Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Direct bend test control
What ifWhat if the mill uses a bend test to qualify sheet with a component index of 0.95?
Claim language“a component index of 0.85 or less”
A steel heat with 0.045 wt% carbon and 0.50 wt% manganese gives a component index of 0.95. Recrystallization annealing restores ductility after cold rolling, and a 180-degree bend around a mandrel with a radius twice the sheet thickness checks for surface cracking.
1.1Chromium bearing stainless substrate
What ifWhat if the nickel coating covers a ferritic stainless steel substrate containing 17 wt% chromium?
Claim language“Cr: less than 0.030%”
Chromium forms a passive oxide on exposed steel at cut edges. Acid activation followed immediately by a nickel strike provides an adherent base for the bulk electrodeposited nickel coating.
1.2Coarser ferrite with temper rolling
What ifWhat if the sheet uses ferrite with a mean lineal intercept of 15 μm?
Claim language“grain size satisfies 11.00-11.70”
A hold after recrystallization lets ferrite grains grow to a mean lineal intercept of 15 μm. A light temper pass suppresses yield-point elongation so the sheet deforms more uniformly at the start of drawing.
1.3Submicrometer cementite dispersion
What ifWhat if the mean circular diameter of the carbides is 0.4 μm?
Claim language“size satisfying 1.0-2.0 μm”
Rapid cooling after recrystallization limits cementite growth, and a short overaging hold precipitates carbon from ferrite as fine cementite. The overaging step reduces dissolved carbon and limits strain aging before forming.
1.4Direct nickel electrodeposition
What ifWhat if electrodeposited nickel bonds directly to activated steel?
Claim language“an Fe—Ni alloy layer”
The strip is recrystallization annealed before plating, then acid activated and plated with a thin nickel strike followed by nickel from a sulfate bath. The strike provides adhesion, and the continuous nickel deposit provides the surface barrier.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Drawn housings for thermostatic switches
Nickel-plated low-carbon steel sheet with an iron–nickel diffusion layer forms the cup of a thermostatic switch housing. A blanking die cuts a circular blank, and a drawing die forms the cup with an outward rim. An insulated terminal header seats in the cup opening, and a roll crimp captures the header under the rim.
Component substitution
Nickel–cobalt plating on low-carbon steel
An electrodeposited nickel–cobalt coating replaces the pure nickel deposit on the low-carbon steel strip. A mixed nickel and cobalt sulfamate bath deposits the coating on cleaned and activated strip. A reducing-atmosphere anneal diffuses iron into the inner portion of the deposit and leaves a nickel–cobalt-rich outer portion.
Parameter or scale variation
Thinner diffusion layer for shallow lids
A 0.20–0.25 mm steel strip carries a 0.30–0.50 μm iron–nickel diffusion layer on each face. Nickel is electroplated after substrate recrystallization, and a separate short anneal develops the diffusion layer. Polished cross sections and elemental line scans calibrated against reference coupons verify layer thickness before the strip is blanked and formed into shallow lids.
Asymmetric diffusion layers for can ends
The face that becomes the can interior carries a 1.6–2.0 μm iron–nickel diffusion layer, and the exterior face carries a 0.4–0.6 μm layer. Separately powered anode banks deposit different nickel masses on the two faces, and a common anneal diffuses iron into both deposits. Trials set the plating currents and anneal schedule from measured cross sections on each face, and coil identification tracks the interior face through stamping.
Combination with existing systems
Prelaminated strip for welded can bodies
A heated roll laminator bonds a thermoplastic polyester film to the face of the nickel-plated strip that becomes the can interior. Longitudinal gaps in the film expose the metal along both edges of each body blank. A resistance seam welder joins the overlapping edges, and a downstream applicator coats the internal weld and adjacent bare metal with a seam sealant.
Automated or data-driven variant
Model-based control of diffusion annealing
An inline X-ray fluorescence gauge measures nickel coating mass before annealing, and pyrometers and a strip encoder record the strip temperature and residence time. A controller estimates iron–nickel layer thickness from those inputs using a model calibrated with metallographic cross sections. The controller adjusts furnace zone setpoints within a qualified temperature window and records the estimate with the coil position for downstream inspection.
Specific version of a part
Low silicon steel chemistry
The steel contains 0.035 wt% C, 0.020 wt% Si, 0.35 wt% Mn, 0.030 wt% Al, 0.010 wt% P, 0.008 wt% S, 0.004 wt% N, and 0.015 wt% Cr, with the balance iron and residual impurities. The carbon and manganese contents give a component index of 0.70.
Ferrite at grain number 11.4
A continuous recrystallization anneal produces equiaxed ferrite with a grain-size number of 11.4. Optical microscopy of a polished, etched strip section supplies the grain counts used to verify the setting.
Micrometer scale spheroidized cementite
A subcritical hold rounds cementite particles in the ferrite and gives them a mean circular diameter of 1.5 μm. Image analysis converts the section area of each particle to the diameter of a circle with that area and averages the diameters.
One micrometer iron–nickel layer
A continuous line electrodeposits nickel on cleaned steel and heats the plated strip in a reducing atmosphere. Iron and nickel interdiffuse during the hold to form a 1.0 μm alloy layer beneath the remaining nickel.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1by weight %, C: 0.020-0.060%, Si: 0.050% or less, Mn: 0.1-0.6%, Al: 0.010-0.060%, P: 0.015% or less, S: 0.015% or less, N: 0.006% or less, Cr: less than 0.030%, and the balance of Fe and inevitable impurities, and having a component index of 0.85 or less, the component index represented by relational expression 1,
The prealloyed powder consists essentially of, in weight percent, carbon 0.5 to 1.2, nitrogen 0.02 to 0.20, silicon 0.3 to 1.3, manganese up to 1, chromium 6 to 9, molybdenum 0.6 to 2, tungsten 0.5 to 3.0, vanadium 0.2 to 2.0, niobium 1.0 to 4.0, and balance iron and incidental impurities.
A · US 2008/0078475 A1 · ¶ 6
A cold-rolled aluminum killed sheet steel, comprising, by weight, between 0.053 and 0.080% carbon, between 0.15 and 0.424% manganese, between 0.010 and 0.100% aluminum, between 0.0020 and 0.0060% nitrogen, the remainder being iron and impurities resulting from production, and wherein the steel has a content of carbon in solid solution (Css) of at least 52 ppm, wherein the sheet has a rate of elongation of between 3 and 8%.
B · US 9,039,846 B2 · claim 1
1.2wherein an ASTM grain size satisfies 11.00-11.70,
Consequently, the more the cold reduction rate increases, the lower the recrystallization temperature, the smaller the grain size and the higher the Re and Rm.
B · US 9,039,846 B2 · ¶ 27
1.3wherein the steel sheet has a steel microstructure containing carbides having an equivalent circular average size satisfying 1.0-2.0 μm,
The graph in FIG. 4 shows that the alloy of invention contains a larger number of carbides smaller than 0.5 μm, while Alloy A contains larger number of carbides with carbide diameter 0.5-2.5 μm. FIG. 5 also shows that the maximum size of carbides in the alloy of invention is less than 1.5 μm and the maximum carbide size in Alloy A is about 2.5 μm.
A · US 2008/0078475 A1 · ¶ 43
1.4wherein an Fe—Ni alloy layer having a thickness of 0.6-1.4 μm is formed on a surface thereof: component index=C×10+Mn [Relational expression 19
1.5where C and Mn indicate weight % of C and Mn, respectively.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.3. Only Document B has a passage for 1.2. Both have a passage for 1.1. Both are classified in CPC C22C, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
Hot isostatic compaction of nitrogen gas atomized prealloyed powder retains the fine distribution of carbides and makes it possible to obtain the microstructure necessary to achieve both the desired toughness and the wear resistance characteristics required for demanding cold-work applications.
A · US 2008/0078475 A1 · ¶ 1
Niobium also forms very hard Nb-rich MC carbides but its usage in tool steels produced by ingot metallurgy has been limited due to its tendency to form large MC carbides, which has detrimental effects on the toughness of Nb-containing tool steel.
A · US 2008/0078475 A1 · ¶ 3
The present invention concerns a cold-rolled aluminum killed steel sheet intended for manufacturing of packaging, as well as a method of manufacturing packaging, with application in the field of metallic packaging for food, non-food or industrial products.
B · US 9,039,846 B2 · ¶ 1
In practice, however, a very great dispersion is observed of the physical properties of packaging obtained after forming and heat treatment of steel sheet.
B · US 9,039,846 B2 · ¶ 7
Cite aspatent.fyi, US 2026/0366113 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366113/, SHA-256 37635d8970c07cb37e3501908d2de427fd17c078a9d2a1ab156c69e66acfd09f