Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Temper after final quenching
What ifWhat if the finished sheet contained zero fresh martensite after a tempering pass that follows the final quench?
Claim language“fresh martensite 5%: or less (excluding 0%)”
The final quench converts susceptible austenite to martensite. A subsequent low-temperature tempering pass relieves transformation stresses and reduces the hardness of the newly formed martensite before the strip cools to room temperature.
1.1Bainitic ferrite forms the matrix
What ifWhat if bainitic ferrite formed the load-bearing matrix of the sheet?
Claim language“tempered martensite: 75% or more and less than 95%”
The strip cools from the austenite region to an isothermal hold above the martensite start temperature, where fine bainitic ferrite plates form. Carbon enriches the austenite between the plates, and the fine plate structure provides strength while the retained austenite accommodates deformation.
1.2Direct transverse bend qualification
What ifWhat if sheet acceptance used a minimum crack-free bend radius and tensile strength without applying a retained-austenite ratio limit?
Claim language“relational expression 1 is satisfied”
A punch bends a strip coupon with its bend axis parallel to the rolling direction, placing the outer surface in transverse tension. The smallest punch radius that produces a crack-free outer surface at the specified bend angle sets the bend result, and a separate tensile coupon verifies strength.
What ifWhat if a continuous transformation curve replaced the separate unstable and stable retained-austenite fractions?
Claim language“a fraction of unstable retained austenite”
X-ray diffraction measures total retained austenite on the same gauge section at successive strain levels during interrupted tensile loading. The change in austenite fraction per increment of plastic strain shows where transformation accelerates or slows.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Formed stiffeners for appliance cabinets
The cold rolled sheet forms hat-section stiffeners behind the side panels of commercial appliance cabinets. A roll former bends the strip in successive passes, and a cutoff shear cuts the formed section to length. The section flanges attach to the cabinet frame with mechanical fasteners, and the raised web increases out-of-plane stiffness.
Component substitution
Nickel replaces boron for hardenability
The steel contains 0.5 to 1.0 wt% nickel in place of the intentional boron addition. Nickel contributes to hardenability and lowers the martensite start temperature. Dilatometry on the modified chemistry establishes the martensite start temperature, and the continuous annealing line sets the interrupted quench temperature below that point to form the initial martensite fraction. Reheating tempers that martensite and permits carbon to partition into the remaining austenite before final cooling.
Parameter or scale variation
Gauge dependent quench control for strip
A continuous annealing line processes the sheet at two nominal thicknesses, 0.8 mm and 1.6 mm. Opposed gas jets cool both faces during interrupted quenching, and the line controller stores a separate jet flow and strip speed recipe for each thickness. Exit pyrometers measure strip temperature before reheating, and the controller adjusts jet flow to hold the selected quench endpoint for each gauge.
Combination with existing systems
Tempered strip with electrolytic zinc coating
An electrolytic zinc coating line receives the cold rolled strip after the heat treatment and final cooling that establish its phase balance. Alkaline cleaning and acid activation prepare both faces, and strip contact rolls supply cathodic current through successive zinc plating cells. The line sets zinc mass per unit area through cell current and strip speed, then rinses and dries the plated strip.
Laser welded blanks with tailored gauges
A laser blank welding cell joins cold rolled sheet of one gauge to a thinner low-carbon steel sheet along a straight butt seam. Clamps align the blank edges, and a traversing laser produces a continuous weld through the joint thickness. The press tooling positions the tempered martensitic sheet in the load-bearing region, the softer sheet in the deeper draw region, and the seam away from the tightest bend.
Automated or data-driven variant
Model control of partitioning conditions
A process controller receives strip temperature from pyrometers at the quench exit and partitioning furnace exit, together with strip thickness, speed and heat chemistry. A model calibrated with dilatometry and phase measurements estimates the tempered martensite fraction and the retained austenite fractions before and after a defined tensile prestrain. The controller updates quench gas flow and partitioning furnace power within preset limits to hold the phase targets. Offline X-ray diffraction measurements before and after the same prestrain supply periodic model checks.
Specific version of a part
Tempered martensite with interlath austenite
The sheet contains 82 area % tempered martensite, 7 area % ferrite, 2 area % fresh martensite, 6 area % retained austenite, and 3 area % bainite. Part of the retained austenite sits in thin films between tempered martensite laths.
Retained austenite ratio of 1.6
Stable retained austenite occupies 5 area % of the sheet microstructure, and unstable retained austenite occupies 3 area %. The two fractions sum to 8 area %, which gives a ratio of 1.6 when divided by the stable fraction.
Classification at five percent strain
X-ray diffraction measures retained austenite in the gauge section before loading and after 5% tensile plastic strain. Under this test definition, the decrease gives the unstable fraction and the remaining austenite gives the stable fraction.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1wherein a microstructure includes, in area %, ferrite: 15% or less (excluding 0%), fresh martensite 5%: or less (excluding 0%), tempered martensite: 75% or more and less than 95%, retained austenite: 12% or less (excluding 0%), and a balance of bainite, and
The area fraction of the tempered martensite phase, which is the primary phase, is 75% or more.
A · US 2018/0237880 A1 · ¶ 50
Thus, the total area fraction of tempered martensite and carbide-containing bainite is 70% to 97%. The lower limit is preferably 75% or more, more preferably 80% or more.
B · US 2020/0165708 A1 · ¶ 41
1.2the following relational expression 1 is satisfied, (RAunstable+RAstable)/RAstable≤2.0 [Relational Expression 1]
1.3where RAunstable refers to a fraction of unstable retained austenite, and RAstable refers to the fraction of stable retained austenite.
Although the mechanism is not entirely clear, we believe that unstable retained austenite in a deformation stress concentrated portion changes immediately into martensite in axial compression and promotes strain propagation. Less than 1% of unstable retained austenite is insufficient for such an effect.
B · US 2020/0165708 A1 · ¶ 44
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document B has a passage for 1.3. Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
However, higher-strength materials often have poorer workability.
B · US 2020/0165708 A1 · ¶ 2
Related claim parts: 1.1
In recent years, from the viewpoint of global environmental protection, improvements in automotive fuel efficiency have been directed in the whole automotive industry for the purpose of regulating CO2 emissions.
A · US 2018/0237880 A1 · ¶ 2
Automotive weight reduction by the gauge reduction of parts used is most effective in improving the fuel efficiency of automobiles.
A · US 2018/0237880 A1 · ¶ 2
From the perspective of assembly and performance of parts, parts should have good spot welds and stable axial compression characteristics.
B · US 2020/0165708 A1 · ¶ 2
Cite aspatent.fyi, US 2026/0366096 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366096/, SHA-256 53ef4c30becaf9791ee2d4e280b59fa8d145a41f0ccb8a873750ec17b282c7eb