patent.fyi
Applications  /  US 2026/0367513
United States Patent Application Publication

US 2026/0367513 A1

Published
Nov 19, 2026
Filed
Mar 28, 2024
Earliest date on the face
Mar 31, 2023
Classification
G03F 7/029
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Using an aromatic ring-containing resin

What ifWhat if the carboxyl group-containing resin includes aromatic rings in its polymer backbone?
Claim language“not containing an aromatic ring”

An aromatic epoxy acrylate resin modified with an acid anhydride supplies the carboxyl groups needed for alkaline aqueous development. The aromatic rings increase thermal stability and glass transition temperature during solder reflow. A high loading of white titanium dioxide pigment offsets yellowing from the aromatic backbone to preserve film reflectance.

1.1Developing a non-carboxyl resin in solvent

What ifWhat if the base polymer is a hydroxyl-functional alicyclic resin without carboxyl groups and is developed in an organic solvent?
Claim language“a carboxyl group-containing resin”

A hydroxyl-functional alicyclic urethane acrylate polymer dissolves in a glycol ether acetate developer in unexposed regions while crosslinked regions resist dissolution. Because the polymer lacks acidic carboxyl groups, it reduces moisture absorption under high-temperature and high-humidity conditions. A blocked isocyanate thermal curing agent reacts with the hydroxyl groups during post-bake to form a dense urethane network.

1.2Replacing inorganic filler with polymer beads

What ifWhat if the composition uses crosslinked organic polymer microbeads as the particulate filler?
Claim language“an inorganic filler”

Crosslinked polymethyl methacrylate or silicone-acrylic microbeads with diameters of 0.5 to 3 micrometers disperse in the resin matrix to control viscosity and reduce cure shrinkage. The organic beads match the refractive index of the cured resin more closely than mineral particles, which improves ultraviolet light penetration through thick films during exposure. During reflow soldering, the crosslinked polymer particles maintain dimensional stability without settling during storage.

1.2Omitting particulate filler from the resin

What ifWhat if the photosensitive resin composition contains no particulate filler at all?
Claim language“an inorganic filler”

A high-molecular-weight alicyclic urethane acrylate oligomer combined with a multifunctional acrylate monomer provides sufficient viscosity for screen or curtain coating without solid particles. Omitting solid fillers eliminates light scattering at particle-resin interfaces, enabling sharper sidewall profiles and finer opening holes during ultraviolet photolithography. Post-exposure thermal crosslinking of the resin network supplies the mechanical strength and heat resistance required for solder masking.

1.3Using an oxime ester photoinitiator

What ifWhat if the photopolymerization initiator is an oxime ester compound lacking any trimethylbenzoyl or phosphine oxide group?
Claim language“a trimethylbenzoyl phosphine oxide group-containing compound”

An oxime ester compound absorbs near-ultraviolet radiation at 365 nanometers and undergoes rapid cleavage to generate free radicals that initiate acrylate polymerization. Because oxime esters exhibit high molar absorptivity and low volatility, a loading below 1 percent by weight achieves full through-cure in pigmented films with minimal outgassing. During post-cure heating, the cleaved initiator fragments remain non-volatile without yellowing the cured solder resist.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Reflective micro-optic arrays for automotive interior lighting

A photosensitive resin composition containing an alicyclic carboxyl-group-containing resin, a titanium dioxide inorganic filler, and a phosphinate-type trimethylbenzoyl phosphine oxide photopolymerization initiator is coated onto a transparent polycarbonate substrate. A patterned photomask defines micro-prism and micro-lens cavities across a 25-micrometer-thick film layer. Exposure to 365-nanometer ultraviolet light crosslinks the irradiated regions, and an alkaline carbonate developer removes unexposed resin to form reflective optical structures. The resulting cured array scatters light from edge-mounted light-emitting diodes uniformly across an automotive instrument panel.

Dielectric barrier ribs for flat display panels

A photosensitive resin paste comprising a cycloaliphatic carboxyl-group resin, an alumina-silica inorganic filler, and a P-O-containing trimethylbenzoyl phosphine oxide initiator is doctor-bladed onto a glass substrate. Photolithographic exposure through a stripe-patterned mask polymerizes the resin into parallel barrier walls with a pitch of 150 micrometers and a height of 80 micrometers. Aqueous alkaline development clears unexposed paste between the walls, leaving clean glass channels for subsequent phosphor deposition. A final thermal bake at 160 degrees Celsius consolidates the polymer network to withstand elevated operating temperatures inside the display assembly.

Component substitution

Barium sulfate filler replacing titanium dioxide

A photosensitive resin formulation substitutes sub-micron barium sulfate particles for titanium dioxide as the inorganic filler alongside a non-aromatic acrylic-acid copolymer resin and a P-O-containing trimethylbenzoyl phosphine oxide photoinitiator. The barium sulfate particles have a median diameter of 0.3 micrometers and are dispersed at 35 percent by weight using a three-roll mill to prevent agglomeration. Because barium sulfate exhibits lower ultraviolet absorption at 365 nanometers than titanium dioxide, actinic light penetrates deeper into the film during pattern exposure. Deep penetration enables complete crosslinking at the bottom of 40-micrometer-thick solder mask openings without undercutting.

Parameter or scale variation

High-loading filler formulation for thick film coating

An inorganic filler of rutile titanium dioxide and spherical silica is loaded at 55 percent by weight into a non-aromatic epoxy-carboxylate resin with 2.5 percent by weight of a phosphonate-bearing trimethylbenzoyl phosphine oxide initiator. The mixture is applied onto a copper-clad laminate via screen printing to a wet thickness of 60 micrometers and tack-dried at 80 degrees Celsius for 25 minutes. Patterned exposure at 405 nanometers uses an exposure dose of 450 millijoules per square centimeter, followed by spray development with 1 weight percent sodium carbonate solution at 30 degrees Celsius. Thermal post-curing at 150 degrees Celsius for 60 minutes yields a 45-micrometer cured layer with high dimensional stability.

Combination with existing systems

Direct-imaging laser system with conveyorized thermal curing

The non-aromatic photosensitive resin composition is applied as a dry film laminated onto a circuit board panel and fed into a maskless laser direct-imaging exposure unit. A 405-nanometer diode laser array scans the panel surface according to digital layout coordinates, activating the P-O-containing trimethylbenzoyl phosphine oxide initiator in selected regions. Immediately after alkaline spray development, a conveyorized infrared-and-convection oven cures the patterned solder resist at 150 degrees Celsius for 45 minutes. Integrating maskless exposure with inline thermal curing eliminates photomask registration drift and reduces panel handling between imaging and curing stations.

Automated or data-driven variant

Closed-loop exposure control using inline reflectance sensors

An automated coating and imaging line incorporates an inline spectrophotometer and a film-thickness interferometer positioned upstream of the ultraviolet exposure station. A supervisory controller reads measured film thickness and diffuse reflectance values for each panel coated with the non-aromatic resin, inorganic filler, and phosphine oxide initiator. Using a regression model trained on historical cure-depth and linewidth data, the controller adjusts ultraviolet exposure energy between 200 and 500 millijoules per square centimeter and modulates conveyor speed in real time. Downstream automated optical inspection measures opening hole diameters and feeds dimensional error back to update the exposure model parameters.

Specific version of a part

Alicyclic epoxy-acrylate resin with anhydride

An alicyclic diepoxide reacts with acrylic acid to form an epoxy acrylate intermediate, which is then esterified with tetrahydrophthalic anhydride to introduce pendant carboxyl groups. The saturated cyclohexane rings prevent conjugated double-bond formation and yellowing under ultraviolet exposure and solder reflow heat. This resin provides an acid value between 50 and 100 milligrams of potassium hydroxide per gram for clean development in dilute sodium carbonate solution.

Rutile titanium dioxide and silica blend

A mixture of surface-treated rutile titanium dioxide particles with a 0.25 micrometer average diameter and spherical fused silica particles with a 1.0 micrometer average diameter serves as the inorganic filler. The titanium dioxide provides high diffuse reflectance across the visible spectrum, while the silica reduces the coefficient of thermal expansion and prevents cracking during thermal cycling. Alumina and silica surface coatings on the titanium dioxide particles suppress photocatalytic degradation of the surrounding resin under humid heat.

Precipitated barium sulfate white filler

Precipitated barium sulfate powder with a narrow particle size distribution centered near 0.5 micrometers is dispersed into the resin at 30 to 50 percent by weight. Because barium sulfate has a lower refractive index than titanium dioxide, it transmits more ultraviolet light into the film interior, enabling full cure at the bottom of deep opening holes. It also exhibits chemical inertness and maintains high surface reflectance after prolonged exposure to elevated temperature and humidity.

Bis(2,4,6-trimethylbenzoyl) phenylphosphine oxide initiator

Bis(2,4,6-trimethylbenzoyl) phenylphosphine oxide is added at 1.0 to 3.0 percent by weight of the solid resin as the photopolymerization initiator. Its absorption extends into the 380 to 410 nanometer range, allowing deep-section radical generation even in heavily pigmented white compositions. Upon photolysis, the phosphine oxide undergoes photobleaching, which reduces residual color and limits volatile outgassing during subsequent reflow soldering.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 8,227,530 B1
Published
Jul 24, 2012
Filed
Jan 12, 2010
Class
C08L 99/00
Document BUS 11,267,977 B2
Published
Mar 8, 2022
Filed
Aug 6, 2018
Class
C09D 11/101
Claim 1
Document A
Document B
1.1(A) a carboxyl group-containing resin not containing an aromatic ring;
Homo- and co-polymers of acrylic acid or methacrylic acid may be used, as may any homo- or co-polymer of any ethylenically unsaturated carboxylic acid.
B · US 11,267,977 B2 · ¶ 79
1.2(B) an inorganic filler; and
A vinyl halide polymer film is provided comprising barium sulfate filler and calcium carbonate filler.
A · US 8,227,530 B1 · abstract
1.3(E) a photopolymerization initiator of a trimethylbenzoyl phosphine oxide group-containing compound having at least one P—O band.
Suitable acylphosphine oxide photoinitiators include, but are not limited to: bis(2,4,6-trimethylbenzoyl)-phenylphosphineoxide; bis(2,6-dimethoxybenzoyl)-2,4,4-trimethylpentylphosphinoxide; diphenyl(2,4,6-trimethylbenzoyl)phosphine oxide; ethyl (2,4,6-trimethylbenzoyl) phenylphosphinate; or phosphinic acid, P-(3-benzoyl-2,4,6-trimethylbenzoyl)-P-phenyl-, ethyl ester; combinations thereof; and the like.
B · US 11,267,977 B2 · ¶ 69

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.2. Only Document B has a passage for 1.1 1.3.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Typical compounds that are used to prepare films or sheets are limited in the amount of filler that can be incorporated, because the sheet tends to lose its integrity and to form pinholes (or much larger holes) if too much filler is incorporated.
A · US 8,227,530 B1 · ¶ 3
Other stability issues also arise if too much filler is incorporated.
A · US 8,227,530 B1 · ¶ 3
Where acylphosphine oxide photoinitiators are used, including those such as bis(2,4,6-trimethylbenzoyl)-phenylphosphineoxide, which have high migration limits, an issue for low migration printing or coating is the production of photodecomposition products from the photoinitiator, and especially aldehydes.
B · US 11,267,977 B2 · ¶ 4
Use of high amounts of monofunctional monomers is also a problem in applications that require cured inks and coatings having low migration of contaminants.
B · US 11,267,977 B2 · ¶ 5
Cite aspatent.fyi, US 2026/0367513 A1, claim 1, first published 2026-11-23T19:07:32-05:00, https://patent.fyi/US20260367513/, SHA-256 d7a29c224911027af1dd6a346345ab7ad5d693aec9bbff5ed6e91d00750b7c65
First published
Permanent addresshttps://patent.fyi/US20260367513/
Content fingerprint (SHA-256)d7a29c224911027af1dd6a346345ab7ad5d693aec9bbff5ed6e91d00750b7c65
Methodv2026-11-18.2 · automated, not reviewed by a person