patent.fyi
Applications  /  US 2026/0366110
United States Patent Application Publication

US 2026/0366110 A1

Published
Nov 19, 2026
Filed
Nov 30, 2023
Earliest date on the face
Dec 5, 2022
Classification
C22C 38/04
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Grain refinement without niobium additions

What ifWhat if the alloy contains no niobium and relies on titanium and vanadium carbonitrides for grain refinement and precipitation strengthening?
Claim language“Nb: from ≥0.01 to ≤0.10”

Titanium at 0.06 to 0.10 wt. % and vanadium at 0.05 to 0.15 wt. % form finely dispersed titanium-vanadium carbonitrides during hot rolling and subsequent cooling. These precipitates pin austenite grain boundaries during reheating and inhibit recrystallization in the finishing rolling stands. The resulting fine prior austenite grain structure transforms into a ferrite, bainite, and martensite matrix exceeding 700 MPa tensile strength.

1.3Low silicon and aluminum alloy chemistry

What ifWhat if the combined silicon and aluminum content stays below 0.30 wt. % and chromium with molybdenum provides hardenability and cementite retardation?
Claim language“Si and Al is in a range of ≥0.60 to ≤1.20”

Keeping combined silicon and aluminum below 0.30 wt. % reduces the formation of surface oxide layers during annealing and improves molten metal wetting. Chromium at 0.60 to 1.00 wt. % and molybdenum at 0.15 to 0.30 wt. % delay pearlite transformation and slow carbide coarsening during isothermal holding. This alloy balance produces a multiphase ferrite-bainite-martensite microstructure with tensile strength above 700 MPa.

1.4Direct thin strip casting to gauge

What ifWhat if the steel strip reaches final gauge through twin-roll strip casting and inline hot rolling without cold rolling?
Claim language“cold rolling the hot-rolled steel strip”

Molten steel solidifies between two counter-rotating, water-cooled casting rolls into an as-cast strip of 1.5 to 2.5 mm thickness. An inline single-stand hot rolling mill reduces the strip at 900 °C to 1050 °C by 20 to 40 percent to reach a final gauge of 1.0 to 1.8 mm. Acid pickling removes surface scale before the strip enters the continuous annealing and coating line.

1.5Ultra-fast induction flash annealing cycle

What ifWhat if the cold-rolled strip undergoes flash annealing in 2 to 8 seconds using transverse-flux induction coils?
Claim language“total duration of 10 s to 1000 s”

Transverse-flux induction heating coils raise the cold-rolled strip temperature at 150 to 500 K/s to a peak intercritical temperature of 780 °C to 860 °C with a total heating and soaking time of 2 to 8 seconds. The rapid heating rate limits ferrite recrystallization before austenite nucleation, creating a fine dispersion of austenite islands along deformed ferrite grain boundaries. Subsequent cooling transforms these fine austenite regions into uniformly distributed martensite and bainite.

1.6Electrolytic zinc plating after final cooling

What ifWhat if the strip is coated by continuous electrolytic zinc plating after final cooling rather than hot-dip coating?
Claim language“hot-dip coating the cold-rolled steel strip”

After isothermal holding and final cooling to ambient temperature, the bare annealed strip passes through a series of electrolytic plating cells filled with an aqueous zinc sulfate electrolyte at 40 °C to 60 °C. Direct current applied between insoluble anodes and the moving steel strip deposits a uniform zinc layer of 5 to 10 micrometers on both surfaces. Decoupling coating from the thermal cycle prevents reheating of martensite or bainite formed during cooling.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Multiphase steel strip for rail freight panels

A cold-rolled and hot-dip coated steel strip with a carbon content of 0.13 to 0.20 wt. %, manganese of 1.40 to 2.40 wt. %, and combined silicon and aluminum of 0.60 to 1.20 wt. % is formed into corrugated side wall panels and structural floor sills for rail freight cars. The strip is fed from a decoiler into a multi-stand roll forming mill that bends the sheet into load-bearing rib profiles at ambient temperature without intermediate reheating. Adjacent corrugated sections are joined to transverse chassis cross-members by resistance spot welding and gas metal arc welding using low-hydrogen filler wire. The zinc-coated multiphase microstructure provides tensile strength above 700 MPa and corrosion resistance under outdoor moisture and bulk cargo abrasion.

Component substitution

Electrolytic zinc-nickel coating replacing hot-dip immersion

An electrolytic plating line replaces the molten hot-dip coating bath downstream of the continuous annealing and isothermal holding sections. After cooling the annealed cold-rolled strip to 250 to 450 °C, holding for 30 to 600 s, and cooling to ambient temperature, the strip passes through an alkaline degreasing tank, an acid pickling rinse, and a series of vertical plating cells containing an acidic zinc-nickel electrolyte at 45 to 60 °C. Direct current is applied between insoluble anodes and the moving steel strip at a current density of 30 to 60 A/dm² to deposit an alloy layer containing 10 to 15 wt. % nickel at a thickness of 3 to 8 micrometers. Because the coating step operates near ambient temperature, the bainite, martensite, and retained austenite fractions established during isothermal holding undergo no thermal tempering during coating.

Thin-slab direct casting replacing conventional slab reheating

A vertical-bending thin-slab continuous caster with an inline tunnel furnace replaces conventional thick-slab casting and batch reheating prior to hot rolling. Molten steel with the specified carbon, manganese, silicon, aluminum, and niobium composition is cast into a slab of 50 to 90 mm thickness and fed directly through a gas-fired tunnel furnace held at 1120 to 1180 °C for 15 to 25 minutes to equalize temperature. The thin slab enters a six-stand finishing mill directly without a separate roughing mill, is hot rolled to a strip thickness of 1.5 to 3.5 mm, and is coiled before pickling and cold rolling. Subsequent cold rolling, continuous annealing at 750 to 950 °C, isothermal holding at 250 to 450 °C, hot-dip coating, and final cooling proceed on the continuous processing line.

Parameter or scale variation

Elevated annealing soak and accelerated quench cooling

The continuous annealing furnace operates at a peak strip temperature of 960 to 1020 °C for a total duration of 40 to 180 s to achieve complete austenitization of the cold-rolled strip before cooling. Immediately downstream of the soaking zone, high-velocity hydrogen-nitrogen jet coolers and a mist quench section cool the strip to a stop temperature of 220 to 250 °C at an average cooling rate of 120 to 250 K/s. The strip then enters an electrically heated overaging section held at 300 to 420 °C for 60 to 300 s to partition carbon from fresh martensite into untransformed austenite prior to hot-dip coating at 450 to 470 °C. Final cooling proceeds at 15 to 40 K/s to ambient temperature, yielding a flat steel strip with a tensile strength exceeding 1000 MPa.

Combination with existing systems

Inline induction heating integrated before hot-dip coating

A transverse-flux induction heating unit is installed in the furnace snout between the 250 to 450 °C isothermal holding zone and the molten coating pot of the continuous hot-dip line. After the cold-rolled strip completes its 30 to 600 s isothermal hold, it passes through water-cooled copper induction coils energized by a medium-frequency power supply operating at 10 to 50 kHz. The induction unit raises the strip temperature rapidly at 30 to 80 K/s to match the 440 to 480 °C molten bath temperature over a strip path length of less than 3 m. A sealed nitrogen-hydrogen protective atmosphere surrounds the induction coils and snout chute to prevent surface oxidation of silicon and aluminum before bath immersion.

Automated or data-driven variant

Closed-loop electromagnetic sensing for cooling rate control

Non-contact electromagnetic induction sensors and infrared pyrometers are mounted along the strip path after the soaking furnace, after the primary cooling zone, and after the final cooling tower of the continuous annealing line. The electromagnetic sensors measure real-time magnetic permeability and coercivity across the strip width to infer phase fractions of ferrite, bainite, martensite, and retained austenite continuously during line operation. A programmable process controller feeds the sensor readings, line speed, and strip gauge into a trained regression model that computes adjustments to gas-jet fan speeds, cooling water valve openings, and furnace zone temperatures. Control setpoints update every 0.5 s to hold the cooling stop temperature and final tensile strength within target tolerances across coil-to-coil variations in strip thickness and carbon content.

Specific version of a part

Titanium-nitrogen stoichiometry for nitride pinning

The steel melt includes 0.025 to 0.035 wt. % titanium and 0.004 to 0.006 wt. % nitrogen, with vanadium held at 0.08 to 0.12 wt. % and the remainder iron. Titanium binds free nitrogen into fine cubic titanium nitride particles during slab solidification, preventing coarse aluminum nitride precipitation and restricting austenite grain growth during slab reheating. Vanadium precipitates as fine carbonitrides in ferrite during cooling to increase yield strength.

Five-stand tandem cold reduction mill

After hydrochloric acid pickling removes hot-mill oxide scale, the hot-rolled strip enters a five-stand tandem cold rolling mill equipped with work-roll bending and automatic gauge control. The mill applies a cumulative thickness reduction of 50 to 70 percent using an oil-in-water rolling emulsion to control roll friction and strip temperature. Interstand tension reels maintain flat strip geometry down to a target thickness of 0.8 to 1.6 mm.

Radiant-tube vertical continuous annealing furnace

A vertical radiant-tube furnace heats the cold-rolled strip under a protective atmosphere of nitrogen with 5 percent hydrogen and a dew point of -35 °C to prevent surface oxidation. The strip reaches a peak intercritical soaking temperature of 810 °C to 840 °C and remains in the heating and soaking zones for a total duration of 120 to 240 seconds. Optical pyrometers and furnace zone thermocouples regulate burner firing rates to maintain uniform cross-strip temperature within 5 K.

Hydrogen-nitrogen jet cooling and zinc bath

High-velocity gas jet coolers circulating a nitrogen-hydrogen mixture cool the strip at 25 to 50 K/s down to an isothermal holding temperature of 380 °C to 410 °C. The strip travels through an electrically heated overaging section for 120 to 240 seconds to form carbide-free bainite and enrich retained austenite with carbon. An induction reheater brings the strip to 460 °C before it enters a molten zinc bath containing 0.20 wt. % aluminum at 460 °C, where nitrogen air knives meter the coating weight.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2009/0308498 A1
Published
Dec 17, 2009
Filed
Jan 9, 2008
Class
C23C 8/10
Document BUS 9,593,399 B2
Published
Mar 14, 2017
Filed
Dec 13, 2013
Class
C22C 38/58
Claim 1
Document A
Document B
1.1the method comprises the steps of: producing a hot-rolled steel strip, consisting of the following elements in wt. %: C: from ≥0.13 to ≤0.20, Mn: from ≥1.40 to ≤2.40, Al: from ≥0.06 to ≤0.60, preferably ≥0.20 to ≤0.50 Si: from ≥0.03 to ≤0.70, Mo: <0.10, Nb: from ≥0.01 to ≤0.10, P: <0.02, S: <0.05, Ca: ≤0.004, B: ≤0.001, Cr: ≤0.50, Ni: ≤0.10, Cu: ≤0.10, and optionally one or more elements from
Thereafter, the transfer bar was subjected to a finishing treatment with an entry temperature of 1090° C. and an exit temperature of 950° C. in order to produce hot rolled strip with a thickness between 2.5 and 5.5 millimeters (mm).
B · US 9,593,399 B2 · ¶ 26
1.2N: ≥0.001 to ≤0.10, Ti: ≤0.05, V: ≤0.20, with the remainder being iron, including typical steel-associated elements
For example, in addition to Si and Mn, the steel may contain, by mass %, C: 0.01 to 0.3%, P: 0.0001 to 0.15%, S: 0.0001 to 0.02%, Al: 0.001 to 0.4%, and N: 0.0002 to 0.02% and have a balance of Fe and unavoidable impurities and may contain, in accordance with the required characteristics, one or more of Ti, Nb, V, Zr, W, Mo, Cr, Ni, Cu, Ca, REM, B, Mg or La, Ce, and other lanthanoid-based elements in the range of 0.0001 to 1%.
A · US 2009/0308498 A1 · ¶ 95
1.3wherein the sum of the proportions in wt. % of Si and Al is in a range of ≥0.60 to ≤1.20
1.4cold rolling the hot-rolled steel strip to form a cold-rolled steel strip
The hot rolled strip is cold rolled with at least a 55% reduction in thickness.
B · US 9,593,399 B2 · abstract
1.5subsequently continuously annealing the cold-rolled steel strip as part of a continuous hot-dip coating process, at a maximum temperature between 750 °C to 950 °C inclusive for the total duration of 10 s to 1000 s
A method using a continuous annealing furnace where a cooling method of a cooling zone including part or all of the temperature range of the steel sheet of 600 to 250° C. following the heating for recrystallization is one or more of gas cooling, effusion cooling, and cooling pipe cooling, or a joint cold rolled steel sheet/hot dip galvanized steel sheet facility having such a continuous annealing furnace, to continuously anneal cold rolled steel sheet to produce high strength
A · US 2009/0308498 A1 · abstract
The hot strip coil is then subjected to cold-rolling with at least a 55% reduction in thickness of the strip followed by intercritical annealing in a CAL. The annealing temperature is between 790-840° C. with an annealing time between 60-90 seconds.
B · US 9,593,399 B2 · ¶ 22
1.6then cooling the continuously annealed, cold-rolled steel strip in one stage or in multiple stages to a cooling stop temperature in a temperature range of 250 °C to 450 °C at an average cooling rate CR1 of 0.5 to 100 K/s and then holding the temperature in the temperature range of 250 °C to 450 °C for 30 to 600 s and subsequently hot-dip coating the cold-rolled steel strip at a temperature between 380 °C and 500 °C as part of the continuous hot-dip coating process
After subjecting the cold-rolled sheet to the intercritical annealing treatment, the sheet is rapidly cooled and/or ultra rapidly cooled using the URC to a temperature between 450-500° C.
B · US 9,593,399 B2 · ¶ 22
1.7then finally cooling the continuously annealed, cold-rolled steel strip at an average cooling rate of 2 K/s to 100 K/s to ambient temperature in order to create the high-strength flat steel product.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.2. Only Document B has a passage for 1.1 1.4 1.6. Both have a passage for 1.5.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

It is known in the art that alloying elements such as manganese, chromium, molybdenum, and vanadium can be used to reduce the rate of cooling required for the transformation of the austenite to martensite.
B · US 9,593,399 B2 · ¶ 4

Related claim parts: 1.2

The present invention relates to a method of production able to produce a high strength cold rolled steel sheet excellent in chemical convertibility even when increasing the contents of Si, Mn, etc. along with the increase in strength and a production facility for realizing the same.
A · US 2009/0308498 A1 · ¶ 1
If for example increasing Si to about 1.0%, the steel sheet surface is left with large amounts of Si, Mn, or other oxide films, the chemical convertibility deteriorates, and parts of the Si oxide film not chemically converted, that is, chemical conversion defects called “bald spots”, occur.
A · US 2009/0308498 A1 · ¶ 7
However, despite their forming and cost advantages over high-strength steels, the relatively low-strength level results in the crash performance of such materials being mainly dependent on a thickness of a sheet thereof.
B · US 9,593,399 B2 · ¶ 2
In particular, the invention makes use of specific cooling strategies using gas jet rapid cooling and utilizing therein ‘Ultra Rapid Cooling’ (URC) to obtain ultra high strength>980 MPa TS cold rolled dual phase steels.
B · US 9,593,399 B2 · ¶ 7
Cite aspatent.fyi, US 2026/0366110 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366110/, SHA-256 723d1086c9af231f9492d33dee8d066bfd568d6bb1077c536aa506672d210348
First published
Permanent addresshttps://patent.fyi/US20260366110/
Content fingerprint (SHA-256)723d1086c9af231f9492d33dee8d066bfd568d6bb1077c536aa506672d210348
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi