patent.fyi
Applications  /  US 2026/0367430
United States Patent Application Publication

US 2026/0367430 A1

Published
Nov 19, 2026
Filed
Sep 15, 2025
Earliest date on the face
May 13, 2025
Classification
G02F 1/025
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Free-space beam between micro-lenses

What ifWhat if light propagates as a collimated free-space beam between micro-lenses?
Claim language“a waveguide”

Two etched micro-lenses collimate and refocus an optical beam across an open gap above the tuning region. An adjustable optical cavity in the gap shifts the resonant wavelength by changing the optical path length between reflective surfaces. The beam exits into an output coupler without lateral confinement by a solid core.

1.5Resistive heater for thermo-optic tuning

What ifWhat if the conductive and dielectric layers are patterned to form a resistive heater rather than a capacitor?
Claim language“to form a capacitor”

The conductive film is etched into a narrow serpentine strip along the trench, while the underlying dielectric electrically isolates the strip from the substrate. Passing direct current through the strip generates localized Joule heat that diffuses into the waveguide. The temperature rise changes the refractive index of the core via the thermo-optic effect to shift the wavelength.

1.2Parallel waveguide with evanescent coupling

What ifWhat if the waveguide runs parallel beside the trench with a lateral gap so it never leads to the trench?
Claim language“the waveguide leads to the trench”

The waveguide core extends straight past the trench, separated from the trench sidewall by a narrow cladding gap of 100 to 300 nanometers. The evanescent tail of the guided optical mode overlaps the tuning region inside the trench. Adjusting the refractive index in the trench shifts the effective index of the mode without interrupting the continuous waveguide path.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Biosensing refractive index transducer in microfluidic channels

A silicon waveguide leads to a patterned trench capacitor structure integrated along the floor of a microfluidic sample channel. The dielectric layer inside the trench is functionalized with a thin receptor coating that binds target biomolecules from an aqueous analyte flowing above the trench. Binding events alter the local refractive index and effective capacitance across the trench electrodes, shifting the optical resonance wavelength of the guided mode. An external photodetector measures the transmitted optical power at a fixed laser wavelength to quantify analyte concentration in real time.

Parameter or scale variation

High-aspect-ratio multi-trench array for wide tuning

Instead of a single trench, the substrate is patterned with an array of five parallel trenches, each measuring 120 nanometers wide and 600 nanometers deep with a 250-nanometer center-to-center pitch along a 40-micrometer waveguide interaction length. A 6-nanometer aluminum oxide dielectric liner coats each trench, followed by a conformal polycrystalline silicon fill that forms five electrically connected capacitors in parallel. Operating the array with a bias sweep from 0 to 3.3 volts increases the total carrier-depletion overlap with the optical mode, achieving a phase shift exceeding pi radians at 1550 nanometers while keeping insertion loss below 1.5 decibels.

Combination with existing systems

Trench capacitor integrated into optical ring resonator

The waveguide and trench capacitor are fabricated along the curved section of a micro-ring optical resonator on a photonic integrated circuit. A straight bus waveguide evanescently couples continuous-wave light into the ring, where the trench capacitor overlaps the circulating optical mode. Applying a bias voltage across the trench capacitor alters the local refractive index and shifts the resonance wavelength of the ring cavity. Varying the bias tunes which wavelength channel passes from the input port to the drop port.

Automated or data-driven variant

Closed-loop thermal drift compensation using neural controller

A tap coupler directs 2 percent of the optical power exiting the waveguide to an integrated germanium photodiode monitored by an analog-to-digital converter. An embedded microcontroller samples the photodiode current and an on-chip resistive temperature sensor at 10 kilohertz, feeding both readings into a pre-trained lightweight neural network model stored in non-volatile memory. The model predicts the bias voltage correction required to counteract ambient thermal drift and fabrication-induced phase offsets, and a digital-to-analog converter updates the voltage across the trench capacitor electrodes. This feedback loop stabilizes the target operating wavelength within 5 picometers across a 40 K ambient temperature swing.

Component substitution

Transparent conductive oxide electrode in trench capacitor

Indium tin oxide replaces a metallic or doped-silicon top conductive layer over the dielectric-lined trench to reduce free-carrier optical absorption in the waveguide. Radio-frequency magnetron sputtering deposits a 40-nanometer indium tin oxide film into the trench at 200 degrees C, followed by liftoff patterning to define the upper capacitor contact. Under applied bias, electron accumulation occurs at the interface between the dielectric and the indium tin oxide layer, producing a large refractive index perturbation near the epsilon-near-zero regime. This electrode material allows strong optical phase modulation over a compact 15-micrometer device length.

Specific version of a part

Silicon rib waveguide on buried oxide

A crystalline silicon device layer with a thickness of 220 nanometers rests on a 2-micrometer-thick silicon dioxide insulating layer over a silicon handle wafer. Photolithography and reactive-ion etching remove part of the silicon layer to leave a central ridge 450 nanometers wide flanked by thinner slab regions. The high refractive-index contrast confines infrared light around 1550 nanometers to the central ridge.

Deep reactive-ion etched vertical trench

A hard mask of silicon dioxide is patterned over the substrate using optical lithography, leaving an opening directly at the end of the waveguide. Alternating cycles of fluorine-based plasma etching and fluorocarbon polymer passivation carve a trench with vertical sidewalls to a depth of 5 micrometers. Stripping the mask leaves a smooth-walled cavity aligned to the waveguide facet.

Conformal atomic-layer-deposited aluminum oxide

Alternating pulses of an aluminum-containing precursor gas and water vapor react at a substrate temperature of 250 degrees Celsius to grow an aluminum oxide film one atomic layer per cycle. The self-limiting surface reactions produce a uniform 15-nanometer-thick dielectric coating across the top surface, vertical trench sidewalls, and trench floor. High dielectric permittivity and low pinhole density support strong electric fields across the trench.

Trench-filled polycrystalline silicon electrode capacitor

A heavily doped polycrystalline silicon film fills the dielectric-lined trench and is planarized and etched back to define the upper electrode plate. Selective wet etching removes excess dielectric outside the contact area while preserving the U-shaped capacitor stack inside the trench. Metal contact vias land on the upper electrode and the doped substrate to apply tuning voltages across the trench capacitor.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2018/0372953 A1
Published
Dec 27, 2018
Filed
Dec 20, 2016
Class
G02B 6/1225
Document BUS 11,817,510 B2
Published
Nov 14, 2023
Filed
Aug 30, 2021
Class
H01L 29/945
Claim 1
Document A
Document B
1.1forming a waveguide on a substrate;
Next, the silicon dioxide mask is stripped from the base wafer and a silicon-on-insulator donor wafer is bonded to the silicon base wafer. The backside of the silicon-on-insulator donor wafer terminating at a silicon dioxide layer of the silicon-on-insulator donor wafer is removed, producing a finalized T-shaped optical waveguide.
A · US 2018/0372953 A1 · ¶ 10
1.2patterning the substrate to form a trench, wherein the waveguide leads to the trench;
Referring to FIG. 1(a), the processing begins with a polished, flat silicon wafer 8 (referred to here as the “base” wafer) that is patterned with a polymer or silicon dioxide mask using conventional photo- or electron-beam-lithography techniques and inductively-coupled plasma reactive-ion-etching (ICP-RIE) to form a narrow post 10 that is in the range of 0.3 to 3 microns in width, w (see FIG. 4), surrounded by deep trenches 12 that are in the range of 3-20 microns in width.
A · US 2018/0372953 A1 · ¶ 40
1.3depositing a dielectric layer overlying the substrate and in the trench;
Next, the wafer is coated with silicon dioxide using plasma-enhanced chemical vapor deposition (PECVD) for a thickness of 100 nm; such a coating has conformal properties, meaning the sidewalls of the etched feature also become coated with silicon dioxide (FIG. 6(c)).
A · US 2018/0372953 A1 · ¶ 44
Each capacitor dielectric layers (218, 222, 226, 230) may be formed by a conformal deposition process such as chemical vapor deposition (CVD) or atomic layer deposition (ALD).
B · US 11,817,510 B2 · ¶ 30
1.4depositing a conductive layer overlying the dielectric layer; and
Each metal electrode layers (216, 220, 224, 228) may be formed by a conformal deposition process such as chemical vapor deposition (CVD) or atomic layer deposition (ALD).
B · US 11,817,510 B2 · ¶ 29
1.5patterning the conductive layer and the dielectric layer to form a capacitor with a trench structure in the trench.
In some embodiments, the process for performing the patterning of the protection dielectric layer 214, the layer stack 215, and the metal electrode layer 232 comprises performing an etching process individually on each of the layers.
B · US 11,817,510 B2 · ¶ 34

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.1 1.2. Only Document B has a passage for 1.4 1.5. Both have a passage for 1.3.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Therefore, there is a need for an integrated photonic platform that can operate over octave-spanning or even multi-octave spectral windows.
A · US 2018/0372953 A1 · ¶ 8
Normally, these requirements are at odds with each other, making it difficult to realize high-performance systems without compromising key features.
A · US 2018/0372953 A1 · ¶ 8
Accordingly, there may be a greatly increased risk of device cracking due to at least uneven stress and the decreased distance between the layers.
B · US 11,817,510 B2 · ¶ 2
Cite aspatent.fyi, US 2026/0367430 A1, claim 1, first published 2026-11-23T18:24:18-05:00, https://patent.fyi/US20260367430/, SHA-256 25a974ea96b9d86781dff8edbf14031a0fbcd24b32dd611e447cd149e538e30a
First published
Permanent addresshttps://patent.fyi/US20260367430/
Content fingerprint (SHA-256)25a974ea96b9d86781dff8edbf14031a0fbcd24b32dd611e447cd149e538e30a
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi