Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Polymer bonding of melt-spun flakes
What ifWhat if rapid solidification and polymer bonding produce the magnet from a single alloy melt?
Claim language“mixing, pulverizing, shaping and sintering”
A rotating copper wheel quenches the melt into a fine-grained magnetic ribbon. The ribbon is crushed into flakes, compounded with a thermoplastic binder, and injection molded so the solidified polymer holds the magnetic particles together.
1.4Lower main alloy iron content
What ifWhat if the main alloy contains 77.8 atomic percent iron?
Claim language“e is 78-80”
The melt contains 15 atomic percent total rare earths, 5.5 atomic percent boron, and 1.7 atomic percent combined aluminum, copper, gallium, zirconium, and titanium. The iron and boron form the hard magnetic phase, while excess rare earth supplies liquid for densification during sintering.
1.5Binary neodymium-copper auxiliary alloy
What ifWhat if a binary neodymium-copper alloy supplies the auxiliary powder?
Claim language“has a composition of RmFenCuoAlp”
An auxiliary powder containing about 70 atomic percent neodymium and 30 atomic percent copper melts during sintering and wets the magnetic grains. On cooling, the liquid forms neodymium-rich boundary phases that reduce magnetic exchange between neighboring grains.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Permanent magnets for magnetic couplings
The main and auxiliary alloy powders are mixed, pulverized, magnetically aligned, pressed into arc segments, and sintered. A heavy rare earth diffusion source is applied to both broad faces of the segments before grain boundary heat treatment. The segments are magnetized through their thickness and mounted with alternating radial polarity on concentric rotors. The rotors transmit torque across a stationary nonmagnetic containment sleeve in a sealed pump.
Component substitution
Vapor deposition replaces slurry coating
A sputtered terbium film replaces a slurry-applied diffusion source on the sintered body. An argon magnetron with a metallic terbium target deposits the film on one broad face, and a rotating fixture exposes the opposite face for a second deposition. A subsequent vacuum heat treatment drives terbium from the films into the grain boundaries and enriches the outer regions of adjacent magnetic grains.
Strip casting replaces ingot crushing
A water-cooled copper wheel replaces a stationary ingot mold and primary crusher in the main alloy feedstock line. The molten main alloy is poured onto the rotating wheel under argon and solidifies as thin flakes. Hydrogen decrepitation breaks up the flakes, and dehydrogenation prepares the crushed feedstock for mixing with the separately powdered auxiliary alloy. The mixed feedstock is jet milled, aligned, pressed, and sintered before grain boundary diffusion.
Parameter or scale variation
Double sided diffusion in thin plates
Sintered blanks are ground into plates 1.5 to 2.5 mm thick before source application. Equal masses per unit area of a heavy rare earth diffusion source are deposited on the two broad faces. The plates sit edge-on in a furnace rack with at least 3 mm between neighboring plates during vacuum heat treatment. The two coated faces supply diffusion fronts with a face-to-midplane distance of 0.75 to 1.25 mm.
Combination with existing systems
Diffusion treated segments in laminated rotors
The two-alloy powder blend is aligned, pressed, and sintered into rectangular segments sized for the magnet pockets of a laminated interior permanent magnet rotor. The segments undergo grain boundary diffusion on both broad faces before final grinding and insertion. A fixture inserts the segments into paired V-shaped pockets in the electrical steel stack, where retaining resin secures them. A pulse fixture magnetizes the installed segments across their thickness to establish alternating rotor poles.
Automated or data-driven variant
Gravimetric control of diffusion source loading
A machine vision camera measures the exposed face area of each sintered blank, and an inline balance records its mass before coating. A controller converts a specified dry source mass per unit area into a dispense quantity using the measured slurry solids fraction. The line dispenses and dries the coating, reweighs the blank, and adds a correction dose when the dry mass gain falls below the setpoint. A turnover fixture presents the opposite face for the same sequence before the blanks enter the diffusion furnace.
Specific version of a part
Jet milling and field pressing
A nitrogen jet mill pulverizes the blended main and auxiliary alloy powders to a median particle size of about 4 micrometers. A magnetic field aligns the particles during die pressing, and vacuum sintering densifies the compact.
Cerium and lanthanum addition
Cerium and lanthanum make up the RE component in a four-to-one atomic ratio. The two metals enter the main alloy melt with praseodymium and neodymium before strip casting.
Neodymium-rich auxiliary composition
The auxiliary alloy contains 50 atomic percent neodymium, 38 atomic percent iron, 6 atomic percent copper, and 6 atomic percent aluminum. The alloy is cast and crushed into powder for blending with the main alloy.
Two-face terbium diffusion
A terbium-rich alloy slurry coats both broad faces of a 2 millimeter thick sintered plate. After drying, the plate is held at about 900 °C under vacuum to drive terbium along grain boundaries and into the outer regions of the hard magnetic grains.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1(1) subjecting a powder of a main alloy and a powder of an auxiliary alloy to mixing, pulverizing, shaping and sintering,
The method includes: 1) providing a master alloy and an auxiliary alloy, the master alloy being a Nd—Fe—B alloy ingot or cast strip, the auxiliary alloy being a heavy rare earth alloy; 2) breaking up the master alloy using a hydrogen decrepitation process to yield a crude powder, conducting hydrogen absorption treatment on the auxiliary alloy and breaking up the hydrogenated auxiliary alloy to yield hydride particles; 3) uniformly mixing and stirring the crude powder of the m
A · US 9,728,311 B2 · abstract
Specifically, in the present invention, a sintered body, comprising 27 to 36 wt % of RE, 64 to 73 wt % of Fe, 0 to 5 wt % of TM, and more than 0 wt % and not more than 2 wt % of B, and produced through an alloy manufacturing process→a powder preparation process→a magnetic field molding process→a sintering process among rare earth magnet production processes, may be used as a starting material.
B · US 2019/0385790 A1 · ¶ 43
1.2wherein the main alloy has a composition of (REaPrbNdc)dFeeAlfCugGahZriTijBk;
To achieve the above objects, the present invention provides a method for producing a heavy rare earth grain-boundary-diffused RE-Fe—B-based rare earth magnet, the method including: step S1 of processing a rare earth magnet sintered body having a composition of RE-Fe-TM-B (where RE=rare earth element, Fe=iron, TM=3d transition metal, and B=boron) according to the specification of the magnet product, and cleaning the processed sintered body by degreasing, pickling and solvent
B · US 2019/0385790 A1 · ¶ 21
1.3RE is a high-abundance rare earth element; RE comprises one or more of La, Ce, Y, Er, Yb, Gd, Tm and Sm;
1.4in terms of atomic percentage, a is 0.05-0.3; b is 0.1-1.2; c is 0.5-0.9; d is 13-15; e is 78-80; f is 0.2-0.4; g is 0.1-0.3; h is 0.2-0.5; i is 0.2-0.4; j is 0.2-0.4; k is 5-6;
1.5wherein the auxiliary alloy has a composition of RmFenCuoAlp;
1.6R is a rare earth element;
To achieve the above objective, in accordance with one embodiment of the invention, there is provided a method for preparing a Nd—Fe—B based sintered magnet, the method comprising: 1) providing a master alloy and an auxiliary alloy, the master alloy being a Nd—Fe—B alloy ingot or cast strip, the auxiliary alloy being a heavy rare earth alloy having a formula of RaMbFe100−a−b, wherein R represents Gd, Tb, Dy, Ho, or a mixture thereof, M represents Co, Mn, Cu, Al, Ti, Ga, Zr, V
A · US 9,728,311 B2 · ¶ 8
1.7in terms of atomic percentage, m is 45-55; n is 35-45; o is 4-8; p is 4-8;
1.8(2) subjecting a sintered body obtained in step (1) and a diffusion source raw material composition to grain boundary diffusion treatment;
It is a method in which a sintered magnet is produced according to a conventional method, and then a heavy rare earth compound is applied to the surface of the magnet by various methods, including powder application, deposition and plating, and heated to a temperature of 700° C. or higher in an argon or vacuum atmosphere so that the heavy rare earth applied to the magnet surface is gradually diffused along the magnet grain boundaries and penetrated into the magnet.
B · US 2019/0385790 A1 · ¶ 13
1.9wherein, in terms of atomic percentage, the diffusion source raw material composition comprises a heavy rare earth element with a content of more than m.
A method for producing a heavy rare earth grain-boundary-diffused RE-Fe—B-based rare earth magnet according to the present invention may comprises: step S1 of processing a rare earth magnet sintered body having a composition of RE-Fe-TM-B (where RE=rare earth element, Fe=iron, TM=3d transition metal, and B=boron) according to the specification of the magnet product, and cleaning the processed sintered body by degreasing, pickling and solvent cleaning; step S2 of applying, to
B · US 2019/0385790 A1 · ¶ 40
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.6. Only Document B has a passage for 1.21.81.9. Both have a passage for 1.1. Both are classified in CPC H01F.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
To improve the comprehensive magnetic performance and the coercivity of the Nd—Fe—B based sintered magnet, a dual-alloy technology is employed to control Dy to be distributed mainly in the vicinity of the grain boundary.
A · US 9,728,311 B2 · ¶ 6
Related claim parts: 1.81.9
On the other hand, the heavy rare earth hydrides must be milled into superfines, which involves a complex and difficult production process, and the resulting product has poor homogeneity.
A · US 9,728,311 B2 · ¶ 6
The resulting Nd—Fe—B based sintered magnet has high coercivity and excellent comprehensive magnetic performance.
A · US 9,728,311 B2 · ¶ 7
On the other hand, the permanent magnets employed in these environmentally friendly vehicles are required to have a high coercive force of 25 to 30 kOe or more, because they should stably maintain their original function without losing their performance even in a high temperature environment at 200° C.
B · US 2019/0385790 A1 · ¶ 7
However, the heavy rare earth element, such as Dy or Tb, which is used in this method, is 4 to 10 times higher in price than a light rare earth element such as Nd or Pr, and has a resource constraint due to its limited global reserves.
B · US 2019/0385790 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0366106 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366106/, SHA-256 8221bd7dd5e43cd84aec1532eb121920acb98f7e90ed815add13b8a7413f3021