Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Single-layer metallic mirror film
What ifWhat if the mask uses a single-layer aluminum film rather than a reflective multilayered stack?
Claim language“reflective multilayered stack”
A single aluminum film of 50 to 100 nanometers thickness is sputtered onto the glass substrate to form a broadband specular reflector for deep ultraviolet wavelengths. Incident radiation at 193 nanometers reflects directly from the top metal surface without constructive interference from alternating layer pairs. The overlying buffer, capping, and absorber layers remain supported on the flat metal mirror.
1.1Freestanding stack on a ring frame
What ifWhat if the reflective multilayered stack is mounted on a hollow ring frame without being supported over a substrate?
Claim language“over a substrate”
The reflective multilayered stack is deposited onto a sacrificial silicon wafer, bonded at its perimeter to a rigid low-expansion ring frame, and released by wet chemical etching of the sacrificial wafer. The resulting freestanding multilayer membrane spans the open aperture of the ring frame without a solid backing plate. Removing the backing substrate allows backside cooling gas flow and dual-sided inspection during mask fabrication.
1.2Omission of the buffer layer
What ifWhat if the capping layer is deposited directly onto the reflective multilayered stack without depositing a buffer layer?
Claim language“depositing a buffer layer”
The capping layer is deposited directly onto the topmost silicon layer of the reflective multilayered stack immediately after stack deposition in the same vacuum chamber. Maintaining continuous vacuum prevents surface oxidation of the top silicon layer and provides a clean interface for capping layer adhesion. The capping layer alone protects the multilayered stack during subsequent absorber etching and mask cleaning.
1.2Silicon nitride dielectric buffer layer
What ifWhat if the buffer layer is formed from silicon nitride without at least one transition metal element?
Claim language“at least one transition metal element”
A thin silicon nitride film of 1 to 3 nanometers is deposited by plasma-enhanced chemical vapor deposition onto the reflective multilayered stack. The dense covalent silicon-nitrogen network blocks interdiffusion between the top silicon layer of the stack and the overlying capping layer during thermal processing. Silicon nitride also exhibits low absorption at 13.5 nanometers, preserving high extreme ultraviolet reflectivity.
1.3Ion implantation of the buffer surface
What ifWhat if the buffer layer surface is modified by boron ion implantation rather than depositing a capping layer?
Claim language“depositing a capping layer”
Low-energy boron ions are implanted at 0.5 to 2 kiloelectronvolts into the upper 1 nanometer of the buffer layer after buffer deposition. The implanted boron forms a chemically resistant surface zone that slows plasma etching when the overlying absorber layer is patterned. Moderate thermal annealing stabilizes the surface bonds without inducing interdiffusion in the underlying reflective multilayered stack.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Reflective mask stack for extreme ultraviolet astronomy optics
An extreme ultraviolet telescope mirror uses the same layered stack on a low-thermal-expansion glass substrate to reflect narrow-band solar radiation. A reflective multilayered stack of alternating molybdenum and silicon pairs sits directly on the polished substrate, topped by a niobium nitride buffer layer and a ruthenium capping layer. A patterned tantalum-based absorber layer over the capping layer forms an apodizing mask or calibration grid at a focal plane or pupil plane. During observation, the buffer layer blocks silicon interdiffusion into the capping layer under sustained thermal and photon loads while the absorber pattern shapes the wavefront or provides spatial reference markers.
Component substitution
Atomic layer deposition for conformal buffer layer formation
An atomic layer deposition reactor deposits the transition metal compound buffer layer over the reflective multilayered stack instead of using ion beam or physical vapor deposition. Sequential alternating pulses of a volatile transition metal halide or metal-organic precursor and a co-reactant gas such as ammonia or water vapor form a conformal tantalum nitride or ruthenium oxide film one atomic monolayer per cycle. Purging with inert argon gas between pulses removes excess precursor and reaction byproducts before the capping layer is deposited in the same vacuum cluster. This self-limiting surface reaction controls buffer thickness to sub-nanometer precision across the full substrate area without introducing energetic ion damage to the underlying multilayered stack.
Amorphous carbon hardmask and phase-shifting absorber layer
The conventional tantalum-based absorber layer over the capping layer is replaced by a low-refractive-index ruthenium-tantalum alloy or a molybdenum-silicon-nitride phase-shifting absorber paired with an amorphous carbon hardmask. The buffer layer beneath the capping layer uses niobium carbide or tantalum boride to resist chemical attack during fluorine-based plasma etching of the substituted absorber stack. During lithographic exposure, the substituted absorber transmits a controlled fraction of incident radiation with a 180-degree phase shift relative to the exposed capping layer, sharpening aerial image contrast at pattern edges. After pattern transfer, the amorphous carbon hardmask is stripped using an oxygen plasma while the capping and buffer layers protect the underlying reflective multilayered stack.
Parameter or scale variation
Ultrathin buffer layer with reduced capping thickness
The buffer layer is deposited to a thickness between 0.5 nanometers and 1.2 nanometers, while the overlying capping layer is thinned to between 1.5 nanometers and 2.5 nanometers. Deposition proceeds at a substrate temperature maintained between 25 degrees Celsius and 80 degrees Celsius and a chamber pressure between 0.01 pascals and 0.1 pascals to limit thermal intermixing at the multilayer interface. Reducing the combined thickness of the buffer and capping layers below 3.7 nanometers limits extreme ultraviolet absorption losses to under 3 percent per reflection pass while preserving diffusion barrier integrity. The absorber layer is then deposited over the thinned capping layer to a thickness of 45 nanometers to 60 nanometers.
Combination with existing systems
Clustered vacuum deposition tool with inline metrology
The mask fabrication sequence is integrated into a multi-chamber vacuum cluster tool connected by a central robotic transfer hub maintained below 10^-6 pascals. Separate dedicated chambers perform multilayer deposition, transition metal buffer deposition, capping layer deposition, and absorber deposition without exposing the substrate to ambient air between steps. An inline spectroscopic ellipsometer and an X-ray reflectometer mounted on a metrology module measure layer thickness, density, and interface roughness immediately after buffer and capping deposition. Transferring substrates under continuous vacuum prevents native oxide formation at the buffer-to-capping interface and allows immediate rework or process adjustment before absorber deposition.
Automated or data-driven variant
Closed-loop thickness control using neural network models
A closed-loop process controller adjusts buffer and capping deposition parameters using real-time optical emission spectroscopy and quartz crystal microbalance sensors mounted inside the deposition chamber. Sensor time-series data feed into a trained regression or neural network model that predicts film stoichiometry, thickness uniformity, and interface stress during growth. When predicted thickness deviates from a target profile by more than 0.05 nanometers, the software automatically modulates precursor flow rates, sputtering power, or substrate rotation speed in real time. Post-deposition defect inspection images are logged alongside sensor traces to retrain the model and reduce run-to-run reflectivity drift across mask blanks.
Specific version of a part
Molybdenum-silicon alternating mirror stack
Forty to fifty alternating layer pairs of molybdenum and amorphous silicon are deposited onto a low-thermal-expansion glass substrate by ion beam sputtering. Each molybdenum-silicon pair has a combined thickness of approximately 6.9 nanometers with a molybdenum thickness ratio near 0.4 to maximize constructive interference at 13.5 nanometers. The stack terminates with a silicon layer prior to buffer deposition.
Reactively sputtered ruthenium oxide buffer
A ruthenium oxide buffer layer with a thickness between 0.5 and 2.5 nanometers is deposited over the reflective multilayered stack by reactive magnetron sputtering. A pure ruthenium target is sputtered in an argon-oxygen gas mixture at room temperature to prevent silicon-molybdenum silicide formation. The thin oxide film forms a continuous diffusion barrier between the top silicon layer and the overlying capping layer.
Ion-beam-sputtered ruthenium capping layer
A metallic ruthenium capping layer of 2.0 to 3.5 nanometers thickness is deposited over the buffer layer using low-energy ion beam sputtering in an argon ambient. The dense, fine-grained ruthenium film resists oxidation during air exposure and provides high etch selectivity against halogen-based plasma chemistries used to pattern the absorber. Smooth surface morphology with root-mean-square roughness below 0.2 nanometers minimizes extreme ultraviolet scattering losses.
Bilayer tantalum-boron-nitride absorber stack
A main absorber film of tantalum boron nitride with a thickness of 50 to 65 nanometers is deposited over the capping layer by reactive sputtering of a tantalum-boron target in argon and nitrogen. A thinner antireflective top sublayer of tantalum boron oxynitride, measuring 5 to 12 nanometers, is formed over the main absorber film by introducing oxygen gas during the final stage of deposition. The bilayer structure absorbs extreme ultraviolet radiation while reducing deep ultraviolet reflectance during optical mask inspection.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1forming a reflective multilayered stack over a substrate;
A reflective mask blank 10 includes a substrate 1, and a multilayer reflective film 2 adapted to reflect exposure light, a protective film 6 composed mainly of ruthenium (Ru) or its compound on the multilayer reflective film 2, and an absorber film 4 adapted to absorb the exposure light, which are formed in this order on the substrate.
A · US 9,229,315 B2 · abstract
A method of forming an extreme ultraviolet (EUV) mask includes forming a multilayer Mo/Si stack comprising alternating stacked Mo and Si layers over a mask substrate; forming a ruthenium capping layer over the multilayer Mo/Si stack; doping the ruthenium capping layer with a halogen element, a pentavalent element, a hexavalent element or combinations thereof; forming an absorber layer over the ruthenium capping layer; and etching the absorber layer to form a pattern in the ab
B · US 11,392,022 B2 · abstract
1.2depositing a buffer layer over the reflective multilayered stack, wherein the buffer layer comprises one or more of a halide, an oxide, a nitride, a carbide, or a boride of at least one transition metal element, and the at least one transition metal element includes at least one of tantalum, ruthenium, niobium, and rhodium;
This reflective mask has a multilayer reflective film formed on a substrate and adapted to reflect exposure light, a buffer film formed in a pattern on the multilayer reflective film, and further an absorber film formed in a pattern on the buffer film and adapted to absorb the exposure light.
A · US 9,229,315 B2 · ¶ 4
1.3depositing a capping layer over the buffer layer; and
In some embodiments, the capping layer 20 is formed by chemical vapor deposition (CVD), plasma-enhanced chemical vapor deposition (PECVD), atomic layer deposition (ALD), physical vapor deposition (PVD), or any other suitable film forming method.
B · US 11,392,022 B2 · ¶ 40
1.4depositing an absorber layer over the capping layer.
An absorber layer 25 is disposed over the capping layer 20.
B · US 11,392,022 B2 · ¶ 43
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.2. Only Document B has a passage for 1.31.4. Both have a passage for 1.1. Both are classified in CPC G03F, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
FIGS. 3A, 3B, 3C and 3D are cross-sectional views of various stages of a process for forming an extreme ultraviolet (EUV) mask in accordance with some embodiments.
B · US 11,392,022 B2 · ¶ 5
Related claim parts: 1.2
The buffer film is provided between the multilayer reflective film and the absorber film for the purpose of protecting the multilayer reflective film in pattern forming and correcting processes of the absorber film.
A · US 9,229,315 B2 · ¶ 4
This scaling down process generally provides benefits by increasing production efficiency and lowering associated costs.
B · US 11,392,022 B2 · ¶ 1
Cite aspatent.fyi, US 2026/0367502 A1, claim 1, first published 2026-11-23T19:07:32-05:00, https://patent.fyi/US20260367502/, SHA-256 f294e43cf62fd89d9fe35f091862d8d7d79f5fcce720854e59d25bf4d0bb03af