patent.fyi
Applications  /  US 2026/0366123
United States Patent Application Publication

US 2026/0366123 A1

Published
Nov 19, 2026
Filed
Jan 19, 2024
Earliest date on the face
Jan 19, 2023
Classification
C22C 38/58
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

No entries.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Parameter or scale variation

Cold rolling to thin strip

A reversing mill reduces solution-annealed strip from 1.6 mm to 0.8 mm in four passes, using target exit gauges of 1.35, 1.15, 0.95, and 0.80 mm. A continuous furnace recrystallizes the cold-worked strip, and a rapid cooling section limits precipitation during cooling. Trial runs establish the furnace temperature and line speed from grain-size measurements and extraction-residue results on finished strip.

Thin wall tubing from strip

A tube mill roll-forms 0.6 mm strip and makes an autogenous longitudinal seam weld to produce tubing with a 12 mm outside diameter. A pilger mill reduces the welded shell to an 8 mm outside diameter and a 0.4 mm wall, working the seam and base metal in the same operation. A final recrystallization anneal and rapid cooling set the finished microstructure, and transverse sections provide separate grain-size measurements at the seam and in the base metal.

Specific version of a part

Silicon trim during ladle refining

A ferrosilicon addition during ladle refining sets the final silicon content to 0.30% by mass. Silicon reacts with dissolved oxygen to form silica-bearing oxides that enter the refining slag.

Phosphorus control through charge selection

The furnace charge uses low-phosphorus iron and screened stainless scrap to target 0.025% phosphorus by mass. Optical emission analysis of a solidified melt sample verifies the phosphorus content before casting.

Molybdenum addition for chloride service

A ferromolybdenum addition sets the molybdenum content to 0.80% by mass. Solution annealing followed by rapid cooling retains molybdenum in the austenitic matrix, where it supports repassivation during chloride exposure.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 7,014,720 B2
Published
Mar 21, 2006
Filed
Mar 5, 2003
Class
C22C 38/48
Document BUS 2022/0228243 A1
Published
Jul 21, 2022
Filed
May 20, 2021
Class
C22C 38/001
Claim 1
Document A
Document B
1.1C: 0.005 to 0.150%,
However, if the content of carbon exceeds 0.12%, Cr nitride is increased and weldability is decreased. Thus, the upper limit was set to 0.12%.
A · US 7,014,720 B2 · ¶ 52
1.2Si: more than 0% and 1.00% or less,
(2) the decomposition of the nitriding alloys added to the slag causes the slag pool to boil, which disturbs the remelting process, and it is easy to increase silicon content when using silicon nitride to increase nitrogen content;
B · US 2022/0228243 A1 · ¶ 4
1.3Mn: 0.50% or more and less than 7.00%,
1.4P: more than 0% and 0.050% or less,
1.5S: more than 0% and 0.010% or less,
1.6Cr: 17.0 to 25.0%,
Therefore, Cr content is set to 15–22% and a preferable range of the Cr content is 17–20%.
A · US 7,014,720 B2 · ¶ 58
1.7Ni: 6.5 to 12.0%,
On the other hand, excessive Ni content not only leads to an increase in cost, but also leads to reduction in creep strength. Accordingly, the upper limit is set to 15% and a preferable range of the upper limit is 8.5–13%.
A · US 7,014,720 B2 · ¶ 60
1.8Al: more than 0% and 0.050% or less,
1.9N: 0.15 to 0.50%,
Among them, pressurized induction melting is easy to achieve nitrogen alloying and precise control of nitrogen content by adopting reasonable gas nitriding pressure and casting pressure.
B · US 2022/0228243 A1 · ¶ 4
1.10O: more than 0% and 0.010% or less,
1.11one or two elements selected from a group consisting of Nb: more than 0% and 1.00% or less and V: more than 0% and 1.00% or less,
1.12Mo: 0 to 1.00%, B: 0 to 0.0100%, Cu: 0 to 0.50%, Co: 0 to 0.50%, Ca: 0 to 0.035%, and rare earth metal: 0 to 0.500%, with the balance being Fe and impurities, satisfies Formula (1), Formula (2), and Formula (3), and has a grain size number of 8.5 or more; wherein: when the chemical composition is taken as 100% in percent by mass, a total content of Nb, V, Cr, N, and C in a residue obtained by an extraction residue method is 0.090 to 0.425% in percent by mass; and when the chemical composition is taken as 100% in percent by mass, a content of Cr in the residue obtained by the extraction residue method is 0.180% or less in percent by mass; 2N+C>0.40 (1) −7.1+2.7Ni+0.49Cr+2.0Mo−2.0Si+0.75Mn−5.7C−24N≤24.0 (2) Nb+V≥0.15 (3) where, a content of a corresponding element in percent by mass in the chemical composition is substituted for each symbol of an element in Formula (1) to Formula (3), and if an element is not contained, “0” is substituted for the corresponding symbol of an element.
In some embodiments, it is maintained for 2-3 minutes after adding rare earth.
B · US 2022/0228243 A1 · ¶ 45

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.1 1.6 1.7. Only Document B has a passage for 1.2 1.9 1.12. Both are classified in CPC C22C, as is this patent.

Additional background

Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.

A steam oxidation scale exfoliates and damages the turbine blades or accumulates on the inner surface of the tube at a bent corner, then overheats the corner, which can lead to a possible breakage accident.
A · US 7,014,720 B2 · ¶ 3
In the methods (3) and (4), a formed fine grain in the surface layer easily becomes a coarse grain during high temperature bending, heating treatment and welding in the manufacturing processes, and fine grain could disappear.
A · US 7,014,720 B2 · ¶ 13
(3) in order to improve the uniformity of the composition of the ingot, it is often necessary to remelt twice or even three times.
B · US 2022/0228243 A1 · ¶ 4
The method provided by the present disclosure makes it possible to realize a high-efficiency nitrogen alloying and a uniform nitrogen distribution.
B · US 2022/0228243 A1 · ¶ 6
To improve the mechanical properties and weldability of steels, various alloying elements such as Ti, Nb, Mo, W, B etc. have been added to low and high alloy steels.
C · US 2008/0138234 A1 · ¶ 3

Related claim parts: 1.12

Document C: US 2008/0138234 A1, published Jun 12, 2008. Cited for this statement only.

Cite aspatent.fyi, US 2026/0366123 A1, claim 1, first published 2026-11-23T20:58:35-05:00, https://patent.fyi/US20260366123/, SHA-256 b7228f0ac0503612de4e379cc3809410085a8993374f16a9d4fc64093d592441
First published
Permanent addresshttps://patent.fyi/US20260366123/
Content fingerprint (SHA-256)b7228f0ac0503612de4e379cc3809410085a8993374f16a9d4fc64093d592441
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi