Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Moisture cure through isocyanates
What ifWhat if the acrylic monomer carries a nitrile group and terminal isocyanate groups in the polyurethane provide the moisture cure?
Claim language“having a silane group”
Acrylonitrile copolymerizes with the other vinyl monomers in a dry, isocyanate-terminated polyurethane prepolymer. After application, water reacts with terminal isocyanates to generate amines, which react with additional isocyanates to form urea crosslinks.
1.1Separate photoinitiator for UV cure
What ifWhat if a separate nonpolymerizable photoinitiator initiates UV cure in an acrylic copolymer with pendant methacrylate groups?
Claim language“having a radical photoinitiator group”
Glycidyl methacrylate supplies pendant epoxide groups during copolymerization in a polyol. Acrylic acid opens those epoxides after polymerization to install pendant acrylate groups, which serve as the UV-reactive sites. A dissolved acylphosphine oxide generates radicals under UV exposure and crosslinks the pendant acrylates.
1.2Molecular weight through feed control
What ifWhat if monomer feed rate and initiator concentration control chain length through radical initiation and termination?
Claim language“with a chain transfer agent”
A semibatch reactor meters the monomers into a heated polyol while a separate feed supplies a peroxide initiator. Dilute monomer conditions and a higher radical flux shorten the average chains through more frequent termination, and size-exclusion chromatography verifies an Mn below 200,000 g/mol.
1.2Higher molecular weight dispersed acrylic
What ifWhat if the acrylic polymer has an Mn of 250,000 to 350,000 g/mol and remains dispersed as particles in the polyol?
Claim language“less than 200,000 g/mol”
A polyether macromer with a terminal methacrylate copolymerizes with the vinyl feed and provides a polyol-compatible steric layer around the acrylic particles. A low chain transfer agent loading permits longer chains, and the continuous polyol phase carries the particles during mixing and dispensing.
1.3Room temperature urethane coupling
What ifWhat if partial coupling between the acrylic polymer and the polyol proceeds at 25 °C through urethane formation?
Claim language“to a temperature of 100 °C to 160 °C”
Copolymerized 2-isocyanatoethyl methacrylate supplies pendant isocyanate groups on the acrylic chains. After polymerization, a bismuth carboxylate catalyst promotes reaction with polyol hydroxyl groups at 25 °C, and a low pendant isocyanate loading limits the extent of coupling.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Edge bonding for acoustic panels
The polymerization runs in an isocyanate-terminated polyurethane prepolymer with the three monomer types and a chain transfer agent. A heated slot nozzle deposits the resulting adhesive along the edge of a porous acoustic panel, where an edge strip overlaps part of the bead. Ultraviolet light sets the exposed shoulder of the bead before the panel leaves the fixture. Moisture entering through the porous panel cures the polyurethane beneath the strip.
Component substitution
Cobalt complex for chain transfer
A cobalt glyoxime complex replaces a thiol chain transfer agent in a dry polyol formulation with a methacrylate as the principal monomer. A metering pump adds the complex in a portion of the methacrylate feed while a separate feed supplies the thermal radical initiator. The complex transfers hydrogen from growing methacrylate radicals during polymerization of the three monomer types. Size exclusion chromatography measures the number-average molecular weight of the acrylic fraction and guides adjustment of the catalyst dose to keep it below 200,000 g/mol.
Parameter or scale variation
Staged monomer feed in a pilot reactor
A 10 L jacketed stirred reactor holds a 5 kg batch, with the dry polyol charged before the monomers. Separate pumps meter the three monomer types, the chain transfer agent and a thermal radical initiator over 120 minutes, with the jacket holding the bulk mixture at 85 °C during the feed. The mixture remains at 85 °C for a further 90 minutes before cooling. A sample is tested for residual monomer and number-average molecular weight before the batch is discharged.
Combination with existing systems
Inline curing on a web coating line
A heated gear pump feeds the polymer composition in an isocyanate-terminated polyurethane matrix to a slot die that coats a moving film. A shielded ultraviolet lamp irradiates the exposed coating between the die and the laminating nip. The lamp spectrum overlaps the absorption band of the incorporated photoinitiator, and the line speed sets the exposure time. The nip bonds the coated film to a moisture-permeable backing while the coating retains tack, and moisture entering through the backing completes the polyurethane cure.
Static mixing for two-component dispensing
One side of a dual-cartridge dispenser contains a dry isocyanate-terminated prepolymer, and the other contains the polyol-based product of the three-monomer polymerization. The cartridge volumes set the dispensing ratio from the measured hydroxyl content of the polyol side and the isocyanate content of the prepolymer side. A disposable static mixer combines the streams and delivers the blend into the joint. Ultraviolet exposure sets the accessible bead surface while the isocyanate and hydroxyl groups react throughout the bead.
Automated or data-driven variant
Spectroscopic control of monomer feed
A Raman probe in a heated recirculation loop measures the residual carbon–carbon double-bond signal during polymerization in a stirred polyol reactor. A calibration against residual monomer measurements relates the signal to total monomer concentration in the reaction mixture. A controller slows the three monomer feeds together when the measured concentration rises above the setpoint and restores the feed rate as the concentration falls. Offline size exclusion chromatography compares the finished batch with the molecular-weight target and informs the chain transfer dose for the next batch.
Specific version of a part
Terminal isocyanate prepolymer carrier
A dry polyether diol reacts with excess hexamethylene diisocyanate to form a prepolymer with terminal isocyanate groups. The prepolymer carries n-butyl acrylate, 3-methacryloxypropyltriethoxysilane, and 4-benzoylphenyl methacrylate during radical polymerization.
Mercaptan controlled radical polymerization
A peroxide initiator starts radical polymerization in the polyol, and n-dodecyl mercaptan transfers hydrogen to growing acrylic radicals. The resulting thiyl radicals initiate new chains, and the mercaptan loading sets the chain transfer frequency for a target Mn of 50,000 g/mol.
Polyol coupling through silane exchange
The mixture contains a hydroxyl-terminated polyether diol, a copolymer with pendant trimethoxysilyl groups and an Mn of 50,000 g/mol, and a titanium alkoxide catalyst. A 30-minute hold at 140 °C under reduced pressure removes methanol as polyol hydroxyl groups replace some of the silane methoxy groups, forming partial crosslinks.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a) Combination of: (i) a polyol or a prepolymer with terminal isocyanate (NCO) groups (ii) an ethylenically unsaturated monomer containing no active hydrogen and having no silane groups (monomer type A), and (iii) an ethylenically unsaturated monomer containing no active hydrogen and having a silane group (monomer type B) (iv) an ethylenically unsaturated monomer containing no active hydrogen and having a radical photoinitiator group (monomer type C)
The copolymers contain, besides the aforementioned photoinitiators, polymerized units of the main monomers generally in major amounts, comprising in most cases from 50 to 99.99 wt % and preferably from 70 to 97.5 wt % of esters of preferably C3-6 α,β-monoethylenically unsaturated mono- and di-carboxylic acids, such as, in particular, acrylic acid, methacrylic acid, maleic acid, fumaric acid, and itaconic acid, with generally C1-C12, preferably C1-8 and more preferably C1-4 al
A · US 7,358,319 B2 · ¶ 67
1.2b) Polymerizing the mixture from step a. using a radical polymerization process with a chain transfer agent to obtain a low molecular weight polymer having an average molecular weight Mn of less than 200,000 g/mol
In some cases, for example, when the novel copolymers are produced by aqueous free-radical emulsion polymerization, it is possible to include conventional regulators in conventional amounts, for example, in concentrations of from 0.1 to 10 parts by weight or from 0.5 to 5 parts by weight per 100 parts by weight of the monomers to be polymerized. Such regulators are used for the regulation of the molecular weight of the copolymers and are known to the person skilled in the art.
A · US 7,358,319 B2 · ¶ 82
1.3c) Optionally heating the mixture from step b) to a temperature of 100 °C to 160 °C for 10 to 60 minutes for partial cross-linking of the polyol with the low molecular weight polymer having an average molecular weight Mn of less than 200,000 g/mol
However, it is also possible here to use all polymers which can be softened by thermal excitation and crosslinked three-dimensionally by the heating or after subsequent cooling.
B · US 8,969,716 B2 · ¶ 14
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.11.2. Only Document B has a passage for 1.3.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
Copolymerizable photoinitiators should be producible in a simple manner and be readily copolymerizable, and the copolymers containing photoinitiators should exhibit, in use, good application-technological properties, particularly high cohesion and adhesion when used as adhesives.
A · US 7,358,319 B2 · ¶ 8
It is an object of the present invention to provide novel copolymerizable photoinitiators, and copolymers containing the photo-initiators of the invention in the form of polymerized units and exhibiting, when used as adhesives, improved cohesion and adhesion.
A · US 7,358,319 B2 · ¶ 9
Furthermore the invention relates to a method for producing a concentrator lens system which can be used in a corresponding photovoltaic device but also in other devices for, e.g. thermal, use of radiation.
B · US 8,969,716 B2 · ¶ 1
Starting herefrom, it was therefore the object of the present invention to provide a photovoltaic device with a concentrator lens system which can be produced in a simple and economical manner.
B · US 8,969,716 B2 · ¶ 6
Cite aspatent.fyi, US 2026/0365895 A1, claim 1, first published 2026-11-23T18:03:07-05:00, https://patent.fyi/US20260365895/, SHA-256 70933660ddbba8fe1fa10be4fff1171e5b0f937c9fa65a35f0dad9f65f3887aa