Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Carburized case over lower-carbon core
What ifWhat if a steel with 0.25 mass % bulk carbon used a carburized surface for contact hardness?
Claim language“C: 0.70 to 0.95%”
Low-pressure carburizing diffuses carbon into the contact surface and establishes a carbon gradient. Quenching forms high-carbon martensite in the case and lower-carbon martensite in the core, and tempering reduces quench stresses.
1.2Vacuum carbon deoxidation
What ifWhat if the melt contained less than 0.05 mass % silicon and used vacuum carbon deoxidation?
Claim language“Si: 0.05 to 0.35%”
Under reduced pressure, dissolved carbon reacts with dissolved oxygen to form carbon monoxide, which leaves the melt as gas. Carbon and oxygen measurements guide the vacuum treatment and the final carbon adjustment before casting.
1.3Sulfur removal before casting
What ifWhat if the steel contained less than 0.05 mass % manganese and used slag refining to control sulfur during hot working?
Claim language“Mn: 0.05 to 0.45%”
A lime-rich reducing slag transfers sulfur out of the liquid steel before casting. Lower dissolved sulfur limits the formation of low-melting iron sulfide films along grain boundaries during hot working.
1.4Nickel-assisted through hardening
What ifWhat if the steel used about 2 mass % chromium and relied partly on dissolved nickel for through hardening?
Claim language“Cr: 3.90 to 4.35%”
A nickel addition delays diffusional transformation of austenite during cooling, while dissolved chromium and molybdenum also contribute to hardenability. Quenching forms martensite, and a subzero treatment before tempering reduces the retained austenite fraction.
1.5Low-temperature tempering for hardness
What ifWhat if the steel used no intentional molybdenum or tungsten addition and obtained its working hardness from low-temperature-tempered martensite?
Claim language“one or both of Mo and W: 3.90 to 4.60%”
Austenitizing dissolves part of the carbide population, and quenching traps dissolved carbon in martensite. Tempering at about 160 to 200 °C reduces quench stresses while retaining high martensitic hardness for service below the tempering temperature.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Bearing rings for industrial spindles
The specified alloy steel forms the inner and outer bearing rings of a high-speed grinding spindle. Forging produces ring blanks, and rough machining leaves stock for finish grinding. After quenching and tempering, the raceways are ground, and the rings are assembled with rolling elements and a cage.
Component substitution
Tungsten substitution for part of molybdenum
Tungsten replaces part of the molybdenum in the melt. The target concentrations are 3.20 mass % Mo and 2.00 mass % W, giving Mo + W/2 of 4.20 mass %. The other alloying elements remain within the stated composition limits, and the cast stock is hot worked before austenitizing and quenching.
Parameter or scale variation
Two aluminum and nitrogen setpoints
Two heats use the same base chemistry with different aluminum and nitrogen targets. One heat contains 0.030 mass % Al and 0.0030 mass % N, giving a negative natural logarithm of the product of about 9.32. The other contains 0.020 mass % Al and 0.0080 mass % N, giving about 8.74. Coupons of the same cross section receive the same austenitizing and quenching cycle, and polished sections are examined for differences in the austenite grain size distribution.
Two austenitizing hold times
Cylindrical coupons 12 mm in diameter are machined from a single forged bar of the specified alloy steel. One batch is held at 1100 °C for 10 minutes, and the other is held at 1100 °C for 30 minutes, with each hold starting when a thermocoupled witness coupon reaches temperature. Both batches use the same quench medium and agitation settings. Sections taken at the same radial locations show how hold time affects the distribution of austenite grain sizes.
Combination with existing systems
Vacuum furnace with gas quenching
Rough-machined rings of the specified alloy steel sit upright on a spaced rack in a vacuum heat-treatment furnace equipped with a recirculating gas quench. A thermocouple on a witness ring tracks temperature during austenitizing. At the end of the hold, the furnace backfills with helium and circulates it through the rack and a heat exchanger to cool the rings. The rings then undergo tempering in a separate furnace.
Automated or data-driven variant
Automated grain mapping across quenched sections
A motorized microscope stage collects overlapping images across polished and etched sections of quenched alloy steel. Software stitches the images, traces the revealed austenite grain boundaries, and flags interrupted traces for operator review. It converts the enclosed areas to physical units using the microscope calibration and reports the largest measured grain area and the grain area distribution by section location.
Specific version of a part
Iron balance with low residuals
Low-residual iron feedstock supplies the balance after the alloying additions. A lime-rich refining slag lowers sulfur, and the finished heat contains up to 0.005 mass % sulfur and 0.010 mass % phosphorus as residual impurities.
Combined aluminum and nitrogen additions
Aluminum wire and a nitrogen-bearing iron addition establish 0.030 mass % aluminum and 0.006 mass % nitrogen in the finished steel. The concentration product gives a negative natural logarithm of about 8.62, and fine aluminum nitride particles restrict austenite grain-boundary motion during heating.
Nitrogen above its stated minimum
The finished steel contains 0.008 mass % nitrogen and 0.015 mass % aluminum. The nitrogen content meets condition (1), and the concentration product gives a negative natural logarithm of about 9.03.
Aluminum and nitrogen product setting
The finished steel contains 0.025 mass % aluminum and 0.004 mass % nitrogen. Multiplying the numerical mass-percent values gives 0.000100, whose negative natural logarithm is about 9.21.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
The cast steel may include 0.08 to 0.12% by weight carbon.
A · US 2008/0138234 A1 · abstract
1.2Si: 0.05 to 0.35%,
The silicon content may be 0.30 to 0.60% by weight, the manganese content may be 0.50 to 0.80% by weight, the chromium content may be 1.20 to 1.50% by weight, the molybdenum content may be 0.90 to 1.10% by weight, and the vanadium content may be 0.20 to 0.30% by weight.
A · US 2008/0138234 A1 · abstract
Preferably the silicon content in the J152 is about 0.8 to 2.1 weight %.
B · US 2014/0076260 A1 · ¶ 34
1.3Mn: 0.05 to 0.45%,
1.4Cr: 3.90 to 4.35%,
1.5according to a relational formula (Mo+W/2), one or both of Mo and W: 3.90 to 4.60%,
1.6V: 0.80 to 1.20%, and
Vanadium can be included in the iron-based alloy in an amount effective to improve the wear resistance and corrosion resistance of the iron-based alloy. Preferably the vanadium content is less than 0.04 weight %.
B · US 2014/0076260 A1 · ¶ 35
1.7a remaining portion: Fe and unavoidable impurities, and
More particularly, the invention provides a heat resistant chromium-molybdenum vanadium steel consisting essentially of 0.08 to 0.12% by weight of carbon, 0.015% by weight or less of sulphur, 0.02% by weight or less of phosphorous, 0.30 to 0.60% by weight of silicon, 0.50 to 0.80% by weight of manganese, 1.20 to 1.50% by weight of chromium, 0.90 to 1.00% by weight of molybdenum, 0.20 to 0.30 by weight of vanadium, the balance being iron apart from incidental impurities, with
A · US 2008/0138234 A1 · ¶ 8
The balance of the J152 alloy is preferably iron and incidental impurities which can include up to 1.0% other elements such as trace amounts of sulfur, and/or phosphorus and carbide formers such as Ti, Zr, Hf, Ta, W and V.
B · US 2014/0076260 A1 · ¶ 35
1.8further comprising Al and N to satisfy the following condition (1) and condition (2),
1.9condition (1): Al: 0.02 mass % or more, or N: 0.005 mass % or more, and
1.10condition (2): 7.5<−ln([Al] %×[N] %)<11.5.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.1. Only Document B has a passage for 1.6. Both have a passage for 1.21.7. Both are classified in CPC C22C, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
It is a further object of this invention is to propose a chromium-Molybdenum-vanadium cast steel containing Nb, having greater creep rupture time, rupture Elongation and reduction of area under high temperature.
A · US 2008/0138234 A1 · ¶ 6
Another object of this invention to propose a chromium-Molybdenum-vanadium cast steel containing Nb, which can be used for manufacturing turbine casings or other components which are subjected to high temperatures and pressures.
A · US 2008/0138234 A1 · ¶ 7
There is a need in the art for improved iron-based alloys for valve seat inserts that exhibit adequate hot hardness, high temperature strength and low cost, as well as corrosion and wear resistance suitable for use in exhaust valve seat insert applications in diesel engines using EGR.
B · US 2014/0076260 A1 · ¶ 6
Further disclosed herein is a valve seat insert for use in an internal combustion engine.
B · US 2014/0076260 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0366114 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366114/, SHA-256 b97e69e3b64cf32b8c9fa74b5a7dfcd9c65455c425f29326c0d4b9dd62d5433f