patent.fyi
Applications  /  US 2026/0365936
United States Patent Application Publication

US 2026/0365936 A1

Published
Nov 19, 2026
Filed
Oct 17, 2025
Earliest date on the face
May 19, 2025
Classification
C10M 103/06
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.2Thicker three-layer transition

What ifWhat if each transition sublayer is 300 nm thick?
Claim language“an interlayer thickness of 50-200 nm”

Calibrated deposition times set the thickness of the three sublayers. Reactive sputtering forms the chromium oxide base, and co-sputtering forms the mixed and tungsten–carbon layers that support the carbon topcoat.

1.2Equiaxed chromium oxide base

What ifWhat if the bottom layer consists of equiaxed chromium oxide grains?
Claim language“a crystalline layer composed of columnar crystals”

Pulsed reactive sputtering with substrate bias promotes renucleation and interrupts grain growth through the film thickness. The resulting dense chromium oxide layer provides a corrosion barrier beneath the mixed transition layer.

1.2Mixed layer with dispersed grains

What ifWhat if the intermediate layer contains dispersed chromium oxide nanocrystals in a continuous tungsten–carbon matrix?
Claim language“a crystalline-amorphous alternating layer with coarse striated morphology”

Simultaneous sputtering from chromium oxide, tungsten and graphite targets produces a mixed film without stacked bands. The continuous matrix supports the upper layer, while the embedded oxide grains maintain an oxide phase next to the base layer.

1.3Silver-bearing nitride topcoat

What ifWhat if a chromium nitride topcoat with dispersed silver provides the sliding surface?
Claim language“a DLC layer”

Reactive co-sputtering from chromium and silver targets in argon and nitrogen deposits a hard chromium nitride matrix containing metallic silver. During sliding, silver smears across the contact and forms a low-shear transfer film, while the nitride matrix carries the load.

1.4Chromium nitride base layer

What ifWhat if the bottom layer is chromium nitride?
Claim language“a Cr2O3 layer”

Reactive sputtering from a chromium target in argon and nitrogen deposits crystalline chromium nitride on the cleaned substrate. The hard base supports the upper films, and its dense structure limits electrolyte access to the substrate.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Coated guide pins for packaging machines

Hardened stainless steel guide pins serve as substrates for the sliding guides of a packaging machine. Each pin carries a columnar chromium oxide layer, an alternating crystalline and amorphous chromium oxide–tungsten–carbon layer, a fine-striated amorphous tungsten–carbon layer, and a diamond-like carbon topcoat. Chromium content falls toward the topcoat, and tungsten content rises through the upper two transition layers. The topcoat runs against a replaceable polymer bushing, and the coated pin finish establishes the specified running clearance.

Component substitution

Molybdenum replaces tungsten in transition layers

Separate chromium oxide, molybdenum, and graphite sputter targets supply the transition layers on polished steel. The stack begins with columnar chromium oxide, followed by alternating chromium oxide-rich and molybdenum–carbon-rich strata, then an amorphous molybdenum–carbon surface layer. Successive deposition cycles lower the chromium oxide contribution and raise the molybdenum contribution toward the surface. A diamond-like carbon film deposited from the graphite target forms the sliding surface.

Hydrogenated carbon deposited from acetylene plasma

A chromium oxide–tungsten–carbon transition stack on polished steel progresses from a columnar chromium oxide bottom layer through an alternating crystalline and amorphous composite layer to an amorphous tungsten–carbon surface layer. Hydrogenated amorphous carbon deposited by plasma-enhanced chemical vapor deposition replaces a sputtered carbon topcoat. After sputtering the transition stack, the chamber introduces acetylene and argon without exposing the surface to air. A pulsed substrate bias controls ion bombardment as the plasma deposits the hydrogenated carbon sliding film.

Parameter or scale variation

Thicker transition layers on valve stems

A polished stainless steel valve stem carries a 180 nm columnar chromium oxide bottom layer, a 150 nm alternating chromium oxide–tungsten–carbon intermediate layer, and a 160 nm amorphous tungsten–carbon surface layer. Sputter deposition reduces the chromium flux through the intermediate layer and increases the tungsten flux into the surface layer. A 0.8 µm diamond-like carbon topcoat brings the total radial buildup to 1.29 µm. The stem diameter before deposition is 2.58 µm below the specified coated diameter.

Combination with existing systems

Coated plungers in packed metering pumps

A reciprocating metering pump uses a hardened stainless steel plunger that slides through a stationary packing stack. The plunger carries a columnar chromium oxide bottom layer, an alternating crystalline and amorphous chromium oxide–tungsten–carbon intermediate layer, an amorphous tungsten–carbon surface layer, and a diamond-like carbon topcoat. The coating covers the full travel of the packing contact band, and its edges lie beyond that band. The plunger displaces liquid through check valves while the packing seals against the coated surface.

Automated or data-driven variant

Deposition controlled by measured film thickness

A programmable sputtering system uses independently powered chromium oxide, tungsten, and graphite targets and a shuttered quartz crystal thickness monitor calibrated against witness coupons. The controller deposits the columnar chromium oxide bottom layer, then alternates chromium oxide-rich and tungsten–carbon-rich deposition to build the intermediate layer. Programmed target power changes lower the chromium fraction and raise the tungsten fraction as the film grows, and thickness readings trigger the change to amorphous tungsten–carbon deposition. At the surface-layer thickness setpoint, the controller closes the tungsten shutter and switches to the validated graphite-target settings for the diamond-like carbon topcoat.

Specific version of a part

Polished martensitic steel substrate

A hardened martensitic stainless steel sleeve serves as the coating substrate. Its sliding surface is polished to an arithmetic mean roughness below 0.05 micrometers and argon ion etched before deposition.

Graded transition with nanometer sublayers

The transition starts with 100 nm of columnar chromium oxide, continues with 150 nm of coarsely banded crystalline and amorphous regions, and ends with 75 nm of finely banded amorphous tungsten–carbon. The deposition recipe reduces the chromium oxide flux toward the surface and increases the tungsten fraction from the intermediate region into the upper layer.

Hydrogenated amorphous carbon topcoat

Plasma-enhanced chemical vapor deposition from acetylene and argon forms a 1 micrometer hydrogenated amorphous carbon film on the transition surface. A pulsed substrate bias controls ion bombardment during growth.

Three layers from sputter targets

A ceramic chromium oxide target deposits the bottom layer, and simultaneous sputtering from chromium oxide, tungsten and graphite targets forms the intermediate composite. The chromium oxide shutter closes while tungsten and graphite sputtering continues to form the surface composite.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2016/0372142 A1
Published
Dec 22, 2016
Filed
Jun 18, 2015
Class
G11B 5/3163
Document BUS 2025/0116537 A1
Published
Apr 10, 2025
Filed
Dec 2, 2024
Class
G01D 5/34707
Claim 1
Document A
Document B
1.1a coating substrate;
1.2a transition layer, provided on the coating substrate, wherein the transition layer contains Cr—O—W—C components, and comprises a bottom layer, an intermediate layer and a surface layer in sequence in a direction from close to the coating substrate to away from the coating substrate, wherein the bottom layer, the intermediate layer and the surface layer are respectively a crystalline layer composed of columnar crystals, a crystalline-amorphous alternating layer with coarse striated morphology and an amorphous layer with fine striated morphology, and the bottom layer, the intermediate layer and the surface layer each have an interlayer thickness of 50-200 nm, wherein a content of Cr in the transition layer is gradually decreased from the bottom layer to the surface layer, and a content of W in the transition layer is gradually increased from the intermediate layer to the surface layer; and
In one embodiment, a side of a chromium oxide layer is exposed to a beam of charged particles for converting an amorphous and/or partially polycrystalline component of at least a portion of a chromium oxide layer to a crystalline state, wherein the side of the chromium oxide layer of extends between adjacent layers of any type.
A · US 2016/0372142 A1 · ¶ 95
1.3a DLC layer, provided on the surface layer of the transition layer, wherein
Where there is no closure, preferably a hard coating is added to the module. One preferred coating is diamond-like carbon (DLC).
A · US 2016/0372142 A1 · ¶ 65
1.4the bottom layer is a Cr2O3 layer, the intermediate layer is a Cr2O3—W—C composite layer, and the surface layer is a W—C composite layer.
In the disclosure, the low reflection region preferably includes the chromium oxide film placed on one surface of the transparent substrate; the chromium nitride film placed on a surface of the chromium oxide film, on opposite side to the transparent substrate; and the metallic chromium film placed on a surface of the chromium nitride film, on opposite side to the chromium oxide film.
B · US 2025/0116537 A1 · ¶ 25

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.2 1.3. Only Document B has a passage for 1.4.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

The present invention relates to processing of thin films, and more particularly, this invention relates to methods for hardening chromium oxide films via crystallization thereof on devices such as magnetic heads.
A · US 2016/0372142 A1 · ¶ 1
However, the development of small footprint, higher performance tape drive systems has created various problems in the design of a tape head assembly for use in such systems.
A · US 2016/0372142 A1 · ¶ 3
As the optical encoder, there is a transmission-type encoder and a reflection-type encoder, and the reflection-type encoder has advantages that the optical path is shorter as compared with the transmission-type encoder, so that it is easy to make the size and thickness thereof smaller.
B · US 2025/0116537 A1 · ¶ 3
In order to prevent false detection by the light detector in the reflection region and non-reflection region formed on the reflection-type optical scale, and to increase the detection accuracy of the signal, reflectance of the reflection region should be high and reflectance of the non-reflection region should be low.
B · US 2025/0116537 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0365936 A1, claim 1, first published 2026-11-23T18:43:34-05:00, https://patent.fyi/US20260365936/, SHA-256 9a611c1067f34fccdaff6f3d755fb516b0ec45d9e3cdf4c7b7a8905f932be62f
First published
Permanent addresshttps://patent.fyi/US20260365936/
Content fingerprint (SHA-256)9a611c1067f34fccdaff6f3d755fb516b0ec45d9e3cdf4c7b7a8905f932be62f