patent.fyi
Applications  /  US 2026/0367518
United States Patent Application Publication

US 2026/0367518 A1

Published
Nov 19, 2026
Filed
Dec 14, 2023
Earliest date on the face
Dec 22, 2022
Classification
G03F 7/11
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.3Transition metal nitride adhesion and barrier

What ifWhat if a transition metal nitride layer is used between the insulating material and the metal layer?
Claim language“at least one transition metal oxide”

A 20 nanometer titanium nitride layer deposited by reactive magnetron sputtering in a nitrogen-argon plasma bonds the insulating material layer to the metal layer. The nitride lattice blocks oxygen diffusion and metal interdiffusion at temperatures up to 600 degrees Celsius while maintaining sheet resistance below 100 ohms per square. Fluorine-based or chlorine-based reactive ion etching patterns the nitride layer together with the adjacent metal layer to form the array.

1.1Freestanding film held by perimeter ring

What ifWhat if the thin film has no substrate and is held as a freestanding membrane by a perimeter ring?
Claim language“at least one substrate”

The insulating material layer is deposited onto a sacrificial polymer carrier, followed by the transition metal oxide layer and the metal layer. A rigid perimeter ring bonds to the outer edge of the stack, and a solvent bath dissolves the sacrificial carrier to leave a taut freestanding membrane. Patterning and etching proceed from both faces without substrate interference or thermal expansion mismatch.

1.3Chalcogenide layer replacing transition metal oxide

What ifWhat if a chalcogenide layer replaces the transition metal oxide between the other two layers?
Claim language“at least one transition metal oxide”

An amorphous tellurium-selenium-antimony film between 15 and 60 nanometers thick is sputtered onto the insulating layer before metal deposition. Localized optical or thermal exposure switches the chalcogenide between amorphous and crystalline states, creating a high-contrast chemical etch rate difference in an alkaline developer. The patterned chalcogenide then acts as a hard mask for transferring the array-like pattern into the adjacent layers.

1.4Conductive polymer replacing the metal layer

What ifWhat if the top layer is a doped conjugated polymer rather than a metal?
Claim language“at least one metal”

A spin-coated film of acid-doped polyaniline between 30 and 120 nanometers thick is deposited over the transition metal oxide and baked at 110 degrees Celsius. The polymer layer provides sheet conductivity for charge dissipation during pattern writing while allowing oxygen-plasma dry etching to open array apertures in a single step. Its lower elastic modulus also reduces interfacial delamination on flexible substrates.

1.5Transition metal oxide placed on top

What ifWhat if the metal layer sits between the insulating material layer and the transition metal oxide layer?
Claim language“sandwiched between said insulating material layer and said metal layer”

The metal layer is deposited directly onto the insulating material layer, and the transition metal oxide layer forms the uppermost exposed surface. Because the oxide sits on top, it acts simultaneously as a surface passivation barrier against ambient oxidation and as a photosensitive imaging medium during pattern exposure. A wet developer selectively removes exposed oxide regions to expose the underlying metal for subsequent etching.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Surface plasmon resonance biosensor array chip

The multilayer stack forms a refractive-index sensing platform for label-free molecular detection in fluidic channels. A glass substrate supports an aluminum oxide insulating barrier, a tantalum pentoxide adhesion layer, and a patterned gold array on the top surface. During operation, polarized light couples into surface plasmons at the metal-dielectric interface, and shifts in the resonance angle track binding events across individual array elements. The intermediate oxide layer prevents metal delamination during repeated aqueous buffer washes and thermal regeneration cycles.

Component substitution

Hafnium oxide adhesion layer with tungsten electrode

A thermally grown aluminum oxide insulating layer replaces silicon dioxide on a fused quartz wafer to improve chemical resistance against alkaline developers. Between this insulator and the top conductor, an atomic-layer-deposited hafnium dioxide film serves as the transition metal oxide adhesion and barrier layer. A sputtered tungsten layer is deposited over the hafnium dioxide to form the conductive top layer for high-temperature pattern transfer. The stack withstands post-deposition annealing at 800 degrees Celsius in an inert nitrogen ambient without interdiffusion between the metal and the dielectric.

Indium tin oxide conductor for transparent arrays

A borosilicate glass substrate supports a plasma-enhanced chemical-vapor-deposited silicon oxynitride insulating film to preserve optical transmission across the visible spectrum. A sputtered niobium pentoxide layer sits between the insulator and a top conductive layer of polycrystalline indium tin oxide. This transparent conductive oxide replaces opaque noble metals, allowing both backside optical alignment and frontside electrical addressing of the patterned array. Thermal annealing at 350 degrees Celsius in oxygen reduces carrier scattering and stabilizes the sheet resistance of the patterned array elements.

Parameter or scale variation

Ultrathin stack on flexible polymer carrier

The total stack thickness is reduced to 50 micrometers by using a 50-micrometer polyimide substrate instead of a rigid wafer. The insulating silicon oxynitride layer measures 100 nanometers, the vanadium pentoxide intermediate layer measures 10 nanometers, and the top nickel layer measures 50 nanometers. This reduced thickness lowers mechanical bending stress while maintaining a sheet resistance below 5 ohms per square across a 150-millimeter-wide web. Patterning proceeds at a substrate temperature of 120 degrees Celsius to prevent thermal deformation of the polymer carrier.

Automated or data-driven variant

Closed-loop spectroscopic ellipsometry deposition control

An in-situ spectroscopic ellipsometer measures optical phase and amplitude changes continuously during sputtering of the insulating, transition metal oxide, and metal layers. A real-time regression algorithm fits the measured spectra to a multilayer optical dispersion model to compute instantaneous film thickness and surface roughness. When the computed thickness of the transition metal oxide layer reaches its target setpoint, a programmable logic controller closes the sputter shutter and initiates gas-flow switching for the metal target. Historical run logs feed a statistical process control model that adjusts magnetron power to compensate for target erosion over multiple deposition batches.

Specific version of a part

Single-crystal silicon wafer substrate

A polished 500 micrometer thick single-crystal silicon wafer with a (100) crystal orientation serves as the rigid substrate layer. Its flat surface with root-mean-square roughness below 0.5 nanometers supports uniform thin-film deposition across a 150 millimeter diameter. The silicon wafer withstands thermal processing above 800 degrees Celsius and aligns with wafer-handling chucks in dry-etching and lithography tools.

Thermally grown silicon dioxide dielectric layer

A 100 nanometer silicon dioxide film formed by dry thermal oxidation at 1000 degrees Celsius acts as the insulating material layer. It provides a breakdown electric field above 8 megavolts per centimeter and blocks direct-current leakage into the underlying substrate. Smooth oxide termination promotes uniform nucleation of the overlying transition metal oxide layer.

Sputtered tungsten trioxide interfacial layer

A 30 nanometer tungsten trioxide film deposited by reactive radio-frequency magnetron sputtering from a tungsten target in an oxygen-argon mixture forms the transition metal oxide layer. The oxide bonds strongly to the underlying dielectric and upper metal while resisting oxidation and delamination at temperatures up to 500 degrees Celsius. Fluorine-based plasma etching removes the tungsten trioxide cleanly when transferring the array-like pattern.

Borosilicate glass wafer with low roughness

A polished borosilicate glass wafer 500 micrometers thick with a root-mean-square surface roughness below 0.5 nanometers serves as the rigid substrate. Its low coefficient of thermal expansion limits pattern distortion during high-temperature annealing steps up to 450 degrees Celsius. Ultrasonic cleaning in deionized water and oxygen plasma treatment prepare the surface prior to film deposition.

Thermal silicon dioxide dielectric barrier layer

A dense silicon dioxide layer 100 nanometers thick is grown by plasma-enhanced chemical vapor deposition at 300 degrees Celsius using silane and nitrous oxide precursors. The amorphous oxide provides high dielectric breakdown strength and resists dry etching chemistries used to pattern overlying layers. Its hydroxyl-terminated surface promotes strong chemical bonding with the subsequent oxide layer.

Sputtered tungsten trioxide adhesion and etch layer

A stoichiometric tungsten trioxide film between 10 and 40 nanometers thick is deposited by reactive direct-current magnetron sputtering from a metallic tungsten target in an argon-oxygen plasma. The oxide forms covalent metal-oxygen bridges at both the underlying insulator interface and the overlying metal interface, preventing delamination under thermal cycling. It remains chemically stable in ambient oxygen while etching cleanly in fluorine-based reactive ion plasmas.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2008/0166857 A1
Published
Jul 10, 2008
Filed
Jan 10, 2007
Class
H01L 21/30
Document BUS 2015/0325484 A1
Published
Nov 12, 2015
Filed
May 9, 2014
Class
H01L 21/823475
Claim 1
Document A
Document B
1.1at least one layer of at least one substrate;
In FIG. 1, a first barrier oxide layer 100 is formed on a semiconductor substrate 102.
A · US 2008/0166857 A1 · ¶ 15
FIG. 1 is a cross-sectional view illustrating a substrate 104 with an insulating layer 106 according to some embodiments.
B · US 2015/0325484 A1 · ¶ 11
1.2at least one layer of at least one insulating material;
Barrier oxide layer 100 may include any now known or later developed oxide material typically used as a dielectric such as silicon oxide (SiO2) and silicon nitride (Si3N4).
A · US 2008/0166857 A1 · ¶ 15
In some embodiments, a silicon dioxide (SiO2) insulating layer 106 is etched with a fluorine based etchant such as hydrofluoric acid (HF), or a silicon nitride (Si3N4) layer is etched with a fluorine or phosphorus based etchant, such as phosphoric acid (H3PO4).
B · US 2015/0325484 A1 · ¶ 14
1.3at least one layer of at least one transition metal oxide; and
The doped metal oxide interlayer is formed from one of tin oxide, titanium oxide or zinc oxide and is doped with fluorine.
B · US 2015/0325484 A1 · abstract
1.4at least one layer of at least one metal;
The resulting trenches are filled with a conductive material 106 in the form of a metal. Metal 106 may be any now known or later developed refractory metal or silicide (melting point>1100° C.) such as tungsten (W), molybdenum (Mo), tungsten silicide (WSi2) or molybdenum silicide (MoSi2).
A · US 2008/0166857 A1 · ¶ 16
The fill layer is deposited in, and extends over, the opening 202 (See FIGS. 2-6) so that the opening 202 is filled with a conductive material that may be a metal such as tungsten (W), copper (Cu), gold (Au) or the like, or an alloy, a polysilicon, or another conductive material.
B · US 2015/0325484 A1 · ¶ 27
1.5wherein said transition metal oxide layer is sandwiched between said insulating material layer and said metal layer.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document B has a passage for 1.3. Both have a passage for 1.1 1.2 1.4. Both are classified in CPC H01L.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

However, the SRAM occupies an increasingly large area on the microprocessor.
A · US 2008/0166857 A1 · ¶ 4
The electrically conductive path allows reduction of SRAM area by forming a wiring path underneath the barrier oxide layer on the SOI substrate.
A · US 2008/0166857 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0367518 A1, claim 1, first published 2026-11-23T19:27:50-05:00, https://patent.fyi/US20260367518/, SHA-256 2abf50fa58874b9b274696d9fc572e00c1597c18c5251929e1281c1510e76e8d
First published
Permanent addresshttps://patent.fyi/US20260367518/
Content fingerprint (SHA-256)2abf50fa58874b9b274696d9fc572e00c1597c18c5251929e1281c1510e76e8d
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi