patent.fyi
Applications  /  US 2026/0366095
United States Patent Application Publication

US 2026/0366095 A1

Published
Nov 19, 2026
Filed
Dec 13, 2024
Earliest date on the face
Dec 15, 2023
Classification
C21D 9/46
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Directional core loss controls acceptance

What ifWhat if acceptance depends on measured core loss in three sheet directions?
Claim language“V{001}<001>/V{011}<001>≤0.65 [Equation 1]”

Cut specimens at 0°, 45°, and 90° to the rolling direction and measure specific core loss at a peak flux density of 1.5 T and a frequency of 50 Hz. Compare the highest of the three readings with a specified loss limit to screen for unfavorable directional behavior.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Laminated yokes for magnetic inspection

A portable magnetic particle inspection yoke uses the specified non-oriented electrical steel in a stack of insulated U-shaped laminations. An alternating-current coil surrounds the center leg, and the two pole faces contact the ferromagnetic workpiece. The coil drives alternating flux through the workpiece, and magnetic particles collect where discontinuities produce flux leakage at the surface.

Component substitution

Gallium in place of aluminum

A trial heat uses Fe with 3.0 wt% Si, 0.30 wt% Mn, and 0.50 wt% Ga in place of the aluminum addition. The route hot rolls the cast slab, pickles and cold rolls the band to 0.35 mm, and recrystallizes the sheet in a dry hydrogen–nitrogen atmosphere. An annealing trial compares texture across several peak temperatures, and the selected sheet has a measured {001}<001> to {011}<001> grain-fraction ratio of 0.65 or less using the 15° windows.

Parameter or scale variation

Thin sheet for higher frequencies

A strip with the specified chemistry is cold rolled from a 1.6 mm hot band to 0.20 mm in two stages with an intermediate recrystallization anneal at about 850 °C. A final annealing trial uses peak temperatures from 850 to 950 °C and a 60 s hold, and texture measurements identify conditions that yield a grain-fraction ratio of 0.65 or less using the 15° windows. A thin insulating coating separates adjacent sheets in the stack, and the 0.20 mm gauge limits the classical eddy-current contribution during operation at 400 Hz.

Alternating angular offsets in ring stacks

A ring core uses 0.35 mm insulated laminations cut from the specified sheet, with the rolling direction marked on each ring. The stack alternates between rings whose rolling directions are 90° apart, and an insulating fixture holds the rings together. Circumferential flux passes through both orientations in parallel, so their directional magnetic responses average across the stack thickness.

Combination with existing systems

Laminated stator in an inverter drive

A three-phase induction motor uses the specified sheet in an insulated stator stack surrounding a squirrel-cage rotor. The stator slots hold a distributed winding connected to a pulse-width-modulated inverter, and a shaft encoder supplies speed feedback to the drive controller. The controller adjusts the amplitude and frequency of the stator currents, and the laminated stack limits eddy-current loss from the alternating flux and its harmonics.

Automated or data-driven variant

Automated grain counting from orientation maps

An automated electron backscatter diffraction station maps polished coupons from the coil head and tail, with the rolling and transverse directions registered before scanning. Software reconstructs grains from the orientation maps and calculates each grain's minimum angular distance to the symmetry variants of each reference orientation in the sheet coordinate system. It counts grains within 15° of each reference, calculates the ratio from the two counts, and flags ratios above 0.65 or maps with a zero denominator for review.

Specific version of a part

Ten degree cube window

Determine a mean orientation for each grain from an electron backscatter diffraction map. Count grains whose minimum misorientation from the symmetry-related {001}<001> orientations is 10° or less, then divide by the total number of indexed grains.

Texture ratio of one half

Use a recrystallized sheet with 3% of the grains in the {001}<001> window and 6% in the {011}<001> window. Apply the 15° window to both populations, which gives a ratio of 0.50.

Grain counts on sheet plane

Polish a surface parallel to the rolling plane at mid-thickness and map it by electron backscatter diffraction. Reconstruct grains from the indexed pixels, assign each grain a mean orientation, and divide the count in each 15° window by the total indexed grain count.

Grain counts across sheet thickness

Map several full-thickness sections parallel to the rolling direction by electron backscatter diffraction and express the orientations in the sheet reference frame. Pool the reconstructed grain counts from the sections and classify each grain using its minimum misorientation from the symmetry-related orientations for each 15° window.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2007/0234542 A1
Published
Oct 11, 2007
Filed
Aug 20, 2004
Class
B21C 1/00
Document BUS 2018/0363103 A1
Published
Dec 20, 2018
Filed
Aug 24, 2018
Class
C22C 21/00
Claim 1
Document A
Document B
1.1V{001}<001>/V{011}<001>≤0.65 [Equation 1]
In one embodiment, the ratio of the area fraction of brass oriented grains (BVF) to the area fraction of Goss oriented grains (GVF) in a recrystallized aluminum alloy is at least about 1.5:1 (BVF:GVF).
B · US 2018/0363103 A1 · ¶ 78
1.2(In Equation 1, V{001}<001> represents the fraction of grains with a crystal orientation within 15° of {001}<001>, and V{011}<001> represents the fraction of grains with a crystal orientation within 15° of {011}<001>.)
Texture annealing at 1100° C. over a period of 60 minutes results in a high-grade recrystallization cube texture which constitutes a share of 94.3% in the structure (FIG. 1), 93.1% of all grain boundaries being small-angle grain boundaries with a misorientation <10° (white in FIG. 1).
A · US 2007/0234542 A1 · ¶ 33
The crystal orientation maps assumes Euler angles of φ1=35° Φ=45° φ2=0° (±15° misorientation angle) for the brass texture component and φ1=0° Φ=45° φ2=0° (±15° misorientation angle) for the Goss texture component.
B · US 2018/0363103 A1 · ¶ 68

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document B has a passage for 1.1. Both have a passage for 1.2.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

There is no universally valid theory concerning the effects of strain and deformation states on the formation of forming and annealing textures of metals, or in particular for nickel, copper, gold, and silver.
A · US 2007/0234542 A1 · ¶ 6

Related claim parts: 1.1

The object of the invention is to provide a method for producing metallic flat wires or strips with a cube texture, by means of which the products have a high-grade cube texture after the last forming step and the final annealing treatment.
A · US 2007/0234542 A1 · ¶ 8
Such substrate strips for coated superconductors may be used in superconducting magnets, transformers, motors, tomography instruments, or superconducting current paths, i.e., cables.
A · US 2007/0234542 A1 · ¶ 1
The aluminum alloy products may exhibit an improved strength to toughness relationship compared to conventional products produced with conventional methods.
B · US 2018/0363103 A1 · ¶ 3
In other embodiments, the sheet product is employed in automotive, transportation or other industrial applications.
B · US 2018/0363103 A1 · ¶ 6
Cite aspatent.fyi, US 2026/0366095 A1, claim 1, first published 2026-11-23T20:11:03-05:00, https://patent.fyi/US20260366095/, SHA-256 2ca32a4ad1f9062d465f0b38b1cb1fc41334f9bf4281a040e4b3d2d7de8ead62
First published
Permanent addresshttps://patent.fyi/US20260366095/
Content fingerprint (SHA-256)2ca32a4ad1f9062d465f0b38b1cb1fc41334f9bf4281a040e4b3d2d7de8ead62
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi