Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Direct low temperature impact testing
What ifWhat if measured impact energy at the service temperature replaces the 10 to 35 composition score?
Claim language“from 10 to 35”
A pendulum breaks notched specimens taken from the finished plate after conditioning at −196 °C. For a requirement of 40 J per full-size specimen, the plate passes when each of three transverse specimens absorbs at least 40 J.
1.1Measured austenite retention
What ifWhat if measured austenite retention after cold deformation replaces the nonnegative composition score?
Claim language“0 or greater”
A tensile frame strains a specimen to 5% plastic strain at the service temperature. X-ray diffraction on the gauge section before and after deformation quantifies the austenite fraction, and a minimum retained fraction of 95 vol % sets the acceptance criterion.
1.2Composition expressed as atomic fractions
What ifWhat if the screening model uses atomic fractions of the alloying elements?
Claim language“in weight percent (wt %)”
The calculation divides each measured elemental mass by its atomic mass and normalizes the resulting amounts by the total, including iron. A regression fitted directly to atomic fractions uses measured low-temperature impact energy and yield strength as its response variables.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Support straps for cryogenic instruments
Cut tension straps from solution-annealed sheet of the specified austenitic stainless steel for mounting an infrared detector cold plate. Use three opposed pairs of straps between the cold plate and the room-temperature frame, with bolted clevises at each end. Set the strap preload so that each pair retains tension after cooldown, and size the strap cross section from the mechanical loads and the allowable conductive heat leak.
Component substitution
Tungsten in place of molybdenum
Replace a 0.30 wt % molybdenum addition with 0.50 wt % tungsten using a ferrotungsten charge addition. Target 0.045 C, 0.40 Si, 18.0 Cr, 9.0 Ni, 3.0 Mn, 0.30 Cu and 0.16 N in wt %, with iron and residual impurities as the balance. With Mo set to zero, the two expressions give approximately 33.5 and 4.5, respectively. Hot roll and solution anneal the steel, then measure the retained ferrite fraction and low-temperature impact energy on the finished plate.
Parameter or scale variation
Thin strip with rapid annealing
Cold roll 2.0 mm pickled hot band of the specified steel to 0.8 mm strip in successive passes. Run the strip through a continuous furnace at a line speed that holds the strip metal at 1050 to 1080 °C for 30 to 60 seconds. Water spray cool the strip immediately after it exits the furnace and check the recrystallized grain structure and surface condition on samples from both edges and midwidth.
Controlled cooling for thick plate
Hot roll the specified steel to 25 mm plate and solution anneal it at 1060 to 1090 °C, holding for 15 minutes after the plate center reaches the target range. Transfer the plate directly to a two-sided water spray quench and adjust the upper and lower flows to limit distortion. Use an instrumented trial plate to record the center and surface cooling histories, then inspect the production plate at mid-thickness for carbide precipitation.
Combination with existing systems
Formed bellows in vacuum jacketed piping
Form a thin-wall tube from the specified steel, longitudinally seam weld it, and hydraulically form annular convolutions. Weld the bellows ends to the inner process pipe of a vacuum-jacketed transfer line and use guides to keep pipe movement axial. Size the convolutions for the calculated cooldown displacement and pressure loads, then helium leak test the completed inner assembly before closing the outer jacket.
Specific version of a part
Weight percent from melt samples
Spark optical emission spectrometry measures nickel, chromium, silicon, manganese, copper, and molybdenum on a ground sample from the heat. Combustion analysis measures carbon, inert gas fusion measures nitrogen, and all eight results enter the equations as numerical weight percent values.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1wherein a value calculated by Equation (1) is from 10 to 35 and a value calculated by Equation (2) is 0 or greater, 1.7*[Ni]+410*[C]−0.9*[Cr]−100*[N]−13*[Si]−1.2*[Mn]+2*[Cu]−5.5*[Mo]+40, Equation (1): ([Ni]+0.52*[Cu]+40*([C]+[N])+0.7*[Mn]+45)−(0.48*([Cr]+[Mo]+1.7*[Si]))−51 Equation (2):
Specifically, when the Md30 of formula (1), which is the index of the austenite stability, is at least −50, and the content of C is more than 0.05% by mass, and when the content of (C+N) is at least 0.15% by mass, then the α′ phase having a suitable intensity effective for ductility improvement may be suitably formed.
A · US 2009/0041613 A1 · ¶ 21
1.2wherein [Ni], [C], [Cr], [N], [Si], [Mn], [Cu], [Mo] each represents the content of nickel, carbon, chromium, nitrogen, silicon, manganese, copper, and molybdenum in weight percent (wt %).).
In this, in the site of the symbol of each element in the above formulae (1) to (3), the content of the corresponding element as a value in terms of % by mass thereof is substituted.
A · US 2009/0041613 A1 · ¶ 18
According to another feature of the invention, the nickel-free austenitic stainless steel comprises in mass percent: chromium in amounts of 15<Cr<21%; manganese in amounts of 10<Mn<20%; molybdenum in amounts of 0<Mo<2.5%; copper in amounts of 0.5≦Cu<4%; carbon in amounts of 0.15%<C<1% nitrogen in amounts of 0<N≦1; silicon in amounts of 0≦Si<2%, nickel in amounts of 0≦Ni<0.5%, tungsten in amounts of 0≦W<4%, aluminium in amounts of 0≦Al<3%, and
B · US 2017/0088923 A1 · ¶ 31
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.1. Both have a passage for 1.2. Both are classified in CPC C22C, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
These contain a large quantity (generally at least about 3% by mass) of Mn, as an austenite-forming element in place of Ni, thereby reducing the Ni content therein.
A · US 2009/0041613 A1 · ¶ 5
Related claim parts: 1.2
However, as Ni raw material prices are rising up these days, SUS301 having an Ni content of more than 6% and SUS304 having an Ni content of at least 8% could not be used in some applications owing to their costs.
A · US 2009/0041613 A1 · ¶ 5
The present invention is to provide an Ni-reduced austenite stainless steel having excellent recyclability with no problem of producibility depression to be caused by the surface property thereof and having good workability, season cracking resistance, corrosion resistance and stress corrosion cracking resistance in point of the material characteristics thereof.
A · US 2009/0041613 A1 · ¶ 16
Nickel-free austenitic stainless steel compositions are advantageous for applications in the fields of watchmaking and jewellery since they are non-magnetic and hypoallergenic.
B · US 2017/0088923 A1 · ¶ 3
However, these elements have the effect of increasing some mechanical properties, such as the hardness, elastic limit and strength of the resulting alloys, which makes it very difficult to shape parts by machining and forging, which are the operations usually used in the fabrication of components for watchmaking and jewellery.
B · US 2017/0088923 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0366119 A1, claim 1, first published 2026-11-23T20:58:35-05:00, https://patent.fyi/US20260366119/, SHA-256 75f39a190948b55e9a72a65f105b852986972861f2cdc69aed95cf38301598f1