patent.fyi
Applications  /  US 2026/0367512
United States Patent Application Publication

US 2026/0367512 A1

Published
Nov 19, 2026
Filed
Jun 17, 2026
Earliest date on the face
Dec 19, 2023
Classification
G03F 7/0046
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Main-chain scission replaces deprotection

What ifWhat if the first polymer undergoes radiation-induced main-chain scission?
Claim language“an acid-dissociable group”

The first polymer has a backbone containing halogen or quaternary carbon linkages that cleave directly upon exposure to electron-beam or deep-ultraviolet radiation. Backbone cleavage lowers the molecular weight in exposed regions, increasing dissolution rate in an organic developer without acid-catalyzed deprotection. Unexposed regions retain high molecular weight and remain insoluble during development.

1.1Molecular glass replaces first polymer

What ifWhat if the composition uses a non-polymeric molecular glass bearing acid-dissociable groups in place of a first polymer?
Claim language“a first polymer”

A monodisperse polycyclic or polyphenolic core molecule functionalized with tertiary ester or acetal groups forms an amorphous film upon coating. Upon exposure and heating, photo-generated acid cleaves the protecting groups to convert the small molecules into an alkali-soluble form. Uniform molecular size reduces line-edge roughness and eliminates polymer chain entanglement during development.

1.2Omission of the second polymer

What ifWhat if the composition omits a second polymer and relies on a single-polymer film?
Claim language“a second polymer”

A single base polymer incorporates both acid-dissociable units and hydrophobic fluorinated side chains on the same macromolecular backbone. During spin-coating, the fluorinated side chains orient toward the air interface to control surface contact angle without a separate polymer additive. Eliminating the second polymer simplifies formulation blending and prevents phase separation between dissimilar resins.

1.2Siloxane polymer replaces fluorinated unit

What ifWhat if the second polymer contains siloxane side chains with no fluorinated groups?
Claim language“derived from a compound represented by formula (F1)”

A methacrylate or acrylate polymer bearing polydimethylsiloxane grafts migrates to the top surface of the resist film during solvent evaporation. The low surface energy of the silicon-oxygen chains provides water repellency during immersion lithography and reduces defect formation. Alkaline developer or an oxygen-plasma descum step removes the silicon-rich surface layer after exposure.

1.3Vapor-phase deposition without a solvent

What ifWhat if the film is formed by dry vapor-phase deposition with no solvent?
Claim language“a solvent”

Volatile monomers or low-molecular-weight precursors are vaporized under vacuum and condensed onto a cooled substrate to form a uniform dry film. Eliminating the liquid carrier removes spin-coating waste, edge-bead buildup, and post-apply baking steps required to drive off residual liquid. Pattern exposure and dry or wet development proceed directly on the vapor-deposited layer.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Microfluidic channel patterning in glass substrates

The radiation-sensitive composition is spin-coated onto a borosilicate glass wafer to form a sacrificial etch mask for microfluidic channel fabrication. The first polymer with its acid-dissociable structural unit provides aqueous alkaline solubility contrast after ultraviolet exposure and post-exposure baking, while the second polymer bearing terminal difluoromethyl groups migrates to the upper air interface to form a water-repellent top layer. After pattern development, the glass wafer undergoes wet chemical etching in hydrofluoric acid, where the fluorinated upper surface of the second polymer resists acid undercut along the mask edges. The remaining polymer film is then stripped in an organic solvent bath to leave recessed microchannels with uniform depth and sidewall profiles.

Component substitution

Ionic liquid solvent replacing organic glycol ethers

An aprotic room-temperature ionic liquid, such as 1-butyl-3-methylimidazolium tetrafluoroborate, replaces conventional propylene glycol monomethyl ether acetate as the casting solvent for the first and second polymers. Both polymers are dissolved at 5 to 12 weight percent total solids in the ionic liquid with mechanical stirring at 50 degrees Celsius until a homogeneous solution forms. During spin-coating onto a silicon substrate, the low vapor pressure of the ionic liquid prevents premature skin formation and promotes uniform phase separation of the difluoromethyl-functionalized second polymer toward the free surface. Following soft baking at 110 degrees Celsius, the film is exposed and developed using standard alkaline aqueous solutions.

Silicon-containing backbone substituting standard hydrocarbon base polymer

The first polymer is synthesized with a siloxane or polycarbosilane main chain carrying pendant acid-dissociable ester groups in place of a purely carbon-backbone acrylic or hydroxystyrene resin. The silicon-rich first polymer is blended with the difluoromethyl-functionalized second polymer in a ketone solvent such as cyclohexanone and coated as a thin imaging layer over a thick organic planarizing underlayer. After exposure and alkaline development of the imaging layer, the pattern is transferred into the organic underlayer using an oxygen-plasma reactive ion etch. The silicon backbone of the first polymer forms a non-volatile silicon dioxide barrier during oxygen plasma exposure, while the second polymer provides surface tension control during coating and development.

Parameter or scale variation

Thick film formulation for high-aspect-ratio electroplating molds

The total solids concentration of the first and second polymers in the casting solvent is increased to 40 to 55 weight percent to achieve a coated film thickness between 25 micrometers and 60 micrometers in a single spin-coating pass. The spin speed is reduced to 800 to 1200 revolutions per minute for 30 seconds, followed by a two-stage soft bake at 95 degrees Celsius for 180 seconds and 120 degrees Celsius for 300 seconds to drive out residual solvent without cracking. The second polymer is incorporated at 0.02 to 0.08 parts by mass per 100 parts of the first polymer so that surface-segregated difluoromethyl groups control top-loss during extended development without inhibiting bulk developer penetration. After exposure and development, the resulting vertical-walled cavities serve as plating molds for copper bump deposition.

Combination with existing systems

Integration with immersion lithography scanner fluid loops

The radiation-sensitive composition is coated onto a 300-millimeter silicon wafer that is transferred into an immersion lithography exposure tool using deionized water as the immersion medium between the final projection lens and the wafer surface. During wafer coating and baking, the second polymer containing terminal difluoromethyl groups segregates to the film surface to establish a static water contact angle above 85 degrees without requiring a separate protective topcoat layer. As the immersion hood scans across the wafer at 500 millimeters per second, the hydrophobic surface prevents water droplet pinning and suppresses leaching of acid-dissociable components or photoacid additives into the recirculating water loop. After exposure, the wafer moves to a developer module where an alkaline aqueous rinse removes the exposed regions and the surface-enriched second polymer simultaneously.

Automated or data-driven variant

Closed-loop spin-coat thickness and surface segregation control

An automated coating track pairs an inline spectroscopic ellipsometer and a goniometer with a proportional-integral-derivative controller to regulate film thickness and surface hydrophobicity of the radiation-sensitive composition in real time. After each wafer is coated and baked, the ellipsometer measures film thickness across 49 radial points while the goniometer records the advancing water contact angle driven by surface migration of the second polymer. A regression model trained on historical bake temperatures, spin speeds, and contact angle measurements calculates adjustments to the hotplate temperature within plus or minus 0.5 degrees Celsius and spin acceleration for subsequent wafers. This feedback loop maintains target film uniformity and surface difluoromethyl enrichment across continuous production batches.

Specific version of a part

Alicyclic methacrylate copolymer with tertiary ester

The first polymer is synthesized by radical copolymerization of 2-methyl-2-adamantyl methacrylate with a lactone-containing methacrylate such as gamma-butyrolactone methacrylate. The tertiary adamantyl ester cleaves in the presence of photo-generated acid during post-exposure baking at 90 to 120 degrees Celsius to form methacrylic acid units. The lactone unit provides substrate adhesion and controlled developer wettability.

Hydrophobic methacrylate with difluoromethyl ester

The second polymer incorporates repeating units polymerized from a methacrylate monomer where the ester oxygen links to an alkyl spacer terminated by a difluoromethyl group. Because the fluorinated additive has lower surface energy than the first polymer, it segregates to the top 5 to 15 nanometers of the spin-coated film. During aqueous alkaline development, base-catalyzed hydrolysis of the ester bond increases surface hydrophilicity to suppress watermark defects.

Branched fluoropolymer with multiple difluoromethyl groups

The structural unit (i) is derived from a compound where a trivalent linking group connects one polymerizable vinyl group to two or three difluoromethyl-terminated chains. Increasing the number of difluoromethyl branches per monomer unit raises the fluorine density at the film surface at a lower additive loading of 1 to 5 percent by mass relative to the first polymer. Lower loading preserves the bulk dissolution contrast and glass transition temperature of the resist film.

Binary glycol ether and ketone solvent

The solvent consists of a 70 to 30 mass ratio mixture of propylene glycol monomethyl ether acetate and cyclohexanone. The glycol ether ester provides low viscosity and uniform film planarization during spin-coating at 1,500 to 3,000 revolutions per minute, while the cyclic ketone completely dissolves polar lactone and fluorinated polymers. A post-apply bake at 100 degrees Celsius evaporates both solvents to yield a tack-free film.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2015/0205204 A1
Published
Jul 23, 2015
Filed
Dec 17, 2014
Class
G03F 7/0388
Document BUS 2020/0012188 A1
Published
Jan 9, 2020
Filed
Jul 3, 2019
Class
G03F 7/0045
Claim 1
Document A
Document B
1.1a first polymer comprising a structural unit (I) which comprises an acid-dissociable group;
The acid-labile polymer may include at least one of repeating units having the acid-labile group, as represented by Chemical Formulas 2 and 3 below:
A · US 2015/0205204 A1 · ¶ 37
The desirability of the method would depend on whether a solubility inhibiting protective group is present on the resin and whether the positive tone response is temperature dependent.
B · US 2020/0012188 A1 · ¶ 23
1.2a second polymer comprising a structural unit (i) derived from a compound represented by formula (F1); and
1.3a solvent:
A photoresist composition includes an acid-labile polymer that is decomposable by reaction with an acid, a photoacid generator, an organic base having a pKa value of 9 or less and a solvent.
A · US 2015/0205204 A1 · abstract
In one implementation, the photoresist composition comprises a novolac (novolac) resin, a diazonaphthoquinone (DNQ) dissolution inhibitor, a bis(azide) crosslinker, and a casting solvent.
B · US 2020/0012188 A1 · abstract

An empty cell means only that no passage was reproduced there.

Why these two documents?

Both have a passage for 1.1 1.3. Both are classified in CPC G03F, as is this patent.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Thus, there is a need for improved photoresist compositions and methods of using photoresists.
B · US 2020/0012188 A1 · ¶ 7

Related claim parts: 1.1 1.3

Embodiments relate to a photoresist composition.
A · US 2015/0205204 A1 · ¶ 3

Related claim parts: 1.1 1.3

However, current approaches can be costly and time-consuming.
B · US 2020/0012188 A1 · ¶ 7
Accordingly, new approaches are needed to more precisely create smaller and more uniform patterns on large substrates.
B · US 2020/0012188 A1 · ¶ 7
Cite aspatent.fyi, US 2026/0367512 A1, claim 1, first published 2026-11-23T19:07:32-05:00, https://patent.fyi/US20260367512/, SHA-256 852fa4288955eff2987d4def07af3565d6804a6ce323b3cafb05921806feacd5
First published
Permanent addresshttps://patent.fyi/US20260367512/
Content fingerprint (SHA-256)852fa4288955eff2987d4def07af3565d6804a6ce323b3cafb05921806feacd5
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi