Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Amorphous aluminosilicate glass substrate
What ifWhat if the article uses a fully amorphous chemically strengthened aluminosilicate glass sheet?
Claim language“a glass-ceramic substrate”
An amorphous lithium aluminosilicate glass sheet undergoes ion exchange in a molten potassium nitrate bath at 400 to 450 degrees Celsius to form a compressive surface layer. Because no ceramming heat treatment is performed, the bulk remains free of crystallites and scatters negligible visible light while achieving high mechanical fracture resistance.
1.1Tinted substrate below 85% transmittance
What ifWhat if the substrate is doped with transition-metal ions to attenuate visible transmittance to between 45% and 70%?
Claim language“average transmittance of at least about 85%”
Iron, cobalt, or nickel oxides are dissolved in the glass-ceramic melt at 0.1 to 0.5 weight percent to absorb a uniform fraction of light across 450 nm to 800 nm. This controlled attenuation reduces glare and internal reflection from underlying display components while preserving neutral color balance through balanced broadband absorption.
What ifWhat if reflection and color shift are controlled by a single porous graded-index layer?
Claim language“a multilayer coating”
A single silica sol-gel layer containing sacrificial polymer porogens is spin-coated onto the first major surface and calcined to leave interconnected 10 nm to 30 nm pores whose volume fraction increases toward the air interface. The continuous refractive index gradient from 1.52 down to 1.22 suppresses Fresnel reflection across 450 nm to 800 nm without discrete layer interfaces.
1.2Coating located on the second surface
What ifWhat if the optical coating is deposited solely on the second major surface facing the interior air gap?
Claim language“disposed on the first major surface”
The multilayer interference stack is sputtered onto the rear face of the substrate, leaving the exterior first major surface uncoated for maximum scratch resistance. Reflected light from the rear interface interferes with the broadband reflectance of the front surface to shift the combined two-surface color coordinate toward neutral values.
1.3Positive yellow-shifted uncoated substrate color
What ifWhat if the uncoated glass-ceramic exhibits a positive yellow-shifted b* value above +0.40?
Claim language“a b*uncoated value of less than or equal to about −0.35”
Glass-ceramics nucleated with titanium dioxide and zirconium dioxide absorb slightly at 400 nm to 450 nm, yielding a positive b*uncoated coordinate between +0.40 and +1.00 in two-surface reflectance. A dielectric interference coating tuned for higher reflectance in the 440 nm to 480 nm blue band compensates for this yellow cast and pulls the net reflected color toward zero.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Color-neutral glass-ceramic cover for automotive instrument clusters
A transparent glass-ceramic cover plate having a blue-tinted uncoated reflection carries a multi-layer dielectric interference stack on its front viewing surface inside an automotive dashboard housing. The coated glass-ceramic plate sits in front of an organic light-emitting diode or liquid crystal instrument panel with the coated surface facing the driver. Ambient cabin light and sunlight entering through the windshield reflect from the front and rear surfaces of the cover plate. The interference stack attenuates short-wavelength blue reflectance and balances green-red reflectance, shifting the combined two-surface reflected spectrum toward neutral gray across driver viewing angles.
Color-balanced glass-ceramic window for multi-spectral camera housings
A polished glass-ceramic protective window with an uncoated average transmittance above 85 percent from 450 nanometers to 800 nanometers carries a broadband multilayer dielectric coating on its exterior face. The coated window is mounted in an elastomeric gasket ahead of a multi-element objective lens and a complementary metal-oxide-semiconductor image sensor inside a weatherproof housing. The multilayer coating suppresses surface reflections and removes the blue-tinted spectral bias of the glass-ceramic across both the visible band and the near-infrared edge up to 800 nanometers. Incoming scene light passes to the image sensor with uniform spectral transmission, while external stray light reflecting from the front surface remains spectrally flat and prevents color artifacts across optical channels.
Component substitution
Fluoride and metal-oxide layers for dielectric color correction
A transparent lithium-aluminosilicate glass-ceramic substrate is coated with alternating low-index magnesium fluoride layers having a refractive index near 1.38 and high-index tantalum pentoxide layers having a refractive index between 2.1 and 2.3. The layers are deposited sequentially onto the first major surface by ion-assisted electron-beam evaporation, starting with a tantalum pentoxide layer and terminating with a magnesium fluoride outer layer. The large refractive index contrast between magnesium fluoride and tantalum pentoxide achieves spectral flattening in fewer total layers than silicon oxynitride stacks. Reflected light from the coated front surface combines with the second-surface reflection to bring the net blue-yellow reflectance coordinate closer to zero while keeping average visible transmittance above 90 percent.
Parameter or scale variation
Thin dual-layer dielectric stack for wide-angle viewing
A 0.5-millimeter-thick glass-ceramic substrate carries a two-layer dielectric coating with a combined physical thickness between 65 nanometers and 95 nanometers. A high-index titanium dioxide layer between 15 nanometers and 25 nanometers thick is sputtered directly onto the first major surface, followed by a low-index silicon dioxide outer layer between 50 nanometers and 70 nanometers thick. Keeping the total optical thickness below one-quarter of a green wavelength reduces angular color shift across incidence angles from 0 degrees to 40 degrees. At normal incidence, this thin interference profile reduces total two-surface reflectance below 1.5 percent and shifts the negative blue-yellow reflectance coordinate upward by at least 60 percent toward neutral.
Combination with existing systems
Color-corrected glass-ceramic integrated with capacitive touch sensor
A color-corrected coated glass-ceramic cover lens is bonded to a patterned indium-tin-oxide capacitive touch electrode array and a liquid crystal display module using an optically clear adhesive layer. The multilayer color-correcting coating resides on the exterior viewing surface of the glass-ceramic substrate, while the opposite surface adheres directly to the transparent conductive electrode film. Refractive index matching near 1.48 between the adhesive and the rear surface of the glass-ceramic suppresses internal rear-surface reflection so that the front-surface interference coating governs the overall reflected color. Capacitive touch signals pass through the glass-ceramic substrate without electrical interference from the non-conductive dielectric layers while ambient reflections remain color-neutral.
Automated or data-driven variant
Closed-loop optical monitoring for real-time sputter color tuning
A multi-cathode magnetron sputtering chamber integrates an in-situ broadband optical spectrophotometer, a programmable logic controller, and an inverse thin-film optimization model. The spectrophotometer sits downstream of each deposition zone inside the vacuum chamber, measuring transmittance and reflectance spectra of the moving glass-ceramic substrate between 380 nanometers and 780 nanometers. Control software converts the live spectra into color coordinates and compares them against a target neutral reflectance trajectory, using a trained regression model to adjust cathode power and reactive gas flow rates for subsequent layers. This closed-loop feedback compensates for target erosion and substrate thickness variations, holding the final two-surface blue-yellow reflectance coordinate within 0.05 units of the target.
A lithium aluminosilicate precursor glass containing 2 to 4 weight percent zirconium dioxide and phosphorus pentoxide as nucleating agents is melted and formed into a 0.6 mm flat sheet. A two-stage thermal ceramming schedule at 580 degrees Celsius and 760 degrees Celsius precipitates 15 nm to 30 nm lithium disilicate and petalite crystals at 60 to 75 volume percent, yielding over 90% average transmittance from 450 nm to 800 nm.
Four-layer silicon nitride and silica stack
Alternating high-index silicon nitride (n = 2.02) and low-index silicon dioxide (n = 1.46) thin films are deposited onto the first major surface by reactive magnetron sputtering. Layer thicknesses of 14 nm, 32 nm, 95 nm, and 88 nm from substrate to air suppress visible reflectance below 0.5% while tuning constructive interference in the 550 nm to 650 nm band.
Rayleigh-scattering crystal size blue shift
Crystallites with diameters of 20 nm to 40 nm and a refractive index mismatch of 0.04 relative to the residual glassy matrix scatter short-wavelength blue light more strongly than red light according to the inverse fourth power of wavelength. This wavelength-dependent scattering produces a two-surface reflectance b*uncoated value between −0.50 and −1.20 under a daylight-spectrum illuminant at 0 to 10 degrees incidence.
Thickened outer silica layer color tuning
Adjusting the outermost silicon dioxide layer thickness by +8 nm to +15 nm relative to a quarter-wave minimum shifts the reflectance spectrum minimum from 550 nm toward 490 nm. This controlled spectral tilt increases reflectance in the yellow-red region above 580 nm relative to 450 nm, raising b*coated from −0.90 to −0.25, which is greater than 50% of b*uncoated.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a glass-ceramic substrate comprising a first major surface and a second major surface opposite the first major surface, wherein the glass-ceramic substrate has an average transmittance of at least about 85% over an optical wavelength regime from 450 nm to 800 nm at normal incidence, from 0 to 10 degrees; and
In such embodiments, the substrate 110 may exhibit an average light transmittance over the optical wavelength regime of about 80% or greater, about 81% or greater, about 82% or greater, about 83% or greater, about 84% or greater, about 85% or greater, about 86% or greater, about 87% or greater, about 88% or greater, about 89% or greater, about 90% or greater, about 91% or greater, about 92% or greater, about 93% or greater, or even about 94% or greater.
A · US 2023/0244004 A1 · ¶ 85
A visible light transmittance of the transparent substrate may be 65% to 85%.
B · US 2023/0348321 A1 · ¶ 24
1.2a multilayer coating disposed on the first major surface;
A transparent article is described herein that includes: a glass-ceramic substrate comprising first and second primary surfaces opposing one another and a crystallinity of at least 40% by weight; and an optical film structure disposed on the first primary surface. The optical film structure comprises a plurality of alternating high refractive index (RI) and low RI layers and a scratch-resistant layer.
A · US 2023/0244004 A1 · abstract
The multilayer thin film coating includes a lower dielectric layer, a lower protective layer, a metal functional layer having an infrared reflection function, an upper protective layer, and an upper dielectric layer, which are sequentially laminated from the transparent substrate, the lower dielectric layer includes at least one barrier layer and at least one impurity collection layer, and the thickness of the metal function layer is 12 nm or more.
B · US 2023/0348321 A1 · abstract
1.3wherein the glass-ceramic substrate in an uncoated state exhibits a b*uncoated value of less than or equal to about −0.35 in two-surface reflectance in the CIE L*,a*,b* colorimetry system under a D65 illuminant measured at normal incidence, from 0 to 10 degrees; and
1.4wherein the article exhibits a b*coated value in two-surface reflectance in the CIE L*,a*,b* colorimetry system under a D65 illuminant as measured at normal incidence, from 0 to 10 degrees, and the b*coated value is greater than or equal to about 50% of the b*uncoated value.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Both have a passage for 1.11.2.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
These cover articles can also be employed in architectural articles, transportation articles (e.g., articles used in automotive applications, trains, aircraft, sea craft, etc.), appliance articles, or any article that requires some transparency, scratch resistance, abrasion resistance, or a combination thereof.
A · US 2023/0244004 A1 · ¶ 3
Related claim parts: 1.11.2
Accordingly, there is a need for improved cover articles for protection of optical articles and devices, particularly transparent articles that exhibit high hardness, photopic transmittance, and low transmitted color, along with damage resistance, high modulus and/or high fracture toughness.
A · US 2023/0244004 A1 · ¶ 7
Further, there is a need for the foregoing transparent articles in which their bare substrate strength levels are retained, or substantially retained (e.g., at or above an application-driven threshold), after the inclusion of their optical film structures.
A · US 2023/0244004 A1 · ¶ 7
However, since such a coating layer has excellent durability to heat, but high emissivity and low infrared reflectance, it is difficult to effectively block the heat transfer from the inside.
B · US 2023/0348321 A1 · ¶ 3
The present disclosure has been made in an effort to provide a transparent substrate including a multilayer thin film coating with improved durability at a high temperature even with excellent transmittance and emissivity.
B · US 2023/0348321 A1 · ¶ 5