United States Patent Application Publication

US 2026/0367304 A1

Published
Nov 19, 2026
Filed
Jun 9, 2026
Earliest date on the face
Dec 27, 2023
Classification
G02B 5/3083
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Forward dispersion support with compensating layer

What ifWhat if the support exhibits forward wavelength dispersibility within a multi-layer broadband retarder?
Claim language“exhibiting reverse wavelength dispersibility”

A stretched polymer film with normal dispersion, where retardation decreases as wavelength increases from 450 nm to 650 nm, is laminated with a half-wave film oriented at a crossing angle. The combined slow axes of the two layers rotate the polarization state uniformly across the visible spectrum. This two-layer geometry achieves achromatic circular polarization without relying on a single reverse-dispersion polymer.

1.2Intermediate alignment layer between film layers

What ifWhat if the liquid crystal layer is bonded to the support through an intermediate alignment layer?
Claim language“directly laminated on the support”

A thin photo-aligned polymer coating is applied onto the support surface and cured before liquid crystal coating. The intermediate layer sets the surface anchoring energy and pretilt angle independently of the support surface chemistry. A pressure-sensitive adhesive or UV-curable bonding resin can also join a separately formed liquid crystal film to the support.

1.2Solution-cast polymer replacing liquid crystal

What ifWhat if an amorphous aromatic polymer coating replaces the liquid crystal layer on the support?
Claim language“a liquid crystal layer”

A non-mesogenic polymer with rigid planar backbone rings is dissolved in an organic solvent and slot-die coated onto the support. During solvent evaporation, the planar polymer chains align parallel to the film plane under drying stress, producing different in-plane and out-of-plane refractive indices. Thermal drying immobilizes the oriented chains into a solid birefringent layer without mesogen alignment.

1.3Subwavelength grating replacing film stretching

What ifWhat if an unstretched polymer support obtains in-plane retardation from a subwavelength surface-relief grating?
Claim language“subjected to a stretching treatment”

An unstretched isotropic polymer substrate is nanoimprinted with parallel periodic grooves having a pitch smaller than 200 nm. Because the groove period is below visible wavelengths, incident light experiences different effective refractive indices parallel and perpendicular to the grating lines. Adjusting the groove depth between 100 nm and 400 nm sets the target quarter-wave in-plane retardation without mechanical stretching.

1.3Tilted optic axis replacing positive c-plate

What ifWhat if the liquid crystal layer is a tilted O-plate with an oblique optic axis?
Claim language“a positive C-plate”

A polymerizable nematic liquid crystal composition is coated onto a rubbed or photo-aligned surface that induces a pretilt angle between 20 degrees and 60 degrees. UV polymerization locks the rod-like molecules in a uniform tilted orientation across the layer thickness. This oblique optic axis compensates both polar and azimuthal light leakage in twisted or hybrid-aligned display modes.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Circularly polarized light filter for machine vision

An optical inspection camera uses a stretched cyclic olefin polymer support laminated directly with a homeotropically aligned liquid crystal positive C-plate and bonded to a linear polarizer. The stretched support provides quarter-wave in-plane retardation with reverse wavelength dispersibility across the visible spectrum from 450 nm to 650 nm. The directly laminated positive C-plate compensates out-of-plane phase shifts at oblique incidence angles up to 50 degrees from the optical axis. Incoming reflected glare from metallic surfaces passes through the compensator stack and linear polarizer, reducing specular reflections before reaching the image sensor.

Folded-optics pancake lens for near-eye headsets

A curved optical combiner in a near-eye display headset incorporates the stretched reverse-dispersion polymer support laminated directly with the immobilized positive C-plate between a half-mirror and a reflective polarizer. Light emitted from a microdisplay passes through the retardation stack, reflects between the reflective polarizer and the half-mirror to fold the optical path, and exits toward the eye after a second pass through the quarter-wave support. Because rays strike the curved lens surface at steep angles near the periphery of the field of view, the positive C-plate balances the out-of-plane phase shift of the stretched support. This compensation maintains polarization purity across the full field of view, reducing ghost images in the folded optical cavity.

Component substitution

Cyclic olefin copolymer support with cellulose ester

A stretched blend film of cyclic olefin copolymer and cellulose acetate propionate serves as the reverse-dispersion support in place of polycarbonate or polyester. The polymer film is uniaxially stretched at a draw ratio between 1.3 and 1.8 at a temperature of 145 degrees Celsius, yielding a photoelastic constant of 8e-12 Pa-1. A rod-like polymerizable liquid crystal mixture containing an ionic surfactant is coated directly onto the stretched film without an intervening alignment layer and cured under ultraviolet light to form an immobilized positive C-plate. The blend composition maintains low stress birefringence under thermal cycling while preserving homeotropic anchoring of the liquid crystal molecules.

Parameter or scale variation

Thick stretched film with high oblique retardation

The stretched polymer support has a thickness of 85 micrometers and an in-plane retardation of 142 nm at a wavelength of 550 nm, with a retardation ratio R(450)/R(550) of 0.84. The directly laminated liquid crystal layer has a dry thickness of 2.4 micrometers and a thickness-direction retardation of -110 nm at 550 nm. During roll-to-roll lamination, the web tension is maintained at 120 N/m and the curing chamber temperature is held at 60 degrees Celsius under a nitrogen purge with oxygen concentration below 200 ppm. These dimensional and process parameters match the phase compensation requirements of wide-viewing-angle displays operating at viewing angles up to 75 degrees.

Combination with existing systems

Integration into an organic light-emitting diode stack

The retardation film is bonded to an iodine-stained polyvinyl alcohol linear polarizer using an acrylic pressure-sensitive adhesive to form an antireflection circular polarizing plate. The slow axis of the stretched polymer support is oriented at 45 degrees relative to the absorption axis of the linear polarizer, and the positive C-plate faces an organic light-emitting diode display panel. Ambient light entering the display passes through the linear polarizer and is converted to circularly polarized light by the stretched support before reflecting off the metallic cathode of the panel. Upon returning through the retardation film, the reflected light is rotated by 90 degrees in linear polarization and absorbed by the polarizer across both normal and oblique viewing angles.

Automated or data-driven variant

Closed-loop tension and coating thickness control system

An inline spectroscopic ellipsometer positioned downstream of the ultraviolet curing station measures in-plane retardation and thickness-direction retardation at 10 Hz across the moving web. A programmable controller compares the measured retardation profile against target dispersion curves and adjusts the nip roller tension and slot-die coating pump flow rate in real time. A regression model trained on historical web-tension, drying-temperature, and photoelastic-response data predicts local retardation drift caused by thermal gradients in the oven. The controller applies compensating micro-adjustments to the infrared heater zones before the liquid crystal layer is immobilized.

Specific version of a part

Copolymer film with fluorene side groups

A polycarbonate copolymer synthesized with fluorene-containing diol monomers and aliphatic diol monomers provides a positive birefringence backbone with negatively birefringent side-chain groups. When stretched, the opposing wavelength dispersions of the main chain and side chains yield an in-plane retardation ratio Re(450)/Re(550) between 0.80 and 0.90. The film thickness is 40 micrometers to 60 micrometers with a quarter-wave in-plane retardation near 138 nm at 550 nm.

Slot-die coated homeotropic layer on support

A liquid crystal coating solution containing a vertical-alignment surfactant is applied directly onto a corona-treated polymer support using a precision slot-die head. After solvent evaporation at 80 degrees Celsius for 60 seconds, the rod-like mesogens align perpendicular to the film plane at the air and substrate interfaces. Ultraviolet irradiation at 300 mJ/cm2 under a nitrogen purge cross-links the acrylate end groups directly on the support surface.

Uniaxially stretched cycloolefin polymer film

A cyclic olefin copolymer resin with a low intrinsic stress-optical sensitivity is melt-extruded into an unstretched web and preheated above its glass transition temperature. Tenter-frame transverse stretching at a draw ratio of 1.4 to 1.8 orients the polymer chains along one in-plane axis. The resulting stretched film exhibits a photoelastic constant below 10×10−12 Pa−1, suppressing birefringence shifts under panel-mounting tension.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 10,935,835 B2
Published
Mar 2, 2021
Filed
Aug 2, 2017
Class
G02F 1/133528
Document BUS 2023/0228928 A1
Published
Jul 20, 2023
Filed
Mar 21, 2023
Class
G02B 5/3016
Claim 1
Document A
Document B
1.1a support having an in-plane retardation exhibiting reverse wavelength dispersibility; and
1.2a liquid crystal layer that is directly laminated on the support,
After the layer of the liquid crystal composition is obtained by applying the liquid crystal composition onto the support, the step of giving orientation to the liquid crystal compound for the first optically anisotropic layer contained in the layer of the liquid crystal composition is performed.
A · US 10,935,835 B2 · ¶ 406
The first optically anisotropic layer included in the optical laminate of the embodiment of the present invention is an optically anisotropic layer that is directly laminated on the above-mentioned second optically anisotropic layer and consists of a liquid crystal layer.
B · US 2023/0228928 A1 · ¶ 291
1.3wherein the support is a polymer film that has been subjected to a stretching treatment in at least one in-plane direction, the liquid crystal layer is a positive C-plate obtained by immobilizing an alignment state of a liquid crystal composition containing a liquid crystal compound, and a photoelastic constant of the support is 30×10−12 Pa or less.
When the material of the support is a resin having a positive intrinsic birefringence value, the molecules are oriented in the stretched direction to exhibit a slow axis in the stretched direction.
A · US 10,935,835 B2 · ¶ 402

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.3. Both have a passage for 1.2.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

The present invention relates to an optically anisotropic layered body, and a polarizing plate and an image display device that each include the optically anisotropic layered body.
A · US 10,935,835 B2 · ¶ 1

Related claim parts: 1.2

Optical films such as an optical compensation sheet and a phase difference film are used in various image display devices in terms of elimination of image coloration, expansion of a viewing angle, and the like.
B · US 2023/0228928 A1 · ¶ 3
In the formation of such an optically anisotropic layer, a photo-alignment film obtained by performing a photo-alignment treatment is used in some cases in order to align a liquid crystal compound.
B · US 2023/0228928 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0367304 A1, claim 1, first published 2026-11-23T17:00:00-05:00, https://patent.fyi/US20260367304/, SHA-256 c9d5368a9de72d1e59013ffb4b71c80b1a618e4fbdeb2b662bbf20a5be3f84ab
First published
Permanent addresshttps://patent.fyi/US20260367304/
Content fingerprint (SHA-256)c9d5368a9de72d1e59013ffb4b71c80b1a618e4fbdeb2b662bbf20a5be3f84ab
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi