patent.fyi
Applications  /  US 2026/0366117
United States Patent Application Publication

US 2026/0366117 A1

Published
Nov 19, 2026
Filed
Sep 4, 2023
Earliest date on the face
Dec 21, 2022
Classification
C22C 38/40
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Direct phase and performance testing

What ifWhat if production lots were accepted using measured phase fraction, corner formability, and hot proof strength?
Claim language“7≤Cr+7Si−3Mn−3Ni−50(C+N)≤14 Formula (1)”

Electron backscatter diffraction measures the ferrite fraction in annealed strip. A trial roll-forming run checks the corners for cracks, and a tensile test at 600 °C measures the 0.2% proof strength against the specified minimum.

1.2Phase calculations with atomic fractions

What ifWhat if the composition inputs were atomic fractions used in a thermodynamic phase calculation?
Claim language“content (wt %) of the respective elements”

The calculation converts each measured elemental mass to moles using its molar mass and divides each result by the total moles, including iron. A thermodynamic model uses those atomic fractions to estimate ferrite and austenite fractions at the annealing temperature.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Square tubing for greenhouse benches

The specified ferritic stainless steel forms the legs and cross rails of greenhouse propagation benches. Roll-form strip into square tubing and weld the longitudinal seam. Bolt the rails to the legs with corner brackets and place removable mesh trays across the rails so irrigation water drains through the bench.

Component substitution

Copper replaces nickel in the melt

Use copper in place of the nickel addition and target 0.40 wt % copper with residual nickel at or below 0.03 wt %. Target 0.010 wt % carbon, 0.015 wt % nitrogen, 0.60 wt % silicon, 0.95 wt % manganese, and 12.0 wt % chromium, with phosphorus and sulfur at the stated limits and iron as the balance apart from residual elements. Add copper during ladle finishing and verify the composition after mixing. Hot-roll the cast slab to strip and check the phase fractions and bend response on coupons before forming tubing.

Parameter or scale variation

Square tube with staged corner forming

Use 2.0 mm strip of the specified steel to make tubing with 60 mm outside flats and a 6 mm inside corner radius. Form and longitudinally weld a round tube, then reshape it in three successive sizing stands with the weld centered on one flat. Set the final stand to the target section and verify the flat dimensions, corner radius, and diagonals on cut sections.

Combination with existing systems

Square tube frame with mineral insulation

Use square tubing made from the specified steel as columns and beams in a bolted frame. Fit mineral wool boards around all four faces of each member and retain them with sheet-metal bands. Stagger board joints and fit separate board pieces around connection plates so the insulation covers the exposed steel. Qualify the assembly under its design load by measuring steel temperature and deflection during a furnace test.

Automated or data-driven variant

Automated ladle chemistry verification

Measure silicon, manganese, chromium, nickel, phosphorus, and sulfur by spark optical emission spectroscopy, carbon by combustion analysis, and nitrogen by inert gas fusion. Software reads the measured weight percentages from the laboratory system, checks each elemental limit, and evaluates Cr + 7Si − 3Mn − 3Ni − 50(C + N). The casting control system releases the heat when every elemental limit passes and the calculated value is between 7 and 14 inclusive. After a chemistry adjustment, the system requires measurements from a fresh ladle sample before release.

Optical feedback for square tube sizing

Install laser profile gauges upstream and downstream of the final sizing stand on a line forming the specified steel into square tube. Fit straight lines to the measured flats and use their intersections to calculate width, height, and the difference between diagonals. Use the downstream measurements to adjust the horizontal and vertical roll gaps within preset limits, with corrections timed to account for the distance from the stand to the gauge. Flag tube lengths with excessive diagonal difference for inspection and use the upstream profile to locate incoming shape errors.

Specific version of a part

Composition near the upper limit

A heat contains 13.30 wt % chromium, 0.70 wt % silicon, 0.80 wt % manganese, 0.30 wt % nickel, 0.010 wt % carbon, and 0.010 wt % nitrogen. Substituting these values into the expression gives 13.90.

Composition near the lower limit

A heat contains 10.80 wt % chromium, 0.45 wt % silicon, 1.10 wt % manganese, 0.75 wt % nickel, 0.012 wt % carbon, and 0.015 wt % nitrogen. Substituting these values into the expression gives 7.05.

Mass percent from heat samples

Spark optical emission spectroscopy measures chromium, silicon, manganese, and nickel on a polished solid heat sample. Combustion analysis measures carbon, and inert gas fusion measures nitrogen. Each result enters the expression in weight percent, so 150 parts per million by mass of nitrogen enters as 0.015.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2011/0061777 A1
Published
Mar 17, 2011
Filed
Jun 18, 2008
Class
C21D 8/02
Document BUS 2022/0090238 A1
Published
Mar 24, 2022
Filed
Sep 21, 2021
Class
C22C 37/10
Claim 1
Document A
Document B
1.17≤Cr+7Si−3Mn−3Ni−50(C+N)≤14 Formula (1):
Vermicular cast iron alloy comprising carbon contents in the range of 2.6% to 3.2%, manganese values between 0.1% to 0.3%, maximum phosphorus of 0.05%, chromium less than 0.06%, tin less than 0.03% and copper less than 0.20%; the alloy characterized by presenting a microstructure with a ferritic matrix comprising at least 90% of ferrite and at least 70% of vermicular graphite; said alloy comprising silicon in the range of 4.60% to 5.70%; and wherein the Ferritization Factor (
B · US 2022/0090238 A1 · claim 1
1.2(wherein Cr, Si, Mn, Ni, C, and N represent the content (wt %) of the respective elements).
Hence, the Cr content is set in the range of 20.5 to 23.5 mass percent.
A · US 2011/0061777 A1 · ¶ 34

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.2. Only Document B has a passage for 1.1.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Hence, development of a punching technique and/or a shearing technique that generates no burrs has been desired.
A · US 2011/0061777 A1 · ¶ 5
However, in the punching work and/or the shearing work, a large burr is generated.
A · US 2011/0061777 A1 · ¶ 8
This set of properties makes it possible to design new engine blocks and heads with complex geometry, high mechanical properties, without compromising machinability, making it attractive both from a technical and economic point of view.
B · US 2022/0090238 A1 · ¶ 1
However, the new requirements of the emission legislation make this search for increasingly resistant materials to be constant, requiring the development of vermicular cast irons with mechanical resistance above 500 MPa.
B · US 2022/0090238 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0366117 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366117/, SHA-256 a40a3e0430b3c571a1603ed9ede9d7438634365e0e450820fb5a9577bc679bff
First published
Permanent addresshttps://patent.fyi/US20260366117/
Content fingerprint (SHA-256)a40a3e0430b3c571a1603ed9ede9d7438634365e0e450820fb5a9577bc679bff
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi