Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.2Titanium nitride reflective barrier film
What ifWhat if a sputtered titanium nitride coating replaces the chromium layer on the first substrate?
Claim language“a chromium layer”
Reactive magnetron sputtering deposits a 40 nm to 120 nm titanium nitride film onto the first substrate from a titanium target in an argon-nitrogen gas mixture at 0.3 Pa to 0.8 Pa. The ceramic metallic film provides optical reflectance, corrosion resistance, and a hard wear surface without elemental chromium. The adhesive layer bonds directly to the nitrided surface after plasma cleaning.
1.2Low-chromium nickel alloy reflective coating
What ifWhat if the metallic layer is a nickel-chromium alloy with 20% chromium by weight?
Claim language“comprising at least 90% chromium, by weight”
Direct-current magnetron sputtering from a single 80% nickel and 20% chromium alloy target deposits a 50 nm to 150 nm metallic film on the first substrate. The nickel-rich matrix lowers internal tensile stress in the film and resists cracking during thermal cycling between -40 C and 85 C. A thin native chromium-nickel oxide skin forms on the film surface and provides hydroxyl sites for bonding to the adjacent layer.
What ifWhat if a thermoplastic polyvinyl butyral interlayer bonds the metallic layer to the second substrate?
Claim language“at least one of epoxy, polyurethane (PU), polysulfide (PS), acrylate, and silicone”
A 0.38 mm to 0.76 mm extruded polyvinyl butyral sheet sits between the coated first substrate and the second substrate. Vacuum de-airing at 80 C removes trapped gas, followed by autoclave lamination at 135 C to 145 C and 1.0 MPa to 1.4 MPa for 45 minutes. The softened thermoplastic flows into surface micro-roughness and forms a cohesive laminated stack upon cooling.
1.4Direct thermal diffusion metallic bonding
What ifWhat if direct solid-state diffusion bonding joins the second substrate to the chromium layer without an adhesive layer?
Claim language“an adhesive layer”
A 20 nm titanium or copper tie layer is sputtered onto both the chromium surface and the mating face of the second substrate inside a vacuum chamber. Pressing the two surfaces together at 300 C to 400 C under 5 MPa to 15 MPa in vacuum drives atomic interdiffusion across the interface. The resulting metallic joint holds the two substrates together without any polymeric bonding material.
1.3Spray-applied protective polymer topcoat
What ifWhat if a liquid-applied curable polymer topcoat replaces the second substrate over the metallic coating?
Claim language“a second substrate”
An airless spray head or slot-die coater deposits a 50 micrometer to 200 micrometer liquid fluoropolymer or polyurea resin directly over the coated side of the first substrate. Thermal curing at 120 C for 20 minutes cross-links the resin into a continuous protective barrier film. The cured topcoat shields the metallic layer from abrasion and moisture without laminating a separate sheet.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Reflective thermal barrier laminate for aerospace cryogenic tanks
A first substrate of polyimide film carries a sputtered metallic chromium layer with at least 95 percent chromium by weight on one face. A silicone pressure-sensitive adhesive bonds a woven aramid fabric second substrate to the chromium surface to form a multi-layer cryogenic insulation blanket. The blanket wraps around liquid propellant storage vessels with the polyimide side facing the external vacuum jacket so infrared radiation reflects away from the cold tank wall. The aramid backing provides tear resistance and mechanical anchoring for tie-down straps during launch vibration and thermal cycling between 20 kelvin and 300 kelvin.
Electromagnetic interference shielding laminate for medical imaging rooms
A rigid gypsum wallboard panel serves as the first substrate coated with a 180 nanometer sputtered metallic chromium layer exceeding 98 percent chromium by weight. A continuous silicone adhesive layer of 100 micrometers thickness bonds a decorative vinyl wall covering as the second substrate directly over the chromium face. Conductive metal seam tape bridges adjacent panels along the wall joints to establish an uninterrupted electrical ground plane across the room enclosure. The laminated wall panels attenuate external radio-frequency signals between 10 megahertz and 1 gigahertz to prevent signal artifacts during magnetic resonance imaging scans.
A magnetron sputtering cathode composed of 80 percent nickel and 20 percent chromium by weight deposits a resistive alloy film onto a polyimide first substrate in place of a 90 percent chromium layer. An epoxy adhesive film of 25 micrometers thickness sits directly on the alloy surface and bonds a fiberglass-reinforced resin second substrate under a heated hydraulic press at 160 degrees Celsius and 1.5 megapascals. Copper terminal strips contact exposed edges of the nickel-chromium layer where the adhesive stops short of the substrate perimeter. Passing direct current through the terminals generates uniform resistive heating across the laminated panel for surface de-icing assemblies.
Parameter or scale variation
Thick electroplated chromium barrier for high-wear industrial chutes
A stainless steel sheet of 2.0 millimeters thickness serves as the first substrate and receives an electroplated metallic chromium layer with a thickness of 15 micrometers and a purity of 99 percent chromium by weight. A two-part structural polyurethane adhesive layer of 400 micrometers thickness covers the chromium surface and cures at 25 degrees Celsius for 24 hours under 0.2 megapascals clamping pressure. A vulcanized rubber sheet of 5.0 millimeters thickness forms the second substrate bonded to the adhesive layer. The resulting thick-gauge laminate absorbs impact energy from abrasive bulk ore on the rubber side while the thick chromium-plated steel provides rigid structural backing and corrosion resistance.
Combination with existing systems
Chromium laminate integrated into roll-to-roll flexible photovoltaic modules
A continuous web of flexible polycarbonate film carries a 50 nanometer vapor-deposited chromium layer and feeds into a rotary laminator paired with an inline thin-film photovoltaic cell assembly line. An optical-grade acrylate adhesive dispenses from a slot-die coater at 15 micrometers wet thickness between the chromium layer and the rear encapsulation sheet of the photovoltaic cell array. Ultraviolet curing lamps positioned downstream of the nip rollers crosslink the acrylate adhesive at a web speed of 10 meters per minute to seal the laminated backsheet to the solar cells. The chromium layer blocks moisture vapor ingress from the rear face and reflects unabsorbed long-wavelength light back into the semiconductor absorber layer.
Automated or data-driven variant
Closed-loop optical control of chromium deposition and lamination
An inline spectroscopic ellipsometer positioned immediately after a vacuum coating chamber measures the real-time thickness and optical reflectance of the chromium layer on the moving first substrate at 100 hertz. A proportional-integral-derivative controller compares the measured thickness against a 40 nanometer setpoint and adjusts the direct-current sputtering power supply and web transport speed to maintain thickness within 1.5 nanometers. Downstream, a line-scan infrared camera inspects the dispensed polyurethane adhesive layer for voids and coating weight deviations before the second substrate enters the lamination nip. A trained convolutional neural network classifies defect maps from the infrared images in real time and modulates the slot-die pump pressure and nip roller force to eliminate air entrapment.
Specific version of a part
Soda-lime float glass optical substrate
The first substrate is a 2.0 mm to 4.0 mm annealed soda-lime silicate float glass sheet with surface roughness below 1 nm root-mean-square. Before coating, an alkaline detergent wash, deionized water rinse, and argon ion-beam etch remove organic residues from the glass face. The smooth, thermally stable glass provides a flat optical base for vapor deposition.
Magnetron-sputtered high-purity chromium film
A planar direct-current magnetron sputter cathode fitted with a 99.95% by weight chromium target deposits a 60 nm to 120 nm metallic film onto the first substrate. Deposition runs in pure argon at 0.25 Pa to 0.5 Pa with a target power density of 4 W/cm^2 to 8 W/cm^2 to produce a dense columnar microstructure. The resulting film exhibits high specular reflectance and forms a 2 nm to 4 nm native chromium oxide passivation layer upon air exposure.
The second substrate is a 1.5 mm to 3.0 mm woven glass-fiber reinforced epoxy laminate sheet positioned parallel to the chromium-coated face of the first substrate. Mechanical abrasion with 320-grit aluminum oxide followed by solvent wiping increases surface area on the bonding face. The composite backing plate adds structural rigidity and impact resistance to the laminated assembly.
A metered static-mixing dispenser applies a 0.5 mm to 1.5 mm thick two-component polyurethane adhesive between the chromium surface and the second substrate. The formulation reacts an aliphatic isocyanate prepolymer with a polyether polyol at a 1:1 stoichiometric index and cures at 23 C and 50% relative humidity over 24 hours. The cured elastomer accommodates differential thermal expansion between the coated first substrate and the second substrate while maintaining peel strength.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
In a case in which the substance responsible for corrosion is generated in the organic solvent, the substance may attack a metal substrate, thereby allowing a polyolefin resin layer to exfoliate.
A · US 10,741,802 B2 · ¶ 51
Alternatively, even if cracks occur, the exposure of a base metal is suppressed by the iron-nickel diffusion layer, thereby enabling the post-working corrosion resistance to be significantly enhanced.
B · US 2021/0324532 A1 · ¶ 24
1.2a chromium layer disposed on the first substrate, the chromium layer comprising at least 90% chromium, by weight;
The hydrated chromium oxide layer is disposed on the metal chromium layer.
A · US 10,741,802 B2 · ¶ 77
The metallic chromium layer includes a flat-like metallic chromium sublayer and a granular metallic chromium sublayer placed on a surface of the flat-like metallic chromium sublayer.
B · US 2021/0324532 A1 · abstract
1.3a second substrate disposed adjacent to the chromium layer opposite to the first substrate; and
The hydrated chromium oxide layer is important for securing favorable adhesiveness to a polyolefin resin layer in the case of forming the polyolefin resin layer on the hydrated chromium oxide layer.
A · US 10,741,802 B2 · ¶ 77
1.4an adhesive layer comprising an adhesive comprising at least one of epoxy, polyurethane (PU), polysulfide (PS), acrylate, and silicone, and at least partially disposed between the chromium layer and the second substrate, wherein the adhesive layer bonds the second substrate to the chromium layer.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.3. Both have a passage for 1.11.2.
Additional background
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
However, decreases in the strength of the containers due to the thinning cause a risk that external force or stabbing allows the containers to be deformed or broken, thereby resulting in leakage of the electrolytic solutions which are contents.
A · US 10,741,802 B2 · ¶ 3
In such trends, attention has been focused on thinning of secondary battery containers as a tool enabling larger quantities of electrolytic solutions and active materials to be put in limited capacities, whereby battery capacities can be increased.
A · US 10,741,802 B2 · ¶ 3
However, in industrial production, there are many problems such as the risk that the contents are contaminated with a metal powder after polishing, an increase in maintenance load such as the cleaning of a can-making machine, and the risk of occurrence of fire due to the metal powder.
B · US 2021/0324532 A1 · ¶ 4
According to this technique, the granular protrusions of metallic chromium break a chromium oxide layer which is a surface welding inhibition factor during welding, thereby enabling the contact resistance to be reduced and the weldability to be improved.
B · US 2021/0324532 A1 · ¶ 5
Therefore, the metal chromium layer exhibits good corrosion resistance together with the chromium-containing layer disposed thereon.
C · US 2021/0254235 A1 · ¶ 29
Related claim parts: 1.2
Document C: US 2021/0254235 A1, published Aug 19, 2021. Cited for this statement only.
Cite aspatent.fyi, US 2026/0366135 A1, claim 1, first published 2026-11-23T20:58:35-05:00, https://patent.fyi/US20260366135/, SHA-256 b7c50c31ec71288a825fef6e54291008c26e7d5427cba5fd5293ef964db24b07