Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
What ifWhat if the pixel electrode is recessed inside etched channels within the substrate?
Claim language“above the substrate”
Reactive ion etching forms shallow channels in the glass or polymer base, and conductive metal or transparent oxide fills the channels flush with the top surface. Planarization produces a coplanar interface where the electrochromic material contacts both the recessed conductor and the surrounding insulator. Voltage applied to the embedded conductor drives ion insertion across the flat boundary without a raised step.
1.4Continuous transparent counter layer without opening
What ifWhat if the counter layer forms a continuous transparent sheet across the pixel with no opening overlapping the electrochromic layer?
Claim language“defining an opening overlapping the electrochromic layer”
A wide-bandgap metal oxide ion-storage film, such as hydrated nickel oxide thin enough to remain transmissive, coats the electrolyte uniformly over the active area. Light passes directly through both the continuous counter film and the underlying electrochromic film along the vertical optical path. Uniform vertical ion transport across the full pixel area reduces lateral voltage drop and speeds up switching.
1.5Coplanar lateral common electrode beside pixel
What ifWhat if the common electrode sits beside the pixel electrode on the substrate surface rather than above the counter layer?
Claim language“above the counter layer”
Photolithography patterns interdigitated conductive traces on the base surface, assigning one set of traces as pixel contacts and an adjacent set as the shared return path. The ion-storage material coats only the return traces, while the ionic medium bridges the lateral gap to the electrochromic film. Placing all conductors in one plane eliminates top-side shadow loss and simplifies external driver bonding.
1.6Top-bridging electrolyte over coplanar active layers
What ifWhat if a top-bridging electrolyte sits over both the electrochromic layer and the counter layer rather than between the electrochromic layer and the counter layer?
Claim language“between the electrochromic layer and the counter layer”
The electrochromic film and the ion-storage film are deposited side by side on separate electrodes with a narrow insulating gap separating their edges. A gel or polymer ionic medium coats the upper surfaces of both films, providing a continuous ionic path over the gap. Ions migrate out of one film, travel laterally through the top medium, and enter the adjacent film during switching.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Automotive rearview mirror with peripheral ion storage
A silver-coated glass substrate supports a transparent conductive pixel electrode, a tungsten trioxide electrochromic layer, a gel polymer electrolyte layer, and a surrounding nickel oxide counter layer. The counter layer includes side portions along the edges of the electrochromic layer and a top lip defining a central viewing opening. A transparent conductive common electrode covers the counter layer without obstructing the central opening. Applying a DC bias between the pixel electrode and the common electrode drives lithium ions through the electrolyte to darken the electrochromic layer across the viewing opening and attenuate reflected glare from behind a vehicle.
Component substitution
Conductive polymer electrochromic layer with solid electrolyte
A poly(3,4-ethylenedioxythiophene) polystyrene sulfonate film serves as the electrochromic layer above an indium tin oxide pixel electrode on a flexible polyethylene terephthalate substrate. A lithium phosphorus oxynitride solid thin-film electrolyte separates the polymer electrochromic layer from a vanadium pentoxide counter layer that wraps around the side surfaces and forms an overhanging top rim with a central aperture. A sputtered aluminum-doped zinc oxide common electrode rests on the top rim and side surfaces of the counter layer. Applying 1.5 V across the pixel and common electrodes drives lithium ions through the solid electrolyte between the vanadium pentoxide rim and the polymer film, switching the aperture between a transparent state and a deep blue state without liquid leakage.
Parameter or scale variation
Fast switching micro pixel with thin electrolyte
Each pixel on a glass substrate has a lateral cell width of 20 micrometers, an electrochromic layer thickness of 150 nanometers, and a solid electrolyte thickness of 80 nanometers separating the electrochromic layer from the surrounding counter layer. The top portion of the counter layer overlaps the perimeter of the electrochromic layer by 2 micrometers while leaving a 16-micrometer central opening. A pulsed drive voltage of 2.8 V applied for 40 milliseconds between the pixel electrode and the common electrode drives rapid ion intercalation across the 80-nanometer electrolyte path, achieving a 70 percent optical transmittance change in 120 milliseconds.
Combination with existing systems
Thin film transistor active matrix backplane integration
Each electrochromic cell is fabricated directly over the drain electrode of an amorphous silicon thin film transistor on a glass backplane, with the drain pad functioning as the pixel electrode. An organic insulating bank isolates adjacent cells while the counter layer, having side walls and a top aperture frame, and the common electrode span across rows of cells. A row driver scans gate lines and a column driver applies analog voltages through the transistors to individual pixel electrodes relative to the shared common electrode. Selecting individual transistors modulates the redox state and optical transmittance of each aperture independently to form a static or low-frame-rate image.
A photodiode ambient light sensor mounted adjacent to the substrate connects to an analog-to-digital converter and a microcontroller that drives a programmable voltage source coupled to the pixel electrode and the common electrode. A thermistor mounted on the rear of the substrate supplies temperature measurements to the microcontroller. Software on the microcontroller samples the ambient illuminance and substrate temperature every 500 milliseconds and queries a calibrated lookup table to select a target drive voltage and pulse duration. The microcontroller adjusts the redox drive pulse to maintain constant contrast and compensate for slower ion diffusion at low temperatures.
Specific version of a part
Thin alkali-free borosilicate glass substrate
An alkali-free borosilicate glass sheet with a thickness between 0.3 mm and 0.7 mm provides dimensional stability and low thermal expansion during high-temperature film annealing. Its low sodium content prevents alkali ion migration into adjacent transparent conductors and electrochromic oxides over prolonged cycling.
Sputtered indium tin oxide pixel electrode
A 120 nm film of indium tin oxide is deposited by magnetron sputtering and patterned into discrete pixel pads by wet chemical etching. Annealing at 250 degrees Celsius reduces sheet resistance below 15 ohms per square while maintaining over 85 percent optical transmittance across the visible spectrum.
Porous tungsten trioxide electrochromic layer
A mesoporous tungsten trioxide film with a thickness of 300 nm to 500 nm is formed by reactive sputtering or sol-gel coating on the pixel electrode. Under negative bias, lithium ions and electrons intercalate into the oxide lattice to form blue tungsten bronze that absorbs red and near-infrared light.
Cross-linked lithium-ion gel polymer electrolyte
A solid-like gel electrolyte combines a poly(methyl methacrylate) or poly(ethylene oxide) host matrix with a lithium perchlorate salt dissolved in propylene carbonate. Ultraviolet curing cross-links the polymer chains in place, yielding ionic conductivity around 1 millisiemens per centimeter while preventing liquid leakage.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
A rigid substrate having light transmittance and no flexibility, such as a glass substrate, a silica substrate, and a sapphire substrate can be used as the substrate SUB.
B · US 2022/0404655 A1 · ¶ 76
1.2a pixel electrode above the substrate;
The pixel electrode PTCO2 is provided above the insulating layer PIL2.
B · US 2022/0404655 A1 · ¶ 43
1.3an electrochromic layer above the pixel electrode and configured to block or transmit light according to a redox reaction;
For example, when the electrochromic layer comprising a reducing electrochromic material is colored, the ion storage layer comprising an oxidizing electrochromic material must also have a colored state, and on the contrary, when the electrochromic layer comprising a reducing electrochromic material is bleached, the ion storage layer comprising an oxidizing electrochromic material must also be in a bleached state.
A · US 2020/0166819 A1 · ¶ 62
The “electro-optic layer” can include a liquid crystal layer, an electroluminescence (EL) layer, an electrochromic (EC) layer, and an electrophoretic layer, as long as there is no technical contradiction.
B · US 2022/0404655 A1 · ¶ 27
1.4a counter layer spaced apart from the pixel electrode and the electrochromic layer, configured to store ions, and comprising a side portion on at least one side surface of the electrochromic layer, and a top portion connected to the side portion and defining an opening overlapping the electrochromic layer in a thickness direction of the substrate;
In one example, the electrochromic device of the present application may further comprise an ion storage layer. The ion storage layer may mean a layer formed to match charge balance with the electrochromic layer and/or the passivation layer upon a reversible oxidation-reduction reaction for electrochromic of the electrochromic material.
A · US 2020/0166819 A1 · ¶ 59
1.5a common electrode above the counter layer; and
The common auxiliary electrode CMTL and the common electrode CTCO are provided above the insulating layer PIL1. The common electrode CTCO is insulated from the pixel electrode PTCO1 and faces the pixel electrode PTCO1.
B · US 2022/0404655 A1 · ¶ 41
1.6an electrolyte layer between the electrochromic layer and the counter layer.
For example, in the case where transparent WO3, which is colored by reduction but is colorless in itself, is contained in the first layer and Prussian blue colored per se is contained in the second layer (counter layer), the bleaching treatment (reduction treatment) on Prussian blue was conventionally performed by applying a high voltage to the second layer of the electrochromic device which was constituted by laminating the electrode layer, the first layer, the electrolyte l
A · US 2020/0166819 A1 · ¶ 62
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.41.6. Only Document B has a passage for 1.11.21.5. Both have a passage for 1.3. Both are classified in CPC G02F, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
However, since it takes a considerable time to insert and/or remove the electrolyte ions for the optical property changes, that is, the color change, of the entire area of a electrochromic layer, there is a disadvantage that the color-switching speed is slow.
A · US 2020/0166819 A1 · ¶ 4
It is another object of the present application to provide an electrochromic film having an improved color-switching speed or electrochromic speed.
A · US 2020/0166819 A1 · ¶ 7
It is known that the transistor using the oxide semiconductor as the channel has higher mobility than the transistor using the amorphous silicon as the channel and has a very low off-current.
B · US 2022/0404655 A1 · ¶ 3
Therefore, there was a problem that it was difficult to form a capacitive element having a sufficient size to drive the pixel circuit.
B · US 2022/0404655 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0367455 A1, claim 1, first published 2026-11-23T18:43:34-05:00, https://patent.fyi/US20260367455/, SHA-256 1965c887370fdeac7856418915194cab05714f416b51055022e80c785ae72e66