United States Patent Application Publication

US 2026/0366097 A1

Published
Nov 19, 2026
Filed
Dec 4, 2023
Earliest date on the face
Dec 19, 2022
Classification
C21D 9/46
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.2Low chromium-to-manganese ratio with casting control

What ifWhat if the chromium-to-manganese weight ratio is kept below 1.0 using 1.2 to 1.6% manganese and 0.2 to 0.6% chromium?
Claim language“2.0<Cr/Mn<6.5 [Relational Expression 2]”

Setting manganese at 1.4% and chromium at 0.4% maintains through-thickness hardenability in heavy sections via substitutional solid-solution strengthening and lowered transformation temperatures. Electromagnetic stirring during continuous casting and mechanical soft reduction near the solidification end limit centerline manganese segregation, preserving core impact energy at subzero temperatures.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Thick alloy steel plates for cold-region mining excavators

The nickel-chromium-molybdenum steel plate is fabricated into structural boom boxes, dipper sticks, and revolving upper frames for surface mining excavators operating at ambient temperatures down to -50 °C. Plates with thicknesses between 140 mm and 240 mm are cut by plasma or oxy-fuel torches, beveled along weld edges, and joined by submerged-arc welding using low-hydrogen nickel-alloyed filler wire at a preheat temperature of 150 °C. After assembly, the welded box sections undergo post-weld stress-relief annealing at 560 °C for 2 hours to reduce residual weld stresses without lowering base-metal hardness. The resulting structural members transfer cyclic digging loads and resist brittle fracture under sub-zero impact loading in open-pit operations.

Component substitution

Partial tungsten substitution for molybdenum in alloy steel

In this steel composition, 0.2 to 0.4 weight percent tungsten and 0.015 to 0.035 weight percent niobium replace half of the molybdenum content, reducing molybdenum to 0.2 to 0.3 weight percent while maintaining the remaining carbon, silicon, manganese, chromium, and nickel concentrations. During slab reheating at 1150 °C and hot rolling, niobium forms fine carbonitride precipitates that pin austenite grain boundaries and refine the final packet size across plate thicknesses of 140 to 280 mm. Tungsten partitions into the ferrite matrix and carbide phases during water quenching and tempering at 600 °C, retarding carbide coarsening and preserving through-thickness hardenability. The alloy index calculated with half the tungsten weight percent added to the molybdenum term remains below 0.95, and the chromium-to-manganese mass ratio remains between 2.0 and 6.5.

Cobalt and vanadium replacing part of nickel content

In this alloy variant, 1.0 to 1.5 weight percent cobalt and 0.04 to 0.08 weight percent vanadium substitute for a portion of the nickel content, lowering nickel to 2.0 to 2.8 weight percent while keeping carbon, silicon, manganese, chromium, and molybdenum within their base ranges. During melting and vacuum degassing, cobalt dissolves uniformly in the iron matrix without forming brittle intermetallic phases, raising the martensite-start temperature across plate thicknesses of 150 to 260 mm. Following water quenching from 880 °C, tempering at 580 °C precipitates fine vanadium carbides that increase yield strength while cobalt suppresses dislocation recovery in the tempered martensite laths. The resulting composition keeps the combined carbon, manganese, chromium, molybdenum, vanadium, copper, and nickel index below 0.95 and maintains a chromium-to-manganese mass ratio between 2.0 and 6.5.

Parameter or scale variation

Ultra-thick plates with two-stage tempering cycles

The cast slab is hot-rolled with a reduction ratio of at least 3.0 to produce an ultra-thick plate measuring between 305 mm and 420 mm in thickness while retaining the nickel-chromium-molybdenum alloy balance. Following austenitizing at 890 °C for 2.5 minutes per millimeter of thickness, the plate undergoes high-pressure water-jet quenching at a surface cooling rate of 25 °C per second down to 120 °C to suppress ferrite formation at the mid-thickness plane. The quenched plate then receives a double-stage tempering treatment consisting of a first hold at 640 °C for 180 minutes, air cooling to ambient temperature, and a second hold at 590 °C for 120 minutes. This thermal schedule relieves deep quenching stresses across the thicker cross-section and decomposes retained austenite into fine carbides and tempered lath structures.

Combination with existing systems

Clad steel plate with austenitic stainless surface layer

The thick nickel-chromium-molybdenum backing plate is metallurgically bonded to a 4 mm to 10 mm thick austenitic stainless steel cladding layer containing 18 weight percent chromium and 10 weight percent nickel. An intermediate nickel-foil barrier of 0.1 mm thickness is placed between the ground backing slab and the cladding plate, and the assembly is perimeter-welded, evacuated to 0.1 Pa, and hot-roll bonded at 1120 °C. After roll bonding, the composite plate undergoes quenching and tempering tailored to the backing steel, followed by pickling and passivation of the stainless surface. The composite structure pairs the load-bearing strength and low-temperature toughness of the thick ferritic backing with continuous corrosion resistance against seawater and sour chemical media.

