patent.fyi
Applications  /  US 2026/0366104
United States Patent Application Publication

US 2026/0366104 A1

Published
Nov 19, 2026
Filed
Jun 30, 2026
Earliest date on the face
Jan 8, 2024
Classification
C22C 21/08
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Lower silicon through charge blending

What ifWhat if the melt targets 0.12 wt. % silicon through charge blending?
Claim language“0.15 wt. % to 0.30 wt. %”

The furnace charge combines low-silicon aluminum with segregated aluminum-magnesium scrap. The lower silicon content limits the amount of magnesium tied up as magnesium silicide, leaving more magnesium in solid solution for strengthening.

1.2Lower iron through feedstock sorting

What ifWhat if the melt targets 0.18 wt. % iron by using scrap streams sorted by measured iron content?
Claim language“0.20 wt. % to 0.35 wt. %”

Spark optical emission analysis identifies scrap lots with low iron content before charging. The lower melt iron content limits the volume of iron-rich intermetallic particles that form during solidification.

1.3Low copper with strain hardening

What ifWhat if the alloy contains 0.01 wt. % copper and the final cold-rolling pass supplies additional strength?
Claim language“0.02 wt. % to 0.10 wt. %”

The furnace charge uses low-copper aluminum-magnesium scrap and low-copper aluminum. A final cold-rolling pass reduces sheet thickness by 15 percent after intermediate annealing, increasing dislocation density and raising yield strength.

1.4Higher manganese for dispersoid formation

What ifWhat if the alloy targets 0.50 wt. % manganese to control recrystallization during sheet processing?
Claim language“0.35 wt. % to 0.45 wt. %”

An aluminum-manganese master alloy sets the manganese content before casting. Homogenization near 500 °C promotes manganese-bearing dispersoid formation, and the dispersoids impede grain boundary motion during subsequent thermal processing.

1.5Higher magnesium for solution strengthening

What ifWhat if the alloy targets 4.20 wt. % magnesium?
Claim language“3.00 wt. % to 3.60 wt. %”

An aluminum-magnesium master alloy brings the melt to the target magnesium content before slab casting. Magnesium dissolved in the aluminum matrix impedes dislocation motion and supplies solid-solution strengthening after rolling and annealing.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Formed panels for irrigation pump enclosures

The aluminum-magnesium alloy with a scrap absorption score of at least 16 forms the side panels of an irrigation pump enclosure. A press brake bends return flanges along the panel edges, and the panel blanks carry punched openings for fasteners and louvers. The return flanges stiffen the panels and provide mounting surfaces for attachment to the enclosure frame.

Component substitution

Magnesium master alloy for melt adjustment

A master alloy containing 50 wt. % magnesium and 50 wt. % aluminum replaces elemental magnesium as the charge material for magnesium adjustment. The furnace operator calculates the addition mass from the measured melt composition, the magnesium recovery measured in previous heats, and the aluminum introduced by the master alloy. The master alloy is submerged in the melt, and a sample taken after mixing confirms a magnesium content of 3.00 to 3.60 wt. % before casting.

Parameter or scale variation

Composition target for low titanium heats

The melt targets 0.27 wt. % Si, 0.32 wt. % Fe, 0.06 wt. % Cu, 0.40 wt. % Mn, 3.45 wt. % Mg, 0.06 wt. % Cr, and 0.06 wt. % Zn, with Ti at or below 0.02 wt. %. Aluminum makes up the balance with residual impurities limited to 0.05 wt. % individually and 0.15 wt. % in total. At the target composition, Si and Fe contribute 12 points and Cu, Mn, Cr, and Zn contribute 8 points, yielding a score of 20 with zero points from Ti.

Two sheet gauges from one heat

One cast heat with a scrap absorption score of at least 16 supplies hot-rolled strip at 3.0 mm thickness. The cold mill reduces one portion to 1.5 mm and a second portion to 1.0 mm, giving total cold reductions of 50% and about 67%, respectively. The mill distributes each reduction over successive passes and uses an exit thickness gauge to control the final pass. Tensile tests at each gauge measure the strength and elongation associated with its cold reduction.

Combination with existing systems

Alloy production with a scrap return loop

A sheet stamping line returns its trim and rejected blanks to the remelt furnace that supplies the casting and rolling line. Dedicated bins keep the alloy returns separate from other grades, and a scale records each return lot before it enters the furnace charge. The melt shop combines the measured returns with other scrap and aluminum feed, then checks furnace samples against the composition limits and the 16-point minimum before casting.

Automated or data-driven variant

Software selection of furnace charge blends

A mixed-integer linear optimizer selects scrap lot masses and aluminum and master alloy additions from inventory records with measured elemental mass fractions. Elemental mass balances account for estimated recovery, and binary variables represent the scoring bands for Si, Fe, Cu, Mn, Cr, Zn, and Ti. The optimizer maximizes scrap mass at a fixed melt mass while enforcing the composition limits and a score of at least 16. After melting and mixing, the controller computes the score from an optical emission spectrometry measurement and checks the measured chemistry before releasing the heat for casting.

Specific version of a part

Chromium addition through master alloy

The furnace charge includes an aluminum master alloy containing 10 wt. % chromium to target 0.06 wt. % chromium in the melt. Spark optical emission analysis of a solidified melt sample verifies the chromium content after mixing.

