Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Biasing through a liquid metal contact
What ifWhat if the surface potential is set by touching the region with a liquid metal droplet rather than depositing a corona charge?
Claim language“depositing a corona charge”
A small droplet of gallium-indium eutectic or mercury contacts the semiconductor surface through a capillary nozzle to form a temporary rectifying junction. A variable voltage source sweeps the direct-current bias across the droplet and a back-side chuck while an impedance meter records the small-signal capacitance at each bias step. After measurement, the droplet retracts into the nozzle, leaving the surface undamaged.
1.2Neutralizing charge with opposing corona ions
What ifWhat if the deposited charge is neutralized by metered bursts of opposing-polarity gas ions rather than ultraviolet (UV) radiation pulses?
Claim language“ultraviolet (UV) radiation pulses”
A secondary corona needle biased at the opposite polarity sits behind a pulsed electrostatic shutter grid above the sample region. Opening the shutter grid for fixed millisecond intervals admits controlled packets of neutralizing ions to the surface, reducing the net surface charge in discrete steps. A current integrator connected to the shutter monitors the ion flux per burst to track the charge increment.
1.2Continuous neutralization under steady illumination
What ifWhat if the deposited charge is neutralized continuously under constant ultraviolet illumination rather than in a series of incremental steps?
Claim language“in a series of incremental steps”
A continuous-wave ultraviolet light source with stabilized optical power illuminates the charged region at a fixed irradiance while a non-contact electrostatic voltmeter logs the decaying surface voltage at a high sampling rate. Because the neutralization current is proportional to the constant photon flux, the time derivative of the recorded voltage waveform directly yields the differential capacitance at every voltage point. Low-pass filtering of the continuous voltage trace reduces measurement noise without interrupting the illumination.
1.3Measuring surface voltage only after pulses
What ifWhat if the surface voltage is measured once before the first pulse and then only after each pulse rather than before and after each UV radiation pulse?
Claim language“before and after each UV radiation pulse”
An electrostatic voltmeter records an initial baseline voltage prior to the first ultraviolet pulse and then takes a single reading immediately following each subsequent pulse. A controller pairs each post-pulse voltage with the preceding post-pulse reading as the starting voltage for that step, halving the total probe acquisition time. Keeping the dark delay between pulses short limits thermal charge leakage between consecutive readings.
1.4Fitting voltage decay directly to parameters
What ifWhat if electrical parameters are extracted by fitting a physical model directly to the surface voltage versus cumulative pulse duration curve rather than computing capacitance (C) values and surface voltage (V) values?
Claim language“capacitance (C) values and surface voltage (V) values”
A nonlinear least-squares solver fits an analytical depletion-approximation equation directly to the measured sequence of surface voltages as a function of cumulative ultraviolet pulse duration. The model relates the known charge neutralization rate per unit time to the dopant concentration, flat-band voltage, and interface trap density as free fitting parameters. Evaluating residuals directly against the raw voltage-time data eliminates numerical differentiation noise.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Component substitution
Deep ultraviolet light emitting diode array illumination
A solid-state deep ultraviolet light emitting diode array replaces a gas-discharge flash lamp as the pulsed radiation source above the charged semiconductor region. A constant-current pulse driver modulates the diode array with sub-microsecond rise times, while a fast photodiode monitors optical output to verify constant photon flux across pulses. An electrostatic voltmeter probe positioned beside the optical path records the surface voltage after each pulse. Replacing the flash lamp eliminates warm-up drift and reduces pulse-to-pulse energy variance.
Piezoelectric cantilever electrometer for microscale voltage sensing
A micro-machined piezoelectric cantilever electrometer replaces a large-area vibrating-reed probe to measure surface voltage over sub-millimeter test structures. The cantilever oscillates at its mechanical resonance frequency of 50 kilohertz approximately 10 micrometers above the semiconductor surface, and a lock-in amplifier nulls the alternating current induced by the surface potential. A focused ultraviolet fiber-optic bundle delivers neutralization pulses coaxially through an annular lens around the cantilever tip. This configuration confines both charge neutralization and potential sensing to localized device regions without averaging over adjacent guard rings.
Parameter or scale variation
Microsecond pulse train for high-capacitance thin films
For thin epitaxial barrier layers below 15 nanometers with high areal capacitance, the ultraviolet pulse duration is reduced to between 20 microseconds and 200 microseconds per step. The photon flux is increased to between 2e14 and 1e15 photons per square centimeter per second to maintain a voltage step of 0.1 volts to 0.5 volts per pulse. Up to 100 consecutive pulses are delivered across a 2-millimeter-diameter aperture to resolve sharp capacitance transitions near accumulation and depletion. A high-speed vibrating capacitor probe settles within 5 milliseconds between pulses to complete a full capacitance-voltage sweep in under 1 second.
Automated or data-driven variant
Adaptive pulse duration control using real-time feedback
A microcontroller reads the surface voltage change after each ultraviolet pulse and dynamically adjusts the duration of the subsequent pulse to maintain a uniform voltage step. In steep regions of the capacitance-voltage curve where small charge increments produce large voltage shifts, the controller shortens the pulse duration; in flat accumulation regions, it lengthens the pulse duration. A regression model fits the resulting capacitance-voltage curve in real time to extract doping concentration profiles and interface trap density. Automated outlier rejection flags pulses where ambient humidity or surface leakage perturbs the linear neutralization rate.
Specific version of a part
Pin-to-plate corona wire source
A tungsten needle electrode positioned 5 to 15 millimeters above the semiconductor wafer is biased at 4 to 8 kilovolts using a regulated high-voltage direct-current power supply. A grounded metallic aperture mask between the needle and the sample confines the ionized air stream to a circular region 1 to 3 millimeters in diameter. The resulting ion flux deposits a uniform surface charge density until the surface potential reaches a preset target.
Vibrating-reed kelvin probe voltmeter
A gold-plated vibrating reference electrode oscillates 50 to 200 micrometers above the charged semiconductor region at a resonant frequency of 1 to 3 kilohertz driven by a piezoelectric actuator. A feedback loop applies a backing direct-current voltage to null the alternating displacement current between the probe and the sample, directly recording the surface potential with millivolt resolution. A stationary optical window or motorized stage allows the probe to sample the exact region before and after each pulse.
Depletion-layer doping and flat-band extraction
A digital processor divides the linear charge increment per pulse by the measured voltage step to obtain differential capacitance values paired with the mean surface voltage of each pulse. Plotting the inverse squared capacitance against the surface voltage yields a linear segment whose slope gives the net ionized dopant concentration in the wide-bandgap epitaxial layer. Extrapolating the linear fit to the voltage axis determines the flat-band voltage and fixed interface charge density.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1depositing a corona charge on a surface of the semiconductor sample in a region;
The metal mask 25 may comprise an aperture configured to block a portion of corona charge flowing toward the sample and tailor the size and/or shape (e.g., a cross-sectional shape and size) of the corona charge flow (e.g., an ion beam) incident on the sample such as on the semiconductor wafer (e.g., the dielectric layer 26 on the semiconductor substrate 27) and thereby the shape and size of a charged region on sample such as on the semiconductor wafer (e.g. the dielectric lay
A · US 2024/0094278 A1 · ¶ 50
After the initial surface voltage measurement, the test site 126 is transferred to a position under the corona charging source (as shown in FIG. 1A and FIG. 1B) and in Step 2 the negative charge with prescribed charge density QC, for example −1.5×1012 q/cm2, is deposited on the surface of epi-layer 103 at test site 126.
B · US 12,027,430 B1 · ¶ 61
1.2irradiating the region with a series of ultraviolet (UV) radiation pulses to neutralize the deposited corona charge in a series of incremental steps;
In Step 4, the test site is illuminated with short wavelength light with a photon energy above the 3.26 eV energy gap of 4H—SiC appropriate to cause photoneutralization of the corona charge. For example, a 325 nm wavelength (hv=3.82 eV) illumination with a near UV LED can be used.
B · US 12,027,430 B1 · ¶ 61
1.3measuring a surface voltage at the region before and after each UV radiation pulse; and
Instead, it is done using a sequence of steps comprising short illumination periods (typically about 10 ms to 20 ms duration) and surface voltage measurements. In this sequence, the charged region is being shifted from a position under the surface voltage measurement probe 132 to a position under the illumination source 144 and then back to surface voltage probe . . . and so on.
B · US 12,027,430 B1 · ¶ 61
1.4determining one or more electrical parameters for the semiconductor sample at the region based on a series of capacitance (C) values and surface voltage (V) values determined for the series of UV radiation pulses.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document B has a passage for 1.21.3. Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The present invention is related to the technical field of semiconductor wafer testing, and more particularly, to non-contact, non-invasive methods for testing and characterizing such wafers.
A · US 2024/0094278 A1 · ¶ 2
Related claim parts: 1.21.3
Using these HV amplifiers can help to maintain stable and/or regulated output voltage in the presence of external current flowing into the outputs of the HV amplifiers (e.g., from the one or more electrodes connected to the HV amplifiers).
A · US 2024/0094278 A1 · ¶ 6
Additionally use of these HV amplifiers can enable production of precisely controlled output voltages independent of a direction of electric current flow at the output port of the HV amplifier (into the output port or out of the output port).
A · US 2024/0094278 A1 · ¶ 6
This generally limits the speed of measurement and the throughput in multiple wafer monitoring with typical 9 or 12 test sites per wafer and 49 sites wafer mapping.
B · US 12,027,430 B1 · ¶ 5
Accordingly, in this disclosure, a charge-biasing method with novel doping measuring principle is described that can increase the measurement speed and the throughput, e.g., by as much as ten times compared with the conventional CnCV techniques described above.
B · US 12,027,430 B1 · ¶ 7