Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.2Silicon-free aluminum-alloyed carbide suppression

What ifWhat if silicon is eliminated to trace levels below 0.01% and aluminum suppresses carbide formation?
Claim language“Si: 0.01% to 3.00%”

Removing silicon eliminates surface silicon oxide films that impair hot-dip metallic coating wettability. Raising soluble aluminum to 1.20% to 1.80% slows cementite precipitation during isothermal holding at 400 to 450 °C, allowing carbon partitioning into austenite to stabilize retained austenite at room temperature.

1.3Low-manganese water-quenched hardenability

What ifWhat if manganese is reduced below 0.80% and hardenability relies on water quenching with chromium?
Claim language“Mn: 1.00% to 5.00%”

Reducing manganese to 0.40% to 0.80% lowers centerline segregation during continuous casting and reduces manganese oxide formation during annealing. Adding 1.20% to 1.80% chromium together with high-pressure water-jet quenching at cooling rates above 500 °C/s suppresses pearlite formation and produces a martensitic-bainitic core.

1.12Dual-phase ferrite and martensite core

What ifWhat if the quarter-thickness microstructure contains less than 2% retained austenite and relies on soft ferrite for ductility?
Claim language“4% to 20% of retained austenite”

Intercritical annealing followed by rapid quenching to room temperature transforms austenite directly into martensite without an isothermal bainite hold, keeping retained austenite below 2% by volume. A continuous matrix of 35% to 50% polygonal ferrite accommodates plastic strain around hard martensite islands, providing uniform elongation without transformation-induced plasticity.

1.12As-quenched martensite with carbide-free bainite

What ifWhat if martensite remains untempered below 20% tempered fraction and toughness comes from carbide-free bainite?
Claim language“tempered martensite in the martensite is 50% or more”

Cooling from the annealing temperature directly to a bainitic transformation hold at 350 to 400 °C produces a matrix of fine carbide-free bainitic ferrite laths that absorb fracture energy. Final cooling to room temperature forms small isolated islands of as-quenched martensite without a reheating tempering step, maintaining high tensile strength while limiting crack propagation.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Specific version of a part

Titanium microalloying for prior austenite refinement

Adding 0.015% to 0.045% titanium during secondary refining binds free nitrogen as cuboidal titanium nitride particles above 1150 °C during slab reheating. Remaining dissolved titanium forms fine titanium carbides during hot-strip coiling at 550 to 620 °C, pinning grain boundaries during subsequent intercritical annealing.

Boron grain-boundary segregation for hardenability

A controlled addition of 0.0010% to 0.0030% boron is protected from boron nitride formation by prior titanium nitrogen fixation in the melt. Free boron segregates to austenite grain boundaries during annealing above 800 °C, delaying polygonal ferrite nucleation during gas-jet cooling so martensite and bainite form at moderate cooling rates.

Dew-point-controlled decarburized soft surface layer

Continuous annealing in a nitrogen-hydrogen furnace atmosphere with a dew point of -15 to +5 °C decarburizes the outer 10 to 20 μm of the cold-rolled strip. Carbon depletion promotes 60% to 85% polygonal ferrite with low dislocation density in the surface layer while the quarter-thickness core transforms into tempered martensite, bainite, and 8% to 14% retained austenite.

Cite aspatent.fyi, US 2026/0366094 A1, claim 1, first published 2026-11-23T20:11:03-05:00, https://patent.fyi/US20260366094/, SHA-256 6d409ee72af203068a6590b7caf26219d00d9f2c4d2a904202eaccf3868d565a
First published
Permanent addresshttps://patent.fyi/US20260366094/
Content fingerprint (SHA-256)6d409ee72af203068a6590b7caf26219d00d9f2c4d2a904202eaccf3868d565a
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi