patent.fyi
Applications  /  US 2026/0366109
United States Patent Application Publication

US 2026/0366109 A1

Published
Nov 19, 2026
Filed
Jun 26, 2026
Earliest date on the face
Dec 29, 2023
Classification
C22C 38/02
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Thinner sheet with less silicon

What ifWhat if the sheet contains 0.4 wt % Si and uses a final thickness of 0.20 mm to control eddy-current loss?
Claim language“0.6 wt % or greater”

Cold rolling sets the sheet thickness to 0.20 mm, and a final anneal recrystallizes the ferrite. The thinner cross section limits eddy-current flow within each lamination and offsets part of the loss reduction associated with higher silicon content.

1.2Vacuum carbon deoxidation

What ifWhat if the sheet contains less than 0.05 wt % Al and the melt is deoxidized under vacuum using dissolved carbon?
Claim language“0.1 wt % or greater”

Under reduced pressure, dissolved carbon and oxygen react to form carbon monoxide, which leaves the melt as gas. Melt sampling tracks dissolved oxygen and residual carbon before casting.

1.3Lower manganese through desulfurization

What ifWhat if the sheet contains 0.10 wt % Mn and upstream desulfurization controls sulfur-related hot-working defects?
Claim language“0.2 wt % or greater”

A lime-based treatment transfers sulfur from the hot metal to the slag, which is removed before steelmaking. A final sulfur target below 10 ppm limits iron sulfide at grain boundaries and reduces the manganese needed to control hot shortness.

1.5Calcium treatment of inclusions

What ifWhat if calcium treatment controls oxide inclusions in a heat with no Y or Ho additions?
Claim language“one or more of: Y”

Calcium-bearing cored wire feeds calcium beneath the surface of the aluminum-deoxidized melt. The calcium converts solid alumina inclusions into calcium aluminates that are liquid at casting temperature when their composition is within the liquid range.

1.6Direct alternating loss measurement

What ifWhat if sheet acceptance uses measured specific core loss in place of a calculated spin alignment value?
Claim language“magnetic domain spin alignment value”

A single-sheet tester drives alternating flux through the specimen with a magnetizing winding and measures flux with a sensing winding. The tester derives loss per unit mass from the hysteresis loop at a peak flux density of 1.5 T and a frequency of 50 Hz.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Component substitution

Cerium addition for inclusion control

Cerium replaces yttrium and holmium in an iron melt containing 1.1 wt % silicon, 0.30 wt % aluminum, and 0.30 wt % manganese. After deoxidation and desulfurization, a cerium-bearing master alloy is fed below the melt surface under an inert cover to target 20 ppm retained cerium by mass. Cerium reacts with residual oxygen and sulfur to form oxide and oxysulfide inclusions. The cast slab is hot rolled, pickled, cold rolled, and recrystallization annealed, and a 20 mm square coupon is mapped at a 10 μm step to verify the average alignment value.

Automated or data-driven variant

Automated orientation mapping for coil release

A motorized electron backscatter diffraction stage maps polished 20 mm square coupons from the head and tail of each coil at a 10 μm step. Software converts indexed crystal orientations into the three axis angles, calculates the alignment value for each indexed point, and reports the arithmetic mean and indexing rate for each coupon. The coil tracking system releases a coil when both means are at most 1.22 and both maps meet the configured indexing coverage requirement. Coupons with insufficient coverage return to the measurement queue for preparation and rescanning.

Specific version of a part

Silicon addition by ferrosilicon

A ferrosilicon addition sets the ladle composition to 1.20 wt % Si. An optical emission measurement on a solidified ladle sample checks the silicon content before casting.

Yttrium addition by cored wire

An iron-sheathed wire with an iron–yttrium alloy core delivers yttrium below the ladle slag. The wire feed mass accounts for measured yttrium recovery and targets 10 ppm total Y in the solidified sheet.

