Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Use a single acid-sensitive polymer
What ifWhat if the photoresist composition omits the first polymer and relies solely on the second polymer?
Claim language“a first polymer”
The second polymer with acid-labile repeating units provides both the film-forming matrix and the solubility switch upon acid-catalyzed deprotection. A monomeric dissolution inhibitor or surface-active additive adjusts film surface energy and developer wetting without requiring a second polymeric binder. Spin-coating, post-apply baking, exposure, post-exposure baking, and alkaline development proceed in a single-resin matrix.
1.2Switch solubility via main-chain scission
What ifWhat if the second polymer undergoes direct radiation-induced main-chain scission without any acid-labile group?
Claim language“an acid-labile group”
High-energy exposure breaks carbon-carbon or carbon-heteroatom bonds directly along the polymer backbone, lowering molecular weight in exposed regions. The fragmented chains dissolve faster in an organic or mild aqueous developer than the intact surrounding matrix, creating a positive-tone relief image without acid-catalyzed deprotection. Post-exposure baking is omitted or reduced to a mild stress-relief step because no catalytic deprotection reaction is needed.
1.2Replace second polymer with small-molecule inhibitor
What ifWhat if the acid-labile group is carried on a monomeric dissolution inhibitor rather than a second polymer?
Claim language“a second polymer”
A low-molecular-weight phenolic or cholate ester bearing tertiary-butyl or acetal protecting groups disperses uniformly within the first polymer matrix. Upon exposure and post-exposure baking, photogenerated acid cleaves the protecting groups on the small molecule, converting it into a hydrophilic carboxylic acid or phenol that accelerates aqueous base dissolution. Because the inhibitor has a small molecular volume, it diffuses minimally while reducing line-edge roughness compared with a two-polymer blend.
1.3Generate photobase rather than photoacid
What ifWhat if the radiation-sensitive component is a photobase generator rather than a photoacid generator?
Claim language“a photoacid generator”
Upon ultraviolet exposure, the photobase generator releases an organic amine or amidine base in the exposed regions. During post-exposure baking, the liberated base catalyzes decarboxylation, imide formation, or base-triggered cross-linking in a base-responsive resin, altering its solubility in developer. Base-catalyzed imaging prevents acid-induced corrosion of underlying metal substrates and reduces airborne amine contamination sensitivity.
1.4Deposit dry film via vapor phase
What ifWhat if the photoresist components are deposited onto the substrate by physical vapor deposition without a liquid solvent?
Claim language“a solvent”
Low-molecular-weight resist components and radiation-sensitive compounds are co-evaporated under vacuum onto a temperature-controlled wafer to form a uniform amorphous film. Eliminating the liquid solvent removes spin-coating edge beads, drying shrinkage, and residual solvent outgassing during vacuum exposure. After exposure and baking, the patterned film is developed in a dry plasma etch or supercritical fluid.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Microfluidic channel patterning on glass substrates
The two-polymer photoresist composition is spin-coated onto a borosilicate glass wafer to form a 5-micrometer thick film for microfluidic channel fabrication. A photomask defining 20-micrometer wide fluidic networks directs ultraviolet radiation at 365 nanometers into the film, activating the photoacid generator to cleave the acid-labile groups on the second polymer. Aqueous alkaline developer removes the exposed regions, while the first polymer migrates to the top surface during baking to maintain uniform wetting and prevent developer-induced delamination along channel walls. The patterned resist layer then serves as an etch mask for wet chemical etching of the glass substrate using buffered hydrofluoric acid.
A third repeating unit bearing a covalently attached sulfonium salt photoacid generator replaces the discrete small-molecule photoacid generator in the second polymer backbone. During synthesis, an acid-labile methacrylate monomer, a lactone-containing polar monomer, and a polymerizable sulfonium salt monomer are copolymerized via free-radical polymerization at a molar ratio of 40 to 40 to 20. When exposed to deep-ultraviolet or extreme-ultraviolet radiation, the tethered photoacid generator releases acid locally without diffusing into unexposed regions, reducing acid blur at sub-20-nanometer feature pitches. The first polymer remains a separate surface-active additive in the propylene glycol methyl ether acetate solvent to segregate to the film-air interface during post-application baking.
Quencher-free basic monomer integration in second polymer
Instead of adding a separate low-molecular-weight amine quencher, a basic tertiary-amine methacrylate repeating unit is copolymerized directly into the second polymer at 1 to 3 mole percent. The second polymer thus contains an acid-labile repeating unit, a polarity-switching repeating unit, and the integrated acid-neutralizing unit within a single macromolecular chain. During post-exposure baking, the covalently bound basic groups neutralize stray acid that diffuses into unexposed regions without volatilizing during the bake step or phase-separating from the matrix. The first polymer remains an independent component in the casting solvent to control surface energy at the air interface.
Parameter or scale variation
High-solids formulation for thick-film electroplating molds
The solvent fraction is reduced so that total solids reach 35 to 45 weight percent, yielding a viscosity between 1,500 and 3,000 centipoise at 25 degrees Celsius for single-coat film thicknesses of 15 to 30 micrometers. Spin-coating proceeds at 800 revolutions per minute for 30 seconds followed by a two-stage soft bake at 90 degrees Celsius for 120 seconds and 115 degrees Celsius for 180 seconds to drive off residual solvent without prematurely cleaving the acid-labile groups. A higher photoacid generator loading of 4 to 6 weight percent relative to total solids compensates for optical attenuation through the thick film during broadband exposure at doses of 400 to 800 millijoules per square centimeter. After alkaline development, the vertical sidewalls of the resulting trenches act as electroplating molds for copper pillar deposition.
Combination with existing systems
Inline immersion lithography track with closed-loop drying
The photoresist composition is dispensed inside an automated wafer-processing track coupled to an immersion lithography scanner that projects 193-nanometer light through a purified water meniscus. During spin-coating and post-application baking at 100 degrees Celsius, the first polymer migrates to the upper surface of the resist film to form a hydrophobic barrier that prevents leaching of the photoacid generator into the immersion water. After exposure, an air-knife drying module removes residual water droplets from the wafer surface before the wafer transfers to a post-exposure bake hotplate at 105 degrees Celsius for 60 seconds. A puddle-dispense developer module then applies 0.26-normal tetramethylammonium hydroxide solution for 30 seconds to resolve the latent image.
Automated or data-driven variant
Inline spectroscopic ellipsometry feedback for bake control
An inline spectroscopic ellipsometer mounted above the post-application bake hotplate measures film thickness and refractive index across 25 radial points on the wafer in real time. A regression model compares the measured optical dispersion curves against a pre-calibrated library of surface-segregation profiles for the first polymer and acid-labile deprotection thresholds for the second polymer. When solvent retention or surface enrichment deviates from target bounds, a feedback controller adjusts hotplate zone temperatures within a plus-or-minus 3 degrees Celsius window and modifies bake duration by up to 15 seconds. Exposure dose parameters are simultaneously updated via a feed-forward link to the lithography scanner to maintain critical dimension uniformity across the wafer.
Specific version of a part
Methacrylate copolymer with cyclic lactone
The first polymer is synthesized by free-radical polymerization of a methacrylate monomer bearing a cyclic lactone or sultone ring in the side chain alongside a polar hydroxyadamantyl methacrylate comonomer. The polymer has a weight-average molecular weight between 5,000 and 15,000 grams per mole and a polydispersity index below 1.6. This backbone provides mechanical film integrity, substrate adhesion, and controlled polarity in aqueous alkaline developer.
Tertiary-butyl ester methacrylate acid-labile unit
The second polymer incorporates repeating units derived from 2-methyl-2-adamantyl methacrylate or tert-butyl methacrylate with a molar fraction between 30 and 50 percent. Upon post-exposure baking at 100 to 120 degrees Celsius in the presence of acid, the tertiary alkyl ester cleaves to form a methacrylic acid unit and a volatile alkene byproduct. The resulting carboxylic acid groups render the exposed polymer soluble in 2.38 weight percent tetramethylammonium hydroxide aqueous developer.
The photoacid generator is an onium salt consisting of a triphenylsulfonium cation paired with a perfluorobutanesulfonate anion, loaded at 2 to 8 weight percent relative to total polymer solids. Upon absorption of 193-nanometer or extreme ultraviolet photons, the sulfonium cation undergoes cleavage to generate a strong perfluorinated sulfonic acid. The bulky fluorinated anion limits acid diffusion length during baking to preserve sub-50-nanometer feature resolution.
Propylene glycol monomethyl ether acetate blend
The solvent is a binary mixture of propylene glycol monomethyl ether acetate and cyclohexanone in a 70-to-30 weight ratio, adjusted to achieve a total solids concentration of 3 to 6 weight percent. This solvent blend dissolves both the first and second polymers as well as the photoacid generator while maintaining a viscosity between 1 and 5 centipoise for spin-coating. Controlled evaporation during a 90-to-110 degree Celsius soft bake yields a uniform 50-to-150 nanometer film free of pinholes.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a first polymer comprising a first repeating unit comprising a group of Formula (1) or (2);
1.2a second polymer comprising a first repeating unit comprising an acid-labile group;
Resists of the invention also may comprise a variety of dissolution inhibitor compounds, which preferably are polymeric and/or fluorinated. Preferred dissolution inhibitor compounds include those that contain a photoacid-labile group, e.g. a photoacid-labile ester or acetal moiety.
A · US 6,858,379 B2 · ¶ 16
For example, in order to form a stable pattern, it is preferable that the alkali developable resin contains 30 to 60 wt % of a repeating unit having a functional group that is dissociated by an acid in the molecule.
B · US 2020/0033724 A1 · ¶ 71
1.3a photoacid generator; and
In another aspect, resists of the invention contain a fluorine-containing resin and one or more photoacid generator compounds, particularly non-aromatic onium salts and imidosulfonates, and other non-ionic photoacid generator compounds.
A · US 6,858,379 B2 · abstract
According to an embodiment of the present disclosure, the chemically amplified positive-type photoresist composition for a thick film may further include, in addition to the above-mentioned non-ionic photoacid generator, a resin dissociated by an acid to increase solubility in an alkali developer (hereinafter, an alkali developable resin), a photoinitiator, and an organic solvent.
B · US 2020/0033724 A1 · ¶ 69
1.4a solvent,
For example, a photoresist composition of the invention can be prepared by dissolving the components of the photoresist in a suitable solvent such as, for example, ethyl lactate, ethylene glycol monomethyl ether, ethylene glycol monomethyl ether acetate, propylene glycol monomethyl ether; propylene glycol monomethyl ether acetate and 3-ethoxyethyl propionate, 2-heptanone and cyclohexanone. 2-heptanonone and slvent blends thereof are generally preferred.
A · US 6,858,379 B2 · ¶ 110
The organic solvent is included to uniformly dissolve various components, to mix them, and to control the viscosity of the photoresist composition.
B · US 2020/0033724 A1 · ¶ 79
An empty cell means only that no passage was reproduced there.
Why these two documents?
Both have a passage for 1.21.31.4.
Additional background
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
While currently available photoresists are suitable for many applications, current resists also can exhibit significant shortcomings, particularly in high performance applications such as formation of highly resolved sub-half micron and sub-quarter micron features.
A · US 6,858,379 B2 · ¶ 8
Accordingly, a photoresist that yields well-resolved images upon 248 nm or 193 nm exposure could enable formation of extremely small (e.g. sub-0.25 μm) features that respond to constant industry demands for smaller dimension circuit patterns, e.g. to provide greater circuit density and enhanced device performance.
A · US 6,858,379 B2 · ¶ 9
Therefore, a chemically amplified photoresist is used to increase sensitivity and resolution in a thick film.
B · US 2020/0033724 A1 · ¶ 6
However, the naphthalimide-type photoacid generator, which has been conventionally used, has a poor solubility in a solvent, so that a large amount of the photoacid generator is required to increase the sensitivity.
B · US 2020/0033724 A1 · ¶ 8
On use of the chemical amplification type, positive working, resist compositions, a resist film is formed by dissolving a resin having acid labile groups as a binder and a compound capable of generating an acid upon exposure to radiation (to be referred to as photoacid generator) in a solvent, applying the resist solution onto a substrate by a variety of methods, and evaporating off the solvent optionally by heating.
C · US 7,393,627 B2 · ¶ 6
Related claim parts: 1.21.31.4
Document C: US 7,393,627 B2, published Jul 1, 2008. Cited for this statement only.
Cite aspatent.fyi, US 2026/0367516 A1, claim 1, first published 2026-11-23T19:27:50-05:00, https://patent.fyi/US20260367516/, SHA-256 b727060a5eeded2f09907f92066b754c26053a7263dadb8ac13daa5e912fbc0f