Zinc from blended scrap lots

A charge calculation blends scrap lots of measured zinc content with low-zinc aluminum to target 0.12 wt. % zinc in the melt. The zinc enters through the scrap feed, and analysis of a solidified melt sample verifies the final concentration.

Titanium addition for grain refinement

An aluminum-titanium-boron master alloy rod feeds into the melt stream upstream of the casting mold and brings the total titanium content to 0.025 wt. %. Titanium diboride particles introduced with the rod provide nucleation sites for aluminum grains during solidification.

Residual elements controlled by blending

The charge calculation tracks residual nickel, lead, tin, and other unlisted elements and uses low-residual aluminum to dilute them. Analysis of a solidified melt sample verifies that each residual element is at most 0.05 wt. %, their sum is at most 0.15 wt. %, and aluminum forms the balance.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2008/0145266 A1
Published
Jun 19, 2008
Filed
Jun 13, 2007
Class
C22C 21/14
Document BUS 2019/0071748 A1
Published
Mar 7, 2019
Filed
Mar 10, 2017
Class
C21D 9/52
Claim 1
Document A
Document B
1.1Si: 0.15 wt. % to 0.30 wt. %,
1.2Fe: 0.20 wt. % to 0.35 wt. %,
1.3Cu: 0.02 wt. % to 0.10 wt. %,
1.4Mn: 0.35 wt. % to 0.45 wt. %,
A method for temperature-treating a manganese steel intermediate product whose alloy includes: a manganese content, which lies in the following manganese range: 3 wt. %≤Mn≤12 wt. %, a fraction of one or more alloying elements of the group: silicon (Si), aluminum (Al), nickel (Ni), chromium (Cr), molybdenum (Mo), phosphorus (P), sulfur (S), nitrogen (N), copper (Cu), boron (B), cobalt (Co), tungsten (W), an optional carbon content (C) of less than 1 wt. %, an optional content
B · US 2019/0071748 A1 · abstract
1.5Mg: 3.00 wt. % to 3.60 wt. %,
1.6Cr: 0.02 wt. % to 0.10 wt. %,
Preferably the Cr content should be in the range of up to about 0.25%, and preferably about 0.05 to 0.25%, more preferably about 0.08 to 0.19%.
A · US 2008/0145266 A1 · ¶ 28
1.7Zn: at most 0.20 wt. %,
1.8Ti: at most 0.05 wt. %,
1.9remainder Al and unavoidable impurities, individually at most 0.05 wt. %, in total at most 0.15 wt. %,
1.10wherein
1.11the aluminum alloy achieves a total score of at least 16 points in an evaluation for the scrap absorption capacity, wherein the total score is obtained from the sum of the scores for the contents of Si, Fe, Cu, Mn, Cr, Zn and/or Ti of the aluminum alloy as follows:
1.12Si content: <0.15 wt. % gives 0 points, 0.15 wt. % to <0.25 wt. % gives 3 points, ≥0.25 wt. % gives 6 points, Fe content: <0.25 wt. % gives 0 points, 0.25 wt. % to <0.30 wt. % gives 3 points, ≥0.30 wt. % gives 6 points, Cu content: <0.03 wt. % gives 0 points, 0.03 wt. % to <0.05 wt. % gives 1 point, ≥0.05 wt. % gives 2 points, Mn content: <0.25 wt. % gives 0 points, 0.25 wt. % to <0.35 wt. % gives 1 point, ≥0.35 wt. % gives 2 points, Cr content: <0.03 wt. % gives 0 points, 0.03 wt. % to <0.05 wt. % gives 1 point, ≥0.05 wt. % gives 2 points, Zn content: <0.03 wt. % gives 0 points, 0.03 wt. % to <0.05 wt. % gives 1 point, ≥0.05 wt. % gives 2 points, Ti content: <0.03 wt. % gives 0 points, 0.03 wt. % to <0.05 wt. % gives 1 point, ≥0.05 wt. % gives 2 points.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.6. Only Document B has a passage for 1.4.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

These known alloys lack, however, sufficient strength for most structural aerospace applications.
A · US 2008/0145266 A1 · ¶ 5
Depending on the design criteria for a particular aircraft component, improvements in strength, fracture toughness and fatigue resistance result in weight savings, which translate to fuel economy over the lifetime of the aircraft, and/or a greater level of safety.
A · US 2008/0145266 A1 · ¶ 5
It also relates to a specific alloy of a manganese steel intermediate product, which is temperature-treated by a special process to achieve a significantly reduced Lüders strain.
B · US 2019/0071748 A1 · ¶ 1
It is therefore necessary to find an optimal compromise between the total elongation A80 and the tensile strength Rm for each application.
B · US 2019/0071748 A1 · ¶ 7
Cite aspatent.fyi, US 2026/0366104 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366104/, SHA-256 8b859e5c924b7f36b6aae453e80362d326a0c103442c0e1f1b812f84f9d83a29
First published
Permanent addresshttps://patent.fyi/US20260366104/
Content fingerprint (SHA-256)8b859e5c924b7f36b6aae453e80362d326a0c103442c0e1f1b812f84f9d83a29
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi