Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Single-layer metallic mirror without multilayers
What ifWhat if the substrate supports a single-layer metallic mirror rather than a multi-layer reflective structure?
Claim language“multi-layer reflective structure”
A single continuous film of high-density metal such as gold, iridium, or ruthenium is deposited directly onto a low-thermal-expansion glass substrate to a thickness of 30 to 50 nanometers. Incident extreme ultraviolet radiation strikes the surface at a grazing angle below the critical angle for total external reflection, reflecting the beam without constructive interference from alternating layer pairs. An absorber pattern above the metal film defines the mask image while eliminating interlayer diffusion and bilayer thickness-matching tolerances.
1.1Self-supporting multilayer membrane on peripheral frame
What ifWhat if the reflective structure is a self-supporting membrane tensioned on a peripheral frame with no underlying substrate?
Claim language“over a substrate”
Alternating silicon and molybdenum layers are deposited onto a sacrificial release layer, which is subsequently etched away to leave a free-standing multilayer foil 250 to 300 nanometers thick. The foil is tensioned and bonded around its outer perimeter to a rigid ceramic ring frame, leaving the central imaging area unsupported from behind. Active backside cooling gas or radiative heat transfer through the open frame dissipates absorbed radiation during exposure.
1.2Wet chemical conditioning of upper surface
What ifWhat if the upper surface of the multi-layer reflective structure undergoes wet chemical conditioning rather than a plasma treatment process?
Claim language“a plasma treatment process”
The coated substrate is immersed in a dilute aqueous hydrofluoric acid bath for 15 to 30 seconds to strip native silicon oxide from the uppermost layer. A subsequent rinse in degassed deionized water and spin-drying in a dry nitrogen atmosphere leaves a hydrogen-terminated, oxide-free surface. The capping material is then deposited in a vacuum chamber immediately after drying to form a clean interface without energetic ion bombardment.
1.2In-situ capping without plasma surface treatment
What ifWhat if the capping layer is deposited directly onto the as-deposited multilayer surface without performing a plasma treatment process?
Claim language“performing a plasma treatment process”
The multilayer stack and the capping layer are deposited sequentially in the same ultra-high-vacuum cluster tool at a base pressure below 10^-7 pascal without breaking vacuum. Because the uppermost silicon surface is never exposed to ambient air, no native oxide or hydrocarbon contamination forms on it before capping. Deposition of the capping material begins within seconds of completing the final silicon layer, preserving a clean interface without a separate plasma step.
1.3Polycrystalline ruthenium capping layer
What ifWhat if the capping layer is a crystalline ruthenium film rather than an amorphous capping layer?
Claim language“an amorphous capping layer”
Pure ruthenium is deposited by magnetron sputtering at an elevated substrate temperature of 250 to 350 degrees Celsius so that adatoms migrate into a hexagonal close-packed crystalline lattice. The resulting dense, textured ruthenium film of 2.5 to 3.5 nanometers thickness resists oxidation and hydrogen-induced blistering during extreme ultraviolet exposure. A 0.5-nanometer silicon-nitride barrier at the bottom interface blocks interdiffusion between the crystalline metal and the underlying multilayer.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Component substitution
Hydrogen-helium microwave plasma treatment before capping deposition
A remote microwave plasma source generates a mixture of hydrogen and helium radicals in place of argon, oxygen, or nitrogen plasma. The gas mixture flows over the uppermost layer of the multi-layer reflective structure inside a vacuum chamber to reduce native oxide and terminate dangling surface bonds without heavy-ion sputter roughening. Immediately after the hydrogen-helium treatment, physical vapor deposition forms the amorphous capping layer over the conditioned surface in the same vacuum environment.
Amorphous titanium-silicon-nitride layer for reflective stack capping
An amorphous titanium-silicon-nitride film replaces the platinum, iridium, rhodium, or ruthenium-alloy capping material over the plasma-treated reflective multilayer. Co-sputtering titanium and silicon targets in a reactive nitrogen-argon atmosphere forms a dense, grain-boundary-free ternary nitride layer over the conditioned upper surface of the stack. The amorphous nitride composition resists oxidation and hydrogen-induced blistering during high-flux photon irradiation while maintaining a smooth top interface.
Parameter or scale variation
Sub-nanometer amorphous capping layer with timed plasma exposure
The plasma treatment process operates at a radio-frequency power of 35 watts and a chamber pressure of 0.4 pascals for a duration of 12 seconds. Magnetron sputtering deposits the amorphous capping layer to a thickness between 0.6 nanometers and 0.9 nanometers at a substrate temperature of 45 degrees Celsius. Keeping the thickness below 1 nanometer reduces extreme ultraviolet absorption losses while the brief low-power plasma exposure limits intermixing at the interface between the reflective stack and the cap.
Combination with existing systems
Cluster vacuum tool integrating plasma and sputter chambers
A central vacuum transfer robot connects an inductively coupled plasma treatment chamber, a multi-cathode ion-beam sputtering chamber, and a magnetron sputtering chamber in a cluster architecture. The substrate receives the alternating reflective layers in the ion-beam chamber, transfers under ultra-high vacuum at 0.0000001 pascals to the plasma chamber for surface conditioning, and then moves to the magnetron chamber for amorphous capping layer deposition. Maintaining continuous vacuum between all three modules prevents ambient air exposure, moisture adsorption, and carbon buildup on the reflective surface prior to capping.
Automated or data-driven variant
Closed-loop optical emission monitoring for plasma surface conditioning
An optical emission spectrometer coupled to a viewport on the plasma chamber measures characteristic emission lines from the plasma discharge and desorbed surface species in real time. A process controller compares the measured spectral intensity ratios against target calibration curves and automatically terminates the plasma treatment when surface oxide removal reaches a predefined endpoint. Following endpoint detection, the controller triggers the sputter power supply and a quartz crystal microbalance rate monitor to deposit the amorphous capping layer to the target thickness without manual intervention.
Specific version of a part
Molybdenum-silicon multilayer by ion-beam deposition
Forty alternating bilayers of molybdenum (2.8 nanometers thick) and silicon (4.1 nanometers thick) are deposited onto a polished ultra-low-expansion glass substrate using dual-target ion-beam sputtering. A krypton ion beam at 600 electron volts sputters each target sequentially at a chamber base pressure below 10^-6 pascal to achieve sub-angstrom interface roughness. The resulting 276-nanometer stack reflects extreme ultraviolet radiation at a 13.5-nanometer wavelength with peak reflectivity above 68 percent.
Hydrogen-argon plasma surface treatment
After the final silicon layer of the multilayer is deposited, the substrate is exposed to an inductively coupled plasma generated from a gas mixture of 80 percent argon and 20 percent hydrogen at a pressure of 1.5 pascal. Radio-frequency power of 150 watts is applied for 20 seconds with a substrate bias below 30 volts to remove native surface oxides and passivate dangling silicon bonds without subsurface damage. The treated surface remains under vacuum for immediate capping.
An amorphous alloy film of 70 atomic percent ruthenium and 30 atomic percent platinum is co-sputtered onto the plasma-treated multilayer surface to a thickness of 2.5 nanometers. Direct-current magnetron sputtering is performed at room temperature with an argon working pressure of 0.3 pascal so that atomic mobility remains low enough to suppress crystallization. The resulting disordered metallic film blocks oxygen and hydrogen diffusion into the underlying silicon layer during mask cleaning and exposure.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1forming a multi-layer reflective structure over a substrate;
Referring to FIG. 3, the method 300 includes operation 302, in which a reflective multilayer stack 210 is formed over a substrate 202, in accordance with some embodiments.
A · US 2022/0121101 A1 · ¶ 63
Referring to FIGS. 2 and 3A, the method 200 includes operation 202, in which a reflective multilayer stack 110 is formed over a substrate 102, in accordance with some embodiments.
B · US 11,815,804 B2 · ¶ 21
1.2performing a plasma treatment process on an upper surface of the multi-layer reflective structure; and
The method includes forming a reflective multilayer stack on a substrate, plasma treating a top layer of the reflective multilayer stack, depositing a capping layer on the reflective plasma treated reflective multilayer stack by an ion assisted ion beam deposition or an ion assisted sputtering, depositing an absorber layer on the capping layer, forming a patterned hard mask layer on the absorber layer, and etching the absorber layer to form a plurality of openings exposing a
B · US 11,815,804 B2 · ¶ 93
1.3forming an amorphous capping layer over the plasma-treated upper surface of the multi-layer reflective structure.
Referring to FIGS. 4B and 4B′, the capping layer 220 is disposed over the topmost surface of the reflective multilayer stack 210.
A · US 2022/0121101 A1 · ¶ 71
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.3. Only Document B has a passage for 1.2. Both have a passage for 1.1. Both are classified in CPC G03F, as is this patent.
Cite aspatent.fyi, US 2026/0367498 A1, claim 1, first published 2026-11-23T19:07:32-05:00, https://patent.fyi/US20260367498/, SHA-256 d2ce6d840ab6ed34b94809e9b9c85cb6b53975f406265136441a6916f1da2e09