Automated or data-driven variant

Closed-loop cooling control using infrared thermal imaging

An automated accelerated-cooling line equips the quenching zone with top and bottom infrared pyrometer arrays, plate-speed encoders, and individually actuated laminar-flow water valves spaced along the roller table. A real-time finite-difference heat-transfer model receives the measured alloy composition from optical emission spectroscopy, the ultrasonic thickness profile, and live surface temperatures to compute the temperature distribution at the quarter-thickness and mid-thickness planes. A feedback controller adjusts water flow rates and roller speeds zone by zone so the mid-thickness cooling curve passes through the target martensite-bainite transformation window without over-cooling the plate edges. After quenching, an automated ultrasonic phased-array scanner maps internal soundness and logs the thermal history alongside mechanical test data to update the heat-transfer coefficients for subsequent plates.

Specific version of a part

Bonded thinner plates replacing monolithic thickness

Three 60 mm quenched-and-tempered steel plates undergo surface grinding, vacuum edge welding, and hot isostatic pressing at 1050 °C and 100 MPa to form a 180 mm bonded section. Because each individual plate experiences a higher core cooling rate during water quenching prior to assembly, the finished section exhibits uniform through-thickness toughness and reduced centerline segregation.

Automated spectrometer feedback for dual expressions

During secondary steelmaking, an optical emission spectrometer samples the molten bath every 10 minutes and feeds measured weight percentages into a process controller that computes both relational expressions in real time. Automated ferroalloy hoppers trim chromium, manganese, and molybdenum additions until the first expression reaches 0.88 and the chromium-to-manganese ratio settles at 3.8 before continuous casting begins.

Heavy 220 mm quenched steel plate

A continuous-cast slab of 400 mm thickness is hot rolled to a 220 mm plate containing 0.16% C, 0.40% Mn, 1.50% Cr, 0.50% Mo, 3.80% Ni, and 0.10% Cu, yielding a first-expression value of 0.89 and a chromium-to-manganese ratio of 3.75. After austenitizing at 890 °C, high-pressure water-jet quenching and tempering at 610 °C produce a tempered bainite-martensite microstructure at the quarter-thickness and center-thickness positions.

Combustion and spectroscopic weight percentage verification

Elemental weight percentages for both relational expressions are measured from solid plate turnings taken at the quarter-thickness position using combustion infrared absorption for carbon and sulfur, inert-gas fusion for nitrogen, and inductively coupled plasma optical emission spectroscopy for metallic alloying elements. Each reported mass fraction is expressed as a percentage of total sample mass prior to substitution into the two expressions.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2011/0253271 A1
Published
Oct 20, 2011
Filed
Oct 13, 2009
Class
C21D 8/02
Document BUS 2018/0355452 A1
Published
Dec 13, 2018
Filed
Jan 15, 2015
Class
C21D 9/46
Claim 1
Document A
Document B
1.1wherein the steel plate satisfies the following Relational Expression 1 and Relational Expression 2, and
A weld crack sensitivity index Pcm of the high-strength steel plate is calculated by Pcm=[C]+[Si]/30+[Mn]/20+[Cu]/20+[Ni]/60+[Cr]/20+[Mo]/15+[V]/10+5[B], and is 0.39 mass % or less.
A · US 2011/0253271 A1 · abstract
1.2has a thickness of more than 133 mm and 300 mm or less, C+Mn/6+(Cr+Mo+V)/5+(Cu+Ni)/15<0.95 [Relational Expression 1] 2.0<Cr/Mn<6.5 [Relational Expression 2]
1.3in Relational Expression 1 and 2 above, each element refers to a content (weight %).
and is 0.39 mass % or less, where [C], [Si], [Mn], [Cu], [Ni], [Cr], [Mo], [V], and [B] are the concentrations (mass %) of C, Si, Mn, Cu, Ni, Cr, Mo, V, and B, respectively, an Ac3 transformation point is equal to or less than 850° C., a percentage value of a martensite structure is equal to or greater than 90%, a yield strength is equal to or greater than 1300 MPa, and a tensile strength is equal to or greater than 1400 MPa and equal to or less than 1650 MPa, a prior austeni
A · US 2011/0253271 A1 · ¶
Weight percentages of components thereof are: C: 0.06-0.13 wt. %, Si: 0.05-0.70 wt. %, Mn: 1.20-2.30 wt. %, Mo: 0-0.25 wt. %, Nb: 0.03-0.11 wt. %, Ti: 0.002-0.050 wt. %, Al: 0.02-0.15 wt. %, and B: 0-0.0020 wt. %, where 2Si+3Mn+4Mo≤8.5, and others being Fe and inevitable impurities.
B · US 2018/0355452 A1 · abstract

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.1. Both have a passage for 1.3. Both are classified in CPC C21D, as is this patent.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Therefore, in order to ensure the strength, additional alloy elements are needed.
A · US 2011/0253271 A1 · ¶ 8

Related claim parts: 1.3

Accordingly, in particular, a steel plate having a yield strength of 1300 MPa-class (and a tensile strength of 1400 MPa-class) requires a high delayed fracture resistance.
A · US 2011/0253271 A1 · ¶ 6
Therefore, the steel plate requires usability that is not lower than an existing high-strength steel of 1100 MPa-class.
A · US 2011/0253271 A1 · ¶ 6
Cite aspatent.fyi, US 2026/0366097 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366097/, SHA-256 1609a755602058217e88f1b27e1466329affaa8c8160a31f4aa9fa6cb189a418
First published
Permanent addresshttps://patent.fyi/US20260366097/
Content fingerprint (SHA-256)1609a755602058217e88f1b27e1466329affaa8c8160a31f4aa9fa6cb189a418
Methodv2026-11-18.2 · automated, not reviewed by a person