patent.fyi
Applications  /  US 2026/0366115
United States Patent Application Publication

US 2026/0366115 A1

Published
Nov 19, 2026
Filed
Nov 24, 2023
Earliest date on the face
Dec 21, 2022
Classification
C22C 38/34
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Chromium replaced by phosphorus and antimony

What ifWhat if the alloy omits chromium additions and uses phosphorus and antimony to raise electrical resistivity and control grain boundary mobility?
Claim language“Cr: 0.005 to 5.0%”

The steel melt contains no intentional chromium addition, keeping residual chromium below 0.003 wt%, while adding 0.04 to 0.10 wt% phosphorus and 0.02 to 0.06 wt% antimony to the iron-silicon-aluminum-manganese base. Dissolved phosphorus raises bulk electrical resistivity to limit eddy current loss and increases yield strength for high-speed rotor laminations. Antimony segregates to grain boundaries during final annealing at 850 to 1000 degrees Celsius, suppressing surface nitridation and promoting {100} texture formation.

1.1Low silicon alloyed with high aluminum

What ifWhat if silicon content stays below 1.0 wt% and electrical resistivity is raised by alloying with 4.0 to 5.5 wt% aluminum?
Claim language“Si: 1.5 to 6.5%”

The strip contains 0.3 to 0.9 wt% silicon and 4.0 to 5.5 wt% aluminum, with aluminum atoms substituting in the body-centered cubic iron lattice to raise electrical resistivity above 55 microohm-centimeters. Cold rolling proceeds in a single stage to a final thickness of 0.20 to 0.35 mm without intermediate annealing because the lower silicon fraction reduces brittle ordering at room temperature. Continuous annealing in dry hydrogen at 900 to 1050 degrees Celsius recrystallizes the strip to an average grain diameter of 80 to 130 micrometers.

1.1Aluminum-free steel using vacuum carbon deoxidation

What ifWhat if the steel eliminates aluminum additions below 0.0003 wt% and relies on vacuum carbon deoxidation and silicon for deoxidation and resistivity?
Claim language“Al: 0.0005 to 3.5%”

Molten steel undergoes decarburization and deoxidation under a vacuum below 100 pascals so dissolved carbon removes oxygen as carbon monoxide gas, keeping residual aluminum below 0.0003 wt%. Without aluminum, fine aluminum nitride precipitates do not form during hot rolling or annealing, permitting unhindered grain growth to 100 to 150 micrometers during continuous annealing at 850 to 950 degrees Celsius. Silicon at 2.8 to 3.5 wt% supplies bulk electrical resistivity to limit eddy current loss.

1.2Elevated surface texture balanced by rotation

What ifWhat if the {110}<001> orientation fraction in the outer 1/10 thickness exceeds 10 area % and directional anisotropy is compensated by rotating successive laminations during core stacking?
Claim language“3 area % or less”

Hot rolling with high roll-strip friction and single-stage cold rolling at 65 to 75% reduction produce a shear-induced {110}<001> orientation fraction of 12 to 20 area % in the outer 1/10 thickness layers. During stator or rotor core assembly, stamped laminations are indexed by 90 degrees or 120 degrees between adjacent sheets before interlocking or welding. The staggered easy-magnetization axes average permeability across all in-plane angles in the assembled laminated stack, reducing net magnetic anisotropy of the core.

1.3Deliberate surface inclusions anchoring insulating film

What ifWhat if the inclusion density in the outer 1/50 thickness is intentionally higher than in the interior to anchor an inorganic insulating coating?
Claim language“equal to or less than”

Vacuum degassing reduces bulk sulfur and oxygen below 15 ppm to keep inclusion density low across the sheet interior, while final annealing in a wet nitrogen-hydrogen atmosphere with a dew point of 10 to 30 degrees Celsius forms a dense band of sub-micrometer silica and alumina inclusions within the outer 1/50 thickness. This surface inclusion zone has a higher particle density than the core and mechanically keys a phosphate or silicate insulating film to the steel substrate. The clean interior preserves low bulk hysteresis loss and domain wall mobility across the primary magnetic flux path.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Specific version of a part

Surface silicon gradient without texture suppression

A rolled strip with 3.0 wt% base silicon undergoes chemical vapor deposition in silicon tetrachloride gas at 1050 to 1200 degrees Celsius, depositing silicon on both surfaces while the shear-rolled {110}<001> fraction remains at 6 to 12 area %. Controlled diffusion annealing establishes a silicon gradient from 6.5 wt% at the surface down to 3.0 wt% at the sheet center. The elevated electrical resistivity in the outer 1/10 thickness suppresses high-frequency skin-effect eddy currents while the lower-silicon core maintains magnetic saturation flux density.

High-silicon chromium composition for thin gauges

The alloy contains 3.1 to 3.4 wt% silicon, 0.8 to 1.2 wt% aluminum, 0.25 to 0.40 wt% manganese, 0.5 to 1.2 wt% chromium, and 0.0015 to 0.0030 wt% sulfur, with the balance iron and trace impurities. The combined silicon, aluminum, and chromium levels raise bulk electrical resistivity to 58 to 64 microohm-centimeters while retaining cold-rolling ductility for 0.20 to 0.25 mm strip gauges. Controlled manganese binds residual sulfur into coarse manganese sulfide particles exceeding 0.5 micrometers in diameter so fine precipitates do not pin grain boundaries.

Lubricated rolling suppressing surface shear texture

Hot finishing rolling applies synthetic ester roll-bite lubrication to hold the friction coefficient below 0.15, minimizing subsurface shear strain from the strip surface to 1/10 of the sheet thickness. Subsequent hot-band annealing at 950 to 1050 degrees Celsius for 60 to 180 seconds grows coarse equiaxed grains before single-stage cold rolling at 75 to 85% reduction. Final continuous annealing at 950 to 1050 degrees Celsius produces a {110}<001> orientation fraction of 0.8 to 2.2 area % within the outer 1/10 thickness layer as measured by electron backscatter diffraction.

Two-stage cold rolling with intermediate annealing

Hot-rolled strip of 2.0 to 2.3 mm thickness undergoes a first cold-rolling pass to an intermediate gauge of 0.6 to 0.8 mm, followed by continuous intermediate annealing at 850 to 950 degrees Celsius for 30 to 90 seconds. A second cold-rolling stage applies a 55 to 70% reduction using emulsion-lubricated work rolls with surface roughness below 0.4 micrometers to prevent near-surface shear banding. Final annealing at 980 to 1050 degrees Celsius yields a {110}<001> orientation fraction below 2.5 area % in the outer 1/10 thickness layer.

Hydrochloric pickling and dry hydrogen annealing

After hot-band annealing, the strip passes through a two-stage hydrochloric acid pickling bath at 80 to 90 degrees Celsius followed by abrasive brush scrubbing to remove internal surface oxides and scale-entrained sulfides down to 1/50 of the final thickness. Cold-rolled strip then undergoes continuous final annealing in a dry nitrogen-hydrogen atmosphere with a dew point below minus 40 degrees Celsius to prevent internal oxidation or nitridation near the surface. Cross-sectional scanning electron microscopy confirms that inclusion density from the surface to 1/50 thickness is 0.4 to 0.8 times the inclusion density in the interior.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2009/0169414 A1
Published
Jul 2, 2009
Filed
Oct 12, 2006
Class
C22C 38/60
Document BUS 2022/0333226 A1
Published
Oct 20, 2022
Filed
Aug 26, 2020
Class
C22C 38/008
Claim 1
Document A
Document B
1.1by weight %, Si: 1.5 to 6.5%, Al: 0.0005 to 3.5%, Mn: 0.01 to 3.0%, Cr: 0.005 to 5.0%, S: 0.0005 to 0.03%, and a balance of Fe and inevitable impurities,
0.02% to 0.15% (on the percent by mass basis; hereinafter the same) of carbon (C); 0.004% or less (exclusive of 0 percent) of silicon (Si); 0.6% to 3% of manganese (Mn); 0.02% to 0.2% of phosphorus (P); 0.35% to 1% of sulfur (S); 0.005% or less (exclusive of 0%) of aluminum (Al); 0.008% to 0.03% of oxygen (O); and 0.007% to 0.03% of nitrogen (N), with the remainder being iron and inevitable impurities, wherein the ratio [Mn]/[S] of the manganese content [Mn] to the sulfur con
A · US 2009/0169414 A1 · ¶
Mn: 0.1-2.0%; at least one of Sn and Sb: 0.003-0.2%; Al: 0.2-1.8%; the balance being Fe and inevitable impurities.
B · US 2022/0333226 A1 · abstract
1.2wherein a Goss orientation fraction in a region from a surface to 1/10 t (t: thickness of the steel sheet) in a thickness direction is 3 area % or less, and
1.3wherein a density of inclusions in a region from a surface to 1/50 t (t: thickness of the steel sheet) in the thickness direction is equal to or less than a density of inclusions in the other region.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Both have a passage for 1.1. Both are classified in CPC C22C, as is this patent.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Accordingly, free-machining steels exhibiting good machinability without adding lead (Pb) (lead-free) are demanded.
A · US 2009/0169414 A1 · ¶ 3
By satisfying this, built-up edges can be suppressed, which built-up edges occur in a tool surface upon machining.
A · US 2009/0169414 A1 · ¶ 8
The increase in cold-rolling reduction ratio provides greater energy (deformation energy) for grain growth during the final recrystallization annealing process.
B · US 2022/0333226 A1 · ¶ 4
Cite aspatent.fyi, US 2026/0366115 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366115/, SHA-256 4afb2eab94e19af937433228981e0b694c8549334733b23652e55a2f387ea955
First published
Permanent addresshttps://patent.fyi/US20260366115/
Content fingerprint (SHA-256)4afb2eab94e19af937433228981e0b694c8549334733b23652e55a2f387ea955