patent.fyi
Applications  /  US 2026/0366118
United States Patent Application Publication

US 2026/0366118 A1

Published
Nov 19, 2026
Filed
Nov 30, 2023
Earliest date on the face
Jan 19, 2023
Classification
C22C 38/42
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.12Interquartile range of nickel concentration

What ifWhat if the nickel concentration check uses the interquartile range in each of the nine squares?
Claim language“a standard deviation of a Ni concentration”

An electron probe microanalyzer maps nickel concentration on a polished section within the 30 μm square. For each 10 μm square, the analysis subtracts the 25th percentile from the 75th percentile and compares the result with a threshold established for that metric.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Guide vane pins for hydropower turbines

Machine guide vane pivot pins from forged bar with a yield strength of 550 to less than 758 MPa and a microstructure containing 10 to 40 volume percent retained austenite, up to 5 volume percent ferrite, and a balance of martensite. Finish-grind the bearing journals after heat treatment and assemble the pins in replaceable bronze bushings in the turbine distributor. The pins transfer hydraulic loads from the guide vanes to the distributor while the bushings support rotation during flow adjustment.

Component substitution

Molybdenum substitution for tungsten in plate

Use molybdenum in place of intentional tungsten additions in a trial plate heat, with 3.0 mass percent molybdenum, 12.0 mass percent chromium, 5.5 mass percent nickel, and 2.0 mass percent copper. Hold the remaining intentional additions within the stated ranges, hot-roll the cast slab, and quench and intercritically temper coupon sets to form martensite and reverted austenite. Qualify the heat treatment by measuring yield strength and phase fractions, mapping local nickel concentration, and measuring pitting resistance in a chloride solution representative of service.

Parameter or scale variation

Expanded nickel mapping across plate thickness

Acquire a 60 μm by 60 μm quantitative nickel map at each of three positions on a polished transverse section at one-quarter, one-half, and three-quarters of the plate thickness. Use a 0.5 μm sampling pitch and divide each map into thirty-six nonoverlapping squares with 10 μm sides. Calculate the nickel concentration standard deviation within each square and record the number of squares at or above 0.50 mass percent separately for each depth.

Two-stage intercritical tempering of thick forgings

Measure the austenite start and finish temperatures on a coupon from the forging heat using dilatometry at the intended heating rate. After quenching the forging, temper it first at 20 °C above the measured start temperature and then at 10 °C above that temperature, cooling to room temperature between stages and holding for 60 minutes per stage after a center thermocouple reaches the setpoint. Set both temperatures below the measured finish temperature so that austenite reversion occurs in a partially transformed structure. Measure yield strength, phase fractions, and local nickel variation at the surface and center to qualify the cycle for the section thickness.

Automated or data-driven variant

Automated scoring of local nickel maps

Use an electron microprobe with wavelength-dispersive detection and a motorized stage to acquire quantitative nickel maps from designated positions on a polished section. Calibrate against a nickel reference of known composition and collect a 60 by 60 grid of measurements at 0.5 μm pitch for each 30 μm square. Software partitions each grid into nine 20 by 20 pixel blocks, calculates the standard deviation of nickel concentration in each block, and flags maps with at least eight blocks at or above 0.50 mass percent. Store the nine results with the specimen identifier, stage coordinates, and calibration record.

Specific version of a part

Manganese at 0.60 mass percent

A low-carbon ferromanganese addition sets the melt to 0.60 mass % manganese. After ladle stirring, optical emission analysis of a solidified sample checks the manganese content.

Nickel at 5.8 mass percent

A metallic nickel addition sets the bulk concentration to 5.8 mass %, as measured on a solidified melt sample. Nickel depresses the martensite start temperature and stabilizes austenite enriched in nickel during tempering.

Molybdenum at 2.5 mass percent

A ferromolybdenum addition sets the melt to 2.5 mass % molybdenum. Molybdenum in solid solution supports repassivation at sites where chloride exposure disrupts the surface film.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2012/0174749 A1
Published
Jul 12, 2012
Filed
Sep 25, 2007
Class
F41H 5/02
Document BUS 11,220,733 B1
Published
Jan 11, 2022
Filed
Dec 1, 2020
Class
C22C 38/44
Claim 1
Document A
Document B
1.1C: 0.030% or less,
Steels G1A and G2A* have the same carbon content of 0.39% C but have two different martensite start temperatures of 196° C. and 255° C. respectively, due to the differences in their manganese and chromium contents.
A · US 2012/0174749 A1 · ¶ 98
1.2Si: 0.50% or less,
1.3Mn: 1.00% or less,
Since excessive residual austenite material is harmful to the performance of the material at high temperature, the contents of Si and Mn are controlled to: Si≤0.6 wt %, Mn≤0.6 wt %, preferably Si: 0.3-0.4 wt %, Mn: 0.2-0.4 wt % in the present application.
B · US 11,220,733 B1 · ¶ 49
1.4P: 0.030% or less,
High P content can result in reduction of toughness at low temperature and high ductile-brittle transition temperature. Therefore, the P content should be also reduced as much as possible in order to avoid or mitigate adverse impacts on the plasticity.
B · US 11,220,733 B1 · ¶ 51
1.5S: 0.0050% or less,
This may be due to S reduces plasticity by forming a sulfide inclusion and leads to crack phenomenon by forming (Fe+FeS) cocrystal in sulfur-containing atmosphere. Therefore, the S content should be reduced as much as possible.
B · US 11,220,733 B1 · ¶ 51
1.6Cu: 0.50 to 3.50%,
1.7Cr: 10.00 to 14.00%,
1.8Ni: 4.50 to 6.50%,
1.9Mo: 1.00 to 3.50%,
1.10W: 0.10 to 0.50%,
1.11Ti: 0.050 to 0.300%,
1.12V: 0.01 to 0.50%, Al: 0.001 to 0.100%, Co: 0.010 to 0.500%, Ca: 0.0002 to 0.0050%, N: 0.0500% or less, O: 0.050% or less, Nb: 0 to 0.500%, Mg: 0 to 0.0050%, As: 0 to 0.100%, Sn: 0 to 0.100%, Sb: 0 to 0.100%, B: 0 to 0.0050%, rare earth metal: 0 to 0.0050%, and the balance: Fe and impurities, wherein: a yield strength is 550 to less than 758 MPa, a microstructure is composed of, in percent by volume, retained austenite in an amount of 10.0 to 40.0%, and ferrite in an amount of 0 to 5.0%, with the balance being martensite, and in the martensitic stainless steel material, a square having sides with a length of 30 μm is defined as a measurement region, and the measurement region is divided into nine specified regions which are each a square having sides with a length of 10 μm, in each of eight or more of the specified regions among nine of the specified regions included in the measurement region, a standard deviation of a Ni concentration is 0.50% by mass or more.
where RA is the volume fraction of the retained austenite in the martensitic microstructure and δ is the thickness of the plate in millimetres.
A · US 2012/0174749 A1 · ¶ 150

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.1 1.12. Only Document B has a passage for 1.3 1.4 1.5.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Current specifications for military and security applications recommend a minimum Brinell hardness range of 540 to 600 BHN or 55 to 60 Rockwell C, and a minimum yield and ultimate tensile strength of 1500 MPa and 1700 MPa respectively, while a minimum Charpy-V impact energy of 13 Joules at −40° C. and a minimum elongation of 6% (50 mm gauge length) is required in South Africa.
A · US 2012/0174749 A1 · ¶ 2

Related claim parts: 1.4 1.5

The inventors believe that neither a higher hardness nor higher mechanical properties are exclusive or even reliable criteria for predicting the ballistic performance of martensitic armour steels.
A · US 2012/0174749 A1 · ¶ 3
Therefore, there are higher requirements for the performance at high temperature, toughness and corrosion resistance and the like of the structural parts used in special working conditions, such as aero-engine pylon.
B · US 11,220,733 B1 · ¶ 2
Cite aspatent.fyi, US 2026/0366118 A1, claim 1, first published 2026-11-23T20:32:38-05:00, https://patent.fyi/US20260366118/, SHA-256 8264c12b93410b7cde956712ab4af26e3e250e41181fd6dadc1024a4d501fcdc
First published
Permanent addresshttps://patent.fyi/US20260366118/
Content fingerprint (SHA-256)8264c12b93410b7cde956712ab4af26e3e250e41181fd6dadc1024a4d501fcdc
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi