patent.fyi
Applications  /  US 2026/0367323
United States Patent Application Publication

US 2026/0367323 A1

Published
Nov 19, 2026
Filed
May 10, 2024
Earliest date on the face
May 19, 2020
Classification
G02B 6/125
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Direct bonding to low-index handle wafer

What ifWhat if the donor wafer is bonded directly to a low-index handle wafer without forming a first insulating layer?
Claim language“forming a first insulating layer”

A fused silica handle wafer with a refractive index near 1.45 provides optical confinement directly beneath the bonded ferroelectric film. The handle wafer surface undergoes plasma activation and hydrophilic cleaning to bond directly to the donor wafer. Thermal annealing at 200 to 300 degrees Celsius strengthens the interface without an intermediate deposited or grown oxide layer.

1.2Sputtering ferroelectric film directly onto insulator

What ifWhat if the first thin film is deposited directly onto the first insulating layer by magnetron sputtering rather than bonding a donor wafer?
Claim language“bonding a donor wafer”

Radio-frequency magnetron sputtering deposits an oriented ferroelectric film onto a buffer seed layer atop the first insulating layer in an oxygen-argon plasma at 550 to 700 degrees Celsius. Post-deposition rapid thermal annealing crystallizes the film to achieve the required electro-optic coefficient. This process forms the active layer directly on the substrate without a separate wafer-bonding or thinning step.

1.3Ion implantation cleavage of donor wafer

What ifWhat if the donor wafer is cleaved along an ion-implanted plane to leave a first thin film rather than polishing the donor wafer?
Claim language“polishing the donor wafer”

Helium or hydrogen ions are implanted into the donor wafer prior to bonding to form a subsurface damage layer at a depth of 400 to 800 nanometers. After bonding to the handle wafer, a thermal anneal at 250 to 400 degrees Celsius induces micro-crack coalescence along the implanted plane, detaching the bulk donor wafer. The detached donor wafer is reclaimed for subsequent cycles while the transferred thin film remains on the insulating layer.

1.4Transparent conductive oxide intermediate bonding layer

What ifWhat if a transparent conductive oxide layer is formed on the first thin film in place of a second insulating layer?
Claim language“a second insulating layer”

Sputtering deposits a 30-nanometer transparent conductive oxide film onto the first thin film, followed by chemical mechanical smoothing to sub-nanometer roughness. The conductive layer provides a hydrophilic surface for bonding the second donor wafer while functioning as a shared buried electrode between the lower and upper optical layers. Optical modes remain confined in the higher-index ferroelectric cores by keeping the conductive layer thickness small relative to the operating wavelength.

1.7Transferring non-ferroelectric film by wafer bonding

What ifWhat if the non-ferroelectric thin film material is transferred onto the insulating layer by wafer bonding and substrate removal rather than by deposition?
Claim language“by deposition”

A silicon-on-insulator donor wafer carrying a crystalline silicon device layer is bonded face-down onto the insulating layer using low-temperature plasma-activated bonding. Mechanical grinding and selective wet etching in potassium hydroxide remove the donor silicon handle and buried oxide, leaving a single-crystal silicon thin film. This transfer produces a low-loss crystalline non-ferroelectric layer without high-temperature deposition thermal budgets.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Component substitution

Lithium tantalate donor wafers with silicon nitride layers

A lithium tantalate donor wafer replaces the lithium niobate donor wafer in the bonded stack, while a silicon nitride layer serves as the deposited non-ferroelectric thin film. The lithium tantalate wafer is bonded onto a thermally grown silicon dioxide insulating layer on a silicon handle wafer and thinned by mechanical grinding and chemical-mechanical polishing to form a waveguiding slab. A second silicon dioxide layer is deposited over the thinned lithium tantalate film, followed by low-pressure chemical vapor deposition of a stoichiometric silicon nitride layer that is patterned into low-loss passive routing waveguides. Vertical adiabatic tapers etched into both the silicon nitride and lithium tantalate layers transfer optical modes between the passive routing layer and the electro-optically active ferroelectric layer.

Parameter or scale variation

Sub-micrometer thin films for dense photonic integration

The first and second ferroelectric thin films are thinned by chemical-mechanical polishing to thicknesses between 200 nanometers and 400 nanometers, while the intermediate insulating silicon dioxide layer has a thickness between 300 nanometers and 800 nanometers. Waveguide cores are patterned by electron-beam lithography and dry etching to widths between 450 nanometers and 900 nanometers for single-mode operation at a wavelength of 1550 nanometers. The intermediate insulating thickness places the evanescent tails of the optical modes in vertical overlap across the two waveguiding layers, achieving a coupling length between 20 micrometers and 150 micrometers for interlayer directional couplers. Direct wafer bonding is performed at a temperature between 200 degrees Celsius and 300 degrees Celsius to limit thermal-expansion mismatch stress between the handle wafer and the ferroelectric layers.

Combination with existing systems

Integration with complementary metal-oxide-semiconductor driver circuits

The multi-layer ferroelectric and non-ferroelectric waveguide stack is fabricated directly on a handle wafer that contains pre-fabricated complementary metal-oxide-semiconductor electronic driver circuits beneath a planarized passivation oxide layer. The first insulating layer is deposited over the passivation oxide and planarized by chemical-mechanical polishing to achieve a surface roughness below 0.5 nanometers before donor wafer bonding. Vertical electrical vias are etched through the insulating layers to connect the buried electronic driver outputs to coplanar electrodes patterned alongside the ferroelectric waveguides. High-speed electrical modulation signals generated by the underlying driver circuits are delivered directly to the optical modulators with reduced parasitic capacitance and inductance compared to wire-bonded assemblies.

Other field of use

Multi-layer waveguides for integrated quantum photonic circuits

The multi-layer ferroelectric and non-ferroelectric waveguide arrangement is applied in an integrated quantum photonic processor that generates, routes, and interferes single-photon states on a chip. The ferroelectric thin film layer is periodically poled by applying high-voltage pulses across surface electrodes to create spontaneous parametric down-conversion sources that generate entangled photon pairs. The deposited non-ferroelectric thin film layer forms a low-loss interferometer network with directional couplers and phase shifters that routes the generated photons without introducing nonlinear background noise. Superconducting nanowire single-photon detectors are deposited onto the top non-ferroelectric waveguide layer to detect the processed quantum states directly on the same substrate.

Automated or data-driven variant

Closed-loop interferometric control of thin-film polishing

An automated optical interferometry system monitors the thickness of the donor wafer in real time during the chemical-mechanical polishing steps to achieve uniform thin-film thickness across the wafer. A broadband white-light reflectometer mounted above the polishing platen acquires spectral interference fringes across multiple radial zones of the rotating wafer at intervals below one second. Control software fits the measured reflectance spectra against a multi-layer optical transfer-matrix model to compute the remaining ferroelectric film thickness and local removal rate. The control loop dynamically adjusts zone pressures on the polishing carrier head and halts the platen when the target film thickness is reached within a tolerance of 5 nanometers.

Specific version of a part

Thermal oxidation of silicon handle wafer

A single-crystal silicon handle wafer is placed in a wet oxidation furnace at 1050 degrees Celsius to grow a silicon dioxide layer with a thickness between 2 and 4 micrometers. The grown oxide provides a refractive index near 1.44 at 1550 nanometers, isolating optical modes in the overlying waveguide from the high-index silicon substrate. Surface roughness remains below 0.3 nanometers root-mean-square, preparing the surface for direct wafer bonding.

Plasma-activated hydrophilic bonding of lithium niobate

The second insulating layer on the first thin film and the second donor wafer of x-cut lithium niobate are exposed to an oxygen plasma to generate hydroxyl surface groups. The two wafers are rinsed in deionized water, aligned, and brought into contact at room temperature to form hydrogen bonds across the interface. A subsequent anneal at 250 degrees Celsius converts the interface into covalent bonds capable of withstanding mechanical thinning.

Chemical mechanical polishing to sub-micrometer thickness

The bonded second donor wafer is first thinned to roughly 10 micrometers using precision diamond grinding with a resin-bonded wheel. Chemical mechanical polishing then uses a colloidal silica slurry on a polyurethane pad to remove the remaining material down to a target film thickness of 300 to 600 nanometers. In-situ optical reflectometry monitors film thickness across the wafer to maintain uniformity within plus or minus 10 nanometers.

Low-pressure chemical vapor deposition of silicon nitride

Stoichiometric silicon nitride is deposited onto the insulating layer by low-pressure chemical vapor deposition using dichlorosilane and ammonia precursors at 780 degrees Celsius. The resulting non-ferroelectric thin film exhibits a refractive index near 2.0 at 1550 nanometers and propagation losses below 0.1 decibels per centimeter. A subsequent anneal in nitrogen reduces residual hydrogen content to eliminate absorption peaks near 1520 nanometers.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2015/0115381 A1
Published
Apr 30, 2015
Filed
Oct 31, 2013
Class
H01L 27/1203
Document BUS 9,058,974 B2
Published
Jun 16, 2015
Filed
Jun 3, 2013
Class
H01L 21/02035
Claim 1
Document A
Document B
1.1forming a first insulating layer on a handle wafer;
The method includes providing a substrate, forming a buried oxide layer over the substrate, and an interface layer is formed between the substrate and the buried oxide layer.
A · US 2015/0115381 A1 · ¶ 55
1.2bonding a donor wafer to the handle wafer;
A typical process for vertically integrating devices on silicon wafers is a wafer-to-wafer integration scheme in which the host wafer and donor wafer are aligned with one another, and the wafers are bonded together using oxide-oxide fusion bonding.
B · US 9,058,974 B2 · ¶ 3
1.3polishing the donor wafer to result in a first thin film
The donor wafer is then thinned to expose through silicon vias that connect to the host wafer, or is thinned followed by fabrication of through silicon vias that connect to the host wafer.
B · US 9,058,974 B2 · ¶ 3
1.4forming a second insulating layer on the first thin film;
The method further includes forming an interlayer dielectric layer in the deep trench and over the silicon layer.
A · US 2015/0115381 A1 · ¶ 55
1.5bonding a second donor wafer to the second insulating layer on the first thin film; and
1.6polishing the second donor wafer to result in a second thin film,
1.7wherein a non-ferroelectric thin film material is formed on the first or second insulating layers by deposition, and
1.8wherein ferroelectric and non-ferroelectric thin films are patterned into optical waveguides.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.1 1.4. Only Document B has a passage for 1.2 1.3. Both are classified in CPC H01L.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Indeed, an SOI-based process may be implemented without special equipment or significant retooling of an existing factory.
A · US 2015/0115381 A1 · ¶ 3
However, there are challenges for forming the RF area.
A · US 2015/0115381 A1 · ¶ 3
A long-recognized challenge in producing vertically integrated devices is reducing distortion of the wafers and wafer stack introduced during the manufacturing process.
B · US 9,058,974 B2 · ¶ 4
Embodiments of the present disclosure describe a method generally for improving wafer-to-wafer bonding alignment.
B · US 9,058,974 B2 · ¶ 6
Cite aspatent.fyi, US 2026/0367323 A1, claim 1, first published 2026-11-23T17:22:56-05:00, https://patent.fyi/US20260367323/, SHA-256 cddc08b8195a11e53dd0b15a3ce920f123e1fe5f8fed533e2b7e021f3036d591
First published
Permanent addresshttps://patent.fyi/US20260367323/
Content fingerprint (SHA-256)cddc08b8195a11e53dd0b15a3ce920f123e1fe5f8fed533e2b7e021f3036d591
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi