surface carries an induced electrostatic charge that pulls the film into intimate contact with a flat glass or polymer surface. Electrostatic attraction and close interfacial contact maintain peel forces of 0.05 to 0.3 N/25 mm during handling and display operation. The sheet lifts off from a corner without leaving chemical residue or tacky polymer transfer.
What ifWhat if the adhesive film uses a crosslinked polyorganosiloxane network with no (meth)acrylic copolymer?
Claim language“a (meth)acrylic copolymer”
A blend of high-molecular-weight polydimethylsiloxane gum and branched silicate resin crosslinks through platinum-catalyzed hydrosilylation to form an optically clear pressure-sensitive adhesive. The siloxane backbone provides low surface energy, stable peel strength across temperatures from -40 °C to 150 °C, and rapid wet-out on glass or polymer panels without air entrapment. Adjusting the ratio of silicate resin to siloxane gum controls tack, shear holding power, and low-residue removability.
1.4Electron-beam crosslinking without an initiator
What ifWhat if the adhesive film crosslinks under an electron beam with no chemical initiator?
Claim language“an initiator”
High-energy electrons accelerated at 100 to 300 kV penetrate the coated adhesive layer and cleave carbon-hydrogen and carbon-carbon bonds directly along the polymer and monomer chains. The generated free radicals recombine to form a dense crosslinked network without adding photoinitiators or thermal initiators. Eliminating residual initiator fragments prevents outgassing, odor, and ultraviolet-induced yellowing in optical assemblies.
What ifWhat if the protective layer obtains surface repellency from a perfluoropolyether compound containing no silicon?
Claim language“a silicon-based compound”
A perfluoropolyether-modified urethane acrylate oligomer blends at 0.5 to 3 weight percent into a multifunctional acrylate hardcoat resin and migrates to the air interface before ultraviolet curing. Curing locks the fluorinated chains at the outer surface, reducing surface energy and imparting oil and fingerprint resistance without siloxane groups. The fluorinated surface layer maintains low sliding friction and optical clarity across repeated wiping cycles.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Protective film for photovoltaic backsheet lamination surfaces
This arrangement protects polymeric backsheets and glass front sheets of solar photovoltaic modules during outdoor transport and frame assembly. A polyester substrate carries a (meth)acrylic copolymer adhesive layer containing an aromatic acrylate monomer, an isocyanate curing agent, and a photoinitiator on its first surface, while its second surface holds a silicon-based hard-coat protective layer with a pencil hardness of F to H and a water contact angle of 90 to 100 degrees at 23 degrees Celsius. During module framing, the adhesive film bonds lightly to the photovoltaic panel surface without leaving residue, and the hydrophobic silicon-based outer layer sheds rainwater and dust. After installation, operators peel the film away or cure the adhesive with ultraviolet light when permanent edge-sealing adhesion is required.
Component substitution
Fluoropolymer outer layer replacing the silicon-based coating
A perfluoropolyether-modified urethane acrylate resin replaces the silicon-based compound in the protective layer formed on the second surface of the substrate layer. The adhesive film on the first surface retains the (meth)acrylic copolymer, crosslinking curing agent, aromatic monofunctional acrylate monomer, and free-radical photoinitiator. Slot-die coating deposits the fluorinated formulation onto a polyethylene terephthalate substrate, and ultraviolet radiation crosslinks the coating to a dry thickness of 2 micrometers. The fluorinated outer surface repels both water and skin oils while maintaining light transmittance above 90 percent across the laminate.
Cycloolefin polymer substrate with dual-cure adhesive chemistry
A cycloolefin polymer film replaces a polyethylene terephthalate film as the central substrate layer to reduce birefringence and moisture vapor transmission. On the first surface of the cycloolefin substrate, a silicone-modified polyurethane acrylate adhesive incorporates an aromatic methacrylate monomer, an aziridine thermal crosslinker, and an acylphosphine oxide photoinitiator. On the second surface, a polysiloxane-acrylate coating cures under ultraviolet light to form the protective layer with a pencil hardness between F and H and a water contact angle between 90 and 100 degrees at 23 degrees Celsius. Thermal drying sets the initial cohesive strength of the adhesive, and subsequent ultraviolet exposure triggers aromatic monomer polymerization to adjust the final peel force.
