patent.fyi
Applications  /  US 2026/0366107
United States Patent Application Publication

US 2026/0366107 A1

Published
Nov 19, 2026
Filed
Jun 25, 2026
Earliest date on the face
Dec 28, 2023
Classification
C22C 38/002
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Higher silicon content

What ifWhat if the slab contains 2.5 wt % silicon?
Claim language“silicon (Si) of 1.0 wt % to 1.5 wt %”

The higher silicon content raises electrical resistivity and reduces eddy-current loss at a given sheet thickness. The hot band is pickled and cold-rolled in multiple passes to reach the final gauge.

1.1Calcium treatment of inclusions

What ifWhat if calcium treatment replaces additions of neodymium, praseodymium, and yttrium?
Claim language“neodymium (Nd), praseodymium (Pr), and yttrium (Y)”

Calcium-bearing cored wire feeds calcium into the aluminum-deoxidized melt after ladle refining. Calcium modifies alumina into calcium aluminates and binds some residual sulfur in calcium-bearing inclusions.

1.1Higher aluminum content

What ifWhat if the slab contains 0.7 wt % aluminum?
Claim language“aluminum (Al) of 0.1 wt % to 0.4 wt %”

Aluminum in solid solution raises the electrical resistivity of the ferritic matrix and reduces eddy-current loss at a given gauge. Ladle refining keeps nitrogen low to limit the formation of fine aluminum nitride particles that pin grain boundaries during annealing.

1.2Warm rolling to gauge

What ifWhat if a heated rolling mill reduces the hot band to final gauge at 450 °C?
Claim language“cold-rolling the hot-rolled steel sheet”

An induction heater brings the descaled hot band to 450 °C before the first stand, and interstand heaters maintain the strip temperature during reduction. The warm passes reduce the flow stress and bring the strip to final thickness before a recrystallization anneal.

1.3Hot band anneal before sizing

What ifWhat if the sheet receives its grain-growth anneal before a light cold sizing pass and leaves the mill in the as-rolled condition?
Claim language“cold-annealing the cold-rolled steel sheet”

Hot rolling produces a band close to the required gauge, and a hot-band anneal recrystallizes the ferrite and grows the grains. A cold sizing pass with about 1% thickness reduction corrects flatness and gauge while limiting the strain retained in the finished sheet.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Laminations for magnetic bearing stators

Hot-roll and cold-roll the specified iron–silicon slab, then anneal the cold-rolled strip for use in radial magnetic bearings. Punch the annealed strip into stator laminations with inward-facing poles and apply an interlaminar insulating coating. Stack the laminations with the poles aligned, fit a coil around each pole, and mount the stack around the rotor with a radial air gap.

Parameter or scale variation

Cold reduction to quarter millimeter gauge

Hot-roll the specified slab to a strip thickness of 2.00 mm and remove the surface scale by pickling. Use a reversing cold mill to reduce the strip to successive exit gauges of 1.20, 0.72, 0.44, 0.30, and 0.25 mm. Anneal the finished strip to recrystallize the deformed ferrite and promote grain growth. The 87.5% total cold reduction produces thin laminations that limit through-thickness eddy currents.

Combination with existing systems

Continuous annealing with insulation coating

Feed the cold-rolled strip through an annealing furnace, a cooling section, a two-sided roll coater, and a curing oven on one continuous line. Cool the strip after annealing and use opposed applicator rolls to deposit a waterborne phosphate coating on both faces. Dry and cure the coating in the oven, then cool and recoil the strip. The coating electrically separates adjacent laminations in an assembled core.

Automated or data-driven variant

Closed loop cold rolling gauge control

Fit the cold mill with X-ray thickness gauges at the entry and exit, a strip speed encoder, and hydraulic roll gap actuators. Use the measured entry thickness and strip speed to time feedforward gap corrections to incoming thickness changes. Use the exit gauge to trim the gap command through a feedback controller that accounts for the travel time from the roll bite to the gauge. Send the gauge-controlled strip to final annealing.

Automated annealing control by strip temperature

Install a purged optical pyrometer at the end of the heating zone and a second pyrometer at the soak zone exit. Use the measured strip temperatures, entry gauge, and line speed to adjust furnace zone power around a stored recipe. Constrain line speed using the heated zone lengths and the required soak time. Log the temperature readings against strip position to identify coil segments that fall outside the selected thermal limits.

Specific version of a part

Neodymium treated hot band

The slab contains 1.25 wt % silicon, 0.25 wt % manganese, 0.20 wt % aluminum, 0.0015 wt % sulfur, and 0.0012 wt % neodymium, with iron and residual impurities as the balance. A roughing mill breaks down the reheated slab, and finishing stands reduce it to a 2.0 mm hot band.

Tandem cold rolling schedule

A pickling line removes oxide scale from a 2.0 mm hot band before it enters a five-stand tandem cold mill. Successive passes in the stands reduce the strip to 0.50 mm, a total thickness reduction of 75%.

Reversing cold mill passes

A four-high reversing mill reduces a pickled hot band from 1.8 mm to 0.65 mm in successive passes. Tension reels on both sides of the stand control strip tension as the rolling direction alternates.

Continuous strip recrystallization anneal

A continuous furnace heats the cold-rolled strip to 850 °C and holds it near that temperature for 60 seconds in a dry nitrogen and hydrogen atmosphere. The soak recrystallizes the ferrite and allows grain growth before the strip cools in a protected section.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2011/0273054 A1
Published
Nov 10, 2011
Filed
May 4, 2010
Class
H02K 1/02
Document BUS 2018/0237876 A1
Published
Aug 23, 2018
Filed
Aug 29, 2016
Class
C21D 8/1266
Claim 1
Document A
Document B
1.1hot-rolling a slab comprising, in wt %, silicon (Si) of 1.0 wt % to 1.5 wt %, manganese (Mn) of 0.1 wt % to 0.4 wt %, aluminum (Al) of 0.1 wt % to 0.4 wt %, sulfur (S) of more than 0 wt % to 0.003 wt %, a sum of one or more elements of more than 0.0006 wt % to 0.0030 wt %, the one or more elements being selected from the group consisting of neodymium (Nd), praseodymium (Pr), and yttrium (Y), remainder iron (Fe), and unavoidable impurities to provide hot-rolled steel sheet;
The slab is then fed to a hot strip mill at step 29. Hot strip from the hot strip mill is then used in step 30 to create hot rolled coil.
A · US 2011/0273054 A1 · ¶ 58
The preliminary material is then, if required, subjected to an annealing treatment and then hot-rolled to give a hot strip.
B · US 2018/0237876 A1 · ¶ 4
1.2cold-rolling the hot-rolled steel sheet to provide a cold-rolled steel sheet; and
Then a cold rolling reduction occurs at step 32.
A · US 2011/0273054 A1 · ¶ 58
Then a cold strip is rolled from the hot strip in one or more stages, with performance of intermediate annealing if required between the cold rolling steps in a multistage cold rolling operation effected in multiple steps.
B · US 2018/0237876 A1 · ¶ 5
1.3cold-annealing the cold-rolled steel sheet.
In a continuous annealing line, the cold rolled strip is annealed to achieve a partial recrystallization with a smaller grain size than would be the grain size with a complete recrystallization.
A · US 2011/0273054 A1 · abstract

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.3. Both have a passage for 1.1 1.2.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

In order to reduce losses, thickness should be decreased and resistivity should be increased.
A · US 2011/0273054 A1 · ¶ 8

Related claim parts: 1.2

However, the technique and strategies used to develop strength are in conflict with the strategies required to develop low electrical losses.
A · US 2011/0273054 A1 · ¶ 3
The resultant cold strip then typically undergoes a decarburization anneal, in order to minimize the carbon content of the cold strip for avoidance of magnetic aging.
B · US 2018/0237876 A1 · ¶ 6
The annealing separator prevents the windings of a coil wound from the cold strip from being welded to one another in a subsequently conducted high-temperature anneal.
B · US 2018/0237876 A1 · ¶ 7
Cite aspatent.fyi, US 2026/0366107 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366107/, SHA-256 5ee717d2bfb3e941482856bfda79a2e0dddb5e2b80221b6ce2c96e67e503f68f
First published
Permanent addresshttps://patent.fyi/US20260366107/
Content fingerprint (SHA-256)5ee717d2bfb3e941482856bfda79a2e0dddb5e2b80221b6ce2c96e67e503f68f
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi