patent.fyi
Applications  /  US 2026/0366124
United States Patent Application Publication

US 2026/0366124 A1

Published
Nov 19, 2026
Filed
Mar 19, 2024
Earliest date on the face
May 26, 2023
Classification
C22C 38/58
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

No entries.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Automated or data-driven variant

Automated ultrasonic mapping of bonded strip

A water-coupled phased-array ultrasonic probe scans the titanium face of the leveled strip while a line encoder records its longitudinal position. The inspection software gates the interface and backwall echoes at depths set using a clad reference coupon with known bonded and unbonded regions. Software maps locations with an increased interface echo and reduced backwall echo and sends their coordinates to a downstream marking station for follow-up inspection.

Specific version of a part

Pickled titanium splash facing

A commercially pure titanium sheet forms a 0.8 mm facing after hot rolling. Pickling removes process scale and exposes a clean titanium surface that develops a passive oxide film in air.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 8,381,631 B2
Published
Feb 26, 2013
Filed
Dec 1, 2008
Class
F41H 5/04
Document BUS 2018/0051365 A1
Published
Feb 22, 2018
Filed
Mar 10, 2016
Class
C22F 1/183
Claim 1
Document A
Document B
1.1wherein the base layer comprises, in addition to Fe and other inevitable impurities, the following chemical elements in mass percentages:
1.2C: 0.050-0.100%, Si: 0.15-0.30%, Mn: 1.0-1.8%, P: 0.0005-0.0030%, S: 0.0005-0.0100%, Cr: 0.80-1.60%, Ni: 0.50-1.20%, Cu: 0.20-0.40%, Al: 0.020-0.050%, Ti: 0.010-0.018%, Nb: 0.020-0.100%, N: 0.0005-0.0050%, and Mo: 0.20-0.50%; and
1.3the corrosion-resistant layer is made of industrial pure titanium, preferably TA1, TA2, TA3, or TA4.
In one embodiment, the outer layer 12 may be formed from commercially pure titanium (CP-Ti) and the inner layer 14 may be formed from a titanium alloy, such as titanium 6Al-4V (Ti-64), also known as “military-grade titanium.” As used herein, the terms “Titanium 6Al-4V,” “Ti-64,” and “military-grade titanium” mean a titanium alloy consisting essentially of about 5.5% to about 6.75% aluminum, about 3.5% to about 4.5% vanadium and about 87.5% to about 91% titanium.
A · US 8,381,631 B2 · ¶ 19
Commercially pure titanium (CP Ti) is used within the chemical and medical industry because of its high corrosion resistance and biocompatibility and is defined within grades 1-4 whereof grade 1 is the purest with the lowest strength.
B · US 2018/0051365 A1 · ¶ 3

An empty cell means only that no passage was reproduced there.

Why these two documents?

Both have a passage for 1.3.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Limiting factors for the usage of CP Ti are basically low yield strength (about 274 MPa) and low tensile strength (about 345 MPa).
B · US 2018/0051365 A1 · ¶ 3

Related claim parts: 1.3

Army Research Lab, however, indicates that relatively thick monolithic titanium 6Al-4V plate suffers from adiabatic shear plugging failures.
A · US 8,381,631 B2 · ¶ 3
In view of the above, it would be advantageous to provide improved titanium-type armor and improved methods of manufacturing titanium-type armor.
A · US 8,381,631 B2 · ¶ 4
Hence, there is still a need for a process that will provide a CP Ti product having a combination of high tensile strength and high ductility and good fatigue properties.
B · US 2018/0051365 A1 · ¶ 6
Hence, the present disclosure will provide a process to improve the combined mechanical properties of a product of commercially pure titanium by applying plastic deformation at cryogenic temperatures on an object until the product is formed, and thereafter heat-treating the obtained product.
B · US 2018/0051365 A1 · ¶ 10
Cite aspatent.fyi, US 2026/0366124 A1, claim 1, first published 2026-11-23T20:58:35-05:00, https://patent.fyi/US20260366124/, SHA-256 a71b92ff08b3434e1a6c3e53fa1c2c384e51f30b37862de56df5db864afad6b7
First published
Permanent addresshttps://patent.fyi/US20260366124/
Content fingerprint (SHA-256)a71b92ff08b3434e1a6c3e53fa1c2c384e51f30b37862de56df5db864afad6b7
Methodv2026-11-18.2 · automated, not reviewed by a person