patent.fyi
Applications  /  US 2026/0366121
United States Patent Application Publication

US 2026/0366121 A1

Published
Nov 19, 2026
Filed
Oct 26, 2023
Earliest date on the face
Dec 20, 2022
Classification
C22C 38/58
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Titanium and boron replacing chromium addition

What ifWhat if the alloy contains no added chromium and uses titanium and boron for hardenability?
Claim language“Cr: 0.10 to 0.30%”

Titanium at 0.015 to 0.030 weight percent binds free nitrogen as titanium nitride precipitates, preventing boron nitride formation during slab reheating. Soluble boron at 0.0010 to 0.0025 weight percent segregates to prior austenite grain boundaries and suppresses coarse ferrite nucleation during accelerated cooling. Controlled finish rolling between 780 and 830 °C followed by water cooling at 15 to 30 °C per second achieves high yield strength and low-temperature impact toughness without chromium.

1.1Ultra-low carbon with copper precipitation hardening

What ifWhat if carbon content stays below 0.025 weight percent and strength comes from copper precipitates?
Claim language“C: 0.030 to 0.100%”

Vacuum degassing lowers carbon to 0.005 to 0.020 weight percent, eliminating brittle cementite networks and improving weld heat-affected zone toughness. Adding 0.80 to 1.20 weight percent copper together with 0.50 to 0.80 weight percent nickel prevents surface hot shortness during hot rolling at 1050 to 1150 °C. Aging the rolled plate between 500 and 580 °C precipitates nanoscale copper-rich clusters that provide the tensile strength needed for high-pressure pipeline service.

1.3Bainite and tempered martensite matrix

What ifWhat if the microstructure consists of lath bainite and tempered martensite?
Claim language“80% or more (including 100%) of ferrite”

Direct quenching after finish rolling at 800 to 840 °C cools the plate at 40 to 70 °C per second to a stop temperature below 300 °C, producing 70 to 85 area percent lath bainite and 15 to 30 area percent martensite. Subsequent tempering at 580 to 640 °C relieves residual transformation stresses and spheroidizes interlath carbides. The resulting fine lath packet structure provides high yield strength and crack-arrest resistance at subzero service temperatures.

1.3Tempered martensite islands as secondary phase

What ifWhat if the secondary phase consists of dispersed tempered martensite islands with no pearlite or bainite?
Claim language“pearlite and bainite as remainders”

Intercritical reheating to 760 to 800 °C partitions carbon into isolated austenite islands occupying 12 to 20 area percent of the ferrite matrix. Rapid water quenching at 50 to 80 °C per second transforms those austenite islands directly into martensite without crossing the pearlite or bainite transformation regions. Low-temperature tempering at 250 to 350 °C toughens the martensite islands, yielding continuous yielding behavior and high uniform elongation for strain-based pipeline service.

1.4Ultrafine surface grains below four micrometers

What ifWhat if the surface layer has an ultrafine average grain size of 1 to 4 μm?
Claim language“average grain size of 10 to 15 μm”

High-reduction finish rolling passes with 35 to 50 percent thickness reduction per pass near the austenite-to-ferrite transformation temperature impose severe shear strain in the outer 2 to 4 millimeters of the plate. Immediate water-spray cooling at 60 to 100 °C per second freezes dynamic recrystallization and limits ferrite grain growth to 1 to 4 μm. The fine surface grain network deflects brittle cleavage cracks and lowers the ductile-to-brittle transition temperature of the pipe wall.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Low-temperature steel plate for liquefied gas storage tanks

A low-carbon microalloyed steel plate with 0.030 to 0.100 wt% carbon, 0.50 to 2.50 wt% manganese, 0.10 to 0.30 wt% chromium, and trace niobium, vanadium, molybdenum, nickel, and aluminum forms the inner structural wall of a refrigerated liquefied gas storage vessel. The plate is rolled to a thickness of 18 to 40 mm with a microstructure containing at least 80 area% ferrite, a remainder of pearlite and bainite, and a surface layer average grain size of 10 to 15 μm in the thickness direction. Curved wall strakes are fabricated by cold bending the plates and joining adjacent edges with multi-pass submerged arc welds using low-hydrogen flux-cored wire. The fine-grained ferritic surface resists brittle crack initiation along weld heat-affected zones at operating temperatures down to -50 °C.

Heavy-wall tubular sections for offshore wind monopile foundations

Heavy-gauge plates of the chromium-manganese low-carbon steel are formed into cylindrical cans with wall thicknesses of 50 to 90 mm and diameters of 6 to 10 meters for offshore wind turbine monopiles. Each plate is thermomechanically rolled to maintain at least 80 area% ferrite with pearlite and bainite remainders and a surface layer average grain size of 10 to 15 μm along both outer and inner faces. Three-roll bending presses form the plates into tubular shells that are joined longitudinally and circumferentially by tandem submerged arc welding. The fine-grained surface microstructure resists fatigue crack initiation under cyclic wave loading and cold marine exposure.

Component substitution

Titanium microalloying substitution for niobium grain refinement

Titanium at 0.010 to 0.025 wt% replaces niobium as the primary precipitation-strengthening and grain-refining microalloy addition in the low-carbon manganese-chromium steel composition. During slab reheating at 1150 to 1220 °C, titanium nitride precipitates pin austenite grain boundaries and limit coarsening before rough rolling. Subsequent finish rolling in the non-recrystallization region and accelerated cooling produce a microstructure with at least 80 area% ferrite, residual pearlite and bainite, and a surface layer grain size between 10 and 15 μm. The resulting steel maintains yield strength through titanium carbide dispersion while eliminating niobium feedstock from the melt charge.

Parameter or scale variation

Ultra-fine surface grain size via high-rate water cooling

A high-pressure laminar water-cooling bank positioned immediately downstream of the finishing mill stand cools the rolled strip surface at 40 to 80 °C per second to a cooling stop temperature of 480 to 540 °C. This accelerated thermal extraction refines the surface layer average grain size in the thickness direction to 5 to 9 μm across the outer 10% of the plate thickness. The core cools at 10 to 20 °C per second, yielding a ferritic matrix exceeding 85 area% ferrite with dispersed bainitic islands and pearlite colonies. Increasing surface cooling intensity raises yield strength by 25 to 45 MPa and lowers the ductile-to-brittle transition temperature by 10 to 20 °C.

Combination with existing systems

Multi-layer fusion-bonded epoxy and polyethylene pipe coating assembly

A welded steel line pipe formed from the ferritic-pearlitic-bainitic chromium-manganese steel is integrated with a three-layer external corrosion-protection system. Abrasive grit blasting prepares the fine-grained steel surface to an anchor profile of 50 to 90 μm, followed by induction heating of the pipe wall to 190 to 210 °C. Electrostatic spray guns apply a 150 to 250 μm fusion-bonded epoxy primer, an extruded copolymer adhesive layer of 200 to 300 μm, and an outer high-density polyethylene jacket of 2.0 to 3.5 mm thickness. The cured composite barrier isolates the low-carbon steel substrate from soil moisture and cathodic disbondment during buried pipeline service.

Automated or data-driven variant

Closed-loop rolling and cooling control using inline sensors

An inline control system pairs optical pyrometers, laser thickness gauges, and an electromagnetic acoustic grain-size sensor with a trained neural network model on the hot strip mill. Sensors sample slab temperature, rolling reduction force, and strip speed at 100 Hz across the roughing stands, finishing stands, and run-out table cooling headers. The model predicts surface ferrite grain size and phase area fractions in real time and adjusts finishing mill roll gaps and water header valve flow rates to hold the surface layer grain size within 10 to 15 μm and ferrite fraction above 80 area%. Post-cooling ultrasonic and metallographic measurements feed back into the training dataset to recalibrate model weights across successive steel heats.

Specific version of a part

Low-carbon niobium-chromium microalloyed steel melt

Basic oxygen steelmaking and ladle refining produce a melt containing by weight 0.055 percent carbon, 0.25 percent silicon, 1.55 percent manganese, 0.20 percent chromium, 0.045 percent niobium, 0.015 percent vanadium, 0.02 percent molybdenum, 0.03 percent nickel, and 0.005 percent copper. Aluminum at 0.030 percent deoxidizes the liquid steel while calcium treatment limits sulfur to 0.003 percent, phosphorus to 0.012 percent, and nitrogen to 0.004 percent. Continuous casting solidifies the melt into 250-millimeter-thick slabs with low centerline manganese segregation.

Polygonal ferrite with fine bainite remainder

Controlled rolling finishes in the non-recrystallization austenite region at 810 to 840 °C to flatten prior austenite grains and increase ferrite nucleation sites. Accelerated laminar water cooling at 12 to 20 °C per second down to a cooling stop temperature of 560 to 600 °C forms 88 area percent polygonal ferrite, 8 area percent fine bainite, and 4 area percent dispersed pearlite. Air cooling to ambient temperature retains this phase balance without forming continuous carbide films along grain boundaries.

Self-tempered surface layer grain control

High-pressure water descaling before roughing and finishing passes maintains uniform surface heat transfer across the upper and lower plate faces. After finish rolling, controlled top-and-bottom laminar cooling lowers the outer 2-millimeter surface layer to 520 °C before internal core heat rebounds the surface temperature to 580 °C. This controlled cooling and self-tempering cycle limits surface ferrite recrystallization and stabilizes an average thickness-direction grain size of 11 to 13 μm.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 8,940,111 B2
Published
Jan 27, 2015
Filed
Sep 28, 2012
Class
C21D 7/13
Document BUS 11,352,683 B2
Published
Jun 7, 2022
Filed
Aug 18, 2020
Class
C22C 38/16
Claim 1
Document A
Document B
1.1by weight %, C: 0.030 to 0.100%, Si: 0.50% or less (excluding 0%), Mn: 0.50 to 2.50%, Nb: 0.070% or less (excluding 0%), V: 0.030% or less (excluding 0%), Mo: 0.05% or less (excluding 0%), Ni: 0.05% or less (excluding 0%), Cr: 0.10 to 0.30%, P: 0.03% or less (excluding 0%), S: 0.050% or less (excluding 0%), Al: 0.050% or less (excluding 0%), N: 0.010% or less (excluding 0%), and Cu: 0.010% or less (excluding 0%), and Fe and unavoidable impurities as a remainder,
By way of example only, the feedstock material for the procedure for achieving the TRIP microstructure with the aid of deformation heat as illustrated in the isothermal transformation curve shown in FIG. 3 may be a high-strength low-alloyed TRIP steel containing 0.2 wt. % C, 1.4 wt. % Si, 1.8 wt. % Mn and a balance of Fe.
A · US 8,940,111 B2 · ¶ 18
The present inventions relates to a steel alloy composition comprising, in weight percent: C: 0.10-0.135, Mn: 0.8-1.2, P: 0.012 max, S: 0.002 max, Si: 0.30-0.40, Cu: 0.20-0.35, Ni: 0.15-0.25, Al: 0.02-0.05, Nb: 0.015-0.030, Mo: 0.06-0.09, the remainder iron and other unavoidable impurities.
B · US 11,352,683 B2 · ¶ 10
1.2wherein the steel material comprises,
1.3as a microstructure, by area %, at least one selected from the group consisting of 80% or more (including 100%) of ferrite, and pearlite and bainite as remainders, and
Both of the above-described methods lead to multi-phase microstructures containing ferrite, bainite and retained austenite.
A · US 8,940,111 B2 · ¶ 6
The material has a ferrite-pearlite microstructure, in normalized and stress relieved condition, appropriate for resisting hydrogen induced cracking, with isolated ferrite and pearlite constituents and no continuous pearlite bands.
B · US 11,352,683 B2 · abstract
1.4a surface layer portion having an average grain size of 10 to 15 μm in a thickness direction.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Both have a passage for 1.1 1.3.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Steel feedstock may preferably be made from low-alloyed steel containing Si, Mn or Al.
A · US 8,940,111 B2 · ¶ 10

Related claim parts: 1.1

The present invention relates generally steel alloys and plates formed therefrom.
B · US 11,352,683 B2 · ¶ 2

Related claim parts: 1.1

The drawback of hot forming lies in that the material is heated to the fully austenitic region, i.e. its temperature is relatively high above Ac3.
A · US 8,940,111 B2 · ¶ 7
These drawbacks are substantially alleviated by the proposed solution.
A · US 8,940,111 B2 · ¶ 8
Plates produced with the alloy exhibit excellent low temperature toughness after normalizing and stress relieving, as well as superior sour gas resistance.
B · US 11,352,683 B2 · ¶ 2
With the increasing exploration of natural oil and gas from sour reserves (rich in H2S), demand for storage vessels for upstream processing units is on the rise and hence steel producing units are challenged with providing steels that offer outstanding resistance to absorbing hydrogen and hence hydrogen-induced delayed cracking.
B · US 11,352,683 B2 · ¶ 3
Cite aspatent.fyi, US 2026/0366121 A1, claim 1, first published 2026-11-23T20:58:35-05:00, https://patent.fyi/US20260366121/, SHA-256 eb512f5b3cb2034eea65c240e1417dedf1dd292e9edfd36a6370b2222605dd09
First published
Permanent addresshttps://patent.fyi/US20260366121/
Content fingerprint (SHA-256)eb512f5b3cb2034eea65c240e1417dedf1dd292e9edfd36a6370b2222605dd09
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi