What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.2Radiant lamps inside substrate transfer tunnel

What ifWhat if the underlayer is modified by radiant lamps mounted directly inside the substrate transfer tunnel?
Claim language“a second chamber”

Narrow-band ultraviolet lamps and resistive radiant heaters line the ceiling of a heated transfer corridor connecting the underlayer module and the resist module. As an end-effector blade carries the substrate at a controlled speed between 10 and 50 millimeters per second, the film receives a calibrated photon and thermal dose. This inline exposure drives cross-linking and surface dehydration during transit without dedicating a separate stationary chamber.

1.2Single-step self-terminating underlayer deposition

What ifWhat if the underlayer is used as deposited with no subsequent treatment step?
Claim language“treat the underlayer to form a treated underlayer”

The precursor chemistry in the deposition module includes terminal hydrophobic or photosensitive ligands that orient toward the top surface during film formation. Controlled substrate temperature and partial pressure during deposition complete ligand cross-linking and surface energy tuning in a single step. The substrate transfers directly to photoresist application without thermal baking, plasma exposure, or chemical rinsing.

1.3Self-assembling block copolymer etch mask

What ifWhat if the third chamber applies a block copolymer film that phase-separates into periodic etch-mask domains with no radiation-sensitive photoresist?
Claim language“form a photoresist”

A spin coater or vapor-phase applicator deposits a diblock copolymer solution containing two immiscible polymer blocks onto the treated underlayer. An annealing bake at 180 to 250 degrees Celsius drives microphase separation into ordered lamellar or cylindrical domains aligned to pre-patterned guide topography. A selective wet rinse or oxygen plasma step removes one polymer block, leaving a high-resolution etch mask directly on the underlayer.

1.3Atmospheric dry-film roll laminator station

What ifWhat if a solid photoresist sheet is pressed onto the treated underlayer by heated rollers in open cleanroom air?
Claim language“a third chamber”

An uncoiler feeds a pre-cast dry-film photoresist ribbon backed by a release liner over the substrate on a vacuum platen. Heated rubber-coated nip rollers apply uniform contact pressure between 0.2 and 0.5 megapascals at 80 to 110 degrees Celsius to bond the resist to the treated underlayer. A peel bar strips away the backing liner immediately after lamination, leaving a uniform solid resist layer ready for exposure.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Cluster tool for diffractive optical grating fabrication

A multi-chamber vacuum cluster tool processes fused silica optical substrates to form surface-relief diffraction gratings for waveguide combiners. A first physical vapor deposition chamber deposits a titanium dioxide underlayer onto the silica substrate. A second plasma treatment chamber exposes the titanium dioxide layer to an oxygen and argon plasma to adjust surface hydroxyl density and refractive index uniformity. A third vapor-priming and spray-coating chamber applies a positive-tone diazonaphthoquinone photoresist over the treated underlayer for subsequent ultraviolet interference patterning.

Component substitution

Atomic layer deposition chamber for underlayer formation

An atomic layer deposition chamber replaces a spin-on or sputter chamber as the first chamber of the cluster tool. The chamber alternates pulses of a metal-organic precursor and an oxygen reactant, separated by inert gas purges, to grow a conformal amorphous metal-oxide underlayer with sub-nanometer thickness control. A second chamber applies an electron-beam flood treatment to cross-link and densify the deposited film under vacuum. A third dry-deposition chamber sublimates and condenses a molecular glass photoresist directly onto the treated underlayer without liquid solvents.

Parameter or scale variation

Reduced pressure cluster processing for ultrathin underlayers

The cluster tool operates its transfer module and all three process chambers at a controlled base pressure between 10 and 50 pascals using a dry roughing pump and nitrogen purge manifold. The first chamber deposits an underlayer to a target thickness between 2.0 nanometers and 5.0 nanometers across a 300-millimeter semiconductor wafer. The second chamber treats the underlayer for 15 to 45 seconds at a platen temperature between 180 degrees Celsius and 240 degrees Celsius to stabilize film density. The third chamber coats a photoresist layer to a thickness between 12 nanometers and 25 nanometers with an edge-bead removal ring width of 1.5 millimeters.

Combination with existing systems

Cluster tool coupled to an inline wafer scanner

The three-chamber cluster tool connects directly to an extreme ultraviolet lithography scanner through a dual-slot vacuum load-lock and robotic wafer handler. A central vacuum transfer robot moves a substrate sequentially from the first deposition chamber, through the second treatment chamber, and into the third resist-coating chamber before staging it at the scanner interface port. The interface port maintains a nitrogen-purged microenvironment with moisture levels below 1 part per million to limit acid-quencher contamination of the coated photoresist prior to exposure. After exposure in the scanner, the same transfer robot retrieves the wafer for post-exposure baking in an auxiliary thermal module.

Cluster tool integrated with cryogenic aerosol precleaning station

The cluster tool integrates an upstream cryogenic aerosol cleaning module ahead of the first underlayer chamber via a sealed transfer tunnel. Before entering the first chamber, the substrate passes under a supersonic nozzle that directs frozen argon-nitrogen particles at the wafer surface to remove sub-50-nanometer organic and particulate residues without liquid chemicals. A load-lock isolation gate separates the cleaning module from the first chamber to prevent outgassing contaminants from reaching the underlayer deposition zone. The cleaned substrate then proceeds directly into the first chamber for underlayer formation, followed by surface treatment in the second chamber and photoresist coating in the third chamber.

Automated or data-driven variant

Closed loop spectroscopic feedback for underlayer treatment

An inline spectroscopic ellipsometer mounted on the cluster tool transfer robot measures the thickness and optical constants of the underlayer before and after processing in the second chamber. A supervisory process controller compares the measured refractive index and film thickness against target reference curves using a multivariable regression model. When drift exceeds a preset threshold, the controller automatically adjusts the gas flow rate, treatment duration, or chamber pressure in the second chamber for the next substrate in the queue. The controller also updates the spin speed or dispense volume in the third chamber to compensate for minor surface-energy variations on the treated underlayer.

Specific version of a part

Atomic layer deposition of tin-oxo underlayer

A heated shower-head reactor chamber pulses tetrakis(dimethylamino)tin vapor and water vapor alternately onto a substrate held at 100 to 180 degrees Celsius. Nitrogen purge cycles between precursor pulses remove excess reactants so each cycle adds roughly 0.1 nanometers of amorphous tin-oxo film. Pressure is regulated between 0.5 and 2 torr by a throttle valve to achieve a target thickness of 3 to 10 nanometers.

Low-pressure oxygen and argon plasma treatment

A capacitively coupled radio-frequency plasma chamber energizes a gas mixture of oxygen and argon at 13.56 megahertz and 50 to 200 watts. Operating at a chamber pressure of 20 to 100 millitorr, the plasma oxidizes residual organic ligands and increases hydroxyl group density on the underlayer surface. A grounded lower electrode with embedded resistive heaters maintains the substrate at 100 to 150 degrees Celsius during a 10-to-30-second exposure.

Chemically amplified resist spin-coating cup

A temperature-controlled dispense arm deposits a propylene glycol monomethyl ether acetate solution containing a poly(hydroxystyrene) resin and a photoacid generator onto the treated underlayer. A servo-driven spindle accelerates the substrate to 2,000 revolutions per minute to spread a uniform 20 to 40 nanometer chemically amplified photoresist film. An integrated chill plate and proximity bake stage at 90 to 110 degrees Celsius evaporate residual casting solvent.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 6,841,006 B2
Published
Jan 11, 2005
Filed
Aug 23, 2001
Document BUS 9,892,946 B1
Published
Feb 13, 2018
Filed
Jul 27, 2016
Class
H01L 21/6719
Claim 1
Document A
Document B
1.1a first chamber configured to form an underlayer over a substrate;
(d) a curing station coupled to the atmospheric chemical vapor deposition chamber; and (e) a substrate handling system adapted to transfer substrates between the atmospheric chemical vapor deposition chamber, the spin coating chamber, and the curing station, wherein the spin coating chamber comprises a first material comprising a sol-gel solution used to form the first porous dielectric layer and wherein the atmospheric chemical vapor deposition chamber comprises a second mat
A · US 6,841,006 B2 · claim 1
For example, in an exemplary low-k dielectric layer formation process, a solution containing a low-k dielectric material can be formed on the substrate W using the spin coating process that is performed in the spin coating chamber 150.
B · US 9,892,946 B1 · ¶ 11
1.2a second chamber configured to treat the underlayer to form a treated underlayer; and
After curing, the substrates can be transferred to a substrate stripping/annealing chamber 118. Annealing can be performed in the chamber 118 to remove surfactant from the cured sol-gel layer and to form a mesoporous oxide layer.
A · US 6,841,006 B2 · ¶ 64
1.3a third chamber configured to form a photoresist over the treated underlayer.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.2. Both have a passage for 1.1.

Additional background

Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.

It would be desirable to reduce the time associated with one or more of these steps to reduce the amount of time needed to process the substrate.
A · US 6,841,006 B2 · ¶ 7
Doing so would increase processing efficiency and would reduce the cycle time associated with manufacturing, for example, semiconductor chips.
A · US 6,841,006 B2 · ¶ 7
Microchip manufacturers deposit various material layers on a wafer during microchip processing.
C · US 2005/0079438 A1 · ¶ 1

Related claim parts: 1.1

Document C: US 2005/0079438 A1, published Apr 14, 2005. Cited for this statement only.

Cite aspatent.fyi, US 2026/0367519 A1, claim 1, first published 2026-11-23T19:27:50-05:00, https://patent.fyi/US20260367519/, SHA-256 105cbd0bf154fd1dbebb8cc3a686da0746b604e7c2c602010774d361cc97d761
First published
Permanent addresshttps://patent.fyi/US20260367519/
Content fingerprint (SHA-256)105cbd0bf154fd1dbebb8cc3a686da0746b604e7c2c602010774d361cc97d761
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi