1.1Small molecule surface stabilization
An alkyl sulfate adsorbs at the particle surface and exposes charged sulfate groups to the water. A fatty alcohol ethoxylate in the same adsorbed layer provides a hydrated barrier that limits particle contact.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
An alkyl sulfate adsorbs at the particle surface and exposes charged sulfate groups to the water. A fatty alcohol ethoxylate in the same adsorbed layer provides a hydrated barrier that limits particle contact.
Nonionic surfactant adsorbs on the latex particles and keeps them dispersed in water. The butyl acrylate fraction lowers the glass transition temperature so the particles deform and coalesce as the water evaporates.
The hydrocarbon tails associate with the fluoropolymer surface, and the sulfate heads impart negative charge to the particles. Deionized water limits charge screening and preserves electrostatic repulsion between particles.
High shear breaks up particle agglomerates and distributes the powder through the hydrofluoroether. Recirculation keeps the particles suspended during application, and solvent evaporation deposits them on the substrate.
Deionized water dilutes the concentrate while preserving the surfactant to polymer mass ratio. Successive spray passes with intermediate drying build the required dry coating mass.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
The aqueous coating contains 55% by mass polytetrafluoroethylene, a water-soluble acrylic polymer bearing carboxyl groups, and a fluorine-free nonionic surfactant with an HLB of 13 dosed at 6% by mass relative to the fluoropolymer. The feed dispersion has a foam height of 140 mm or less in the foamability test. A dip coater applies the dispersion to woven glass fabric used in food processing conveyor belts, and a metering roll removes excess liquid. The coated fabric passes through a drying zone and then through a sintering zone that fuses the fluoropolymer around the fibers.
A fluorine-free C10–C12 alkyl polyglucoside grade with an HLB of 13 replaces the nonionic wetting agent in a dispersion containing water, a carboxylated acrylic polymer, and 50% by mass polytetrafluoroethylene. The alkyl polyglucoside enters the aqueous phase at 5% active mass relative to the fluoropolymer. Slow agitation distributes the surfactant through the dispersion, where its alkyl chains adsorb at particle interfaces and its glucoside groups face the water. The finished blend proceeds to coating after the foamability test records a foam height of 140 mm or less.
The dispersion contains 35–38% by mass polytetrafluoroethylene, a carboxylated acrylic polymer, and a fluorine-free nonionic surfactant with an HLB of 13 at 6% by mass relative to the fluoropolymer. Deionized water added under gentle agitation sets the final fluoropolymer concentration, and the working bath operates at 20–25 °C. A dip tank wets the fabric, a squeeze nip meters the pickup, and successive dip and dry passes build the specified coating mass. A sample of the diluted bath proceeds through the foamability test before the line starts, with a 140 mm maximum foam height.
A sealed vessel receives an aqueous dispersion containing 55% by mass polytetrafluoroethylene, a carboxylated acrylic polymer, and a fluorine-free nonionic surfactant with an HLB of 13 at 6% by mass relative to the fluoropolymer. A vacuum regulator lowers the headspace pressure to 40–60 kPa absolute for 5–10 minutes at 20–25 °C, and a sight glass allows the operator to track foam expansion. The vessel returns to atmospheric pressure before a bottom outlet transfers the deaerated dispersion to the applicator. A separate foamability test confirms a foam height of 140 mm or less under test agitation.
A slot die web coater draws from a covered tank containing an aqueous dispersion with 50% by mass polytetrafluoroethylene, a hydrophilic acrylic polymer, and a fluorine-free nonionic surfactant with an HLB of 13 at 6% by mass relative to the fluoropolymer. A low shear metering pump feeds the die through a screen sized to retain agglomerates, and a bypass returns excess flow below the tank liquid surface. The die deposits a wet film on the moving web, which passes through a drying oven. The feed tank receives batches that produce a foam height of 140 mm or less in the foamability test.
A controller uses tank load cells and the measured fluoropolymer content of the incoming concentrate to meter water, a hydrophilic acrylic polymer solution, and a fluorine-free nonionic surfactant with an HLB of 13. The dosing calculation targets 55% fluoropolymer by total batch mass and 6% active surfactant by fluoropolymer mass. An automated sampler transfers a fixed volume to a transparent vessel, and a camera calibrated against a vertical scale measures the distance from the liquid surface to the top of the foam at the specified read time. The controller opens the batch transfer valve when the dosing records meet the setpoints and the measured foam height is 140 mm or less.
A copolymer of butyl acrylate and acrylic acid supplies hydrophobic segments and water-facing carboxyl groups. Partial neutralization with ammonia converts carboxyl groups to carboxylate groups that hydrate in the aqueous phase.
Polytetrafluoroethylene forms the dispersed phase as particles with a median diameter of approximately 200 nm. Drying deposits the particles, and heating above the polymer melting point fuses them into a continuous layer.
A C12 to C14 fatty alcohol ethoxylate with an average of nine ethylene oxide units supplies a nonionic surfactant with an HLB above 8. Its alkyl groups adsorb at the particle surface, and its hydrated ethoxylate chains extend into the water.
The dispersion contains 6.0 parts by mass of active nonionic surfactant per 100 parts by mass of dry fluoropolymer. For a dispersion containing 55% fluoropolymer by mass, this loading corresponds to 3.3% active surfactant by mass of the full dispersion.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Fluoroplastics that may be employed in this invention are semi-crystalline fluoropolymers and include, but are not limited to polytetrafluoroethylene (PTFE), modified PTFE (e.g. acrylic modified PTFE) and copolymers of tetrafluoroethylene (e.g. tetrafluoroethylene/perfluoro(propyl vinyl ether)).A · US 9,290,624 B2 · ¶ 28
In some embodiments, a first nonionic surfactant may have an HLB greater than 10, a second nonionic surfactant may have an HLB greater than 10, and a third nonionic surfactant may have an HLB of less than 10.B · US 11,787,996 B1 · ¶ 14
The concentration of the fluoroplastic particles may vary from 0.1 wt % to 70 wt %, based on total weight of dispersion. Preferably, the fluoroplastic particles are dispersed in a polar liquid within a concentration range of 10 to 70 wt %, most preferably 50 to 70 wt %.A · US 9,290,624 B2 · ¶ 29
Generally, the nonionic surfactant may be included to the single-phase cleanout fluid in any desired concentration, including at a point in a range of from about 0.1% to about 20% by weight of the single-phase cleanout fluid.B · US 11,787,996 B1 · ¶ 13
An empty cell means only that no passage was reproduced there.
Only Document A has a passage for 1.2 1.7. Only Document B has a passage for 1.3 1.8.
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
It would be desirable to have a more commercially feasible process for introducing fibrillating fluoroplastic filler into a fluoroelastomer composition.A · US 9,290,624 B2 · ¶ 6
B) adding a liquid dispersion of fibrillatable fluoroplastic particles to said fluoroelastomer gum while applying shear in said mixer, thereby forming a fluoroelastomer composition containing fluoroplastic fibrils dispersed therein.A · US 9,290,624 B2 · ¶ 7
Displacement fluids may also be placed between different drilling fluids during drilling change outs or between a drilling fluid and a completion brine, for example.B · US 11,787,996 B1 · ¶ 2
A particular challenge in designing displacement fluids is that some displacement fluids require multiple incompatible components to be present to be effective.B · US 11,787,996 B1 · ¶ 4
By modifying the PTFE dispersion with certain wetting agents, it may be possible to increase the product weight with subsequent coating passes, but the increase in PTFE weight per coating pass will, typically, be very low.C · US 2006/0046063 A1 · ¶ 17
Related claim parts: 1.3
Document C: US 2006/0046063 A1, published Mar 2, 2006. Cited for this statement only.
patent.fyi, US 2026/0365922 A1, claim 1, first published 2026-11-23T18:24:18-05:00, https://patent.fyi/US20260365922/, SHA-256 859c2ef0787a5452be3e594c620ddea56393a049e04f915c8e2eba7118a4aba8