United States Patent Application Publication

US 2026/0367397 A1

Published
Nov 19, 2026
Filed
Apr 21, 2026
Earliest date on the face
May 19, 2025
Classification
G02B 27/0101
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Continuously curved freeform optical interface

What ifWhat if the inclined surface is a continuously curved freeform profile whose slope varies across its length with no single angle?
Claim language“forming a particular angle”

A multi-axis diamond turning tool cuts a smooth aspheric or freeform curve between the two ends of the first lens piece. The varying local slope combines beam redirection and optical focusing power in a single interface. Light reflecting from different positions along the curve converges to the eyebox without a separate curved mirror.

1.2Adhesive bonding of pre-cast lens piece

What ifWhat if the second lens piece is pre-formed as a solid polymer block and joined to the first lens piece with an optical adhesive?
Claim language“injecting a monomer material”

A separately molded solid second lens piece with a matching complementary angle is aligned to the first lens piece in a precision fixture. A thin layer of index-matched ultraviolet-curable optical adhesive is dispensed onto the inclined interface and pressed to a uniform 5-micrometer thickness. Ultraviolet exposure cures the adhesive bond without flowing liquid monomer around the entire lens.

1.2Open-air dip coating without a mold

What ifWhat if the first lens piece is dip-coated in a liquid resin bath in open air with no mold?
Claim language“into a mold”

The first lens piece is mounted on a vertical translation stage and immersed into a temperature-controlled bath of high-viscosity optical resin. Withdrawing the piece at a controlled speed of 1 to 5 millimeters per second leaves a uniform liquid layer covering the optical element. Surface tension and gravity leveling smooth the outer boundary before curing, eliminating mold cavities and parting lines.

1.3Cooling molten thermoplastic resin in mold

What ifWhat if the second lens piece is formed by cooling a molten thermoplastic resin?
Claim language“polymerizing the monomer material”

Pre-polymerized optical-grade thermoplastic pellets, such as polycarbonate or cyclic olefin copolymer, are heated to 260 degrees Celsius until molten and injected around the first lens piece. Heat is extracted through water-cooled mold channels until the melt drops below its glass transition temperature and solidifies. Because the polymer chains are already formed, no chemical curing reaction or photoinitiator is needed.

1.3Sealed refractive-index gel and cover sheet

What ifWhat if a transparent refractive-index-matching gel fills the space over the optical element and is sealed by a thin cover plate with no solid second lens piece?
Claim language“fabricating a second lens piece”

A non-curing silicone optical gel with a refractive index matching the first lens piece is dispensed over the inclined optical element. A flat, thin glass cover sheet is placed over the gel and sealed around its perimeter with an epoxy edge bead. The gel maintains optical continuity across the inclined interface while accommodating thermal expansion differences without mechanical stress.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Embedded beam splitter for automotive head-up display

A first polymer prism piece includes a flat inclined surface oriented at 45 degrees relative to the optical axis of a windshield combiner assembly. A semi-reflective metallic thin film is deposited onto the inclined surface by vacuum evaporation. The prism piece is placed inside a curved outer mold cavity, and liquid acrylic monomer is injected around the coated surface before ultraviolet polymerization forms a monolithic combiner block. Projected dashboard telemetry enters the first piece, reflects off the embedded film toward the driver eyebox, and transmits ambient road light through the polymerized interface without visible seam distortion.

Component substitution

Surface relief grating replacing thin-film reflector

A nanoimprinted surface relief diffraction grating replaces the planar reflective coating on the inclined surface of the first lens piece. A master stamp presses periodic sub-wavelength grooves into an ultraviolet-curable resin layer applied to the inclined facet prior to overmolding. After the first lens piece is positioned in the secondary mold, a high-index monomer with a refractive index matching the grating resin fills the cavity and polymerizes. Incident display light diffracts at the embedded grating interface to exit toward the viewer while ambient light passes straight through the matched-index boundary.

Silicone elastomer overmolding for impact-resistant waveguide lenses

A two-part optical-grade liquid silicone rubber replaces the rigid acrylic monomer during the secondary molding step around a polycarbonate first lens piece. Before mold insertion, the inclined surface of the polycarbonate piece receives a plasma surface treatment and a silane coupling primer to promote interfacial adhesion. The liquid silicone elastomer is metered at a one-to-one ratio, vacuum degassed, and thermally cured at 110 degrees Celsius around the coated inclined facet. The resulting composite lens absorbs mechanical shock while preserving the optical path across the refractive-index-matched interface.

Parameter or scale variation

Multi-angle stepped facets with controlled polymerization temperature

The inclined surface on the first lens piece is segmented into three parallel facets tilted at 28 degrees, 34 degrees, and 40 degrees relative to the lengthwise axis, each spanning a 2.5-millimeter width. The first lens piece is preheated to 65 degrees Celsius inside the mold before a thiol-ene monomer is injected at a pressure of 0.4 megapascals. Thermal polymerization proceeds at 85 degrees Celsius for 45 minutes followed by a controlled ramp down at 1 degree Celsius per minute to minimize interfacial birefringence. The stepped embedded surfaces expand the exit pupil horizontally across a 12-millimeter eyebox.

Combination with existing systems

Prescription ophthalmic lens integrated with liquid-crystal dimmer

The outer surface of the polymerized second lens piece is ground and polished to form a spherical or toric prescription curvature for vision correction. A flexible guest-host liquid-crystal shutter film is laminated onto the outer face of the finished two-piece waveguide lens using an optically clear adhesive. Drive electrodes along the frame perimeter apply a variable alternating-current voltage across the shutter film to modulate ambient light transmission between 15 percent and 70 percent. The embedded optical element reflects virtual imagery into the eye while the outer dimmer maintains display contrast under bright outdoor illumination.

Automated or data-driven variant

Closed-loop interferometric alignment and adaptive curing control

An inline laser interferometer measures the angular orientation of the inclined surface after the first lens piece is seated inside the mold cavity. A motorized micro-positioning stage adjusts the piece orientation based on real-time fringe error signals until alignment deviation falls below 0.02 degrees. During monomer injection and polymerization, embedded ultrasonic velocity sensors and infrared thermistors feed cure-state measurements to a feedback controller that modulates ultraviolet lamp intensity. The closed-loop control compensates for polymerization shrinkage and maintains uniform optical power across the bonded interface.

Specific version of a part

Stepped micro-prism facets on flat plane

A precision diamond-turning process forms parallel micro-prism steps with 45-degree facets along a planar face of the first lens piece. Each micro-prism facet reflects image light toward the viewer eyebox while keeping the overall lens piece thickness uniform across its length. An optical coating is deposited directly onto the angled facet faces before joining.

Injection-molded polycarbonate with dielectric mirror

The first lens piece is injection-molded from optical-grade polycarbonate at a melt temperature of 280 degrees Celsius with an inclined face angled at 45 degrees to the lengthwise axis. An electron-beam evaporator deposits alternating quarter-wave layers of titanium dioxide and silicon dioxide onto the inclined surface to form a partial reflective mirror. The multilayer stack reflects 50 percent of visible display light while transmitting 50 percent of ambient scene light.

Cast acrylic with volume holographic grating

A first lens piece is cast from polymethyl methacrylate and precision-polished to create an inclined surface at 30 degrees to the lengthwise direction. A 10-micrometer photopolymer film is laminated onto the exposed inclined surface and exposed to two interfering 532-nanometer laser beams to record a volume Bragg grating. The recorded interference fringes diffract narrowband display light at the designed exit angle.

Vacuum-assisted casting of urethane-acrylate monomer

The first lens piece is clamped inside a two-part nickel-plated steel mold with silicone perimeter gaskets that align its outer faces to the mold cavity. A degassed liquid urethane-acrylate monomer mixture is injected through a bottom gate at 0.2 megapascals while a vacuum port at the top draws air out to prevent bubbles over the optical element. Filling continues until monomer exits the top vent, ensuring complete coverage of the inclined surface.

Ultraviolet curing with thermal post-bake

The monomer material containing a 1 percent photoinitiator is polymerized inside a quartz-windowed mold by exposing it to 365-nanometer ultraviolet light at 50 milliwatts per square centimeter for 90 seconds. After demolding, the joined lens undergoes a 2-hour thermal post-bake at 85 degrees Celsius to complete cross-linking and relieve internal shrinkage stress. The resulting second lens piece matches the refractive index of the first lens piece within 0.002.

Cite aspatent.fyi, US 2026/0367397 A1, claim 1, first published 2026-11-23T18:03:07-05:00, https://patent.fyi/US20260367397/, SHA-256 0973692dcffc5d78e916f19302e3eb63453c689fa394a30879f1837e47a937d2
First published
Permanent addresshttps://patent.fyi/US20260367397/
Content fingerprint (SHA-256)0973692dcffc5d78e916f19302e3eb63453c689fa394a30879f1837e47a937d2
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi