patent.fyi
Applications  /  US 2026/0365888
United States Patent Application Publication

US 2026/0365888 A1

Published
Nov 19, 2026
Filed
Dec 18, 2023
Earliest date on the face
Dec 28, 2022
Classification
C09J 7/387
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Submillimeter flange gasket

What ifWhat if the sealing member is a 0.5 mm solid silicone gasket for a machined flange?
Claim language“1 mm to 40 mm”

The gasket follows the perimeter of the flange opening. Bolts draw the flange faces against compression stops, squeezing the gasket by 0.1 mm to close surface leakage paths.

1.2Thin skin over foam

What ifWhat if the face of the sealing member has a 100 μm polyurethane skin over a closed-cell foam core?
Claim language“a thickness of 300 μm”

The skin forms a continuous barrier across the exposed face. The foam core compresses to fill irregularities between the mating surfaces.

1.3Compression seal with mechanical retention

What ifWhat if a groove retains a gasket whose exposed face breaks at 250% tensile strain?
Claim language“a breaking strain of 500% or more”

A dovetail groove captures the gasket base and holds it during assembly. The mating flange compresses the projecting gasket crown to form the seal.

1.4Force at service extension

What ifWhat if the tensile comparison uses the force at 100% strain?
Claim language“a maximum test force”

The tester records the force when the 10 mm initial grip separation reaches 20 mm and scales it to a 20 mm specimen width. The comparison with the peel force uses the tensile load at the specified service extension.

1.7Slower tensile loading

What ifWhat if the grips separate at 100 mm/min during the tensile test?
Claim language“1000 mm/min”

A motorized test frame pulls the specimen at the set speed and records force and extension through rupture. The resulting curve gives the peak force and breaking strain at the slower loading rate.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Peelable seals for brewing cabinet covers

A 4 mm closed-cell elastomer strip seals the perimeter of a removable cover on a brewery control cabinet. A 300 μm extensible adhesive skin bonds the strip to the cabinet flange, and the cover compresses the exposed foam face when latched. The skin has a breaking strain of at least 500%, and its tensile force per 20 mm of width exceeds the 90° peel force after seven days at 100 °C.

Component substitution

Silicone adhesive skin on silicone foam

An addition-cured silicone pressure-sensitive adhesive replaces the adhesive skin material on a closed-cell silicone foam core. The adhesive is cast on a release liner at a cured thickness of 300 μm and bonded to the foam with a silicone-compatible primer. The adhesive cure formulation is set using tensile and heat-aged 90° peel measurements to obtain at least 500% breaking strain and a tensile force greater than the peel force at a common width of 20 mm.

Parameter or scale variation

Thicker adhesive skin for textured flanges

A 6 mm foam seal carries a 600 μm elastomeric adhesive skin on the face that contacts a textured metal flange. A pressure roller presses the adhesive into the flange texture during installation. A coupon cut from the skin is tested using a 10 mm grip separation and a crosshead speed of 1000 mm/min, and the measured peak force is multiplied by the skin thickness and the 20 mm reference width and divided by the coupon cross-sectional area. The resulting force is compared with the 90° peel force per 20 mm after aging bonded specimens at 100 °C for seven days.

Short thermal cycling for seal qualification

An 8 mm foam seal with a 300 μm extensible adhesive skin is applied to a painted metal test plate. The bonded assembly undergoes ten cycles of four hours at 80 °C and four hours at 20 °C, with each dwell timed after the plate reaches the target temperature. After the final dwell, a fixture peels the seal at 90°, and the force per 20 mm of width is compared with the normalized peak tensile force measured on a separate skin coupon.

Combination with existing systems

Replaceable seals on duct access doors

A die-cut elastomeric foam frame fits inside the perimeter recess of a hinged air duct access door. A 300 μm extensible adhesive skin bonds the frame to the door, and adjustable cam latches compress the exposed foam against the duct flange. A pull tab extends from one corner of the frame and starts the peel when the seal is replaced. The adhesive skin has a breaking strain of at least 500%, and its normalized peak tensile force exceeds the heat-aged 90° peel force on the door material.

Automated or data-driven variant

Automated tensile and peel test station

A motorized test frame accepts interchangeable tensile grips and a 90° peel fixture, and a barcode links skin coupons and bonded plates from the same production lot. Software runs the tensile test on 10 mm by 40 mm skin coupons at 1000 mm/min with an initial grip separation of 10 mm, capturing peak force from a load cell and breaking strain from grip displacement. The station measures peel force on bonded specimens aged at 100 °C for seven days and reports it per 20 mm of width. Software normalizes the tensile peak using the measured coupon cross-sectional area and skin thickness, then records whether the tensile force exceeds the peel force and the breaking strain reaches 500%.

Specific version of a part

Six millimeter foam strip

A closed-cell ethylene propylene diene rubber foam strip measures 6 mm between its broad faces in the uncompressed state. The strip compresses between an access panel and its frame to fill variations in the gap.

Cast polyurethane face layer

A cured 300 μm polyurethane elastomer film forms the exposed face of the sealing member. The film bonds to the compliant core across its inner face and stretches as the core conforms to the mating surface.

Die cut tensile rectangle

A rectangular steel-rule die cuts a 10 mm wide by 40 mm long coupon from the surface portion on a flat backing pad. The long axis aligns with the pull direction and the two ends sit in the grips.

Right angle peel fixture

A 20 mm wide strip remains bonded to a stainless steel test plate for seven days at 100 °C. During peeling, a sliding carriage moves the plate beneath the vertical pull line to hold the peel angle at 90°, and a load cell records the peel force in N/20 mm.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2012/0034447 A1
Published
Feb 9, 2012
Filed
Apr 15, 2010
Class
C09J 7/02
Document BUS 2018/0305975 A1
Published
Oct 25, 2018
Filed
Apr 3, 2018
Class
E06B 3/9616
Claim 1
Document A
Document B
1.1the sealing member having a thickness of 1 mm to 40 mm,
A gasket, comprising a compliant sealing portion having an uncompressed gasket thickness; and a less compliant compression control portion having opposing exposed surfaces wherein a perimeter of the less compliant compression control portion is surrounded by the compliant sealing portion, and wherein a thickness of the less compliant compression control portion is less than the uncompressed gasket thickness.
B · US 2018/0305975 A1 · claim 1
1.2the sealing member comprising a surface portion having a thickness of 300 μm, the surface portion including a surface in a thickness direction of the sealing member, wherein
The thickness of the heat expanding agent-containing pressure-sensitive adhesive layer is selected properly depending on the use purpose of the heat-expandable removable pressure-sensitive adhesive tape according to the present invention and the decrease of the adhesive power thereof by heating, but, for assurance of surface smoothness, it is preferably larger than the maximum diameter of the heat expanding agent (in particular, heat-expandable microsphere) and specifically,
A · US 2012/0034447 A1 · ¶ 101
1.3the surface portion has a breaking strain of 500% or more and satisfies the following requirement: tensile force FA [N/20 mm]> adhesive force FB [N/20 mm],
1.4the tensile force FA is expressed as F1·tA·20/S1, where F1 [N] is a maximum test force in a tensile test conducted on a test piece prepared from the surface portion, S1 [mm2] is a cross-sectional area of the test piece, and tA [mm] is a thickness of the surface portion,
1.5the test piece in the tensile test has a rectangular shape having a width of 10 mm and a length of 40 mm in a plan view,
1.6a chuck-to-chuck distance in the tensile test is 10 mm,
1.7a test speed in the tensile test is 1000 mm/min, and
1.8the adhesive force FB is a 90° peel adhesion [N/20 mm], which is obtainable by maintaining an environmental temperature at 100 °C for 7 days for a test piece prepared from the sealing member while the test piece being adhered to a test plate, and by conducting a measurement by peeling the test piece from the test plate in accordance with Japanese Industrial Standards (JIS) Z 0237:2022.
The heat-expandable removable acrylic pressure-sensitive adhesive tape or sheet according to the present invention includes at least a heat expanding agent-containing pressure-sensitive adhesive layer, and the tape or sheet has an initial 90° peel adhesive strength to a polycarbonate plate as adherend of 10 N/25 mm or more and a 90° peel adhesive strength after storage in an atmosphere at 80° C. for 2 months as bonded to the polycarbonate adherend and after heat expansion tre
A · US 2012/0034447 A1 · abstract

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.2 1.8. Only Document B has a passage for 1.1.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

The present invention relates to a heat-expandable removable acrylic pressure-sensitive adhesive tape or sheet that has high normal-state adhesive power when bonded independently of whether the adherend has or does not have irregular surface and yet has lowered adhesive power when removed under heat.
A · US 2012/0034447 A1 · ¶ 1
The expandable material-like acrylic adhesive tapes of Patent Documents 1 to 7 have been known as the expandable material-like acrylic adhesive tapes, but it was difficult for the adhesive tapes to show both favorable normal-state adhesive power to irregular-surfaced adherend (adhesive power at 23° C. and 50% RH (normal state)) and easy releasability (removability) at the same time.
A · US 2012/0034447 A1 · ¶ 7
Specifically, the present disclosure is directed to components for sealing between components of an entryway.
B · US 2018/0305975 A1 · ¶ 3
Therefore, there is a need for a device that seals between entryway components under the proper degree of compression.
B · US 2018/0305975 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0365888 A1, claim 1, first published 2026-11-23T18:03:07-05:00, https://patent.fyi/US20260365888/, SHA-256 8cc4b535ccb160b5f6911c1a632b6cbf7d1e3fa4278eacf721567f58178d0a13
First published
Permanent addresshttps://patent.fyi/US20260365888/
Content fingerprint (SHA-256)8cc4b535ccb160b5f6911c1a632b6cbf7d1e3fa4278eacf721567f58178d0a13
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi