Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Rotating cylindrical sputtering surface
What ifWhat if the sputtering surface is the curved outer wall of a rotating tube?
Claim language“a central planar region”
A stationary magnet assembly inside the tube confines the plasma along a longitudinal strip. The tube rotates through the strip to distribute erosion around its circumference, and coolant flows through the tube interior.
1.1Vertical perimeter wall
What ifWhat if the planar sputtering face ends at a vertical perimeter wall?
Claim language“a tapered peripheral edge region”
The target has a constant diameter from its sputtering face to its backing plate. A grounded annular shield overlaps the perimeter with a clearance gap that maintains electrical isolation and intercepts deposition near the wall.
1.1Concave central sputtering surface
What ifWhat if the central sputtering surface forms a shallow spherical recess?
Claim language“a central planar region”
A machined target blank presents a continuous concave face to the plasma, and a magnet assembly behind the blank confines the discharge to an annular band on that face. The recess changes the local surface angle across the band and thereby changes the angular distribution of sputtered material.
1.2Shielded polished target taper
What ifWhat if a polished target taper sits behind a replaceable annular shield?
Claim language“comprises a roughened portion”
A grounded shield overlaps the taper and leaves a clearance gap to the biased target. The shield intercepts redeposition directed toward the taper, and maintenance replaces the shield when its coating reaches the specified thickness.
1.2Fine blasted taper texture
What ifWhat if the roughness on the taper is Ra 12 to 20 micrometers?
Claim language“greater than or equal to 60 micrometers”
Fine abrasive blasting produces a distributed texture on the taper, and a stylus profilometer verifies Ra along the sloped surface. The asperities provide anchoring sites for redeposited material.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Reflective coatings for telescope mirrors
An aluminum sputtering target with a planar center and a tapered rim faces a rotating fixture that holds a glass mirror blank. A band on the tapered rim terminates near the upper outer edge and has a profile roughness Ra of at least 60 micrometers. An argon discharge sputters aluminum onto the optical surface while fixture rotation averages the deposition rate around the mirror axis.
Component substitution
Stepped rim with a textured terrace
A machined annular step replaces the tapered rim of a circular titanium target and forms a recessed horizontal terrace between the central sputtering face and the outer wall. A pulsed laser textures the terrace to a profile roughness Ra of at least 60 micrometers, measured after removing the nominal terrace form from the profile. The mounting clamp bears on a separate outer land and leaves the textured terrace exposed to collect redeposited coating material.
Parameter or scale variation
Wide target with a localized rough band
A circular aluminum target has a 300 millimeter outside diameter and a 280 millimeter diameter planar face. The surrounding taper descends outward at 30 degrees to the face, with a 4 millimeter wide circumferential band centered on the taper and measured along its slope. The band has a profile roughness Ra of 75 to 100 micrometers after removal of the nominal taper from the measured profile. The target mounts with the magnetron erosion track inside the planar face and the band exposed to material redeposited at the perimeter.
Combination with existing systems
Inline coating of stainless steel web
A rectangular chromium target mounts on a planar magnetron above a stainless steel web that travels between unwind and rewind rolls in a vacuum chamber. The target has a planar sputtering face surrounded by a tapered border, with a roughened band of at least 60 micrometers Ra along both long sides. A chilled drum supports the web beneath the target, and the long axis of the target spans the web width. The web drive holds a constant line speed while an argon discharge deposits chromium on the moving strip.
Dual cathodes for reactive oxide deposition
Two aluminum targets mount side by side on electrically isolated magnetron cathodes in a chamber supplied with argon and oxygen. Each target has a planar center and a tapered perimeter with an exposed band of at least 60 micrometers Ra. A bipolar power supply alternates the polarity of the two cathodes so that each target serves in turn as the sputtering surface and the electron return surface. A substrate carrier passes beneath both cathodes as aluminum reacts with oxygen to form an aluminum oxide film.
Automated or data-driven variant
Closed-loop laser texturing of the taper
A rotary fixture holds a circular titanium target beneath a pulsed laser and an optical profilometer, with both heads aligned to a band on the tapered perimeter. The controller indexes the target through successive angular sectors and textures each sector with overlapping laser passes. After each pass, the profilometer scans along the taper, and the controller removes the nominal slope and calculates profile Ra using the same cutoff and evaluation length in every sector. The controller repeats texturing in sectors below 60 micrometers Ra and stops when all sampled sectors meet the threshold.
Specific version of a part
Aluminum disk with conical taper
A machined aluminum disk has a flat circular sputtering face and a conical peripheral band inclined 30 degrees to the face. The band terminates at a circular upper outer edge.
Copper plate with straight tapers
A rectangular copper target plate has a ground central planar face and a milled tapered band along each side. The bands meet at mitered corners and terminate at the upper outer edges of the plate.
Coarse blasted titanium taper
Coarse abrasive blasting roughens a masked annular portion of the titanium taper to Ra 65 to 85 micrometers. A stylus profilometer traces the band along the slope and removes the nominal taper form before calculating Ra.
Laser textured molybdenum taper
A pulsed laser scans a band on the molybdenum taper in overlapping passes to form a distributed pattern of depressions and ridges. Profile measurements along the band verify Ra 70 to 90 micrometers after removal of the nominal taper form.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a material to be sputtered having a central planar region, the central planar region having a tapered peripheral edge region which terminates at an upper outer edge
Moreover, the term “tapered part” refers to a portion which was subject to chamfering relative to the lateral face of the target at the outer peripheral edge of the sputter surface of the sputtering target, and is a portion which substantially does not contribute, or which hardly contributes, to the deposition.
A · US 2019/0078195 A1 · ¶ 30
And the term “tapered part” refers to the part that is subject to chamfering at the outer peripheral part on the sputtering surface of the sputtering target, and is a part that does not substantially contribute, or hardly contributes, to the deposition. Moreover, the term “flat part” refers to the part of the sputtering surface excluding the tapered part which substantially contributes to the deposition.
B · US 10,984,992 B2 · ¶ 29
1.2wherein a portion of the tapered peripheral edge comprises a roughened portion have an average roughness (Ra) of greater than or equal to 60 micrometers.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The present invention relates to a sputtering target capable of stably exciting/generating initial plasma (also referred to as ignition or plasma ignition) at the start of sputtering.
A · US 2019/0078195 A1 · ¶ 1
Related claim parts: 1.1
Thus, considered was the production of a target comprising characteristics that would only affect the ignition process, and would not contribute to the subsequent deposition.
B · US 10,984,992 B2 · ¶ 8
Related claim parts: 1.1
Under the foregoing circumstances, an ultrahigh purity target material entails a problem in that the ignition process tends to become unstable, and there is a dilemma of using a low purity product to increase the ignition success rate, or using a high purity product to improve the quality.
A · US 2019/0078195 A1 · ¶ 8
The present invention relates to a sputtering target capable of stably performing ignition (plasma ignition) during sputtering.
B · US 10,984,992 B2 · ¶ 1
Under the foregoing circumstances, an ultrahigh purity material tends to cause the ignition process to become unstable, and there is a dilemma of using a low purity product in order to improve the ignition success rate, or using a high purity product in order to improve the quality.
B · US 10,984,992 B2 · ¶ 7
Cite aspatent.fyi, US 2026/0366137 A1, claim 1, first published 2026-11-23T20:58:35-05:00, https://patent.fyi/US20260366137/, SHA-256 9688172ca15ba8b38b095b00b1f6f4ebb2254a781d1eb8a6783ea50992183b6a