Tiled electron backscatter mapping

A scanning electron microscope collects electron backscatter diffraction patterns on a 10 μm grid across a polished 20 mm by 20 mm specimen using overlapping stage tiles. The software registers the tiles in a common coordinate frame and removes duplicate grid points before deriving the three axis angles from the indexed orientations.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2012/0025073 A1
Published
Feb 2, 2012
Filed
Jul 27, 2011
Class
G01N 23/20
Document BUS 11,633,940 B2
Published
Apr 25, 2023
Filed
Jul 1, 2021
Class
B32B 15/013
Claim 1
Document A
Document B
1.1a) Si in an amount of i) 0.6 wt % or greater and ii) 1.6 wt % or less,
1.2b) Al in an amount of i) 0.1 wt % or greater and ii) 0.5 wt % or less, and
1.3c) Mn in an amount of i) 0.2 wt % or greater and ii) 0.4 wt % or less, and
In at least one aspect, manganese content of a zinc-manganese alloy of the present disclosure is from about 0.1 wt % manganese to about 20 wt % manganese based on the total weight of the alloy.
B · US 11,633,940 B2 · ¶ 27
1.4d) one or more of: C in an amount of i) greater than 0 ppm and ii) 30 ppm or less, S in an amount of i) greater than 0 ppm and ii) 30 ppm or less, N in an amount of i) greater than 0 ppm and ii) 30 ppm or less, Ti in an amount of i) greater than 0 ppm and ii) 30 ppm or less, and P in an amount of i) greater than 0 ppm and ii) 1000 ppm or less, and
1.5e) one or more of: Y in amount of i) greater than 0 ppm and ii) 30 ppm or less and Ho in an amount of i) greater than 0 ppm and ii) 30 ppm or less, with the balance being Fe and other unavoidable impurities,
1.6wherein an average (MAVG) of a magnetic domain spin alignment value (M) calculated by General Formula 1 below is 1.22 or less: M=(sin2α sin2β)+(sin2β sin2γ)+(sin2γ sin2α), [General Formula 1]
1.7in General Formula 1 above, α, β, and γ are derived from crystal orientations measured under a step size condition of 10 μm via EBSD on a specimen of 20 mm in width and 20 mm in length manufactured from the non-oriented electrical steel sheet, and with respect to x-, y-, and z-axes defined in a three-dimensional crystal coordinate system, α is an angle formed between the x-axis and a crystal grain orientation, β is an angle formed between the y-axis and a crystal grain orientation, and γ is an angle formed between the z-axis and a crystal grain orientation.
Diffraction patterns obtained with wide angle convergent electron beam may be used to calculate crystallographic orientations of grains in the microstructure.
A · US 2012/0025073 A1 · ¶ 6

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.7. Only Document B has a passage for 1.3.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

This application relates generally to materials imaging, and more specifically to imaging and processing samples to determine grain orientation using transmission electron microscopy (TEM).
A · US 2012/0025073 A1 · ¶ 2
However, the accuracy of the orientation maps reduces when the grain sizes are less than 60 nm, which is the case with nanomaterials.
A · US 2012/0025073 A1 · ¶ 3
However, zinc-manganese alloys are not easily receptive to (e.g., have poor adhesion to), for example, trichrome passivation coatings, because of poor reactivity.
B · US 11,633,940 B2 · ¶ 5
Therefore, there is a need in the art for improved electrolyte solutions for electrodeposition of zinc-manganese alloys, methods of forming electrolyte solutions, methods of electrodepositing zinc-manganese alloys, and multilayered zinc-manganese alloys.
B · US 11,633,940 B2 · ¶ 6
Cite aspatent.fyi, US 2026/0366109 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366109/, SHA-256 57a063c7df2201c708d026848437f97aa358b68c3205d8b04557a8cda8925752
First published
Permanent addresshttps://patent.fyi/US20260366109/
Content fingerprint (SHA-256)57a063c7df2201c708d026848437f97aa358b68c3205d8b04557a8cda8925752
Methodv2026-11-18.2 · automated, not reviewed by a person