Parameter or scale variation
High-temperature adhesive film with increased protective hardness
This variation scales the laminate for thermal processing up to 180 degrees Celsius by using a 125-micrometer polyimide substrate layer paired with a 15-micrometer adhesive layer and a 5-micrometer silicon-based protective layer. Raising the crosslinking density of the silsesquioxane resin in the protective layer increases the pencil hardness to a range of 2H to 4H and shifts the water contact angle to 105 to 115 degrees at 23 degrees Celsius. The adhesive formulation increases the aromatic group-containing monomer concentration to 25 to 40 parts by weight per 100 parts of (meth)acrylic copolymer and uses a thermal peroxide initiator that activates above 130 degrees Celsius. The thicker substrate and higher-hardness coating withstand heated lamination rolls and solder reflow cycles without curling or surface marring.
Combination with existing systems
Roll-to-roll slot-die coating and ultraviolet curing line
The multilayer film structure integrates directly into a continuous roll-to-roll web-converting system equipped with tandem slot-die coaters, multi-zone hot-air drying ovens, and nitrogen-purged ultraviolet light-emitting diode curing stations. An unwind station feeds the substrate web through a corona surface treater before the first slot-die head deposits the silicon-based protective coating, which passes through a 365-nanometer curing tunnel to reach a pencil hardness of F to H. Turn-bar rollers invert the web so the second slot-die head applies the (meth)acrylic adhesive mixture containing the aromatic monomer, curing agent, and photoinitiator, followed by solvent evaporation in a three-zone oven at 80 to 120 degrees Celsius. Inline lamination rollers mate a silicone-coated release liner to the adhesive side before a turret winder collects finished rolls at line speeds of 15 to 40 meters per minute.
Automated or data-driven variant
Closed-loop optical inspection and coating thickness control
An automated web-monitoring system pairs inline white-light interferometers, automated goniometer cameras, and ultraviolet radiometers with a programmable logic controller to regulate protective film production in real time. The interferometers measure wet and dry thicknesses of both the (meth)acrylic adhesive layer and the silicon-based protective layer across the web width, while a machine-vision camera tracks water droplet contact angles on periodic edge samples to verify the 90 to 100 degree target at 23 degrees Celsius. A trained regression model correlates coating pump pressure, oven exhaust temperature, and ultraviolet lamp irradiance with final peel strength and pencil hardness values. When sensor readings drift outside preset tolerance bands, the controller adjusts metering pump speed and ultraviolet lamp power automatically to keep layer properties within specification.
Specific version of a part
Biaxially oriented polyethylene terephthalate substrate film
An optically clear biaxially oriented polyethylene terephthalate film with a thickness of 38 to 75 micrometers serves as the substrate layer. Both faces undergo inline acrylic or urethane primer coating to increase surface energy above 48 mN/m for high interfacial adhesion to the adhesive and protective coatings. The stretched polyester film provides total light transmittance above 91 percent, haze below 0.5 percent, and high tensile dimensional stability during roll-to-roll lamination.
Slot-die coated optically clear adhesive layer
A solvent-borne adhesive composition deposits onto the first surface of the substrate layer through a precision slot-die coater at a controlled wet gap and passes through a multi-zone convection oven at 80 °C to 120 °C. Drying removes residual ethyl acetate solvent to form a uniform dry adhesive thickness of 15 to 25 micrometers with thickness variation under 5 percent. Laminating a silicone-coated release liner onto the exposed adhesive face protects the film during winding and storage.
The adhesive film combines 100 parts by weight of a butyl acrylate and hydroxyethyl acrylate copolymer with 0.5 to 2 parts of a hexamethylene diisocyanate trimer curing agent, 5 to 15 parts of 2-phenoxyethyl acrylate as the aromatic monofunctional monomer, and 0.5 to 2 parts of a hydroxyketone photoinitiator. Thermal drying triggers urethane crosslinking between the isocyanate curing agent and hydroxyl groups on the copolymer backbone to establish cohesive strength. Subsequent ultraviolet irradiation at 300 to 800 mJ/cm² polymerizes the aromatic monomer in situ to raise the refractive index toward 1.50 and reduce peel force after curing.
The protective layer forms from an ultraviolet-curable coating containing a hexafunctional aliphatic urethane acrylate oligomer, a reactive silicone-modified polyether acrylate at 0.5 to 2 weight percent, and a photoinitiator cured to a dry thickness of 3 to 5 micrometers. The crosslinked urethane acrylate matrix yields a pencil hardness between F and H under a 750 g load while maintaining crack-free flexibility on curved or foldable panels. Surface-enriched siloxane segments produce a water contact angle between 90° and 100° at 23 °C for low sliding friction and reduced oil adhesion.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
[3] Patterned pressure-sensitive adhesive tape including: a support (A); and a pressure-sensitive adhesive layer, in which the pressure-sensitive adhesive layer is formed by using the pressure-sensitive adhesive composition for patterned pressure-sensitive adhesive tape according to [1] or [2], the pressure-sensitive adhesive layer has two or more pressure-sensitive adhesive portions (B) and a non-pressure-sensitive adhesive portion region having no pressure-sensitive adhesiv
B · US 2024/0052211 A1 · ¶ 9
1.2an adhesive film on a first surface of the substrate layer; and
[8] A method of producing patterned pressure-sensitive adhesive tape, including: a pressure-sensitive adhesive layer forming step of forming a pressure-sensitive adhesive layer on a surface of a support (A) using the pressure-sensitive adhesive composition for patterned pressure-sensitive adhesive tape according to [1] or [2], in which the pressure-sensitive adhesive layer has two or more pressure-sensitive adhesive portions (B) and a non-pressure-sensitive adhesive portion r
B · US 2024/0052211 A1 · ¶ 9
1.3a protective layer on a second surface of the substrate layer,
In one general aspect, a hard coating film includes: a substrate; a cured layer of a composition for forming a hard coating layer including an epoxy siloxane resin, disposed on the substrate; and an antifouling layer including a fluorine-substituted silsesquioxane resin, disposed on the cured layer.
A · US 2020/0056056 A1 · ¶ 11
1.4wherein the adhesive film comprises a (meth)acrylic copolymer, a curing agent, an aromatic group-containing monofunctional or higher monomer, and an initiator, and
When the isocyanate crosslinking agent is used, it is preferable to use an acrylic polymer containing a hydroxyl group as the acrylic polymer.
B · US 2024/0052211 A1 · ¶ 80
1.5the protective layer comprises a silicon-based compound and has a pencil hardness value of F to H and a water contact angle value of 90° to 100° at 23 °C.
Therefore, the antifouling layer 120 may have a water contact angle of 100° or more. In addition, the antifouling layer 120 may have excellent hardness, fraction resistance, and anti-curling property.
A · US 2020/0056056 A1 · ¶ 101
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.31.5. Only Document B has a passage for 1.11.21.4.
Additional background
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
However, the tempered glass has a disadvantage of being not suitable for weight reduction of portable devices due to its heavy weight, is vulnerable to external shock so that it is difficult to implement an unbreakable property, and does not bend above a certain level so that the tempered glass is unsuitable as a flexible display material having a bendable or foldable function.
A · US 2020/0056056 A1 · ¶ 5
However, these polymer plastic substrates exhibit insufficient physical properties in terms of hardness and scratch resistance and also does not have sufficient impact resistance, as compared with tempered glass used as a window cover for display protection.
A · US 2020/0056056 A1 · ¶ 6
Further, under the circumstances that reduction of the thickness of the pressure-sensitive adhesive layer is also examined to realize the reduction of the thickness described above, adhesive strength sufficient for practical use cannot be maintained in some cases with the pressure-sensitive adhesive layer with a reduced thickness and simply provided with an escape route for air bubbles.
B · US 2024/0052211 A1 · ¶ 7
One or more embodiments of the present invention provide patterned pressure-sensitive adhesive tape with excellent adhesive strength, which is capable of quickly releasing air bubbles from an interface with an adherend and preventing air bubbles from remaining at the interface.
B · US 2024/0052211 A1 · ¶ 8
When a plastic substrate is used, a scratch-resistant layer is formed on a surface of the plastic substrate to enhance the hardness and avoid the scratch of the surface of the substrate.
C · US 2008/0151549 A1 · ¶ 19
Related claim parts: 1.31.5
Document C: US 2008/0151549 A1, published Jun 26, 2008. Cited for this statement only.
Cite aspatent.fyi, US 2026/0365883 A1, claim 1, first published 2026-11-23T18:03:07-05:00, https://patent.fyi/US20260365883/, SHA-256 a705d3d4470ce1e4eeea951d9308368c04373a93a624db6a1e7693af0c19af74