patent.fyi
Applications  /  US 2026/0366111
United States Patent Application Publication

US 2026/0366111 A1

Published
Nov 19, 2026
Filed
Dec 15, 2023
Earliest date on the face
Dec 21, 2022
Classification
C22C 38/04
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Vanadium precipitation strengthening

What ifWhat if the sheet contains less than 0.005 wt% niobium and uses vanadium carbonitrides for precipitation strengthening?
Claim language“0.03 to 0.05% of niobium (Nb)”

The melt contains 0.05 to 0.06 wt% vanadium and 0.008 to 0.010 wt% nitrogen. Controlled cooling after finish rolling forms fine vanadium carbonitrides in ferrite, where they impede dislocation motion.

1.1Thermal control of grain growth

What ifWhat if the titanium content stays below 0.003 wt% and a shorter slab reheating cycle controls austenite grain growth?
Claim language“0.005 to 0.017% of titanium (Ti)”

The slab reheats at 1080 to 1120 °C and enters rough rolling after its core reaches the target temperature. Roughing passes promote recrystallization, and finish rolling below the austenite recrystallization temperature prepares the deformed grains for fine ferrite formation during cooling.

1.1Lower manganese with molybdenum

What ifWhat if the sheet uses 0.8 to 1.0 wt% manganese and 0.15 to 0.25 wt% molybdenum to control transformation during cooling?
Claim language“1.2 to 1.6% of manganese (Mn)”

Molybdenum delays pearlite formation during accelerated cooling after finish rolling. The cooling cycle produces fine ferrite and bainite, which provide grain refinement and transformation strengthening.

1.2Bainite as the main constituent

What ifWhat if bainite occupies at least 80% of the sheet area and polygonal ferrite occupies less than 15%?
Claim language“60 to 85% of ferrite”

Accelerated water cooling begins above the ferrite transformation start temperature and brings the sheet into the bainite transformation range. A hold in that range promotes bainite formation, and its fine lath structure and high dislocation density provide strength.

1.2Weld testing for production release

What ifWhat if production release depends on weld coupon tests for each heat and the composition sum has no acceptance limit?
Claim language“[C]+[Mn]/6+[V]/5≤0.43 [Relational Expression 1]”

A coupon from each heat is welded at the minimum production preheat and low end of the specified heat input range. Hardness traverses assess local hardening in the heat-affected zone, and delayed inspection checks for cracking before the heat is released.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Web plates for overhead crane girders

The specified ferrite–pearlite steel sheet forms the two vertical webs of a welded box girder for an overhead crane. The webs are cut with their rolling direction along the girder span and joined to upper and lower flange plates by continuous longitudinal welds. Transverse diaphragms connect the webs at the end supports, and a rail centered on the upper flange carries the traveling trolley.

Component substitution

Molybdenum in place of vanadium

A low-carbon manganese steel uses 0.05 to 0.10 weight percent molybdenum as an intentional alloy addition in place of vanadium, while retaining niobium and titanium. The steel is hot rolled and air cooled after finishing, with the cooling rate set to account for the effect of molybdenum on transformation kinetics. Polished cross sections are examined by optical point counting to verify 60 to 85 percent ferrite by area, with pearlite as the principal balance.

Parameter or scale variation

Controlled rolling with timed air cooling

A slab of the specified composition is reheated to 1150 to 1200 °C, descaled, and rough rolled. The final three passes apply a cumulative thickness reduction of 25 to 35 percent, with the last pass ending at a measured surface temperature of 820 to 880 °C. The sheet cools in still air on an open rack with both faces exposed, and metallographic point counts verify the ferrite fraction and identify the remaining phases.

Low carbon and manganese subrange

The melt targets 0.105 to 0.120 weight percent carbon, 1.20 to 1.30 weight percent manganese, and 0.010 to 0.020 weight percent vanadium, with the remaining elements held in the specified ranges. At the upper limits of those three intervals, the composition index is approximately 0.341. After hot rolling and cooling, optical point counts on etched transverse sections verify 60 to 85 percent ferrite by area and identify pearlite in the balance.

Combination with existing systems

Plate with cathodic corrosion protection

The specified steel sheet forms welded shell courses in the submerged section of a tubular support. Aluminum alloy sacrificial anodes mount on external brackets and connect electrically to the shell through welded steel cores. A corrosion-resistant coating covers the shell while the anode surfaces remain exposed, and the anodes supply protective current through seawater to exposed steel at coating defects.

Automated or data-driven variant

Sensor feedback for plate cooling

Infrared pyrometers measure plate surface temperature immediately before and after a water cooling bank, and a roller encoder tracks the position of each plate segment. A process controller uses the measured entry temperature, plate speed, and thickness to set the water flow for each header zone. The controller compares the measured exit temperature of each segment with the target and trims flow for subsequent segments. Metallographic measurements from trial plates establish the target temperatures for a ferrite area fraction of 60 to 85 percent.

Specific version of a part

Niobium titanium steel chemistry

The melt contains 0.13 wt% carbon, 0.30 wt% silicon, 1.40 wt% manganese, 0.008 wt% phosphorus, 0.002 wt% sulfur, and 0.025 wt% aluminum. It also contains 0.040 wt% niobium, 0.030 wt% vanadium, 0.012 wt% titanium, and 0.005 wt% nitrogen, with iron and residual impurities making up the balance.

Ferrite and pearlite from cooling

Runout table cooling allows polygonal ferrite to form before the remaining austenite transforms mainly to pearlite during slower cooling. Quantitative point counting on etched cross sections verifies a ferrite area fraction near 80%.

Composition sum with low vanadium

The sheet contains 0.14 wt% carbon, 1.45 wt% manganese, and 0.020 wt% vanadium. The weighted sum is approximately 0.386, below the 0.43 limit.

Mass percentages from heat analysis

Combustion with infrared detection measures total carbon in a solid sample from each heat. Spark optical emission spectrometry measures manganese and vanadium, and the calculation uses all three results as numerical weight percentages.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2008/0138234 A1
Published
Jun 12, 2008
Filed
Mar 20, 2006
Class
C22C 38/12
Document BUS 11,466,349 B2
Published
Oct 11, 2022
Filed
Dec 27, 2018
Class
C22C 37/04
Claim 1
Document A
Document B
1.1more than 0.10 to 0.17% of carbon (C), 0.2 to 0.5% of silicon (Si), 1.2 to 1.6% of manganese (Mn), 0.012% or less of phosphorus (P), 0.003% or less of sulfur(S), 0.015 to 0.045% of aluminum (Al), 0.03 to 0.05% of niobium (Nb), 0.06% or less of vanadium (V), 0.005 to 0.017% of titanium (Ti), 0.002 to 0.01% of nitrogen (N), with a remainder of Fe and inevitable impurities, the steel sheet satisfying the following Relational Expression 1,
More particularly, the invention provides a heat resistant chromium-molybdenum vanadium steel consisting essentially of 0.08 to 0.12% by weight of carbon, 0.015% by weight or less of sulphur, 0.02% by weight or less of phosphorous, 0.30 to 0.60% by weight of silicon, 0.50 to 0.80% by weight of manganese, 1.20 to 1.50% by weight of chromium, 0.90 to 1.00% by weight of molybdenum, 0.20 to 0.30 by weight of vanadium, the balance being iron apart from incidental impurities, with
A · US 2008/0138234 A1 · ¶ 8
A spheroidal graphite cast iron of the present disclosure comprises C: 3.5 mass % to 4.2 mass %, Si: 2.0 mass % to 2.8 mass %, Mn: 0.2 mass % to 0.4 mass %, Cu: 0.1 mass % to 0.7 mass %, Mg: 0.02 mass % to 0.06 mass %, Cr: 0.01 mass % to 0.15 mass %, and the balance: Fe and inevitable impurities, wherein Mn+Cr+Cu is 0.431 mass % to 1.090 mass %.
B · US 11,466,349 B2 · ¶ 35
1.2wherein a microstructure of the steel sheet comprises, by area fraction, 60 to 85% of ferrite and a remainder of pearlite and inevitable structures, [C]+[Mn]/6+[V]/5≤0.43 [Relational Expression 1]
The pearlite fraction of the spheroidal graphite cast iron is calculated by performing an image processing on a metal structure photograph of a cross section of a cast iron including (1) extracting a structure by excluding graphite and (2) extracting a pearlite structure by excluding graphite and ferrite, and then calculating the pearlite fraction of the spheroidal graphite cast iron in accordance with (area of pearlite)/(areas of pearlite+ferrite).
B · US 11,466,349 B2 · ¶ 67
1.3where [C], [Mn], and [V] are contents (weight %) of each component.
In the spheroidal graphite cast iron of the present disclosure, a carbon equivalent (CE value=Content of C (mass %)+⅓×Content of Si (mass %)), which is a value that may be considered in this technical field, is not limited.
B · US 11,466,349 B2 · ¶ 59

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document B has a passage for 1.2 1.3. Both have a passage for 1.1. Both are classified in CPC C22C, as is this patent.

Additional background

Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.

It is a further object of this invention is to propose a chromium-Molybdenum-vanadium cast steel containing Nb, having greater creep rupture time, rupture Elongation and reduction of area under high temperature.
A · US 2008/0138234 A1 · ¶ 6
Another object of this invention to propose a chromium-Molybdenum-vanadium cast steel containing Nb, which can be used for manufacturing turbine casings or other components which are subjected to high temperatures and pressures.
A · US 2008/0138234 A1 · ¶ 7
The present disclosure relates to a spheroidal graphite cast iron, more particularly, to a spheroidal graphite cast iron having an excellent impact strength at low temperature and a method for producing the same.
B · US 11,466,349 B2 · ¶ 2
Therefore, a decrease in an impact strength for the applied impact due to low-temperature embrittlement becomes a problem.
B · US 11,466,349 B2 · ¶ 5
Centerline segregation is directly related to the chemical composition of the steel such as carbon, manganese, sulfur, phosphorus and oxygen and is also primarily responsible for developing shrinkage cavities.
C · US 11,352,683 B2 · ¶ 4

Related claim parts: 1.1

Document C: US 11,352,683 B2, published Jun 7, 2022. Cited for this statement only.

Cite aspatent.fyi, US 2026/0366111 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366111/, SHA-256 105075b37923e0667e7adf5da673378399ca9ba25ca208a58e2a30dcba989f0f
First published
Permanent addresshttps://patent.fyi/US20260366111/
Content fingerprint (SHA-256)105075b37923e0667e7adf5da673378399ca9ba25ca208a58e2a30dcba989f0f
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi