Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Unfused single-crystal alloy nanoparticles
What ifWhat if the core consists of unfused single-crystal iron-platinum nanoparticles?
Claim language“fusing superparamagnetic iron oxide nanocrystals”
Monodisperse iron-platinum nanocrystals are synthesized by thermal decomposition in high-boiling organic solvents to a uniform diameter of 18 to 22 nanometers. Each individual crystal exhibits high saturation magnetization and sharp magnetization reversal in a 25 kilohertz drive field without inter-particle lattice fusion. A silica shell coats each separate crystal surface to provide attachment sites for surface ligands.
What ifWhat if a cross-linked polymer shell locks particle rotation without binding a paramagnetic quencher?
Claim language“binding a paramagnetic quencher”
A dense cross-linked hydrogel network surrounds each magnetic core and restricts physical rotation in an alternating magnetic field. Restricting physical rotation broadens the magnetization curve and reduces third-harmonic and fifth-harmonic signal amplitudes. Cleavage of the cross-links releases the core into solution, restoring rotational relaxation and increasing the harmonic signal.
1.3Reversible non-covalent displacement without bond cleavage
What ifWhat if the sensing species undergoes non-covalent competitive displacement without any cleavable bond?
Claim language“cleavable by a target chemical species”
A single-stranded nucleic acid aptamer tethers the paramagnetic complex to the nanoparticle surface through complementary base-pair hybridization to a surface-anchored capture strand. When the target molecule binds to the aptamer, the aptamer folds into a tertiary structure that dissociates from the capture strand without breaking covalent bonds. Separation of the paramagnetic complex from the core surface restores the magnetic particle imaging harmonic signal.
1.4Benchtop magnetic susceptometry without spatial imaging
What ifWhat if alternating-current magnetic susceptibility spectroscopy replaces magnetic particle imaging?
Claim language“performing magnetic particle imaging”
A sample of fluid containing the nanoparticles sits inside a paired circular excitation coil and a concentric gradiometric pickup coil without spatial gradient fields. A swept-frequency sinusoidal magnetic field from 100 hertz to 100 kilohertz excites the nanoparticles while a lock-in amplifier records the in-phase and quadrature susceptibility spectra. Changes in the relaxation peak frequency and amplitude quantify target concentration directly in the bulk sample.
1.5Sensitivity to local tissue temperature
What ifWhat if the nanoparticle signal responds to local tissue temperature rather than chemical species concentration?
Claim language“sensitive to concentration of the target chemical species”
A thermoresponsive polymer brush with a lower critical solution temperature of 40 degrees Celsius tethers the paramagnetic complex to the magnetic core. Below 40 degrees Celsius, the extended polymer holds the quencher away from the core surface, whereas heating above 40 degrees Celsius collapses the polymer and brings the quencher into close proximity. The resulting drop in harmonic signal maps thermal gradients across the subject during hyperthermia.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Industrial pipeline corrosion monitoring with cleavable probes
Fused iron oxide nanocrystal clusters are functionalized with acid-labile hydrazone or sulfide-cleavable disulfide linkers tethered to a paramagnetic chelate quencher and dispersed into a process fluid stream or an internal pipe coating matrix. When localized metal corrosion or sour gas ingress elevates hydrogen ion or hydrogen sulfide concentrations, the target chemical species cleaves the linker and releases the paramagnetic quencher from the cluster surface. An external magnetic particle imaging coil array scans the pipe wall at an excitation frequency between 20 kHz and 25 kHz. The system maps the resulting unquenched harmonic magnetization signal to locate active corrosion zones through opaque metallic or composite walls.
Component substitution
Photo-cleavable organic radical quenchers on cluster surfaces
An organic nitroxide radical species, such as a stable piperidine-based radical, replaces the metal-ion paramagnetic quencher on the fused iron oxide cluster surface. A photocleavable ortho-nitrobenzyl ester serves as the sensing linker between the cluster surface and the organic radical. Exposure to ultraviolet or near-infrared two-photon illumination cleaves the ester bond, releasing the nitroxide radical and restoring the superparamagnetic harmonic response of the cluster. This metal-free quenching assembly prevents heavy-metal ion leaching while enabling spatially gated probe activation prior to magnetic particle imaging readout.
Microwave-assisted polyol synthesis for fused nanocrystal clusters
Microwave-assisted polyol synthesis replaces hydrothermal synthesis to form the fused superparamagnetic iron oxide nanocrystal clusters using diethylene glycol or triethylene glycol as both solvent and reducing agent. Iron acetylacetonate or iron chloride precursors are heated by 2.45 GHz microwave irradiation to 200 degrees Celsius for 15 to 45 minutes in the presence of a polyacrylic acid stabilizer to yield fused clusters with controlled inter-crystallite grain boundaries. After washing, the carboxyl-terminated cluster surfaces are conjugated via carbodiimide coupling to a protease-cleavable peptide carrying a terminal paramagnetic complex. Rapid volumetric microwave heating produces narrow cluster size distributions that reduce baseline magnetic signal variance across imaging batches.
Parameter or scale variation
Large-cluster hydrodynamic probes at low excitation frequencies
Fused nanocrystal clusters are grown to diameters between 80 nm and 120 nm from primary nanocrystals of 8 nm to 12 nm so that rotational hydrodynamic relaxation contributes significantly alongside internal magnetic switching. The magnetic particle imaging drive field operates at a reduced excitation frequency between 1 kHz and 5 kHz with a drive field amplitude of 10 mT to 20 mT to match the slower rotational relaxation timescale. A cleavable peptide linker is grafted at a surface density of 50 to 150 molecules per cluster to hold the paramagnetic quencher within 2 nm of the cluster surface. Enzymatic cleavage alters both dipole coupling and hydrodynamic drag, producing a measurable shift in the third- and fifth-harmonic signal amplitudes.
Combination with existing systems
Dual-modality magnetic particle and ultrasound imaging catheter
The activatable quenched magnetic nanoparticles are combined with an intravascular or endoscopic ultrasound imaging catheter that includes a localized acoustic trigger. A flexible catheter tip houses a miniature piezoelectric transducer array alongside a single-sided magnetic particle imaging transmit-receive coil assembly. Following administration of nanoparticles bearing thermally or mechanically labile azo or cycloaddition linkers, the ultrasound transducer focuses acoustic energy onto a target region to accelerate linker cleavage in the presence of a target chemical species. The co-registered magnetic particle coil measures the resulting rise in harmonic magnetization while the ultrasound channel provides real-time anatomical boundary images for spatial alignment.
Automated or data-driven variant
Automated multi-harmonic deconvolution for target concentration mapping
A software signal-processing pipeline ingests raw multi-harmonic voltage waveforms from magnetic particle imaging receive coils and outputs quantitative spatial maps of target chemical concentration. The software applies a pre-calibrated system matrix alongside a trained regression model or non-negative least-squares solver to separate intact quenched clusters from cleaved unquenched clusters using the ratio of third- to fifth-harmonic amplitudes. An automated feedback controller adjusts selection-field gradient strength and drive-field sweep trajectories in real time to zoom into regions where the unquenched-to-quenched ratio exceeds a set threshold. The pipeline logs time-series concentration curves and compensates for baseline drift caused by local nanoparticle clearance or temperature changes.
Specific version of a part
Hydrothermal polyol-fused magnetite nanoclusters
Iron(III) chloride hexahydrate dissolves in ethylene glycol with sodium acetate and polyacrylic acid and reacts in a sealed autoclave at 200 degrees Celsius for 12 hours. Primary magnetite nanocrystals of 8 to 10 nanometers nucleate and fuse along crystallographic planes into spherical secondary clusters of 80 to 120 nanometers. The polyacrylic acid coating provides dense surface carboxylates for subsequent covalent conjugation.
Gadolinium-chelate quencher via amide coupling
A macrocyclic gadolinium(III) chelate carrying a terminal primary amine reacts with carboxylate groups on the cluster surface using carbodiimide and N-hydroxysuccinimide activation at pH 7.4. Each cluster binds approximately 500 to 1500 paramagnetic gadolinium complexes within 2 to 5 nanometers of the iron oxide surface. Magnetic dipole coupling between the gadolinium ions and the fused cluster suppresses the third-harmonic magnetization response.
Disulfide-bridged linker for glutathione cleavage
A heterobifunctional polyethylene glycol spacer containing an internal disulfide bond connects the surface amine of the cluster to the paramagnetic chelate. Intracellular reducing agents such as glutathione at millimolar concentrations cleave the disulfide bridge via thiol-disulfide exchange. Cleavage releases the paramagnetic chelate from the cluster surface and restores the magnetic particle imaging signal.
Field-free point scanner with drive coils
Opposing permanent magnets generate a static selection gradient of 2.5 tesla per meter with a central field-free point. Orthogonal paired circular drive coils apply a 25 kilohertz sinusoidal excitation field at 15 millitesla peak amplitude to translate the field-free point across a three-dimensional volume. A tuned gradiometric receive coil captures higher-order harmonic voltages for image reconstruction.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1forming nanocrystal clusters by fusing superparamagnetic iron oxide nanocrystals;
In the present invention, a magnetic property may be imparted to the multi-component mesocrystalline nanoparticles through the iron oxide cluster.
B · US 2022/0135424 A1 · ¶ 50
1.2binding a paramagnetic quencher to surfaces of the nanocrystal clusters with a sensing species to provide quenched magnetic nanoparticles;
1.3wherein the sensing species includes at least one bond that is cleavable by a target chemical species;
1.4performing magnetic particle imaging on a subject using the quenched magnetic nanoparticles;
The invention relates to an MPI-(=Magnetic Particle Imaging) apparatus comprising a magnet system designed for the generation of a time-varying and position-dependent magnetic field in a detection volume and a detection system detecting signals from MPI contrast agents exposed to said magnetic field within said detection volume, said signals being suitable for reconstructing an image of the spatial—and where required also temporal—distribution of said MPI contrast agents.
A · US 2016/0216353 A1 · ¶ 1
1.5wherein the magnetic particle imaging is sensitive to concentration of the target chemical species in the subject.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.4. Only Document B has a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The advantage of FFL scanners is that they obtain signal from a larger volume at each instant of time, thereby achieving a higher SNR.
A · US 2016/0216353 A1 · ¶ 5
To avoid the slow mechanical movement of the sample, the first successful 3D scanner used three orthogonal drive field coil pairs operating at slightly different frequencies, thereby sampling the field of view along a Lissajous trajectory.
A · US 2016/0216353 A1 · ¶ 7
Also, research on the complexation of other materials into forms such as a core-shell structure, a Janus structure, a dimeric structure, a multi-component mesocrystalline nanoparticle cluster structure, and the like has been conducted to impart multi-functionalities to one nanoparticle.
B · US 2022/0135424 A1 · ¶ 4
Therefore, there is a need for a novel method of manufacturing multi-component mesocrystalline nanoparticles having multi-functional properties.
B · US 2022/0135424 A1 · ¶ 7
In certain methods, the position of the nanocrystal can determined by imaging.
C · US 2014/0193841 A1 · ¶ 24
Related claim parts: 1.4
Document C: US 2014/0193841 A1, published Jul 10, 2014. Cited for this statement only.
Cite aspatent.fyi, US 2026/0367039 A1, claim 1, first published 2026-11-23T05:16:15-05:00, https://patent.fyi/US20260367039/, SHA-256 d1dcecc27565d42f70813980ebe7f2549863e418735134c26e8f2d8ecec86b97