Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.6Aluminum replaces silicon for carbide suppression
What ifWhat if aluminum at 1.0% to 1.5% by weight replaces silicon in the alloy while silicon stays below 0.10%?
Claim language“1.35% to 1.65% silicon”
Aluminum dissolves in the iron matrix and remains insoluble in iron carbide, which delays cementite precipitation during the repeated thermal cycles of laser melting and solidification. Carbon partitions from bainitic ferrite into untransformed austenite, stabilizing film-like retained austenite at room temperature to absorb impact energy. Lowering silicon below 0.10% also reduces silicate slag formation on the melt pool surface during layer-by-layer deposition.
1.7Niobium replaces vanadium for grain pinning
What ifWhat if niobium at 0.04% to 0.08% by weight replaces vanadium in the alloy with vanadium omitted?
Claim language“0.09% to 0.11% vanadium”
Niobium combines with carbon and trace nitrogen during solidification and reheating to form nanoscale niobium carbonitride precipitates along austenite grain boundaries. These precipitates pin grain boundaries against coarsening in the heat-affected zone of adjacent laser tracks and contribute precipitation strengthening to the ferrite matrix. Omitting vanadium shifts secondary hardening to higher solutionizing temperatures while maintaining fine prior austenite grain size.
1.4Tungsten replaces molybdenum for hardenability
What ifWhat if tungsten at 0.90% to 1.20% by weight replaces molybdenum in the alloy with molybdenum omitted?
Claim language“0.54% to 0.66% molybdenum”
Tungsten enters substitutional solid solution in iron and slows carbon diffusion during rapid cooling from the laser melt pool, which promotes bainitic and martensitic transformation throughout thick sections. The larger tungsten atomic radius strengthens the matrix and resists softening during multi-pass thermal cycling between 400 °C and 600 °C. Tungsten also suppresses phosphorus segregation at prior austenite grain boundaries, limiting temper embrittlement without molybdenum.
1.5Copper replaces nickel for matrix toughening
What ifWhat if copper at 0.75% to 1.15% by weight replaces nickel in the alloy with nickel omitted?
Claim language“0.675% to 0.825% nickel”
Rapid solidification at cooling rates of 10^4 to 10^6 K/s during laser melting traps copper in supersaturated solid solution without grain-boundary segregation. Subsequent intrinsic reheating from overlying layers precipitates coherent nanoscale copper-rich clusters that strengthen the ferrite matrix while preserving ductility. Copper also acts as an austenite stabilizer, lowering the transformation temperature and refining lath packet size.
1.2Trace boron replaces chromium for hardenability
What ifWhat if boron at 0.0015% to 0.0030% by weight paired with 0.02% titanium replaces chromium in the alloy?
Claim language“0.279% to 0.34% chromium”
Titanium reacts preferentially with dissolved nitrogen to form titanium nitride, leaving boron free to segregate to prior austenite grain boundaries during cooling. Segregated boron lowers grain-boundary energy and delays proeutectoid ferrite nucleation, raising hardenability across the heat-affected zone without chromium. Because boron does not form coarse alloy carbides, the resulting lath microstructure retains high impact toughness.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Wire feedstock for electric arc additive deposition
The iron-based alloy containing carbon, chromium, manganese, molybdenum, nickel, silicon, and vanadium is drawn into solid welding wire with a diameter of 1.2 millimeters for electric arc additive manufacturing. A robotic gas metal arc welding torch feeds the wire continuously onto a preheated low-carbon steel substrate under a shielding gas mixture of 82 percent argon and 18 percent carbon dioxide. The electric arc melts the wire at a deposition rate of 2.5 kilograms per hour to build structural brackets and heavy machinery housings layer by layer. Interpass temperature is held at 250 degrees C between successive beads to control cooling rates and maintain a fine bainitic and martensitic microstructure across thick wall sections.
Component substitution
Niobium microalloying in place of vanadium additions
In the iron-based alloy composition, vanadium at 0.09 to 0.11 weight percent is replaced by niobium at 0.03 to 0.06 weight percent while maintaining the carbon, chromium, manganese, molybdenum, nickel, and silicon weight percentages. The melt is vacuum induction melted and gas atomized using high-purity argon into spherical powder particles ranging from 15 to 45 micrometers in diameter. During laser powder bed fusion and subsequent tempering at 550 degrees C for two hours, niobium forms nanoscale carbide precipitates that pin prior austenite grain boundaries. This grain boundary pinning restricts grain coarsening during repeated thermal cycling and supports high yield strength and notch impact toughness in the consolidated component.
Electron beam fusion replacing laser heat sources
An electron beam powder bed fusion system replaces the optical laser heat source to consolidate the low alloy steel powder inside a vacuum chamber maintained at 0.001 pascals. The electron beam scans each newly spread 70-micrometer powder layer at high speed with defocused current to preheat and lightly sinter the powder bed to 650 degrees C before selective melting. Operating in vacuum eliminates oxygen and nitrogen pickup from shielding gas while the elevated bed temperature reduces thermal gradients and residual stress during solidification. After build completion, the sintered powder cake is removed from the solidified part by media blasting with identical alloy powder inside an enclosed recovery cabinet.
Parameter or scale variation
Coarse powder fraction for high-power directed deposition
The alloy feedstock is gas atomized and sieved to a coarse particle size distribution of 53 to 150 micrometers instead of fine powder bed fusion fractions. A coaxial blown-powder directed energy deposition head delivers the powder at 18 grams per minute into a melt pool generated by a 3000-watt fiber laser with a 3.0-millimeter spot diameter. The deposition head traverses at 12 millimeters per second with a layer height of 0.8 millimeters and a hatch overlap of 45 percent to fabricate near-net-shape forging dies and drive shafts. The silicon content of 1.35 to 1.65 weight percent deoxidizes the large melt pool and inhibits cementite precipitation during the slower solidification cycles of high-power deposition.
Combination with existing systems
Integrated hot isostatic pressing and vacuum tempering line
Components printed from the low alloy steel powder via laser powder bed fusion are transferred directly into a combined hot isostatic pressing and high-pressure gas quenching vessel. The vessel pressurizes the sealed chamber with argon to 150 megapascals at 950 degrees C for two hours to close internal gas pores and lack-of-fusion voids without separate encapsulation. Integrated convective cooling fans circulate chilled argon through internal heat exchangers to cool the parts at 80 degrees C per minute directly to room temperature, forming a uniform martensitic matrix. A secondary thermal cycle inside the same furnace holds the quenched parts at 300 degrees C for two hours to relieve residual stresses and stabilize retained austenite films.
Automated or data-driven variant
Closed-loop optical melt pool control during printing
A laser powder bed fusion machine processing the low alloy steel powder incorporates coaxial high-speed photodiodes and an infrared pyrometer aligned with the scanning optics to measure melt pool emission intensity at 50 kilohertz. A real-time controller compares measured thermal emission against a target cooling curve trained on metallographic datasets linking thermal history to bainite and martensite phase fractions. When thermal accumulation near overhangs or thin walls pushes the predicted cooling rate below the critical threshold, the controller reduces laser power by 5 to 20 percent or increases scan velocity within 200 microseconds. This closed-loop feedback maintains uniform solidification rates across complex geometries and prevents localized cracking or soft heat-affected zones.
Specific version of a part
Prealloyed powder with manganese loss compensation
A vacuum induction melting furnace charges electrolytic manganese to 0.74% by weight before argon gas atomization to account for selective manganese vaporization during laser melting. During powder bed fusion at laser powers of 200 W to 350 W, roughly 0.04% to 0.08% manganese evaporates from the melt pool, leaving a solidified deposit near 0.68% by weight. The retained manganese binds residual sulfur as dispersed manganese sulfide inclusions and stabilizes the austenite phase during cooling.
High-purity electrolytic iron base melt
The alloy balance uses vacuum-degassed electrolytic iron containing less than 0.010% phosphorus, less than 0.008% sulfur, and less than 0.015% oxygen by weight. Limiting these tramp elements prevents low-melting-point eutectic films from forming along interdendritic boundaries during rapid laser solidification. Argon gas atomization converts the molten iron-base alloy into spherical powder particles sized between 15 micrometers and 53 micrometers for uniform powder bed spreading.
High-silicon composition for retained austenite stabilization
Setting silicon at 1.50% by weight suppresses cementite formation during the repeated 300 °C to 450 °C reheating cycles generated by adjacent laser scan tracks. Carbon rejected from newly formed bainitic ferrite laths enriches the surrounding austenite films, stabilizing 5% to 12% retained austenite by volume at room temperature. Under mechanical load, these austenite films transform to martensite and absorb fracture energy.
Vanadium carbide precipitation via post-build tempering
Incorporating 0.10% vanadium by weight keeps vanadium dissolved in the as-built martensitic-bainitic matrix after rapid laser cooling. A post-build tempering treatment at 500 °C to 550 °C for 2 hours precipitates nanoscale vanadium carbide particles 3 nanometers to 10 nanometers in diameter throughout the ferrite laths. These fine carbides pin dislocations to raise yield strength without embrittling prior austenite grain boundaries.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
One embodiment of the present disclosure provides a low carbon steel alloy composition including 98.5-99.7 parts by weight of iron (Fe), 0.1-0.3 parts by weight of carbon (C), 0.1-0.6 parts by weight of silicon (Si) and 0.15-0.45 parts by weight of chromium (Cr).
A · US 2018/0133795 A1 · ¶ 7
1.2about 0.279% to 0.34% chromium;
1.3about 0.63% to 0.77% manganese;
1.4about 0.54% to 0.66% molybdenum;
1.5about 0.675% to 0.825% nickel;
The steel alloy may also include up to 0.03 weight percent phosphorus, up to 0.25 weight percent nickel, up to 0.20 weight percent copper, up to 0.03 weight percent titanium, up to 0.03 weight percent nitrogen, and up to 0.002 weight percent boron.
B · US 2020/0063248 A1 · abstract
1.6about 1.35% to 1.65% silicon;
1.7about 0.09% to 0.11% vanadium; and
The steel alloy includes iron, about 0.34 to about 0.40 weight percent carbon, about 0.8 to about 1.2 weight percent manganese, about 0.40 to about 0.60 weight percent silicon, about 0.04 to about 0.07 weight percent sulfur, about 0.9 to about 1.2 weight percent chromium, about 0.20 to about 0.35 weight percent molybdenum, about 0.08 to about 0.15 weight percent vanadium, and about 0.02 to about 0.06 weight percent aluminum.
B · US 2020/0063248 A1 · abstract
1.8balance comprising essentially iron, wherein % is weight percent based on the entire weight of
The steel alloy comprises at least 95 weight percent iron, about 0.34 to about 0.40 weight percent carbon, about 0.40 to about 0.60 weight percent silicon, about 0.8 to about 1.2 weight percent manganese, about 0.04 to about 0.07 weight percent sulfur, about 0.9 to about 1.2 weight percent chromium, about 0.20 to about 0.35 weight percent molybdenum, about 0.08 to about 0.15 weight percent vanadium, and about 0.02 to about 0.06 weight percent aluminum.
B · US 2020/0063248 A1 · ¶ 6
1.9the low alloy steel composition.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.1. Only Document B has a passage for 1.51.71.8.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The present disclosure relates generally to steel alloys, and more particularly, to steel alloys that have improved castability, as well as components made therefrom, such as crankshafts and transmission shafts.
B · US 2020/0063248 A1 · ¶ 1
Related claim parts: 1.1
Traditional low carbon steel materials contain relatively high amounts of manganese (Mn), which easily evaporates after laser sintering, thus directly influencing the mechanical strength and toughness of the as-formed carbon steel materials.
A · US 2018/0133795 A1 · ¶ 4
When low carbon steel alloy powders with high circularity and high flowing property are used for laser additive manufacturing, the as-formed objects have better mechanical properties and hardness than that of traditional low carbon steel materials.
A · US 2018/0133795 A1 · ¶ 4
Thus, casting of steel saves costs over what is required to harden a forged steel automotive component, but cast parts may have porosity issues.
B · US 2020/0063248 A1 · ¶ 2
This disclosure provides hard steel alloys that can be created by casting with little porosity without the need for the QT process after the forging step.
B · US 2020/0063248 A1 · ¶ 3
Cite aspatent.fyi, US 2026/0366116 A1, claim 1, first published 2026-11-23T20:58:35-05:00, https://patent.fyi/US20260366116/, SHA-256 875a12197657f552774c485ce0660683d441d74986d11cf1875361de161d57b2