1.1Waterborne acrylic adhesive film
Soft acrylic particles dispersed in water coalesce as the applied layer dries. The resulting tacky film grips skin and conforms to surface fibers in the fabric under light pressure.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Soft acrylic particles dispersed in water coalesce as the applied layer dries. The resulting tacky film grips skin and conforms to surface fibers in the fabric under light pressure.
Natural rubber latex is blended with an aqueous dispersion of a hydrogenated rosin ester. Water evaporation leaves an elastic film, and the rosin ester increases tack at the fabric interface.
Propylene glycol is mixed into the aqueous copolymer solution before coating. It remains in the film as water evaporates and lowers the film's stiffness so the bond flexes with skin movement.
A low loading of sorbitol is dissolved in the water phase before the copolymer is added. Sorbitol retains moisture in the dried layer, helping the film conform to skin and fabric as they move.
An ethanol-soluble grade of vinylpyrrolidone and vinyl acetate copolymer is dissolved in anhydrous ethanol, and glycerin is blended into the solution. Ethanol evaporates after application and leaves a flexible adhesive film.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
An aqueous blend of VP/VA copolymer and glycerin temporarily holds a fabric appliqué on a washable base fabric. A stencil deposits small dots of the blend on the back of the appliqué, and light pressure brings the two fabric layers into contact. The dots dry before stitching, and a water wash removes the temporary adhesive after the stitches secure the appliqué.
Pullulan replaces VP/VA copolymer as the film-forming polymer, with glycerin retained as the plasticizer and water as the solvent. One batch contains 10 parts pullulan, 3 parts glycerin, and 87 parts water by mass. The pullulan is stirred into water until dissolved, then the glycerin is blended in and the liquid is spread in a thin layer. Fabric is pressed onto the layer while it is tacky, and water rehydrates the dried film during removal.
An aqueous VP/VA copolymer and glycerin blend is drawn onto a smooth release liner at wet thicknesses of 50, 100, and 150 micrometers. Each coating covers a 20 by 50 millimeter rectangle, with the same blend used for all three thicknesses. Matching fabric strips are pressed into the wet coatings and left at 23 degrees Celsius until their mass stabilizes. The strips are peeled from the liner and weighed to compare the dry coating mass per unit area.
An aqueous VP/VA copolymer and glycerin blend fills a collapsible reservoir connected to a roller applicator. A squeeze valve feeds the blend into a chamber behind the roller, and a flexible wiper meters the liquid carried out on the roller surface. The roller lays a continuous stripe along the garment edge, and the coated edge is pressed into place while the stripe is tacky.
A mixing vessel sits on a load cell, and a controller operates a water valve, a glycerin pump, and a screw feeder for powdered VP/VA copolymer. The controller adds water first, feeds the copolymer into the stirred water, and adds glycerin after the polymer disperses. Each feed stops when the measured mass gain reaches its programmed target, and the controller records the delivered mass of each ingredient.
An overhead camera images a garment panel held flat on a vacuum table. Software traces the panel edge and generates a path 3 millimeters inward from the detected boundary. A motorized gantry moves a dispensing nozzle along the path while a pump delivers the aqueous VP/VA copolymer and glycerin blend. The controller reduces the pump rate as the nozzle slows at corners to maintain the deposited volume per unit length.
A copolymer with a 60:40 vinylpyrrolidone-to-vinyl acetate mass ratio serves as the film former. The powder is stirred into water until dissolved, and the deposited layer forms a continuous film as water evaporates.
Glycerin is blended into the aqueous polymer solution at two percent by mass of the wet formulation. It remains in the deposited film after drying and increases flexibility.
Deionized water serves as the sole solvent for the vinylpyrrolidone and vinyl acetate copolymer. The polymer powder is added gradually under stirring at room temperature, and the applied liquid dries by water evaporation.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
It shall be understood that as used throughout the specification and the claims crude glycerin, industrial grade glycerin, purified grade glycerin, recycled glycerin, glycerin product, and glycerin solution shall be understood to mean a solution comprising glycerol.A · US 2009/0198088 A1 · ¶ 27
An exemplary additive composition for grinding an inorganic material in a ball mill or roller mill, comprises: a crude glycerin byproduct obtained using a heterogeneous catalytic process(es) process during biodiesel fuel production, the crude glycerin byproduct comprising: (i) 1,2,3-propanetriol in an amount of 50-99 percent;B · US 2020/0048148 A1 · ¶ 25
An empty cell means only that no passage was reproduced there.
Both have a passage for 1.2.
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The magnitude of the volume of crude glycerin produced as a result of biodiesel production makes disposal undesirable and ultimately uneconomical.A · US 2009/0198088 A1 · ¶ 3
There are several well documented uses of refined glycerin as a replacement for petrochemicals but in general, the glycerin quality must be upgraded to remove contaminants.A · US 2009/0198088 A1 · ¶ 3
As clinker grinding requires substantial time and energy, the cement industry typically employs grinding additives to increase efficiency of the operation.B · US 2020/0048148 A1 · ¶ 3
Addition of such grinding aids enables the mill to grind the clinker to a smaller size with less energy by prohibiting the buildup of a coating of finer material on the grinding media and/or walls of the grinding mill.B · US 2020/0048148 A1 · ¶ 4
This is because glycerol is obtained in a proportion of 100 kg per tonne of biodiesel produced by transesterification of vegetable oils.C · US 9,315,440 B2 · ¶ 4
Related claim parts: 1.2
Document C: US 9,315,440 B2, published Apr 19, 2016. Cited for this statement only.
patent.fyi, US 2026/0365893 A1, claim 1, first published 2026-11-23T18:03:07-05:00, https://patent.fyi/US20260365893/, SHA-256 fb9b50d7cca520b27a45eef8d8d4293dca2851b5300fb16fd80b69218bb9a2f1