Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Thin film bonded to carrier lens
What ifWhat if the waveguide layer has a thickness below 0.05 mm and is laminated onto a separate structural carrier lens?
Claim language“thickness of 0.1 to 1.5 mm”
A 0.04 mm high-index polymer film is cast onto a release liner and embossed with input and output diffractive couplers. An optically clear low-index adhesive bonds the thin film onto a curved 2.0 mm structural ophthalmic lens, which provides mechanical rigidity. The refractive index step between the 0.04 mm film and the low-index adhesive layer confines guided rays by total internal reflection.
What ifWhat if the substrate material has a density above 2.3 g/cm3 due to a high volume fraction of inorganic oxide nanoparticles?
Claim language“density of 0.93 to 2.10 g/cm3”
Zirconium dioxide nanoparticles with diameters below 10 nm are dispersed at high loading into a transparent polymer matrix to reach a bulk density of 2.4 g/cm3. The high inorganic content raises the effective refractive index and increases thermal conductivity across the optical member. Lightweight temple arms and nose pads in the eyewear frame redistribute the added substrate mass to maintain wearer balance.
1.3Low-index substrate with fluoropolymer cladding
What ifWhat if the substrate has a refractive index of 1.50 and relies on a low-index cladding layer for light confinement?
Claim language“refractive index of 1.60 or more”
A transparent polymer plate with a refractive index of 1.50 is coated on both major faces with a 1.34 refractive index amorphous fluoropolymer cladding layer. The index contrast between the 1.50 core and 1.34 cladding sustains total internal reflection for guided field angles within the projection cone. Steeply slanted Bragg gratings couple the image light into and out of the waveguide at angles that match the narrower acceptance cone.
1.4High-retardation substrate with polarized input
What ifWhat if the substrate exhibits an in-plane retardation above 150 nm and operates with a single linear polarization state?
Claim language“retardation value of 30 nm or less”
A linear polarizer at the microdisplay projector aligns the input light polarization axis parallel to the fast optical axis of the high-retardation substrate. Because the incident electric field vector lies entirely along one eigenmode of the birefringent plate, the propagating beam experiences a single refractive index and no polarization mode dispersion. A polarization-selective diffractive grating extracts the single-polarization image light toward the eyebox without ghost images.
1.5Anisotropic retardation gradient along expansion axis
What ifWhat if the substrate has a retardation variation ratio A/B exceeding 6.0 between two orthogonal axes?
Claim language“a relationship represented by a formula (1) below is satisfied”
The waveguide layout orients the primary horizontal pupil-expansion path along the substrate axis that has the smaller retardation variation B. Along the orthogonal axis with the larger retardation variation A, a polarizing beamsplitter film rejects the orthogonal polarization component before outcoupling. A spatial phase-correction coating applied to the outcoupling zone compensates for residual wavefront distortion across the eyebox.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Waveguide substrate for automotive heads-up display
A resin substrate with a thickness of 0.1 to 1.5 mm, a density of 0.93 to 2.10 g/cm3, a refractive index of 1.60 or more, and a retardation of 30 nm or less serves as a combiner plate in an automotive heads-up display. Surface-relief diffraction gratings are imprinted directly onto a primary face of the resin substrate to couple projected dashboard imagery toward a driver eyebox. Maintaining the orthogonal retardation variation ratio A/B at 3.5 or less prevents polarized windshield reflections from creating double images or color shifts across the viewing zone. The high refractive index expands the angular field of view of the projected symbology while keeping the combiner assembly thin and lightweight.
Polarization-preserving substrate for optical coherence tomography
A resin substrate meeting the 0.1 to 1.5 mm thickness, 1.60 or greater refractive index, and 30 nm or less retardation parameters functions as a beam-splitting window in a handheld optical coherence tomography probe. Broadband near-infrared light from a swept-source laser passes through the substrate toward tissue samples while a portion reflects to a reference arm. Keeping the orthogonal retardation difference ratio A/B at 3.5 or less prevents polarization mode dispersion from degrading axial resolution and signal-to-noise ratio in polarization-sensitive scans. The lightweight resin construction replaces heavier glass beam splitters in portable diagnostic handpieces.
Component substitution
Cyclic olefin copolymer and inorganic nanoparticle composite
A cyclic olefin copolymer blended with surface-modified zirconium dioxide nanoparticles replaces a single-component resin matrix to form the optical substrate. The nanoparticles are dispersed at 20 to 40 percent by weight using a silane coupling agent to raise the bulk refractive index to 1.62 while preserving low intrinsic birefringence. Injection-compression molding under controlled cooling rates yields a substrate thickness between 0.3 and 1.0 mm with a density of 1.35 g/cm3 and a retardation below 20 nm. Because the polymer backbone exhibits a low stress-optical coefficient, the orthogonal retardation difference ratio A/B remains below 2.5 across the clear aperture.
Parameter or scale variation
Ultra-thin flexible waveguide film for compact optics
The resin substrate is scaled down to a thickness of 0.04 to 0.09 mm and a maximum retardation of 12 nm or less for curved wearable optics. Solvent casting on a polished carrier belt followed by tension-free thermal annealing keeps the orthogonal retardation difference ratio A/B at 2.0 or below across a 150 mm web width. The refractive index is set between 1.68 and 1.74 while maintaining a resin density of 1.25 to 1.45 g/cm3. This thinner profile permits lamination onto curved prescription lenses without introducing optical distortion or excessive mass.
Combination with existing systems
Substrate integrated with electrochromic dimming layer
The low-retardation resin substrate is bonded to a solid-state electrochromic film stack to form a variable-tint optical waveguide for near-eye displays. Transparent conductive oxide electrodes are sputtered onto the outer surface of the resin substrate, followed by sequential deposition of an ion storage layer, a solid electrolyte, and a tungsten oxide electrochromic layer. Applying a 1.5 V bias drives lithium ions across the electrolyte to modulate ambient light transmission from 75 percent down to 15 percent without altering the internal polarization state of the substrate. Because the resin substrate maintains a retardation of 30 nm or less and an A/B ratio of 3.5 or less, display contrast remains uniform across both clear and darkened operating states.
Automated or data-driven variant
Closed-loop birefringence control during substrate molding
An inline polarimetric imaging sensor and a machine-learning process controller regulate mold temperature and clamping pressure during substrate fabrication. After each molding cycle, a polarized light camera scans the substrate along two orthogonal axes to compute the maximum retardation, the uniaxial variation A, and the orthogonal variation B. A regression model trained on historical process logs maps spatial deviations in the A/B ratio to localized heater zone setpoints and holding pressure profiles for the next cycle. This feedback loop keeps the retardation at 30 nm or less and holds the A/B ratio below 3.5 across high-volume production runs.
Specific version of a part
Injection-compression molded 0.6 mm planar plate
Molten optical resin enters a heated mold cavity equipped with a movable compression core set to a final gap of 0.6 mm. The mold closes uniformly during cooling to apply even packing pressure across the entire plate area, holding thickness variation within plus or minus 0.005 mm. The 0.6 mm thickness balances low eyewear weight against sufficient mechanical stiffness to resist frame-induced warping.
Sulfur-containing episulfide resin at index 1.71
An episulfide-based thermosetting resin formulation with sulfur-rich thioether linkages cures inside a glass mold to achieve a refractive index of 1.71 at 587.6 nm. The high refractive index widens the angular field of view supported by total internal reflection inside the light guide plate. A hard-coat siloxane layer on the outer faces protects the high-index surface from abrasion.
Annealed cast sheet with symmetric retardation
After demolding, the resin substrate undergoes isothermal annealing just below its glass transition temperature for two hours on a flat ceramic setter. Thermal relaxation equalizes residual stress gradients along both the machine direction and the transverse direction, keeping the retardation variation ratio A/B below 1.8. Scanning ellipsometry along orthogonal lines confirms uniform optical isotropy across the active waveguide aperture.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1wherein the resin substrate has a thickness of 0.1 to 1.5 mm,
A 3 mm thick panel was manufactured using a resin composition including 100 parts by weight of the polymer blend of Example 1, 2.5 parts by weight of a polycarboxylic acid fluidizing agent having a molecular weight of 1,000, and 0.1 parts by weight of SrCO3 as an optical compensation additive, followed by measuring birefringence and retardation of the panel.
A · US 2013/0164518 A1 · ¶ 80
The thickness THm of the sheet member 1 (gasket) is 40 μm or more and 450 μm or less, preferably 50 μm or more and 350 μm or less, and more preferably 100 μm or more and less than 200 μm, which is further thinned than a gasket manufactured by conventional injection molding.
B · US 2022/0367887 A1 · ¶ 105
1.2the resin has a density of 0.93 to 2.10 g/cm3,
1.3the resin substrate has a refractive index of 1.60 or more,
1.4the resin substrate has a retardation value of 30 nm or less, and
1.5when A represents a difference between a maximum value and a minimum value of retardation as measured along a straight line in a uniaxial direction of the resin substrate, and B represents a difference between a maximum value and a minimum value of retardation as measured along a straight line in a direction substantially orthogonal to the uniaxial direction, a relationship represented by a formula (1) below is satisfied: A/B≤3.5 (1).
An empty cell means only that no passage was reproduced there.
Why these two documents?
Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
However, in the borderless front glass panel, it is difficult to form glass and application thereof is not easy due to poor bonding properties to a cabinet.
A · US 2013/0164518 A1 · ¶ 5
Another aspect of the present invention is to provide a front panel for a TV which is manufactured by an injection-compression molding method using the composition, thereby minimizing birefringence, being easily applied to a borderless display apparatus, and reducing manufacturing costs.
A · US 2013/0164518 A1 · ¶ 8
A fuel cell gasket manufactured by press working on a thin resin film obtained by extrusion molding is inferior in dimensional stability.
B · US 2022/0367887 A1 · ¶ 4
The thin resin sheet member of the present invention manufactured by such injection molding has excellent dimensional stability as compared with a thin resin sheet member made of extruded thin resin film.
B · US 2022/0367887 A1 · ¶ 9
Cite aspatent.fyi, US 2026/0367407 A1, claim 1, first published 2026-11-23T18:24:18-05:00, https://patent.fyi/US20260367407/, SHA-256 48fb13a3dd7febf5082b8359284c1e92d72fd458f90da1be0b10d11b8d87822e