Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Lower silicon with ultra-thin gauge
What ifWhat if the steel contains 2.0 to 2.5 weight % silicon and reduces high-frequency eddy current loss through cold rolling to a gauge below 0.15 millimeters?
Claim language“Si: 3.3 to 4.3%”
Reducing silicon content to 2.0 to 2.5 weight % lowers lattice ordering and raises room-temperature ductility, allowing multi-pass cold rolling on a cluster mill down to 0.10 to 0.15 millimeters final thickness. Because classical eddy current loss scales with the square of sheet thickness, the thinner lamination offsets the lower bulk electrical resistivity of the lower-silicon alloy. Continuous annealing at 850 to 950 degrees Celsius recrystallizes the thin strip into an equiaxed grain structure with low hysteresis loss.
1.1Antimony grain-boundary segregation replacing tin
What ifWhat if antimony at 0.02 to 0.15 weight % controls grain-boundary mobility and surface oxidation while tin is omitted?
Claim language“Sn: 0.01 to 0.1%”
Adding 0.02 to 0.15 weight % antimony during secondary steelmaking provides equilibrium segregation to grain boundaries and free surfaces during final annealing at 900 to 1050 degrees Celsius. The segregated antimony layer blocks nitrogen and oxygen ingress from the annealing atmosphere and retards nucleation of unfavorable {111} grains during recrystallization. This mechanism stabilizes grain growth and maintains magnetic flux density without requiring tin additions.
What ifWhat if copper is omitted and trace cerium and lanthanum additions modify sulfide inclusions into coarse oxysulfides?
Claim language“Cu: 0.03 to 0.5%”
Injecting 0.003 to 0.015 weight % combined cerium and lanthanum into the ladle melt binds dissolved sulfur into high-melting-point rare-earth oxysulfides of 1 to 5 micrometers diameter. Because these coarse inclusions have low surface-area-to-volume ratios, they exert minimal pinning force on migrating grain boundaries during final annealing. Eliminating copper also removes surface hot-shortness defects caused by liquid copper enrichment at the scale-metal interface during slab reheating.
1.1Ultra-low sulfur via ladle desulfurization
What ifWhat if deep ladle slag desulfurization reduces sulfur below 0.0010 weight % to remove sulfide pinning?
Claim language“S: 0.002 to 0.01%”
Treating molten steel with a calcium-aluminate synthetic slag under argon stirring and vacuum degassing lowers dissolved sulfur below 0.0010 weight % before continuous casting. With manganese and copper sulfide precipitation suppressed during hot rolling and annealing, recrystallized grains grow uniformly to 80 to 150 micrometers at lower annealing temperatures. The reduction in fine sulfide inclusions decreases domain wall pinning and lowers hysteresis loss.
1.3In-plane cube fiber texture control
What ifWhat if the sheet develops a dominant {100}<0vw> planar fiber texture with suppressed {112} components and a ratio below 1.5?
Claim language“texture (112)[1-31]/texture (112)[1-10] strength ratio is 2.0 or more”
Applying two-stage cold rolling with a 5 to 15 percent temper reduction after intermediate annealing at 800 to 900 degrees Celsius drives strain-induced boundary migration that favors {100}<0vw> grains. These grains align two orthogonal <001> easy magnetization axes directly within the rolling plane across all in-plane angles. Because magnetization proceeds along easy crystallographic directions with minimal domain rotation, core loss drops and rotational magnetic isotropy increases without relying on {112}[1-31] dominance.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Laminated magnetic cores for high-frequency power transformers
Thin strips of the silicon-aluminum-manganese-copper-tin alloy sheet with a (112)[1-31] to (112)[1-10] texture strength ratio of 2.0 or higher form stacked E-I or toroidal transformer cores for solid-state power converters. An inorganic phosphate-chromate insulating coating of 1 to 2 micrometers thickness separates adjacent stamped laminations to suppress interlaminar eddy currents under alternating magnetic flux at 1 to 10 kilohertz. Primary and secondary copper windings wrap around the central leg of the clamped lamination stack, and forced dielectric oil circulates through cooling channels machined into the outer core frame. High electrical resistivity from the silicon and aluminum content reduces core heating while the crystallographic texture supports uniform magnetic flux distribution across the corner junctions of the magnetic circuit.
Active magnetic bearing cores for high-speed spindles
Laser-cut laminations of the silicon-aluminum-manganese-copper-tin electrical steel sheet stack onto a rotating shaft sleeve and stationary housing to form radial and axial actuator cores for active magnetic bearings. Each stator pole carries an electromagnetic control coil driven by a pulse-width-modulated power amplifier switching at 10 to 20 kilohertz in response to inductive shaft displacement sensors. The high electrical resistivity of the alloy and the (112)[1-31] to (112)[1-10] texture ratio of 2.0 or more limit iron losses and phase lag caused by high-frequency switching ripple and rotational flux reversals at spindle speeds above 30000 revolutions per minute. Reduced core heating prevents thermal distortion of the bearing air gap and maintains stable rotor levitation without liquid lubrication.
Component substitution
Selenium inclusion control in place of sulfur
Selenium at 0.003 to 0.015 weight percent replaces sulfur in the iron-silicon-aluminum-manganese-copper-tin alloy melt while maintaining sulfur below 0.0005 weight percent. During slab reheating at 1100 to 1180 degrees Celsius and hot rolling, selenium combines with manganese and copper to precipitate fine manganese selenide and copper selenide particles measuring 20 to 80 nanometers in diameter. These dispersed selenide particles pin grain boundaries during cold rolling and continuous final annealing at 950 to 1050 degrees Celsius, suppressing abnormal grain growth while favoring recrystallization of the (112)[1-31] texture component over the (112)[1-10] orientation. The finished sheet retains high electrical resistivity and a texture strength ratio above 2.0 with reduced inclusion clustering at the sheet surface.
Parameter or scale variation
Ultra-thin gauge sheets via double cold rolling
Hot-rolled bands of the iron-silicon-aluminum-manganese-copper-tin alloy with an initial thickness of 1.8 to 2.2 millimeters undergo two-stage cold rolling with an intermediate annealing step to reach a final gauge between 0.08 and 0.15 millimeters. The first cold-rolling pass applies a 65 to 75 percent thickness reduction, followed by intermediate annealing at 850 to 920 degrees Celsius for 45 to 90 seconds in a dry hydrogen-nitrogen atmosphere. The second cold-rolling pass applies a 55 to 70 percent reduction to the final gauge, and continuous final annealing at 980 to 1060 degrees Celsius for 20 to 40 seconds develops an average ferrite grain diameter of 60 to 100 micrometers with a (112)[1-31] to (112)[1-10] texture ratio above 2.0. Reducing sheet thickness into this range lowers classical eddy current loss during alternating magnetization at frequencies from 1000 to 4000 hertz.
Combination with existing systems
Adhesive-bonded stator core with direct oil cooling
Stamped stator laminations made from the silicon-aluminum-manganese-copper-tin electrical steel sheet carry a 3 to 5 micrometer thermosetting epoxy-phenolic bonding lacquer on both surfaces in place of mechanical interlocking dimples or perimeter welds. A hydraulic press compresses the stacked laminations at 2 to 4 megapascals and cures the lacquer at 180 to 220 degrees Celsius for 30 minutes to form a rigid stator core with axial cooling passages integrated into the stator back-iron slots. The bonded stator mounts inside a cast aluminum housing coupled to a closed-loop dielectric oil pump and heat exchanger that sprays cooling fluid across the copper end windings and through the back-iron channels. Eliminating welds and mechanical interlocks prevents local compressive stress and short-circuit paths between laminations, preserving low high-frequency core loss and texture uniformity across the assembled traction motor stator.
Automated or data-driven variant
Closed-loop texture control using inline diffraction sensors
A continuous annealing and cold-rolling line incorporates an inline energy-dispersive X-ray diffraction sensor downstream of the final soaking zone to measure the (112)[1-31] and (112)[1-10] pole intensity ratio on the moving steel strip at 2-second intervals. Pyrometers, laser thickness gauges, and optical emission spectrometers feed real-time strip temperature, reduction ratio, and melt composition data into a trained gradient-boosted regression model running on a programmable industrial controller. When the measured texture strength ratio drifts toward 2.0, the controller adjusts furnace soaking zone setpoints within 950 to 1080 degrees Celsius, strip line speed within 40 to 120 meters per minute, and dew point of the hydrogen-nitrogen gas mixture. Automated feedback keeps the crystallographic texture ratio and grain size within target tolerances across coil-to-coil variations in silicon, aluminum, copper, and tin concentrations.
Specific version of a part
High-silicon aluminum alloy with controlled manganese
The steel composition targets 3.8 weight % silicon, 1.2 weight % aluminum, and 0.6 weight % manganese, with 0.12 weight % copper, 0.04 weight % tin, and 0.004 weight % sulfur in a balance of iron. Combined silicon and aluminum additions raise bulk electrical resistivity above 65 microohm-centimeters to suppress eddy current loss at high frequencies. Continuous slab casting with electromagnetic stirring minimizes centerline segregation of silicon and manganese before hot rolling.
Copper-tin balanced composition for warm rolling
The alloy sets silicon at 3.4 weight %, aluminum at 1.5 weight %, manganese at 1.1 weight %, copper at 0.25 weight %, tin at 0.06 weight %, and sulfur at 0.005 weight % with iron forming the remainder. Keeping silicon near the lower end of the range while increasing aluminum and manganese preserves high electrical resistivity while reducing brittleness during strip processing. Preheating the hot-band strip to 180 to 250 degrees Celsius prior to tandem rolling prevents edge cracking during gauge reduction.
Hot-band annealing and single-stage cold reduction
Hot-rolled strip of 2.0 millimeters thickness undergoes continuous normalizing annealing at 950 to 1020 degrees Celsius for 60 to 120 seconds to produce a uniform initial grain size of 120 to 180 micrometers. Subsequent single-stage cold rolling at a 75 to 85 percent reduction ratio followed by rapid-heating final annealing at 20 to 50 degrees Celsius per second up to 1000 degrees Celsius develops a (112)[1-31] to (112)[1-10] texture strength ratio of 2.5 to 3.2 as measured by electron backscatter diffraction. This crystallographic balance increases in-plane magnetic permeability and lowers core loss at 400 hertz.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1by weight %, Si: 3.3 to 4.3%, Al: 0.8 to 1.7%, Mn: 0.3 to 2.0%, Cu: 0.03 to 0.5%, Sn: 0.01 to 0.1%, S: 0.002 to 0.01%, and a balance of Fe and inevitable impurities,
(5) Grain-oriented electrical steel sheet superior in core loss characteristic as set forth in any one of (1) to (4) characterized in that said grain-oriented electrical steel sheet contains, by mass %, in addition to Si: 0.8 to 7%, at least one of Mn: 1% or less, Cr: 0.3% or less, Cu: 0.4% or less, P: 0.5% or less, Ni: 1% or less, Mo: 0.1% or less, Sn: 0.3% or less, and Sb: 0.3% or less.
A · US 2009/0173413 A1 · ¶ 32
A silicon steel alloy including, by wt %, silicon (Si): 5%, aluminum (Al): 1%, chromium (Cr): 12%, carbon (C): 0.002%, and nitrogen (N): 0.003% was cast to obtain strips having a thickness of 2.0 mm by using a vertical twin roll strip caster.
B · US 2016/0319387 A1 · ¶ 82
1.2wherein relational expression 1 is satisfied, and
1.3wherein texture (112)[1-31]/texture (112)[1-10] strength ratio is 2.0 or more:
An empty cell means only that no passage was reproduced there.
Why these two documents?
Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
High-silicon steel sheets are commonly used to manufacture the cores of transformers, electric motors, generators, and other electronic devices, and are thus known as “electrical steel sheets.” High-silicon steel sheets are typically required to have a high magnetic flux density and a low degree of core loss.
B · US 2016/0319387 A1 · ¶ 2
Related claim parts: 1.1
The present invention relates to grain-oriented electrical steel sheet superior in core loss characteristic used as a soft magnetic material as a core of a transformer, electrical equipment, etc.
A · US 2009/0173413 A1 · ¶ 1
However, the <001> axes of crystal grains of actual products, as shown in FIG. 3(a), are also dispersed around the ND and/or TD, so making the <001> axes of the individual crystal grains match in the rolling direction of the steel sheet is difficult.
A · US 2009/0173413 A1 · ¶ 7
The present disclosure relates to a soft high-silicon steel sheet, and more particularly, to a soft high-silicon steel sheet able to be manufactured through a rolling process without an additional siliconizing process due to the soft high-silicon steel sheet having ductility even in the case that the silicon content of the soft high-silicon steel sheet is greater than 4%.
B · US 2016/0319387 A1 · ¶ 1
In general, if the silicon content of steel sheets is 3.5 wt % or greater, it is very difficult to manufacture such steel sheets using a normal cold rolling process.
B · US 2016/0319387 A1 · ¶ 5